CS241449B1 - The method of strengthening the granules of the preparation for poisoning and other children - Google Patents

The method of strengthening the granules of the preparation for poisoning and other children Download PDF

Info

Publication number
CS241449B1
CS241449B1 CS837516A CS751683A CS241449B1 CS 241449 B1 CS241449 B1 CS 241449B1 CS 837516 A CS837516 A CS 837516A CS 751683 A CS751683 A CS 751683A CS 241449 B1 CS241449 B1 CS 241449B1
Authority
CS
Czechoslovakia
Prior art keywords
granules
preparation
strengthening
urea
poisoning
Prior art date
Application number
CS837516A
Other languages
Czech (cs)
Other versions
CS751683A1 (en
Inventor
Frantisek Markalous
Pavel Letko
Josef Dittrich
Original Assignee
Frantisek Markalous
Pavel Letko
Josef Dittrich
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Frantisek Markalous, Pavel Letko, Josef Dittrich filed Critical Frantisek Markalous
Priority to CS837516A priority Critical patent/CS241449B1/en
Publication of CS751683A1 publication Critical patent/CS751683A1/en
Publication of CS241449B1 publication Critical patent/CS241449B1/en

Abstract

Účelem vynálezu bylo prodloužit životnost granulí přípravku ve vlhkém prostředí. Tohoto cíle se dosáhne tak, že směs složek přípravku se granuluje v přítomnosti 0,5 ež 20 % hmot. kondenzátu močoviny a formaldehydu nebo se kondenzát močoviny a formaldehydu nanáší na povrch granulí přípravku.The purpose of the invention was to extend the shelf life of the granules of the preparation in a humid environment. This objective is achieved by granulating the mixture of the components of the preparation in the presence of 0.5 to 20% by weight of urea-formaldehyde condensate or by applying the urea-formaldehyde condensate to the surface of the granules of the preparation.

Description

Vynález se týká způsobu zpevnem granulí přípravku pro hubení hrabošů a dalších škůdců.BACKGROUND OF THE INVENTION The present invention relates to a method for solidifying granules of a composition for controlling voles and other pests.

Požerový přípravek pro hubení hrabošů a dalších škůdců se vyrábí míšením jednotlivých komponent a granulaci. Granulovaný přípravek již se při krátké expozici ve vlhkém prostředí rozpadá, což má za následek ztrátu funkčních vlastností přípravku. Aby se těmto potížím zabránilo, byly prováděny pokusy s hydrofobizací povrchu granulí různými látkami, jako jsou alifatické aminy, mastné kyseliny, jejich soli atd. nebo pokusy se zpevněním granulí, například sádrou. Zkoušená opatření se nejeví optimálními.The food preparation for the control of voles and other pests is produced by mixing individual components and granulating. The granular preparation already disintegrates upon brief exposure in a humid environment, resulting in a loss of functional properties of the preparation. To avoid these problems, attempts have been made to hydrophobize the surface of the granules with various substances, such as aliphatic amines, fatty acids, salts thereof, etc., or attempts to solidify the granules, such as gypsum. The measures tested are not optimal.

Podstatně výhodnějším se jeví způsob zpevnění granulí přípravku pro hubení hrabošů a dalších škůdců podle předkládaného vynálezu, jehož podstata spočívá v tom, že směsThe method of strengthening the granules of the composition for controlling pests and other pests according to the invention seems to be substantially more advantageous in that the mixture consists of:

241 449 složek přípravku se granuluje v přítomnosti 0,5 až 20 % hmot. kondenzátu močoviny a formaldehydu nebo se kondenzát močoviny a formaldehydu nanáší na povrch granulí přípravku.241 449 of the formulation ingredients are granulated in the presence of 0.5 to 20 wt. urea-formaldehyde condensate or urea-formaldehyde condensate is applied to the granule surface of the formulation.

Způsobem podle vynálezu se podstatně sníží podíl prachových a zlomkových částic při míchání, granulaci a dalších manipulací, což má za následek pronikavé zlepšení pracovního prostředí. Zvýšení pevnosti granulí má za následek i snížení recyklu při granulaci.The process according to the invention significantly reduces the proportion of dust and particulate matter during mixing, granulation and other handling, resulting in a sharp improvement in the working environment. Increasing the granule strength also results in a reduction of the granulation recycling.

Způsob podle vynálezu se realizuje tak, že do směsi komponent přípravku se vmísí určité množství kondenzátu močoviny a formaldehydu, například 8,7 % hmot. Po protlačení granulátorem směs zgranuluje a přítomný kondenzát vlivem teploty granulaoe ještě dále zkondenzuje a vytvoří tak pevnou kostru, která umožňuje požadované prodloužení rozpadu granulí vlivem prostředí z původních 7 minut na 5 a více hodin, což závisí na množství kondenzátu. Zpěvně ní granulí lze rovněž provést nástřikem kondenzátu na povrch hotových granulí přípravku.The process according to the invention is carried out by mixing a certain amount of urea-formaldehyde condensate, for example 8.7 wt. Upon passing through the granulator, the mixture granulated and the condensate present further condensed under the granular temperature to form a solid skeleton which allows the desired prolongation of the granule disintegration under environmental conditions from the original 7 minutes to 5 hours or more, depending on the amount of condensate. The granulation of the granules can also be effected by spraying condensate onto the surface of the finished granules of the formulation.

Příklad provedeníExemplary embodiment

Do směsi 108 kg vitaminozních úsušků, 52 kg ovesného šrotu, 8,6 kg sušeného mléka, 12 kg fosfidu zinku bylo vmíšeno 17,4 kg dimetylolmočoviny (diakol M) a směs byla granulována.17.4 kg of dimethylurea (diacol M) was added to a mixture of 108 kg of vitamin driers, 52 kg of oat meal, 8.6 kg of milk powder, 12 kg of zinc phosphide and the mixture was granulated.

Claims (1)

PŘEDMĚTSUBJECT VYNÁLEZUOF THE INVENTION 241 449241 449 Způsob zpevnění granulí přípravků pro hubení hrabošů a dalších škůdců, vyznačený tím, že směs složek přípravku se granuluje v přítomnosti 0,5 až 20 % hmot. kondenzátu močoviny a formaldehydu a/naloo kondenzát močoviny a formaldehyduVhanáší na povrch granulí přípravku..A method of strengthening granules of a composition for killing voles and other pests, characterized in that the mixture of the ingredients of the composition is granulated in the presence of 0.5 to 20% by weight. urea and formaldehyde condensate and / naloo urea and formaldehyde condensateBlown onto the granules of the preparation.
CS837516A 1983-10-13 1983-10-13 The method of strengthening the granules of the preparation for poisoning and other children CS241449B1 (en)