CN2813141Y - Beam cooling device for twisted steel - Google Patents
Beam cooling device for twisted steel Download PDFInfo
- Publication number
- CN2813141Y CN2813141Y CN 200520041984 CN200520041984U CN2813141Y CN 2813141 Y CN2813141 Y CN 2813141Y CN 200520041984 CN200520041984 CN 200520041984 CN 200520041984 U CN200520041984 U CN 200520041984U CN 2813141 Y CN2813141 Y CN 2813141Y
- Authority
- CN
- China
- Prior art keywords
- sleeve seat
- cavity
- outer sleeve
- outer casing
- cooling device
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model relates to a beam cooling device of twisted steel, which comprises an outer sleeve seat containing a cavity and an opening, an inner sleeve seat, an and a discharge guiding sleeve seat, wherein the outer sleeve seat is provided with an intake channel communicated with the cavity, the inner sleeve seat is inserted in the cavity of the outer sleeve seat, and the middle of the inner sleeve seat is provided with a channel corresponding with the opening of the outer sleeve seat. A gap, which is formed on top of a cavity assembled by the outer sleeve seat and the inner sleeve seat, forms a 360 DEG circular beam air spout. The two ends of the discharge guiding sleeve seat are matched with the outer sleeve seat and the channel corresponding to the opening of the outer sleeve seat is arranged in the middle. A plurality of beam cooling devices can be connected in series. After a billet is discharged at low temperature and is rolled, a steel bar passes through each group of on-line multichannel beam type water cooling devices and a beam type air drying device. Water and air are uniformly blown to the circumferential surface of the steel bar through a beam ring at high speed. The cold treatment of on-line surface of wire materials can be realized so as to enhance the strength and the surface quality of the product. The utility model solves the problems of low strength, poor surface quality, etc. of the wire materials which are caused by the slow air cooling.
Description
Technical field
The utility model relates to metal controlled rolling and controlled cooling field, relates generally to the rolling cooling of spiral.
Background technology
Spiral is widely used in cement prefab, cassette ceiling structural member, concrete duct of the bar-mat reinforcement in airport, highway, tunnel etc. and protection network and civil buildings etc.Under identical service condition, improve the yield strength of spiral, can reduce the diameter of reinforcing bar, save steel to reduce cost; Under identical mechanical property condition, can promote the selling price that product uses class and final raising product by improving the rebar surface quality.
For improving the intensity of building bar, the technical measures that adopt mainly are carbon content and employing alloying and the micro-alloying technologies by improving steel at present, and its essence is to reach the purpose that improves reinforced steel bar strength by means of solution strengthening, precipitation strength and structure refinement etc.But thereby this technology is because of having increased Si, Mn content and/or having added the cost that microalloy elements such as Nb, V, Ti have improved reinforcing bar.
China Patent No. 00109495.5 discloses " production method of low-carbon screw thread reinforcing bar ", and its technical characterictic is that steel is at Ae
3And Ar
3Temperature range surpasses the finally rolling of 50% deformation quantity, carries out the water cooling of wearing that cooling rate surpasses 20 ℃/S after rolling, and it is cold to be cooled to 300~600 ℃ of laggard line spaces.Adopt this technology can improve the yield strength of reinforcing bar.It is high that but this patent of invention requires equipment, and general producer equipment is difficult to satisfy its production requirement.
Summary of the invention
Usually adopt the online water cooling of wearing in view of existing spiral cooling, be i.e. directly pass the tank of filling water after the reinforcing bar finish to gauge and cool off, require cooling water inflow big, pairing circulation power increases, in addition, this kind technology cooling velocity is less, and cold rear surface residual water can't be removed.The utility model purpose is to provide a kind of line cooling device of spiral, and is with low cost, simple to operate, cooling capacity is big, can improve the line cooling device of rebar surface quality simultaneously.
For achieving the above object, the technical solution of the utility model is, the line cooling device of spiral comprises, outer casing seat, in a cavity and an opening are arranged, also be provided with the intake channel that is connected with cavity on it; Inner casing base is inserted in the outer casing seat cavity, is provided with passage in the middle of it, and is corresponding with the outer casing seat opening; Outer casing seat, inner casing base assembling form cavity, and a gap is formed on the top of cavity, and the gap forms 360 ° of hoop line nozzles thus; Lead and let out block set, its two ends cooperate with outer casing seat, are provided with passage in the middle of it, and are corresponding with the outer casing seat opening.
Further, described leading let out the block set outer face and matched with the outer casing seat end face and form one and lead and let out groove.
The utility model also is provided with a base plate, described outer casing seat, leads and lets out block set and be fixed on this base plate.
Described line cooling device can arranged in series many.
The utility model steel billet adopts low temperature to come out of the stove and after rolling, reinforcing bar is by online every group of multiple tracks beam current type water cooling plant and beam current type gas equipment for drying, the even reinforcing bar circumferential surface of jetting at a high speed of the gentle transmitted beam under high pressure of water head piece hoop, realize that thereby the online surperficial cold treatment of wire rod improves the intensity and the surface quality of product, solve the problem of the on the low side and surface quality difference of intensity level that wire rod slowly causes because of air cooling.
The beneficial effects of the utility model
The utility model device can fast, evenly cool off reinforcing bar whole circumference surface by gentle the doing of multiple tracks hoop beam current type water-cooled under Gao Shui (gas) pressure, gas equipment for drying subsequently can rebar surface is residual the water mark evenly dry up and the remained on surface iron scale blown off, thereby improve surface quality of products and improve its intensity.
Description of drawings
Fig. 1 is a structural representation of the present utility model;
Fig. 2 is the left view of Fig. 1;
Fig. 3 is the vertical view of Fig. 1;
Fig. 4 is the A portion enlarged drawing of Fig. 1.
The specific embodiment
Referring to Fig. 1~Fig. 4, spiral line cooling device of the present utility model comprises, outer casing seat 1, in a cavity 101 and an opening 102 are arranged, also be provided with the intake channel 103 that is connected with cavity 101 on it; Inner casing base 2 is inserted in the outer casing seat cavity 101, is provided with passage 201 in the middle of it, and is corresponding with outer casing seat 1 opening 102; Outer casing seat 1, inner casing base 2 assemblings form cavity 3, and a gap 4 is formed on the top of cavity 3, and the gap forms 360 ° of hoop line nozzles thus; Lead and let out block set 5, its two ends cooperate with outer casing seat 1, are provided with passage 501 in the middle of it, and are corresponding with outer casing seat 1 opening 102.
Referring to Fig. 1, described leading let out block set 5 outer faces and matched with outer casing seat 1 end face and form one and lead and let out groove 6, the effect of leading drain port is to discharge cooling medium fast, makes the screw-thread steel surface constantly expose new surface and cools off, and leads drain port simultaneously and also can in time discharge iron scale.。
See also Fig. 1 again, the utility model also is provided with a base plate 7, described outer casing seat 1, leads and lets out block set 5 and be fixed on this base plate 7 by bolt 8.Adjust the direction that screw-thread steel advances by regulating the base plate position subsequently.
According to on-the-spot milling train actual conditions is that different cooling requires to design a plurality of line cooling device arranged in series.
Design intake channel 103 water inlet or air inlets on outer casing seat 1, aqueous vapor is directly injected to the screw-thread steel surface by the gap 4-line nozzle at cavity 3 tops, reduce the temperature on screw-thread steel surface and the oxide skin of washing away the screw-thread steel surface rapidly, improve the intensity of screw-thread steel surface quality and raising screw-thread steel.
The screw thread steel billet after heating, by blooming mill rolling-screw-thread steel that the rolling back of middle mill milling-finishing mill forms directly fast transmitted beam flow cooling device targeting port, lead and let out cover and enter next covering device again; Also can be directly fast the transmitted beam flow cooling device, lead drain port and targeting port enters next covering device again.The effect of targeting port is used for fixing the direction of screw advancement.The effect of leading drain port is to discharge cooling medium fast, makes the screw-thread steel surface constantly expose new surface and cools off, and leads drain port simultaneously and also can in time discharge iron scale.
Along with the continuous development of the development of the national economy and the investment of national project construction increase year by year, to the demand of the essential main ferrous materials-screw-thread steel of concrete structure engineering also in continuous increase.Improved the intensity rank of reinforcing bar after patent of the present invention is cooled off by line, not only can save steel product cost, and obviously improve the surface quality of steel, similar at home and abroad producer has very big popularizing application prospect.
Claims (4)
1. the line cooling device of spiral is characterized in that, comprise,
Outer casing seat, in a cavity and an opening are arranged, also be provided with the intake channel that is connected with cavity on it;
Inner casing base is inserted in the outer casing seat cavity, is provided with passage in the middle of it, and is corresponding with the outer casing seat opening; Outer casing seat, inner casing base assembling form cavity, and a gap is formed on the top of cavity, and the gap forms 360 ° of hoop line nozzles thus;
Lead and let out block set, its two ends cooperate with outer casing seat, are provided with passage in the middle of it, and are corresponding with the outer casing seat opening.
2. the line cooling device of spiral as claimed in claim 1 is characterized in that, described leading let out the block set outer face and matched with the outer casing seat end face and form one and lead and let out groove.
3. the line cooling device of spiral as claimed in claim 1 is characterized in that, also is provided with a base plate, described outer casing seat, leads and lets out block set and fix on this base plate.
4. the line cooling device of spiral as claimed in claim 1 is characterized in that, described line cooling device can arranged in series many.