CN2197369Y - Improved rotating plating cylinder - Google Patents
Improved rotating plating cylinder Download PDFInfo
- Publication number
- CN2197369Y CN2197369Y CN 94209108 CN94209108U CN2197369Y CN 2197369 Y CN2197369 Y CN 2197369Y CN 94209108 CN94209108 CN 94209108 CN 94209108 U CN94209108 U CN 94209108U CN 2197369 Y CN2197369 Y CN 2197369Y
- Authority
- CN
- China
- Prior art keywords
- cylinder
- utility
- plating cylinder
- vertical panel
- model
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model relates to an improved rotating plating cylinder. A rotating gear and a vertical panel are integrally formed and then are combined with the body of the cylinder in a heat melting way, and therefore, the improved rotating plating cylinder prevents the rotating gear from being loosened and dropped when the fixing bolt of the rotating gear is broken due to being repeatedly rubbed and grinded by an electroplating piece during the rotation of the cylinder and reduces the possibility that belt clamping drug liquid flows to next one groove. A depression on the outer surface of the rotating gear of the improved rotating plating cylinder and the outer end face of the gear form the arc-face transition, and therefore, the utility model is not easy to accumulate the drug liquid and is easy to be cleaned. Concentric-circle groove lines or spiral groove lines are formed on the inner side face of the vertical panel of the improved rotating plating cylinder, and therefore, the utility model reduces the possibility that the electroplating piece is attached on the inner side face and raises the coating uniformity of the electroplating piece.
Description
Produce or mass-produced requirement in response to more trending towards high-quality a small amount of variation Surface Treatment Engineering day in diversification epoch, electro-mech equipment tends to comprehensive automation gradually in recent years, the full-automatic crane type of the highly reliable computer program control mode design of employing, rotary type, upper rail type, following rail formula or the like electroplating device; Fig. 2 is the plating flow process in the fully automatic electric coating apparatus that generally adopts.About carry out the electro-mech of several work function in liquid bath, most convenient is operated in the most general being considered to of general use, the revolution of the plating crane type that uniformity coefficient is preferable, the current lead-through rate is higher connects dress cylinder (as shown in Figure 3) more.Adopt the portable automatic lifting revolving cylinder of crane of installing electric eye, comprising that material loading, blanking are mechanical operation need not the manpower transport, and the automatic controlled function that sets computer promotes the production efficiency of electroplating industry really greatly.
But, because the barrel plating cylinder of commonly using (as shown in Figure 4) is by bolt sealed up cylinder 2 to be combined with single-revolution gear 21, driving the cylinder that plated item is housed through driving gear 21 rotates to promote the plating uniformity coefficient, therefore when the cylinder that plated item is housed in it immerse turn round in the liquid bath deoil → wash → during pickling → washing → plating → washing → aftertreatment → washing complicated multiple handling procedure like this (consulting Fig. 3), will the following ill effect of generation:
Be described below in conjunction with Fig. 4,
(1), thereby must often shut down reparation and influence production schedule because the plated items in the barrel plating cylinder 2 concentrate on the below thereby its weight is born by the bolt 22 that is positioned at the below, and this will cause stress concentration and joint bolt 22 rupture easily.
(2) because galvanizing process usually is not only limited to single action, these revolution barrel plating cylinder 2 necessary repetitiousness liftings (shown in the flow arrow of Fig. 3) are through the washing of multiple tracks repetitiousness, neutralization even re-plating program; Because the swiveling gear 21 of barrel plating cylinder 2 both sides is to combine with vertical panel 23 by bolt 22; the plating soup is often accumulated in the gap that exists between the two; these soups that accumulate can't clean up really by water washing process; thereby when cylinder 2 enters next groove; these residual soups will influence the soup quality of next groove, thereby influence electroplating quality.
(3), thereby also can cause above-mentioned the 2nd described problem owing to also will accumulate soup at swiveling gear 21 outside surface concave edges 211 formed dead angles 212.
(4) because swiveling gear 21 is to combine with vertical panel 23 by bolt 22, therefore, an end that exposes to cylinder 2 inboards of bolt 22 will wearing and tearing occur because of with the plated item that rolls friction takes place in cylinder 2, thereby reduce the solid effect of spiral shell, the work-ing life of reducing cylinder 2.
(5), cause the plated item (as tool planar objects such as nuts) of dipping soup to be attached on the even surface, thereby influence electroplating effect because the inboard of the vertical surface 23 of cylinder 2 is an even surface.
(6) the barrel plating roller component is numerous and diverse owing to commonly using, assembling is difficult for, so bring inconvenience in using maintenance process.
Therefore, main purpose of the present utility model is to provide a kind of improvement barrel plating cylinder that can prevent that swiveling gear from may come off owing to its standing bolt fracture.
Secondary objective of the present utility model is to provide a kind of can reduce the improvement barrel plating cylinder of carrying residual liquor secretly.
Another purpose of the present utility model is to provide a kind of plated item that can reduce attached to the improvement barrel plating cylinder on the vertical surface medial surface of cylinder.
The technical solution that realizes the purpose of this utility model is the swiveling gear and the vertical panel of barrel plating cylinder both sides integrally formed, the concave edges of swiveling gear outside surface is designed to the cambered surface transition, the vertical panel inboard is designed to have concentric circles rill or spirrillum rill.
Now barrel plating cylinder of the present utility model is as follows with the relative merits contrast of commonly using the barrel plating cylinder.
1. swiveling gear of the present utility model directly connects by hot integration technology with cylinder system, in conjunction with closely, does not stay the gap; Commonly use the vertical panel bolt combination of swiveling gear, easily stay the gap, thereby be easy to carry secretly soup, influence electroplating quality to next groove with the cylinder both sides.
2. swiveling gear of the present utility model does not have combination member with cylinder, so there is not the anxiety that gets loose; The standing bolt of commonly using swiveling gear is easily rubbed by the plated item repetitiousness in the cylinder rotation and weares and teares, so that fracture is loosening easily, needing to cause shutdown maintenance, thereby influence is produced.
3. the concave edges of swiveling gear outside surface of the present utility model is designed to the cambered surface transition, is not easy to accumulate soup, can fully clean up during cleaning; Commonly use swiveling gear outside surface concave edges and form the dead angle, accumulate soup easily and be difficult to fully clean up, bring next groove into and influence electroplating quality.
4. the vertical panel inboard of swiveling gear of the present utility model is provided with concentric circles rill or spirrillum rill, and it is attached thereto that the plated item of being stained with liquid is not easy, thereby guarantees that plated item applies evenly; The inboard of commonly using the vertical panel of cylinder both sides is a smooth-flat-surface, and the plated item of being stained with liquid is easily attached on the wall, and it is inhomogeneous to cause plated item to apply.
5. the stress that weight constituted that accumulates in the plated item below the cylinder causes stress concentration and fracture easily owing to bearing when forwarding lower portion to commonly use the standing bolt of swiveling gear of barrel plating cylinder; The utility model does not have combination member, thereby does not have this shortcoming.
Technique means and the effect thereof setting forth the utility model in conjunction with the accompanying drawings below and adopted.In the accompanying drawings:
Figure 1A is a perspective exploded view of the present utility model, and part breaks so that the vertical panel inboard of swiveling gear to be shown;
Figure 1B is the sectional view of the swiveling gear that cuts of the A-A line along Figure 1A;
Fig. 2 is the block diagram of electroplating process;
Fig. 3 is the motion flow synoptic diagram of electro-mech;
Fig. 4 is a perspective exploded view of commonly using the barrel plating cylinder.
Consult Figure 1A and 1B, improvement barrel plating cylinder of the present utility model is shown, be formed by connecting by hot amalgamation mode by cylinder 1 and vertical panel 11 two portions members with swiveling gear 111, wherein:
Vertical panel 11 is formed with swiveling gear 111 in the outside, swiveling gear forms depression 112 on the outer surface, and this depression forms cambered surface transition 113 with the swiveling gear outer face, is formed with concentric(al) circles rill or spirrillum rill 114 on vertical panel 11 inboards;
The barrel plating cylinder that the vertical panel 11 that will have swiveling gear 111 during combination is combined into one with hot amalgamation mode with the two ends of cylinder 1.
In sum, the utility model can reach really eliminates the shortcoming of commonly using the barrel plating cylinder, the purpose of promoting the plating effect, can increase substantially the practical effect of barrel plating cylinder, improve the electroplating device of comprehensive automation efficient, reduce failure rate and improve electroplating quality.Its design that breaks through traditional structure never appears in the barrel plating cylinder of commonly using, thereby should be creative.
Claims (1)
1, a kind of barrel plating cylinder of improvement includes roller tube, vertical panel and swiveling gear, it is characterized in that,
The vertical panel of cylinder both sides combines with integrally formed the melting with roller tube heat then of swiveling gear;
The swiveling gear depression on the outer surface and the outer face formation cambered surface transition of swiveling gear;
Be formed with concentric(al) circles rill or spirrillum rill on the vertical panel inboard.