CN2933776Y - Ultraviolet light-cure resin lacquer veneer surface-decoration fiberboard composite laminated wood board - Google Patents
Ultraviolet light-cure resin lacquer veneer surface-decoration fiberboard composite laminated wood board Download PDFInfo
- Publication number
- CN2933776Y CN2933776Y CN 200620021152 CN200620021152U CN2933776Y CN 2933776 Y CN2933776 Y CN 2933776Y CN 200620021152 CN200620021152 CN 200620021152 CN 200620021152 U CN200620021152 U CN 200620021152U CN 2933776 Y CN2933776 Y CN 2933776Y
- Authority
- CN
- China
- Prior art keywords
- board
- lacquer
- thickness
- coating
- ultraviolet
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model relates to an ultraviolet light-cure resin lacquer wood veneer surface-decoration density composite block board. The existing civil decorative board uses benzene, formaldehyde or other aromatic hydrocarbon solvent paint to prevent surface corrosion, damp and to decorate buildings. Countless children are infected with leukemia because of the curing and volatilization of those harmful organic substances, which brings heavy burden and undue disaster to the state and nation. The utility model comprises a block board (1), the side of which has a composite wood veneer surface-decoration board (6). The wood veneer surface-decoration board (6) is painted with the ultraviolet light-cure resin coat. The product can be used as the high quality boards for modern office, cabinets, furniture, sanitary and decorating, satisfy the requirements of pollution-free occasion.
Description
Technical field:
The invention relates to a kind of dalle that adopts the photocuring lacquer painting.
Background technology:
Existing civilian decorative panel employing contains benzene, formaldehyde or other aromatic hydrocarbon solvent paint and carries out surface anticorrosion and damp proof insulation and decoration as nitrate paint, polyester lacquer.Volatilization by solvent is solidified.Produce pernicious gas in the volatilization process, drying time is long, brings huge pollution for producer and user's environment.These harmful organic substances can be encroached on health, have caused countless leukaemia children, have brought heavy burden and unnecessary disaster for our country and nationality.
Summary of the invention:
The purpose of the invention provides the solid lacquer type organic coating veneer decorative density board composite joiner's board of a kind of ultraviolet that does not contain these harmful and noxious substances, reduces or avoids fitting up the bad infringement that human body is caused, and has firm beautiful structure.
The purpose of the invention is achieved in that
The solid lacquer type organic coating veneer decorative density board composite joiner's board of ultraviolet, its composition comprises: core-board, the side of described core-board is compounded with medium-density plate, and the opposite side of described medium-density plate is compounded with the veneer facing, scribbles the solid resin enamelled coating of ultraviolet on the described veneer facing.
The solid lacquer type organic coating veneer decorative density board composite joiner's board of above-mentioned ultraviolet, described resin enamelled coating is three layers, the ground floor and the second layer are the priming paint with two positive one contrary coating roller brushings, wherein ground floor thickness is the thickness of every square metre of 15-20 gram lacquer brushing, the thickness of the second layer is the thickness of every square metre of 10-30 gram lacquer brushing, described lacquer type organic coating is brushed the back at every turn and is solidify to form enamelled coating by ultraviolet lamp illumination, the 3rd layer of finish paint that uses flow coating machine to drench, thickness is the thickness of every square metre 120 gram lacquer brushing, solidify to form enamelled coating by the smooth back of thermal advection machine by ultraviolet lamp illumination after the leaching paint.
This technical scheme has following beneficial effect:
1. changed traditional brushing paint, the sheet material fine finishining pattern that is cured by solvent flashing in the air dry lacquer painting dry run is by adopting light-cured resin enamelled coating, the harmful effect of having avoided solvent evaporates that human body is caused.Use does not particularly have harmful substances such as benzene, methyl alcohol in the manufacture process, has protected consumer and direct labor's health, and photocuring resinoid lacquer is not poisoned, and is used to medical-therapeutic treatment of human body fields such as dental prosthetic for a long time.
2. after traditional lacquer painting brushing.Solidified 90% in 24 hours, solidified fully at 3 months to 1 year, occupied ground is big, the requirement condition harshness, and the worker laboring environment is poor, by natural volatilization.Adopt the product of new paint film only just can finish curing in a few minutes, solidify at once the back, packing can to check paint film to meet the requirements, and occupied ground is little.In addition, owing to adopt light-cured resin, do not shine and just not solidify, avoided continuous work, day shift production fully, no pernicious gas improves work situation and environment for use, having improved efficiency and production safety degree, is nontoxic environmental protection dalle.
3. have three layers of lacquer painting, lacquer painting is full, and outward appearance is tough and tensile beautiful, and the hardness high-wear resistance is good, and can show luxurious.By two positive one contrary coating rollers japannings, make the lacquer painting layer smooth full evenly, enter wooden in, strengthened the adhesive force of priming paint and veneer facing, guarantee that lacquer painting connects and stablize not delamination.The second layer of japanning decorations combines stable with priming paint for the second time, formation has the enamelled coating of good adhesion, guarantee the brushing quality flatness and the basic thickness of finish paint, make priming paint and finish paint effectively in conjunction with transition, can avoid the flake-off lacquer effectively, the 3rd layer of formation be last lacquer painting layer, combine with the firm of veneer by preceding finishing coat, make the 3rd layer of lacquer can have firm adhesive force, thermal advection machine by 80 ℃ after the leaching paint makes lacquer painting more level and smooth, and is glittering and translucent, discharges the micro-bubble that wherein may exist, improve its light sensation and intensity, behind the check composite demand, use ultraviolet photo-curing.Stable strong and beautiful lacquer painting have been guaranteed on wooden substrate, to form thus.
4. the veneer facing has not only embodied wooden essence, and is more exquisite by meticulous enamelling process, can avoid wooden natural shortcoming by rejecting, and improves the utilization rate of the timber of knowing clearly.This product of compound back significantly improves than traditional core-board intensity, can exempt the facing finishing and directly use.
4. the curing rate of this product is fast, and is with short production cycle, and corrosion resistance and good can be acidproof, alkaline-resisting, the setting by three layers of lacquer painting makes its intensity height, paint film is full, exquisiteness is elegant, and is firm and luxurious.
Description of drawings:
Accompanying drawing 1 is the structural representation of this product.
The specific embodiment:
Embodiment 1:
The solid lacquer type organic coating veneer decorative density board composite joiner's board of ultraviolet, core-board 1, the side of described core-board 1 is compounded with medium-density plate 2, the opposite side of described medium-density plate 2 is compounded with veneer facing 6, the veneer facing is preferably through polishing cleaning surface, prime with two positive one contrary coating rollers in the cleaning back, ground floor priming paint is every square metre of 15-20 gram with the lacquer amount, the thickness of Xing Chenging is ground floor 3 thus, be coated with lacquer through the speed process ultraviolet lamp box of conveyer belt with 10 meters of per minutes, the intensity of illumination of uviol lamp can be 9.7 kilowatts on 2 lamps.After prime paint solidifies, enter into two road coating machines of japanning station with conveyer belt, it also is the coating machine of two reverse rollers of a forward roller, the thickness of the second layer is the film thickness that forms with every square metre of 10-30 gram of lacquer amount, the composition of lacquer is between priming paint and finish paint for the second time, be coated with the back and form the obvious transparent layer at substrate surface, on substrate, form relatively thin enamelled coating but connect by second painting and further strengthened and firm, after japanning is finished for the second time, enter into the ultraviolet photo-curing machine of second layer lacquer with conveyer belt, irradiation by ultraviolet light is solidified, and forms second layer lacquer painting 4.Be only then and formally be coated with i.e. the 3rd layer of lacquer of finish paint, the 3rd layer is used flow coating machine, what drench is last high-grade finish paint, with every square metre of 100-150 gram, the stable film thickness that forms of the lacquer amounts of 120 grams preferably, thermal advection machine by 80 ℃ after the leaching paint is smooth, make lacquer painting more level and smooth, glittering and translucent, discharge the micro-bubble that wherein may exist, improve its light sensation and intensity, after lacquer painting experience part is qualified, through the speed process ultraviolet lamp box of conveyer belt, solidify to form the solid resin enamelled coating 5 of ultraviolet with 10 meters of per minutes.Check edging once more, be trimmed to the specification of regulation, attached diaphragm, packing.
Claims (2)
1. a ultraviolet is consolidated lacquer type organic coating veneer decorative density board composite joiner's board, its composition comprises: core-board, it is characterized in that: the side of described core-board is compounded with medium-density plate, the opposite side of described medium-density plate is compounded with the veneer facing, scribbles the solid resin enamelled coating of ultraviolet on the described veneer facing.
2. the solid lacquer type organic coating veneer decorative density board composite joiner's board of ultraviolet according to claim 1, it is characterized in that: described resin enamelled coating is three layers, the ground floor and the second layer are the priming paint that is coated with map brushing with two positive one contrary coating rollers, wherein ground floor thickness is the thickness of every square metre of 15-20 gram lacquer brushing, the thickness of the second layer is the thickness of every square metre of 10-30 gram lacquer brushing, described lacquer type organic coating is brushed the back at every turn and is solidify to form enamelled coating by ultraviolet lamp illumination, the 3rd layer of finish paint that uses flow coating machine to drench, thickness is the thickness of every square metre 120 gram lacquer brushing, solidify to form enamelled coating by the smooth back of thermal advection machine by ultraviolet lamp illumination after the leaching paint.