CN218257262U - Screen printing plate for testing performance of conductive silver paste - Google Patents

Screen printing plate for testing performance of conductive silver paste Download PDF

Info

Publication number
CN218257262U
CN218257262U CN202221718966.5U CN202221718966U CN218257262U CN 218257262 U CN218257262 U CN 218257262U CN 202221718966 U CN202221718966 U CN 202221718966U CN 218257262 U CN218257262 U CN 218257262U
Authority
CN
China
Prior art keywords
broken line
line section
conductive silver
printing plate
screen printing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202221718966.5U
Other languages
Chinese (zh)
Inventor
胡继林
沈剑
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Jiuyin Electronic Technology Co ltd
Original Assignee
Shanghai Jiuyin Electronic Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Jiuyin Electronic Technology Co ltd filed Critical Shanghai Jiuyin Electronic Technology Co ltd
Priority to CN202221718966.5U priority Critical patent/CN218257262U/en
Application granted granted Critical
Publication of CN218257262U publication Critical patent/CN218257262U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides a half tone for conductive silver thick liquid capability test makes the half tone through screen frame and screen cloth, uses conductive silver thick liquid printing film pattern, and the film pattern includes first broken line section, second broken line section, third broken line section and fourth broken line section, and first broken line section, second broken line section, the length of third broken line section and fourth broken line section is the same, and the line width proportion of first broken line section, second broken line section and third broken line section is 4, and the line width of second broken line section and fourth broken line section is the same. The utility model discloses a half tone for conductive silver thick liquid capability test through ingenious design, has designed different film pattern, and the isometric perpendicular line section of folding and a horizontal line section of three different linewidths make conductive silver thick liquid can select the film pattern of the line width direction that is fit for, and rectangular block and equilateral triangle series further test conductive silver thick liquid's performance to promoted printing quality at to a great extent, saved the human cost.

Description

Screen printing plate for testing performance of conductive silver paste
Technical Field
The utility model relates to a conductive silver thick liquid performance detects technical field, especially relates to a half tone for conductive silver thick liquid capability test.
Background
The materials used for manufacturing the prior screen printing plate mainly consider the combination of factors such as production cost, technology, effect and the like, and are biased. Except the material used for manufacturing the screen printing plate, the design of the screen printing plate is the design of the screen printing plate. Different customers and products are different, and the screen sizes and patterns can be various.
Currently, many users of conductive silver paste, using screen printing plates, are often modified as the production line or slightly. Under the condition that the feeding of the conductive silver paste is detected, the problem that the conductive silver paste cannot be used can still occur in a production line. Due to the design of the screen plate, the width of the conductive silver paste is not manufactured, so that deviation occurs, and problems occur when the conductive silver paste is used for a batch production line, so that economic loss is caused. To the researcher of conductive silver thick liquid, need the reason that various circumstances appear in discernment analysis conductive silver thick liquid, often need multiple processes, multiple operation seeks multiple factor, will get rid of the exception again simultaneously, can not reflect the conductive silver thick liquid performance condition as much as possible on a half screen printing, causes the unable line width film pattern that is fit for of performance selection according to conductive silver thick liquid to influence holistic printing quality.
SUMMERY OF THE UTILITY MODEL
In view of the foregoing prior art, an object of the present invention is to provide a screen printing plate for testing conductive silver paste performance, which is used to solve the problem in the prior art that a suitable line width film pattern cannot be selected according to the performance of conductive silver paste.
In order to solve the technical problem, the utility model discloses a realize according to following mode: the utility model provides a half tone for electrically conductive silver thick liquid capability test, makes half tone through screen frame and screen cloth, uses electrically conductive silver thick liquid printing film pattern, the film pattern includes first broken line section, second broken line section, third broken line section and fourth broken line section, the length of first broken line section, second broken line section, third broken line section and fourth broken line section is the same, the line width ratio of first broken line section, second broken line section and third broken line section is 4.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in a half tone for electrically conductive silver thick liquid capability test, first broken string section, second broken string section and third broken string section are perpendicular broken string section, fourth broken string section is the cross-fold line section.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in being used for conductive silver thick liquid capability test's half tone, the linewidth of first broken line section is 0.4 millimeter to 0.6 millimeter.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in the half tone for conductive silver thick liquid capability test, the linewidth of second fold line section is 0.2 millimeter to 0.3 millimeter.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in the half tone for electrically conductive silver thick liquid capability test, the linewidth of third broken line section is 0.1 millimeter to 0.15 millimeter.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in the half tone for electrically conductive silver thick liquid capability test, the film pattern still includes the rectangular block.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in the half tone for electrically conductive silver thick liquid capability test, the film pattern still includes equilateral triangle cluster line.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in the half tone for electrically conductive silver thick liquid capability test, the screen frame is the aluminum alloy frame.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of in a half tone for conductive silver thick liquid capability test, the screen cloth is 300 mesh polyester screen cloth.
In order to further solve the technical problem to be solved by the utility model, the utility model provides a pair of a half tone for conductive silver thick liquid capability test, the length of first broken line section, second broken line section, third broken line section and fourth broken line section is 2 meters.
As above, the utility model discloses a half tone for electrically conductive silver thick liquid capability test through ingenious design, has designed different film pattern, and the isometric perpendicular broken line section of three different linewidths and a horizontal broken line section make electrically conductive silver thick liquid can select the film pattern of the line width direction that is fit for, and rectangular block and equilateral triangle series line further test the performance of electrically conductive silver thick liquid to a great extent has promoted printing quality, has saved the human cost.
Drawings
Fig. 1 is a schematic structural diagram of a screen for testing conductive silver paste performance according to an embodiment of the present invention.
Reference is made to the following in corresponding reference numbers in the drawings of the specification:
the device comprises a first broken line segment 1, a second broken line segment 2, a third broken line segment 3, a fourth broken line segment 4, a rectangular block 5 and an equilateral triangle string line 6.
Detailed Description
The following description is given for illustrative embodiments of the present invention, and other advantages and effects of the present invention will be apparent to those skilled in the art from the disclosure of the present invention.
In order to make the technical means, embodiment and technical solution advantages of the present invention realized more clear, the following description will be combined with the drawings in the embodiment of the present invention to clearly and completely describe the technical solution in the embodiment of the present invention. It is to be understood that the embodiments described are some, not all embodiments of the invention. The components of embodiments of the present invention, as generally described and illustrated in the figures herein, may be arranged and designed in a wide variety of different configurations.
Thus, the following detailed description of the embodiments of the invention, as presented in the figures, is not intended to limit the scope of the invention, as claimed, but is merely representative of selected embodiments of the invention. Based on the embodiments of the present invention, all other embodiments obtained by a person skilled in the art without making creative efforts belong to the protection scope of the present invention.
It should be noted that like reference numerals and letters refer to like items in the following figures, and thus, once an item is defined in one figure, it need not be further defined and explained in subsequent figures.
The structure, ratio, size and the like shown in the drawings of the present specification are only used for matching with the content disclosed in the specification, so as to be known and read by people familiar with the technology, and are not used for limiting the limit conditions which can be implemented by the present invention, so that the present invention does not have the substantial significance in the technology, and any structure modification, ratio relationship change or size adjustment should still fall within the scope which can be covered by the technical content disclosed by the present invention without affecting the efficacy which can be produced by the present invention and the achievable purpose.
In the description of the present invention, it should be noted that the directions or positional relationships indicated by the terms "upper", "lower", "left", "right", "inner", "outer", "middle", etc. are based on the directions or positional relationships shown in the drawings, or the directions or positional relationships usually placed when the product of the present invention is used, and are only for the convenience of description of the present invention and simplification of the description, but not for indicating or suggesting that the indicated device or element must have a specific direction, and the change or adjustment of the relative relationship thereof is made without substantial technical change, and it is also regarded as the scope of the present invention which can be implemented. Furthermore, the terms "first," "second," and the like are used merely to distinguish one description from another, and are not to be construed as indicating or implying relative importance.
In the description of the present invention, it should also be noted that, unless otherwise explicitly specified or limited, the terms "disposed," "mounted," and "connected" are to be construed broadly, e.g., as meaning fixedly connected, detachably connected, or integrally connected; can be mechanically or electrically connected; they may be connected directly or indirectly through intervening media, or they may be interconnected between two elements. The specific meaning of the above terms in the present invention can be understood in specific cases to those skilled in the art.
As shown in figure 1, the utility model provides a half tone for electrically conductive silver thick liquid capability test makes the half tone through screen frame and screen cloth, uses electrically conductive silver thick liquid printing film pattern. The net frame is an aluminum alloy frame, and the net cloth is 300-mesh polyester net cloth. The film pattern comprises a first broken line segment 1, a second broken line segment 2, a third broken line segment 3 and a fourth broken line segment 4, wherein the lengths of the first broken line segment 1, the second broken line segment 2, the third broken line segment 3 and the fourth broken line segment 4 are the same and are all 2 meters. The line width ratio of the first fold line segment 1, the second fold line segment 2 and the third fold line segment 3 is 4.
The first broken line segment 1, the second broken line segment 2 and the third broken line segment 3 are vertical broken line segments, and the fourth broken line segment 4 is a transverse broken line segment. The line width of the first broken line segment 1 is 0.4 mm to 0.6 mm. The line width of the second fold line segment 2 is 0.2 mm to 0.3 mm. The line width of the third fold section 3 is 0.1 mm to 0.15 mm.
When the device is used, the line width of the first fold line section 1 is 0.6 mm, the line width of the second fold line section 2 is 0.3 mm, and the line width of the third fold line section 3 is 0.15 mm. The resistances of the first broken line segment 1, the second broken line segment 2 and the third broken line segment 3 are respectively represented as R1, R2 and R3, under ideal conditions, when the first broken line segment 1, the second broken line segment 2 and the third broken line segment 3 are in the same line length, the discrete degree of the resistance of the conductive silver paste and the proportion of the line width is as follows: r1: r2: r3= 1.
Comparing the resistance of the same pattern of the silver paste detection screen plates corresponding to different conductive silver pastes, wherein if the resistance is higher, the resistance performance is worse; the lower the resistance, the better the resistance performance. And secondly, comparing the proportional discrete degree of the resistance and the line width of the same conductive silver paste to track the line width range of the conductive silver paste suitable for printing, wherein the resistance begins to suddenly change under the line width of a plurality of thin lines, and the resistance value exceeds a proportional value. For example, if R2 is greater than 2R1 and R3 is greater than 4R1, the excess is not suitable for the line printing of the current line width.
The conductive silver paste has the characteristics of no line expansion after printing, small film thickness, small consumption (lower mold quantity) and small resistance. The above items are often difficult to satisfy simultaneously due to mutual influence, and in addition, the situations of large consumption and small resistance and the situation of wide line width and small resistance need to be eliminated by measuring the thickness and the line width of the die. Some conductive silver pastes are thinner and thinner along with the line, the resistance can suddenly change over a proportion, and the conductive silver pastes are not suitable for fine line printing. Some conductive silver paste has small resistance and large fine line resistance, and is not suitable for fine lines. Some conductive silver paste may have a slightly larger resistance, but the fine line proportion is good, and the line width does not influence the resistance increase over the proportion. For example, if R2 is close to 2R1 and R3 is larger than 4R1, it indicates that the conductive silver paste is suitable for the wiring of the second fold section 2, and it is not proper if the wiring is used for the third fold section 3. If R3 is equal to or close to 4R1, the conductive silver paste is suitable for line width printing of the third fold line section 3; if R2 exceeds 2R1 and R3 exceeds 4R1, the conductive silver paste is suitable for line width printing of the first broken line segment 1. Ideally, the closer R2 is to 2R1, the better R3 is to 4R1, and the more widely separated (i.e., the more the resistance drift) the less suitable it is for printing fine lines in this range.
According to the resistance of the fourth broken line segment 4 and the second broken line segment 2, the suitable direction of the customer routing printing can be judged, the resistance value of the fourth broken line segment 4 is represented as R4, if R4 is larger than R2, the printing direction is suitable for the vertical printing direction, and if R4 is smaller than R2, the printing direction is suitable for the horizontal printing direction.
By testing the adhesive force, bending and hardness of the first fold line segment 1, the second fold line segment 2 and the third fold line segment 3, the adhesive force, bending and hardness of the same silver paste under different widths are obtained, and the relation between diffusion broadening and adhesive force of conductive silver pastes with different line widths is compared.
The film pattern also includes rectangular blocks 5 and equilateral triangular strings 6. Rectangular block 5 can shine through the light source lamp and observe out bubble, sand eye and levelling nature, can survey the line width through the microscope, and the thick membrane of coarse appearance survey is thick. The resistance measurement of the equal-side triangular string line 6 can judge the trailing degree of the expanded side, the more serious the expanded side is, the more the triangular is expanded, the more the conductive silver paste adhered to the next triangular is, and the resistance is small.
To sum up, the utility model discloses a half tone for electrically conductive silver thick liquid capability test through ingenious design, has designed different film patterns, and the isometric perpendicular broken line section of three different linewidths and a horizontal broken line section make electrically conductive silver thick liquid can select the film pattern of the line width direction that is fit for, and rectangular block and equilateral triangle series line further test the performance of electrically conductive silver thick liquid to a great extent has promoted printing quality, has saved the human cost. Therefore, the utility model effectively overcomes all sorts of shortcomings in the prior art and achieves better practical effect.
The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Any person skilled in the art can modify or change the above embodiments without departing from the spirit and scope of the present invention. Accordingly, it is intended that all equivalent modifications or changes which may be made by those skilled in the art without departing from the spirit and technical spirit of the present invention be covered by the claims of the present invention.

Claims (10)

1. The utility model provides a half tone for electrically conductive silver thick liquid capability test, makes the half tone through screen frame and screen cloth, uses electrically conductive silver thick liquid printing film pattern, its characterized in that: the film pattern includes first broken line section (1), second broken line section (2), third broken line section (3) and fourth broken line section (4), the length of first broken line section (1), second broken line section (2), third broken line section (3) and fourth broken line section (4) is the same, the line width proportion of first broken line section (1), second broken line section (2) and third broken line section (3) is 4.
2. The screen printing plate for testing the performance of conductive silver paste of claim 1, wherein: the first fold line segment (1), the second fold line segment (2) and the third fold line segment (3) are vertical fold line segments, and the fourth fold line segment (4) is a transverse fold line segment.
3. The screen printing plate for testing conductive silver paste performance of claim 2, wherein: the line width of the first broken line segment (1) is 0.4 mm to 0.6 mm.
4. The screen printing plate for testing conductive silver paste performance of claim 2, wherein: the line width of the second fold line segment (2) is 0.2 mm to 0.3 mm.
5. The screen printing plate for testing conductive silver paste performance of claim 2, wherein: the line width of the third fold line section (3) is 0.1 mm to 0.15 mm.
6. The screen printing plate for testing the performance of the conductive silver paste according to claim 1, wherein the screen printing plate comprises: the film pattern further comprises a rectangular block (5).
7. The screen printing plate for testing the performance of the conductive silver paste according to claim 1, wherein the screen printing plate comprises: the film pattern also comprises equilateral triangle string lines (6).
8. The screen printing plate for testing the performance of conductive silver paste of claim 1, wherein: the screen frame is an aluminum alloy frame.
9. The screen printing plate for testing the performance of the conductive silver paste according to claim 1, wherein the screen printing plate comprises: the mesh is a 300-mesh polyester mesh.
10. The screen printing plate for testing the performance of the conductive silver paste according to claim 1, wherein the screen printing plate comprises: the length of the first broken line segment (1), the second broken line segment (2), the third broken line segment (3) and the fourth broken line segment (4) is 2 meters.
CN202221718966.5U 2022-07-05 2022-07-05 Screen printing plate for testing performance of conductive silver paste Active CN218257262U (en)