CN2678797Y - Water cooling mould for alloy cast - Google Patents

Water cooling mould for alloy cast Download PDF

Info

Publication number
CN2678797Y
CN2678797Y CN 200420032938 CN200420032938U CN2678797Y CN 2678797 Y CN2678797 Y CN 2678797Y CN 200420032938 CN200420032938 CN 200420032938 CN 200420032938 U CN200420032938 U CN 200420032938U CN 2678797 Y CN2678797 Y CN 2678797Y
Authority
CN
China
Prior art keywords
water
casting
moulds
pattern
water cooling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200420032938
Other languages
Chinese (zh)
Inventor
侯仁义
李克清
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sichuan Xin Ju Xinxing new Mstar Technology Ltd
Original Assignee
Sichuan Xinju Mineral Resource Development Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sichuan Xinju Mineral Resource Development Co ltd filed Critical Sichuan Xinju Mineral Resource Development Co ltd
Priority to CN 200420032938 priority Critical patent/CN2678797Y/en
Application granted granted Critical
Publication of CN2678797Y publication Critical patent/CN2678797Y/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model provides a water cooling mould for alloy cast, which is characterized in that water cooling moulds are formed into a plurality of sets of water cooling moulds by casting slots (1) and two split-ring moulds (2) in pairs, every pair of moulds is provided with casting ports (3), and the casting ports are conducted with the casting ports of the casting slots; waste channels (4) are arranged among the moulds, the waste channels at the lower ends of the moulds are provided with water inlets (5), the waste channels at the upper ends of the moulds are provided with water outlets (6), and the water inlets and the water outlets are respectively movably connected with a main waste channel via flexible pipes; sealing boards (7) are arranged out of the moulds and the waste channels, the sealing boards are provided with fixing clamps (8), and the fixing clamps are used for fixing or disassembling the moulds via bolts (9). The water cooling mould for alloy cast has reasonable design, uniform heat radiation and stable production quality; the disadvantage of deformation of the moulds due to heating and the segregation of alloy component is overcome, and production efficiency is effectively increased.

Description

Water-cooled pattern in the alloy casting
One, technical field
The utility model relates to the water-cooled pattern in a kind of alloy casting, belongs to alloy smelting and casting mold field.
Two, background technology
Chinese patent 96193274.0 discloses " continuous casting mould ", this pattern complex structure, and the pattern that can not do in the alloy founding uses.Alloy material is widely used in various fields, and the uniformity of alloy is to influence the physical property of material and the key of mechanical property.And this technical barrier fails to be well solved always.Existing pattern is divided into swage and water cooled mo(u)ld, and swage can only be applied to experimental stage or small-scale production because of its volume heaviness, production capacity are little; The water-cooled pattern causes component segregation and die deformation because of unreasonable structure, and utilization rate is low, and the scrappage height can not adapt to the needs of large-scale mass production far away, has greatly restricted the development of alloy casting.
Three, summary of the invention
The purpose of this utility model is to provide the pattern of the water-cooled in a kind of alloy casting at the deficiencies in the prior art, can solve the low defective of alloying component segregation, die deformation and production efficiency.
The purpose of this utility model is realized by following technical measures:
Water-cooled pattern in the alloy casting is formed many group patterns in pairs by casting groove and two split-ring molds, establish casting gate on every pair of mould, the tapping hole conducting of casting gate and casting groove, establish water channel between pattern, establish water inlet on the water channel of pattern lower end, set out water on the water channel of pattern upper end, water inlet and delivery port flexibly connect main channel with flexible pipe respectively, pattern and water channel peripheral hardware sealing plate are established geometrical clamp on the sealing plate, geometrical clamp is by bolting or dismounting pattern.
Have the tapping hole that the casting gate on some and the split-ring mold is complementary on the casting bottom land.
The utlity model has following advantage:
1, reasonable in design, dispel the heat even, constant product quality have overcome mould temperature distortion and alloying component segregation defective.
2, the pattern access times are many, and the life-span is long.
3, adopt and use water as cooling medium, can fully guarantee no eddy current and vaporization in the cooling procedure, water velocity is fast, the cooling effectiveness height.
4, simple to operate, easy to loading and unloading, scrappage is low, and production capacity is big, has improved production efficiency effectively.
Four, description of drawings
Fig. 1 is a water-cooling type mode structure schematic diagram.
Fig. 2 is a water-cooled pattern vertical view.
1 casting groove, 2 split-ring molds, 3 casting gates, 4 water channels, 5 water inlets, 6 water outs, 7 sealing plates, 8 geometrical clamps, 9 bolts.
Five, the specific embodiment
Below by embodiment the utility model is specifically described, but can not be interpreted as restriction the utility model protection domain.
Embodiment
The utlity model has simple in structure, easily manufactured, shown in Fig. 1~2.Water-cooled pattern in the alloy casting is formed many group water-cooled patterns in pairs by casting groove 1 and two split-ring molds 2, establish casting gate 3 above every pair of mould, the tapping hole conducting of casting gate and casting groove, establish water channel 4 between pattern, establish water inlet 5 on the water channel of pattern lower end, set out the mouth of a river 6 on the water channel of pattern upper end, water inlet and delivery port flexibly connect main channel with flexible pipe respectively, and the dismounting of being convenient to pattern like this is with mobile.Pattern and water channel peripheral hardware sealing plate 7 are established geometrical clamp 8 on the sealing plate, geometrical clamp is by bolt 9 fixing or dismounting patterns.
The casting groove has the tapping hole that the casting gate 3 on some and the split-ring mold 2 is complementary at 1 the end.
The utility model is achieved in that
Two split-ring molds 2 are formed many group patterns in pairs, load onto water channel 4 between pattern, pattern and water channel are adorned sealing plate 7 outward, geometrical clamp is by bolt 9 stationary moulds, the groove 1 of will casting at last is placed on the pattern, allows casting gate 3 aim at conducting with tapping hole, connects main channel with flexible pipe respectively.After the alloy molten material was put into casting groove watered full pattern, logical cold water cooling was treated to close cooling water after the alloy cast ingot cooling, withdraws from bolt, unclamps geometrical clamp, takes out alloy cast ingot, finishes an ingot casting moulding.

Claims (2)

1, the water-cooled pattern in the alloy casting, it is characterized in that this water-cooled pattern forms to organize the water-cooled patterns by casting groove (1) and two split-ring molds (2) in pairs, establish casting gate (3) above every pair of mould, the tapping hole conducting of casting gate and casting groove, establish water channel (4) between pattern, establish water inlet (5) on the water channel of pattern lower end, set out the mouth of a river (6) on the water channel of pattern upper end, water inlet and delivery port flexibly connect main channel with flexible pipe respectively, pattern and water channel peripheral hardware sealing plate (7), establish geometrical clamp (8) on the sealing plate, geometrical clamp is fixing or dismounting pattern by bolt (9).
2, the water-cooled pattern in the alloy casting according to claim 1, the groove (1) that it is characterized in that casting have the tapping hole that the casting gate (3) on some and the split-ring mold (2) is complementary at the end.
CN 200420032938 2004-02-23 2004-02-23 Water cooling mould for alloy cast Expired - Fee Related CN2678797Y (en)