CN215305186U - Heat-insulating container with bottom sealed by gluing - Google Patents
Heat-insulating container with bottom sealed by gluing Download PDFInfo
- Publication number
- CN215305186U CN215305186U CN202022619370.7U CN202022619370U CN215305186U CN 215305186 U CN215305186 U CN 215305186U CN 202022619370 U CN202022619370 U CN 202022619370U CN 215305186 U CN215305186 U CN 215305186U
- Authority
- CN
- China
- Prior art keywords
- glue
- cup
- bottom fitting
- containing groove
- fitting piece
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model relates to the field of small household appliances, in particular to a heat-insulating container with a bottom sealed by gluing, which comprises: the cup with vacuum insulation layer with install the bottom fitting piece of cup lower part, be equipped with an at least glue containing groove between cup and the bottom fitting piece, it has adhesive material to hold gluey inslot intussuseption, adhesive material is in form the sealing layer between cup and the bottom fitting piece, through the setting in glue containing groove, for adhesive material provides the interval that stops and gather, makes it be in form effective shutoff between cup and the bottom fitting piece, promoted the bottom fitting piece with sealed effect between the cup.
Description
Technical Field
The utility model relates to the field of small household appliances, in particular to a heat-insulating container with a bottom sealed by gluing.
Background
The existing heat preservation containers, such as thermos bottles, thermos cups and the like, are isolated from the outside by applying a vacuumizing technology to a double-layer structure and forming a vacuum heat preservation layer to prevent heat in the containers from dissipating. In the prior art, a double-layer vacuumizing heat-insulating container is mostly made of metal materials and is convenient to carry outside.
In order to further endow more functions to the traditional heat preservation container, the prior art replaces the traditional cup bottom with a functional base with the functions of heating, cooling, stirring and the like by a mode of replacing the bottom on the basis of using a vacuum heat preservation layer with a double-layer structure, so that the traditional heat preservation container is upgraded into a multipurpose heat preservation container with special functions.
However, during the process of bottom replacement, the first problem to be solved is the sealing problem between the vacuum-pumping heat-insulating layer and the multifunctional bottom fitting piece. After the bottom fitting piece replaces the common bottom, the bottom fitting piece is usually a metal shell wrapped with various modules such as an electric control element and the like, so that the bottom fitting piece is not suitable for high temperature, and the cup body with the vacuum heat-insulating layer is not suitable for a high-temperature process; the prior art can not popularize the technology of connecting the bottom matching piece with the cup body with the vacuum insulation layer in advance before vacuumizing, so that the cup body with the vacuum insulation layer and the bottom matching piece are difficult to be combined in a traditional welding mode.
The prior art is not enough to form effective sealing by means of buckling or screw thread fixing, so the sealing effect is usually enhanced by means of gluing. The bottom matching piece is matched with the cup body with the vacuum insulation layer in a tight fit mode, so most glue can be extruded out along the matching surface in the assembling process after gluing. Because the glue flows uncontrollably, and the gap left by tight fit is smaller, the glue can not completely fill the existing small gap, and the cup body with the vacuum insulation layer and the bottom matching piece can not obtain the expected sealing effect after being glued.
SUMMERY OF THE UTILITY MODEL
The utility model aims to overcome at least one defect (deficiency) of the prior art, and provides an insulation container with a glued and sealed bottom, which is used for solving the problem that a bottom fitting piece and a cup body with a vacuum insulation layer are not good in sealing effect after being glued, and improving the sealing effect of the glued bottom fitting piece and the cup body.
The utility model adopts the technical scheme that the heat preservation container with the bottom sealed by gluing comprises: the vacuum cup comprises a cup body with a vacuum heat-insulating layer and a bottom matching piece arranged on the lower portion of the cup body, wherein at least one glue containing groove is formed between the cup body and the bottom matching piece, an adhesive material is filled in the glue containing groove, and a sealing layer is formed between the cup body and the bottom matching piece.
The bottom fitting piece can be functional components such as a heating disc, a mechanical stirring disc, an electromagnetic stirring disc, a blowing cooling disc and the like, and is provided with a metal shell; or the shell can be wrapped by a plastic shell, and the upper surface of the shell is a metal surface. The bottom fitting has embedded therein various electrical modules. The cup body comprises an inner wall and an outer wall. The cup body and the bottom matching piece form a tight fit, and a gap is still left after the matching because the cup body and the bottom matching piece are both made of hard materials. Before the installation, through in the bottom fitting piece with scribble coating adhesive material on the face of cup contact, work as the in-process that the inner wall of cup and bottom fitting piece carried out the assembly, adhesive material filled the gap to form the sealing layer in holding gluey groove, further shutoff makes the bottom fitting piece with airtight combination between the cup solves the problem that the sealed effect of cup and bottom fitting piece that has the vacuum heat preservation is not good.
In this technical scheme, at least one holds gluey groove and includes: the glue filling device comprises a first glue containing groove and a second glue containing groove, wherein the first glue containing groove and the second glue containing groove form an upper sealing layer and a lower sealing layer. The two glue containing grooves are arranged at different positions, so that the two glue containing grooves do not conflict with each other. According to the bottom fitting piece with the machining precision difference of the fitting surface of cup, can select to set up arbitrary appearance gluey groove or set up two kinds of appearance gluey grooves simultaneously to further promote the bottom fitting piece with the sticky sealed effect of cup.
In the technical scheme, the first glue containing groove is formed by incomplete contact caused by the shape difference of the matching surfaces of the cup body and the bottom matching piece.
The incomplete contact of the matching surfaces caused by the shape difference means that the surfaces of the cup body and the bottom matching piece cannot be completely attached due to different structures such as different gradients or different chamfers of the matching surfaces after the cup body and the bottom matching piece are matched through design. The known positions in the matching process, where the sealing gap cannot be formed through tight matching or leakage often occurs, are enlarged through design, so that the positions with poor contact and difficult sealing have larger space, the adhesive material can be more easily stopped and stored in the positions, and the sealing effect between the bottom matching piece and the cup body is improved through guiding and enhancing the effect of the adhesive material on the positions.
In the technical scheme, the second glue containing groove is formed in the outer surface of the inner wall of the cup body and/or the outer surface of the bottom fitting piece.
The glue containing groove can retain more adhesive materials in the gluing process before matching; in the matching process, excessive overflow glue is discharged outwards along the matching surface, after the glue containing groove is arranged, the overflow glue near the matching surface of the glue containing groove is extruded and stored in the glue containing groove in the assembling process, and the adhesive material is accumulated in the glue containing groove to form a circle of annular sealing layer, so that the sealing effect between the bottom matching piece and the cup body is further improved.
In this technical scheme, first appearance gluey groove and second appearance gluey groove are the annular groove. The annular groove enables the adhesive material to be solidified to form end-to-end sealing layers, and the whole sealing effect can be improved.
In this technical scheme, the bottom of annular groove is the arcwall face. The arcuate surfaces facilitate the flow of the adhesive material in the recess to concentrate at the lower edge of the notch to substantially fill the gap between the cup and the bottom fitting.
In the technical scheme, the inner wall of the cup body is also provided with a positioning step for limiting the position of the bottom fitting piece.
The location step prevents to assemble the destruction of the fitting surface that causes excessively hard, has protected first appearance gluey groove simultaneously, prevents that first appearance gluey groove opening dislocation from leading to airtight effect inefficacy.
In the technical scheme, the positioning step is a convex ring arranged at the lower part of the inner wall. The convex ring has the advantage of effectively and comprehensively limiting the edge of the upper surface of the bottom fitting piece, so that the bottom fitting piece is more accurately installed.
In the technical scheme, the positioning step is formed by deforming the inner wall. The processing is simpler and more convenient, and new problems of fixation, falling prevention, food contact sanitation and the like caused by introducing other independent parts are avoided.
In the technical scheme, a first fillet is formed between the lower part of the positioning step and the positioning step, and a second fillet is arranged at the edge of the top of the bottom fitting piece; the radian of the first fillet is smaller than that of the second fillet, and the interval formed after the first fillet is matched with the second fillet is a first glue accommodating groove.
After the positioning step is formed by machining deformation of the inner wall, the first fillet is formed due to the machining characteristics of the deformation. The top edge of the bottom fitting piece is fitted with the first rounded corner, so the top edge is made into a second rounded corner. In the actual fitting process, the first round corner and the second round corner are difficult to be completely tightly fitted, and leakage often occurs at the position. Through the adjustment design, make first fillet be less than the second fillet, form first appearance gluey groove during first fillet and the cooperation of second fillet, through enlargeing the gap between first fillet and the second fillet that is difficult to closely cooperate completely, adhesive material can gather in first appearance gluey inslot, forms the sealing layer, solves closely cooperate the back in the past, and adhesive material is difficult to evenly fill and the problem in shutoff gap completely.
Further, preferably, the adhesive material is silicone. Food-grade silica gel is more favorable for safety as an adhesive material.
Further, as preferred, the top opening of cup installs the sealed lid that can dismantle, and the bottle lid can with cup and bottom fitting piece form airtight container.
Compared with the prior art, the utility model has the beneficial effects that: through the setting of holding gluey groove, for sticky material provides the interval that stops and gather, make it be in form the sealing layer between cup and the bottom fitting piece, effective shutoff gap has promoted the bottom fitting piece with sealed effect between the cup.
Drawings
Fig. 1 is an overall schematic view of the present invention.
FIG. 2 is a partially enlarged view of the second glue receiving groove on the inner wall of the present invention.
FIG. 3 is a partially enlarged view of the second glue receiving groove formed on both the inner wall and the outer wall according to the present invention.
Fig. 4 is a partially enlarged view of the second glue receiving groove formed on the outer wall according to the present invention.
Fig. 5 is a partially enlarged view of the first glue receiving groove and the second glue receiving groove which are simultaneously arranged in the present invention.
The attached drawings indicate the following: cup 100, outer wall 110, inner wall 120, location step 121, bottom fitting piece 200, first appearance gluey groove 301, second appearance gluey groove 302, first fillet 122, second fillet 201, fitting surface 400.
Detailed Description
The drawings are only for purposes of illustration and are not to be construed as limiting the utility model. For a better understanding of the following embodiments, certain features of the drawings may be omitted, enlarged or reduced, and do not represent the size of an actual product; it will be understood by those skilled in the art that certain well-known structures in the drawings and descriptions thereof may be omitted.
Example 1
As shown in fig. 1, an insulated container having a bottom sealed by adhesion, comprises: cup 100 with vacuum insulation layer and bottom fitting piece 200 of installing in cup 100 lower part are equipped with at least one between cup 100 and the bottom fitting piece 200 and hold gluey groove, and what adopt in this embodiment only set up second and hold gluey groove 302, and second holds gluey inslot 302 intussuseption and is filled with adhesive material, and adhesive material forms the sealing layer between cup 100 and bottom fitting piece 200.
In fact, the glue tank also comprises other types such as: the first glue containing groove 301, the first glue containing groove 301 and the second glue containing groove 302 form an upper sealing layer and a lower sealing layer. The two glue containing grooves are arranged at different positions, so that the two glue containing grooves do not conflict with each other. Depending on the machining precision of the mating surfaces 400 of the bottom fitting member 200 and the cup body 100, different arrangements may be selected to ensure the adhesive sealing effect between the bottom fitting member 200 and the cup body 100.
Cup 100 includes an inner wall 120 and an outer wall 110. Although the cup 100 forms a tight fit with the bottom fitting 200, there is still a gap left after fitting because both are hard materials. As shown in fig. 2, 3 and 4, the second glue receiving groove 302 between the cup body 100 and the bottom fitting member 200 is disposed on the mating surface 400 of the cup body 100 and the bottom fitting member 200, specifically on the inner wall 120 of the cup body 100 and/or the outer surface of the bottom fitting member 200. Before the installation, through scribbling the sticky material on the face that bottom fitting piece 200 and cup 100 contact, in the in-process that cup 100 and bottom fitting piece 200 carried out the assembly, the sticky material fills the gap to form further shutoff with the mode of sealing layer in second glue containing groove 302, make bottom fitting piece 200 form sealed bottom in cup 100, solve the not good problem of cup 100 and bottom fitting piece 200 sealed effect.
The second glue accommodating groove 302 can retain more adhesive materials in the gluing process before matching; in the matching process, the excessive glue overflow is discharged outwards along the matching surface 400, after the second glue containing groove 302 is arranged, the glue overflow near the matching surface 400 is extruded and stored in the second glue containing groove 302 in the assembling process, and the adhesive material is accumulated in the second glue containing groove 302 to form a ring-shaped sealing layer, so that the sealing effect between the bottom matching piece 200 and the cup body 100 is further improved.
The second glue containing groove 302 is an annular groove. The annular groove enables the adhesive material to be solidified to form a first sealing layer, and the whole sealing effect can be improved. The bottom of the annular groove is an arc-shaped surface. The arcuate surfaces help the flow of the adhesive material in the recess to concentrate at the lower edge of the notch to substantially fill the gap between the cup 100 and the bottom fitting 200.
The inner wall 120 of the cup body 100 is further provided with a positioning step 121 for limiting the position of the bottom fitting 200. The positioning step 121 prevents the mating surface 400 from being damaged by excessive assembly force.
The positioning step 121 is a convex ring provided at a lower portion of the inner wall 120. The bead has the advantage of effectively and fully restraining the edge of the upper surface of bottom fitting piece 200, which provides a more accurate fitting of bottom fitting piece 200. The bead is formed by deformation of the inner wall 120. The processing is simpler and more convenient, and the new problems of fixation, falling prevention, food contact sanitation and the like caused by introducing other parts are avoided. The adhesive material in this embodiment is silicone.
Example 2
As shown in fig. 1, an insulated container having a bottom sealed by adhesion, comprises: the vacuum cup comprises a cup body 100 with a vacuum insulation layer and a bottom fitting piece 200 arranged at the lower part of the cup body 100, wherein at least one glue containing groove is arranged between the cup body 100 and the bottom fitting piece 200, the glue containing groove is filled with adhesive materials, and the adhesive materials form a sealing layer between the cup body 100 and the bottom fitting piece 200.
Bottom fitting piece 200 can be functional components such as dish, mechanical stirring dish, electromagnetic stirring dish, the cooling dish of blowing of generating heat, and what adopt in this embodiment is the electromagnetic stirring dish, and during the actual implementation, the practitioner can adopt the functional component of different functions as required. The bottom fitting 200 is cylindrical, and the bottom fitting 200 cannot be directly coupled to the cup body 100 by welding due to the insertion of various electrical modules. Cup 100 includes an inner wall 120 and an outer wall 110. Although the cup 100 forms a tight fit with the bottom fitting 200, there is still a gap left after fitting because both are hard materials.
As shown in fig. 5, a first glue receiving groove 301 is formed at the upper edge of the bottom fitting member 200 and at the corresponding position of the vacuum insulation inner wall 120, and the first glue receiving groove 301 utilizes the incomplete contact caused by the shape difference between the mating surfaces 400 of the cup body 100 and the bottom fitting member 200. The incomplete contact of the mating surface 400 due to the difference in shape is designed such that the surfaces of the cup 100 and the bottom fitting member 200 cannot be fitted together incompletely due to the difference in the size of the chamfer of the mating surface 400 after the mating. This location is a known gap that cannot form a seal with a tight fit. Enlarging it so that the gap, which is poorly contacted and difficult to close, has more room to encourage the mastic material to settle and be stored more easily in these locations, enhancing the effect of the mastic material in this location and promoting the sealing effect between bottom fitting 200 and cup 100.
In this embodiment, the first glue containing groove 301 forms a first fillet 122 with the positioning step 121 through the lower part of the positioning step 121, and the top edge of the bottom fitting piece 200 is provided with a second fillet 201; the radian of the first fillet 122 is smaller than that of the second fillet 201, and the interval formed after the first fillet 122 is matched with the second fillet 201 is a first glue accommodating groove 301.
After the positioning step 121 is formed by machining deformation of the inner wall 120, the first rounded corner 122 is formed due to the machining characteristics of the deformation. Mating with the first rounded corner 122 is the top edge of the bottom fitting 200, so the top edge would be made as a second rounded corner 201. In the actual fitting process, it is difficult to completely mate the first rounded corner 122 and the second rounded corner 201, and leakage often occurs at this position. Through the adjustment design, make first fillet 122 be less than second fillet 201, form first appearance gluey groove 301 when first fillet 122 and the cooperation of second fillet 201, through enlargeing the gap between first fillet 122 and the second fillet 201 that is difficult to closely cooperate completely, let adhesive material can gather in first appearance gluey groove 301, form the sealing layer, solve closely cooperate the back in the past, adhesive material is difficult to evenly fill and the problem in shutoff gap completely.
As shown in fig. 2, 3 and 4, a second glue receiving groove 302 is further formed on the sidewall of the bottom fitting member 200, and the second glue receiving groove 302 is formed on the mating surface 400 of the cup body 100 and the bottom fitting member 200, specifically on the outer surface of the bottom fitting member 200. More adhesive materials can be reserved in the gluing process of the first glue containing groove 301 and the second glue containing groove 302 before matching; in the matching process, excessive overflow glue is discharged outwards along the matching surface 400, after the first glue containing groove 301 and the second glue containing groove 302 are arranged, the overflow glue near the matching surface 400 is extruded and stored in the first glue containing groove 301 and the second glue containing groove 302 in the assembling process, the adhesive material is accumulated in the first glue containing groove 301 and the second glue containing groove 302 respectively to form two rings of annular sealing layers, and the sealing effect between the bottom matching piece 200 and the cup body 100 is further improved.
Before the installation, through scribbling the sticky material on the face that bottom fitting piece 200 and cup 100 contact, in the in-process that inner wall 120 and bottom fitting piece 200 of cup 100 assembled, the sticky material fills the gap to form further shutoff with the mode of sealing layer in first glue containing groove 301 and second glue containing groove 302, make bottom fitting piece 200 form inclosed bottom in cup 100, solve the not good problem of cup 100 and bottom fitting piece 200 sealed effect.
The first glue containing groove 301 and the second glue containing groove 302 are both annular grooves. The annular groove enables the adhesive material to be solidified to form end-to-end sealing layers, and the whole sealing effect can be improved. The bottom of the annular groove is an arc-shaped surface. The arcuate surfaces help to flow the mastic material in the recess so that it collects at the lower edge of the notch, substantially filling the gap between the cup 100 and the bottom fitting 200.
The inner wall 120 of the cup body 100 is further provided with a positioning step 121 for limiting the position of the bottom fitting 200. The positioning step 121 prevents the mating surface 400 from being damaged due to excessive assembly force, protects the formation of the first glue receiving groove 301, and prevents the first glue receiving groove 301 from being misaligned to generate an excessive gap.
The positioning step 121 is a convex ring provided at a lower portion of the inner wall 120. The bead has the advantage of effectively and fully restraining the edge of the upper surface of bottom fitting piece 200, which provides a more accurate fitting of bottom fitting piece 200. The bead is formed by deformation of the inner wall 120. The processing is simpler and more convenient, and the new problems of fixation, falling prevention, food contact sanitation and the like caused by introducing other parts are avoided.
The adhesive material used in this example is silicone. Food-grade silica gel is more favorable for safety as an adhesive material. The upper opening of the cup body 100 is provided with a detachable sealing cover which can form a closed container together with the cup body 100 and the bottom fitting piece 200.
It should be understood that the above-mentioned embodiments of the present invention are only examples for clearly illustrating the technical solutions of the present invention, and are not intended to limit the specific embodiments of the present invention. Any modification, equivalent replacement, and improvement made within the spirit and principle of the present invention claims should be included in the protection scope of the present invention claims.
Claims (10)
1. An insulated container having a bottom sealed by adhesive, comprising: the vacuum cup is characterized in that at least one glue containing groove is formed between the cup body and the bottom fitting piece, the glue containing groove is filled with adhesive materials, and a sealing layer is formed between the cup body and the bottom fitting piece by the adhesive materials.
2. A thermal container having a sealed bottom by adhesive according to claim 1, wherein said at least one glue-receiving well comprises: the glue filling device comprises a first glue containing groove and a second glue containing groove, wherein the first glue containing groove and the second glue containing groove form an upper sealing layer and a lower sealing layer.
3. An insulated container with a sealed bottom by gluing according to claim 2, characterized in that the first glue receiving groove is formed by incomplete contact due to the difference in shape of the mating surfaces of the cup and the bottom fitting member.
4. An insulated container with a sealed bottom by gluing according to claim 2, characterized in that the second glue receiving groove is provided on the inner wall of the cup body and/or on the outer surface of the bottom fitting piece.
5. The thermal container with the bottom sealed by gluing according to claim 2, wherein the first glue receiving groove and the second glue receiving groove are both annular grooves.
6. An insulated container with an adhesively sealed bottom according to claim 5, characterized in that the bottom of the annular recess is curved.
7. The thermal container with an adhesive-sealed bottom according to claim 2, wherein a positioning step for limiting the position of the bottom fitting member is further provided on the inner wall of the cup body.
8. An insulated container with an adhesive sealed bottom according to claim 7, characterized in that the positioning step is a bead provided at the lower part of the inner wall.
9. An insulated container with an adhesively sealed bottom according to claim 7, characterized in that the positioning step is formed by deformation of the inner wall.
10. The thermal container with the adhesive sealed bottom as claimed in claim 7, wherein the lower portion of the positioning step and the positioning step form a first rounded corner, and the top edge of the bottom fitting member is provided with a second rounded corner; the radian of the first fillet is smaller than that of the second fillet, and the interval formed after the first fillet is matched with the second fillet is a first glue accommodating groove.