CS270786B1 - Slag pan - Google Patents

Slag pan Download PDF

Info

Publication number
CS270786B1
CS270786B1 CS891201A CS120189A CS270786B1 CS 270786 B1 CS270786 B1 CS 270786B1 CS 891201 A CS891201 A CS 891201A CS 120189 A CS120189 A CS 120189A CS 270786 B1 CS270786 B1 CS 270786B1
Authority
CS
Czechoslovakia
Prior art keywords
slag
ladle
wall
ring
welded
Prior art date
Application number
CS891201A
Other languages
Czech (cs)
Other versions
CS120189A1 (en
Inventor
Ladislav Doc Ing Csc Strakos
Vlastimil Ing Tomis
Karel Ing Csc Jasiok
Frantisek Doc Ing Csc Havlicek
Milan Ing Harok
Miloslav Ing Slovak
Original Assignee
Strakos Ladislav
Tomis Vlastimil
Jasiok Karel
Havlicek Frantisek
Harok Milan
Slovak Miloslav
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Strakos Ladislav, Tomis Vlastimil, Jasiok Karel, Havlicek Frantisek, Harok Milan, Slovak Miloslav filed Critical Strakos Ladislav
Priority to CS891201A priority Critical patent/CS270786B1/en
Publication of CS120189A1 publication Critical patent/CS120189A1/en
Publication of CS270786B1 publication Critical patent/CS270786B1/en

Abstract

Řešení spočívá v konstrukční^úpravě horní části struskové pánve, umožňující uložení a upevnění tepelně izolační bandáže. Za tímto účelem je přlvařen ke zkrácené stěně (2) struskové pánve (1) kuželový prstenec (4) s tlouštkou menší než stěna (2) pánve (1) a k hornímu okraji kuželového prstence (4) je přivařeno límcové okruží (5).The solution consists in the structural modification of the upper part of the slag pan, enabling the placement and fixing of the thermal insulation bandage. For this purpose, a conical ring (4) with a thickness smaller than the wall (2) of the pan (1) is welded to the shortened wall (2) of the slag pan (1) and a collar ring (5) is welded to the upper edge of the conical ring (4).

Description

Vynález se týká konstrukční úpravy horní části struskové pánve sloužící k uložení tepelné izolace, zabraňující tepelnému pnutí a trvalým deformacím této části struskové pánve.The invention relates to a structural modification of the upper part of a slag ladle serving to store thermal insulation, preventing thermal stress and permanent deformations of this part of the slag ladle.

Struskové pánve jsou odlévané nádoby kuželového tvaru s oblým dnem, u horního okraje vyztužené zesilujícím prstencem, a používají se pro jímání a přepravu tekuté strusky od vysokých pecí na odval nebo k místu jejího dalšího zpracování. Struskové pánev je zavěšena ve své spodní třetině na čtyřech táhlech, upevněných v závěsných okách na sténé pánve, v horní třetině jsou na stěnách pánve vytvořeny dvě vidlice, vyztužené do stran horizontálními žebry, do nichž zapadají palcovité výstupky na nosném prstenci, který je sklopně uložen okolo osy procházející jeho průměrem. Na nosném prstenci jsou také upevněny konce táhel, na nichž je struskové pánev zavěšena. Při vylévání strusky se pánev otáčí okolo osy proložené průměrem nosného prstence spolu s ním o 120° a tíha pánve a strusky je držena v rovnováze silami v zavěšovacích táhlech a silami mezi vidlicemi pánve a palcovitými výstupky na nosném prstenci. Nosný prstenec umístěný po obvodu pánve zabraňuje jejímu volnému ochlazování prouděním okolního vzduchu kolem jejího povrchu v uvedené části pánve. Tento jev se dále zvyšuje při zmenšování mezery mezi povrchem pánve a nosným prstencem. Tyto okolnosti vedou k enormnímu nárůstu teploty ve stěně struskové pánve v oblasti jejího uložení v nosném prstenci. Horní část pánve, která se nachází nad hladinou strusky a není s ní v přímém styku, se ochlazuje na teplotu podstatně nižší než stěna v oblasti nosného prstence. Tento gradient poklesu teploty ve stěně pánve vyvolává v této tepelně exponované oblasti stěny tlaková napětí, která překračují mez kluzu materiálu pánve. Následkem toho dochází v oblasti nosného věnce v místě výztužných žeber vidlic pánve k trvalým plastickým deformacím, které způsobují, že se stěny pánve v místě pod vyztuženými vidlicemi postupně deformují dovnitř pánve, což po určité době ztěžuje odstraňování strusky z pánve, která musí být po asi tisícinásobném použití vyřazena z provozu. 3e nutno podotkout, že nejen samotné tepelné rozhraní ve stěně pánve, ale i lokální odvod tepla dvěma vidlicemi se čtyřmi výztužnými žebry na pánvi přispívají nepříznivě k růstu deformačních napětí ve stěně pánve, požadavku na snížení teplotního gradientu vyhovuje struskové pánev, která je v horní části opatřena tepelně izolující bandáží nebo v jejíž stěně je slévárenskou technologií vytvořeno prstencové zahloubení, do něhož se vkládá a připevňuje tepelná izolace. Nevýhodou je potřeba změny modelového zařízení, jímž se zajistí při odlévání potřebné zeslabení horních částí stěny struskové pánve.Slag ladles are cast cones of conical shape with a round bottom, reinforced at the upper edge with a reinforcing ring, and are used for collecting and transporting liquid slag from blast furnaces to the dump or to the place of its further processing. The slag ladle is suspended in its lower third on four rods fixed in hanging eyes on the walls of the ladle, in the upper third two forks are formed on the walls of the ladle, reinforced to the sides by horizontal ribs into which the thumb protrusions fit on a support ring around an axis passing through its diameter. The ends of the rods, on which the slag ladle is suspended, are also fastened to the support ring. When pouring the slag, the ladle rotates about an axis interspersed with the diameter of the support ring together with it by 120 ° and the weight of the ladle and slag is kept in balance by the forces in the suspension rods and the forces between the ladle forks and inch protrusions on the support ring. A support ring located around the circumference of the pelvis prevents its free cooling by the flow of ambient air around its surface in said part of the pelvis. This phenomenon is further increased as the gap between the surface of the pelvis and the support ring is reduced. These circumstances lead to an enormous increase in the temperature in the wall of the slag ladle in the area of its bearing in the support ring. The upper part of the ladle, which is located above the surface of the slag and is not in direct contact with it, is cooled to a temperature substantially lower than the wall in the area of the support ring. This temperature drop gradient in the ladle wall induces compressive stresses in this thermally exposed area of the wall which exceed the yield strength of the ladle material. As a result, permanent plastic deformations occur in the area of the support ring in the place of the reinforcing ribs of the pelvis forks, which cause the pelvic walls to gradually deform inside the pelvis under the reinforced forks, making it difficult to remove slag from the pelvis after some time. decommissioned for thousands of times. 3e it should be noted that not only the thermal interface in the basin wall, but also local heat dissipation by two forks with four reinforcing ribs on the basin contribute unfavorably to the growth of deformation stresses in the basin wall, the requirement to reduce the temperature gradient meets provided with a thermally insulating bandage or in the wall of which an annular recess is formed by foundry technology, into which thermal insulation is inserted and fixed. The disadvantage is the need to change the model equipment, which ensures the necessary weakening of the upper parts of the slag ladle wall during casting.

Popsaná nevýhoda se odstraní u struskové pénve podle vynálezu, jehož podstata spočívá v tom, že ke zkrácené stěně pánve je přivařen kuželový prstenec s tloušťkou menší než stěna struskové pánve a k hornímu okraji kuželového prstence je přivařeno límcové okruží.The described disadvantage is eliminated in the slag ladle according to the invention, the essence of which consists in that a conical ring with a thickness smaller than the wall of the slag ladle is welded to the shortened ladle wall and a collar ring is welded to the upper edge of the conical ring.

Konstrukční úpravou horní části struskové pánve podle vynálezu se v této tepelně namáhané oblasti vytvoří nová, zeslabená část stěny, která se vlivem ji obklopující tepelné izolace snadněji ohřívá ze spodní, relativně teplejší oblasti, a proto se u ní využívá všech výhod tepelně izolovaných struskových pánví, nehledě k tomu, že takto konstrukčně upravená a renovovaná struskové pánev má vlastnosti lepší než pánev nová s neproměnnou tloušťkou stěny.The design of the upper part of the slag ladle according to the invention creates a new, weakened part of the wall in this thermally stressed area, which is more easily heated from the lower, relatively warmer area due to the surrounding thermal insulation and therefore takes full advantage of thermally insulated slag ladles. notwithstanding the fact that such a structurally modified and renovated slag ladle has better properties than a new ladle with a constant wall thickness.

Vynález je objasněn na příkladu praktického provedení, patrného z výkresu, znázorňujícího svislý řez horní částí struskové pánve.The invention is elucidated on the example of a practical embodiment, seen from the drawing, showing a vertical section of the upper part of the slag ladle.

Struskové pánev £ s původně neproměnnou tloušťkou stěny 2 je řezy 3 zkrácena. V místě řezů 3 je ke stěně 2 pánve £ přivařen kuželový prstenec 4 s límcovým okružím 5. Tloušťka kuželového prstence 4 je přitom menší než tloušťka zbývající stěny 2 pánve, a tak na vnější ploše kuželového prstence 4 a límcového okruží 5 vzniká prostor pro uložení tepelně izolační bandáže 6, tvořené například rohožemi nebo deskami z minerálních vláken, ukotvených k této ploše nestřelenými kotevními trny. Tepelně izolační bandáž 6 přitom zasahuje celou horní částí pánve £ až k jejímu uložení na nosném prstenci 7 nástavby struskového vozu.The slag ladle £ with the initially constant wall thickness 2 is shortened by the cuts 3. At the cuts 3, a conical ring 4 with a collar ring 5 is welded to the wall 2 of the pelvis 6. insulating bandages 6, formed for example by mats or boards of mineral fibers, anchored to this surface by unburned anchoring pins. The thermal insulation bandage 6 extends over the entire upper part of the ladle 6 up to its bearing on the support ring 7 of the slag car body.

Claims (1)

PŘEDMĚT VYNÁLEZUOBJECT OF THE INVENTION Strusková pánev pro jímání a přepravu tekuté vysokopecní etrusky, na jejíž stěně nebo v zahloubení stěhy je od okrajového zpěvňujícího lemu až k místu uložení struskové pánve na nosném prstenci připevněna tepelně izolační bandáž, vyznačující se tím, že ke zkrácené stěně (2) struskové pánve (1) je přivařen kuželový prstenec (4) s tloušťkou menší než tloušťka stěny (2) struskové pánve (1) a k jeho hornímu okraji je přivařeno límcové okruží (5).Slag ladle for collecting and transporting liquid blast furnace slag, on the wall or in the recess of the sieve a thermally insulating bandage is attached from the edge reinforcing rim to the place of placement of the slag ladle on the support ring, characterized in that a slag ladle (2) 1) a conical ring (4) with a thickness less than the wall thickness (2) of the slag ladle (1) is welded and a collar ring (5) is welded to its upper edge.
CS891201A 1989-02-24 1989-02-24 Slag pan CS270786B1 (en)