CN218593899U - Fingerprint-proof PCM panel - Google Patents

Fingerprint-proof PCM panel Download PDF

Info

Publication number
CN218593899U
CN218593899U CN202223096982.8U CN202223096982U CN218593899U CN 218593899 U CN218593899 U CN 218593899U CN 202223096982 U CN202223096982 U CN 202223096982U CN 218593899 U CN218593899 U CN 218593899U
Authority
CN
China
Prior art keywords
fingerprint
pcm panel
panel body
pcm
glued membrane
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202223096982.8U
Other languages
Chinese (zh)
Inventor
赵东明
许日民
汪兴坤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hefei Hesheng New Materials Co ltd
Original Assignee
Hefei Hesheng New Materials Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hefei Hesheng New Materials Co ltd filed Critical Hefei Hesheng New Materials Co ltd
Priority to CN202223096982.8U priority Critical patent/CN218593899U/en
Application granted granted Critical
Publication of CN218593899U publication Critical patent/CN218593899U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The application relates to the field of PCM panels and discloses a fingerprint-proof PCM panel. In this application, including PCM panel body and fingerprint glue membrane, the surface of PCM panel body bonds and has the fingerprint glue membrane, and the joint recess has been seted up to the long limit both sides edge of PCM panel body, and it is protruding to prevent that fingerprint glue membrane both sides limit is close to the fixed surface of PCM panel body to be connected with the installation, installs protruding joint in the inside of joint recess. The protruding joint of installation that will prevent fingerprint glued membrane both sides is in the inside of the joint recess that PCM panel body both sides were seted up, this moment the installation arch will the butt in the inside of joint recess, and with produce the friction between the inner wall of joint recess, make can not take place to drop easily between joint recess and the installation arch, make prevent that the fingerprint glued membrane is more firm when using, simultaneously, when the surface of preventing the fingerprint glued membrane has taken place the damage, also can in time change preventing the fingerprint glued membrane, thereby the convenience of PCM panel body in the use has been increased.

Description

Prevent fingerprint PCM panel
Technical Field
This application belongs to PCM panel technical field, specifically is a prevent fingerprint PCM panel.
Background
The pcm color coated plate belongs to a steel material, the main material of the pcm color coated plate is a cold-rolled steel plate and a galvanized steel plate, the surface of the pcm color coated plate is subjected to a series of treatment processes such as degreasing, cleaning, chemical conversion and the like, and the pcm color coated plate is a product which is formed by baking and cooling in a continuous roll coating mode and has good bending property and curing property. The pcm color-coated sheet is commonly used on the surfaces of household appliances such as door panels, side panels, microwave oven shells and the like of refrigerators. The pcm color-coated sheet has bright color, a paint film on the surface of the pcm color-coated sheet has corrosion resistance, and the pcm color-coated sheet is relatively flexible in material and has good processability. The PCM composite board is widely applied to the production of household appliance panels at present. In the using process, a layer of anti-fingerprint film is usually adhered on the surface of the panel to ensure that the surface of the panel can not generate fingerprints easily, thereby increasing the aesthetic property of the panel in the using process
However, in the use process of the pcm panel, the left side edge and the right side edge of the fingerprint-proof film are frequently contacted with a user, so that the edges are easily warped and cannot be replaced, and the use is inconvenient.
SUMMERY OF THE UTILITY MODEL
The purpose of this application lies in: in order to solve the above-mentioned proposed problems, a fingerprint-proof PCM panel is provided.
The technical scheme adopted by the application is as follows: the utility model provides a prevent fingerprint PCM panel, includes PCM panel body and prevents the fingerprint glued membrane, the surface of PCM panel body bonds and has prevented the fingerprint glued membrane, the joint recess has been seted up to the long limit both sides edge of PCM panel body, it is protruding to prevent that fingerprint glued membrane both sides limit is close to the fixed surface of PCM panel body and is connected with the installation, the protruding joint of installation is in the inside of joint recess.
Through adopting the above technical scheme, will prevent that fingerprint glued membrane pastes the outside surface at PCM panel body, later will prevent the inside of the protruding joint of installation of fingerprint glued membrane both sides at the joint recess that PCM panel body both sides were seted up again, the installation arch will the butt in the inside of joint recess this moment, and with produce the friction between the inner wall of joint recess, thereby increased the frictional force between joint recess and the installation arch, make can not take place to drop easily between joint recess and the installation arch, make it is more firm when using to prevent the fingerprint glued membrane, and simultaneously, when the surface of preventing the fingerprint glued membrane has taken place the damage, also can in time change preventing the fingerprint glued membrane, thereby the convenience of PCM panel body in the use has been increased.
In a preferred embodiment, the thickness of the anti-fingerprint adhesive film is 0.2-0.6 mm, and the anti-fingerprint adhesive film is a high-transmittance AF anti-fingerprint protective film.
By adopting the technical scheme, the PCM panel body is not easily stained with fingerprints in the using process, and the convenience in use is improved.
In a preferred embodiment, an adhesive layer is arranged on one side surface of the PCM panel body close to the fingerprint-proof adhesive film, a metal substrate is arranged on one side surface of the adhesive layer far away from the fingerprint-proof adhesive film, and an anti-corrosion layer is arranged on one side surface of the metal substrate opposite to the adhesive layer.
In a preferred embodiment, the thickness of the adhesive layer is 0.1 to 0.4mm, and the adhesive layer is a polyurethane adhesive layer.
Through adopting above-mentioned technical scheme, the fastness when the installation of PCM panel body has been increased.
In a preferred embodiment, the thickness of the metal substrate is 5 to 8mm, and the metal substrate is a stainless steel plate.
Through adopting above-mentioned technical scheme, increased metal substrate's mechanical strength, improved the durability of PCM panel body.
In a preferred embodiment, the thickness of the corrosion prevention layer is 0.3 to 0.8mm, and the corrosion prevention layer is an epoxy resin base layer.
By adopting the technical scheme, the bottom of the PCM panel body cannot be easily corroded, and the durability of the PCM panel body is improved.
In conclusion, due to the adoption of the technical scheme, the beneficial effects of the application are as follows:
in this application, will prevent that fingerprint glued membrane pastes the outside surface at PCM panel body, later will prevent the inside of the protruding joint of installation of fingerprint glued membrane both sides at the joint recess that PCM panel body both sides were seted up again, the installation arch will the butt in the inside of joint recess this moment, and with produce the friction between the inner wall of joint recess, thereby increased the frictional force between joint recess and the installation arch, make can not take place to drop easily between joint recess and the installation arch, make prevent that the fingerprint glued membrane is more firm when using, and simultaneously, when the surface of preventing the fingerprint glued membrane has taken place the damage, also can in time change preventing the fingerprint glued membrane, thereby the convenience of PCM panel body in the use has been increased.
Drawings
FIG. 1 is a schematic view of a PCM panel structure according to the present application;
FIG. 2 is a schematic diagram of a PCM panel body structure according to the present application;
FIG. 3 is a schematic view of the fingerprint-proof adhesive film structure in the present application;
FIG. 4 is an enlarged view taken at A in FIG. 3 of the present application;
fig. 5 is a schematic diagram of a layered structure of a PCM panel according to the present application.
The labels in the figure are: 1. a PCM panel body; 2. a fingerprint-proof adhesive film; 3. clamping the groove; 4. mounting a boss; 5. an adhesive layer; 6. a metal substrate; 7. and an anti-corrosion layer.
Detailed Description
In order to make the objects, technical solutions and advantages of the embodiments of the present application clearer, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the embodiments of the present application, and it is obvious that the described embodiments are some embodiments of the present application, but not all embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present application.
With reference to figures 1-5 of the drawings,
example (b):
the utility model provides a prevent fingerprint PCM panel, including PCM panel body 1 with prevent fingerprint glued membrane 2, PCM panel body 1's surface bonds and has prevents fingerprint glued membrane 2, the joint recess 3 has been seted up to PCM panel body 1's long limit both sides edge, prevent that fingerprint glued membrane 2 both sides limit is close to PCM panel body 1's fixed surface is connected with installation arch 4, installation arch 4 joint is in the inside of joint recess 3, will prevent fingerprint glued membrane 2 and paste the outside surface at PCM panel body 1, later will prevent the inside of the protruding 4 joints of installation of fingerprint glued membrane 2 both sides at the joint recess 3 that PCM panel body 1 both sides were seted up again, installation arch 4 will the butt in the inside of joint recess 3 this moment, and produce the friction with the inner wall of joint recess 3, thereby the frictional force between joint recess 3 and the installation arch 4 has been increased, make can not take place to drop easily between joint recess 3 and the installation arch 4, make fingerprint glued membrane 2 more firm when using, and simultaneously, when the surface of fingerprint glued membrane 2 has taken place the damage, also can be in time to prevent fingerprint glued membrane 2 changes, thereby the convenience of PCM panel body in the use has been increased.
The thickness of the anti-fingerprint adhesive film 2 is 0.2-0.6 mm, and the anti-fingerprint adhesive film 2 is a high-transmittance AF anti-fingerprint protective film, so that the PCM panel body 1 cannot be easily infected with fingerprints in the using process, and the convenience in use is improved.
A side that PCM panel body 1 is close to preventing fingerprint glued membrane 2 is provided with adhesive linkage 5, and adhesive linkage 5 keeps away from preventing that a side of fingerprint glued membrane 2 is provided with metal substrate 6, and a side that metal substrate 6 and adhesive linkage 5 are relative is provided with anti-corrosion coating 7, and adhesive linkage 5's thickness is 0.1 ~ 0.4mm, and adhesive linkage 5 is the polyurethane adhesive layer, has increased the fastness when PCM panel body 1 when the installation.
The thickness of the metal substrate 6 is 5-8 mm, the metal substrate 6 is a stainless steel plate, the mechanical strength of the metal substrate 6 is increased, and the durability of the PCM panel body 1 is improved.
The thickness of the anti-corrosion layer 7 is 0.3-0.8 mm, and the anti-corrosion layer 7 is an epoxy resin base layer, so that the bottom of the PCM panel body 1 cannot be easily corroded, and the durability of the PCM panel body 1 is improved.
The implementation principle of this application prevents fingerprint PCM panel embodiment does: during the use, will prevent fingerprint glued membrane 2 and paste the outside surface at PCM panel body 1, later will prevent the inside of the protruding 4 joints of installation of fingerprint glued membrane 2 both sides at the joint recess 3 that PCM panel body 1 both sides was seted up again, installation arch 4 will the butt in the inside of joint recess 3 this moment, and with production friction between the inner wall of joint recess 3, thereby increased the frictional force between joint recess 3 and the installation arch 4, make and can not take place to drop easily between joint recess 3 and the installation arch 4, make and prevent fingerprint glued membrane 2 more firm when using, and simultaneously, when the surface of preventing fingerprint glued membrane 2 has taken place the damage, also can be in time to preventing fingerprint glued membrane 2 and change, thereby PCM panel body 1 has increased the convenience of use.
The above embodiments are only used to illustrate the technical solutions of the present application, and not to limit the same; although the present application has been described in detail with reference to the foregoing embodiments, it should be understood by those of ordinary skill in the art that: the technical solutions described in the foregoing embodiments may still be modified, or some technical features may be equivalently replaced; and such modifications or substitutions do not depart from the spirit and scope of the corresponding technical solutions of the embodiments of the present application.

Claims (6)

1. The utility model provides a prevent fingerprint PCM panel, includes PCM panel body (1) and prevents fingerprint glued membrane (2), its characterized in that: the surface bonding of PCM panel body (1) has prevents fingerprint glued membrane (2), joint recess (3) have been seted up to the long limit both sides edge of PCM panel body (1), prevent that fingerprint glued membrane (2) both sides limit is close to the surperficial fixedly connected with installation arch (4) of PCM panel body (1), the inside of joint recess (3) is connected in installation arch (4) joint.
2. The anti-fingerprint PCM panel of claim 1, wherein: the thickness of the anti-fingerprint adhesive film (2) is 0.2-0.6 mm, and the anti-fingerprint adhesive film (2) is a high-transmittance AF anti-fingerprint protective film.
3. The anti-fingerprint PCM panel of claim 1, wherein: a side of the PCM panel body (1) close to the fingerprint-proof adhesive film (2) is provided with an adhesive layer (5), a side of the adhesive layer (5) far away from the fingerprint-proof adhesive film (2) is provided with a metal substrate (6), and a side of the metal substrate (6) opposite to the adhesive layer (5) is provided with an anti-corrosion layer (7).
4. The anti-fingerprint PCM panel according to claim 3, wherein: the thickness of the bonding layer (5) is 0.1-0.4 mm, and the bonding layer (5) is a polyurethane adhesive layer.
5. The anti-fingerprint PCM panel according to claim 3, wherein: the thickness of the metal substrate (6) is 5-8 mm, and the metal substrate (6) is a stainless steel plate.
6. The anti-fingerprint PCM panel according to claim 3, wherein: the thickness of the anti-corrosion layer (7) is 0.3-0.8 mm, and the anti-corrosion layer (7) is an epoxy resin base layer.
CN202223096982.8U 2022-11-22 2022-11-22 Fingerprint-proof PCM panel Active CN218593899U (en)