CN214276498U - Intermediate alloy smelting crucible with cooling function - Google Patents
Intermediate alloy smelting crucible with cooling function Download PDFInfo
- Publication number
- CN214276498U CN214276498U CN202120190886.6U CN202120190886U CN214276498U CN 214276498 U CN214276498 U CN 214276498U CN 202120190886 U CN202120190886 U CN 202120190886U CN 214276498 U CN214276498 U CN 214276498U
- Authority
- CN
- China
- Prior art keywords
- crucible
- fixedly connected
- cooling function
- plate
- crucible cover
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses an intermediate alloy melting crucible with cooling function relates to melting crucible technical field. Including the crucible body, the top swing joint of crucible body has the crucible lid, the through-hole groove has been seted up on the crucible lid, the crucible is covered and is provided with the dwang, the first bevel gear of left side fixedly connected with of dwang, it is connected with the gear to rotate on the inner wall of crucible lid. This crucible is smelted to intermediate alloy with cooling function, the through-hole groove has been seted up on the crucible lid, can drive the rack plate through rotating the dwang and move, the effect that removes at the rack plate drives the closing plate downwards and moves, it can be more convenient to add the solder flux through the through-hole groove, need not open the crucible lid, the crucible is smelted to intermediate alloy with cooling function at present has been solved, when increasing solder flux and reactant inside the crucible, need open whole crucible lid, make this operation very troublesome and dangerous problem.
Description
Technical Field
The utility model relates to a smelt crucible technical field, specifically be an intermediate alloy smelt crucible with cooling function.
Background
Melting crucibles are the most important equipment for thermite welding. Most of the flux-cored brick adopts a funnel type with a narrow lower part and a wide upper part, and is provided with refractory brickwork, and flux is poured into the funnel type flux-cored brick for reaction. Since the specific gravities of various substances produced after the reaction are greatly different from each other, the precipitated substances can be separated out immediately after the reaction in the crucible form. The lower portion of the crucible has a safe and easily openable tap hole through which molten steel flows into the mold.
The crucible is smelted to present master alloy that has cooling function, when increasing solder flux and reactant to the crucible inside, need open whole crucible lid for this operation is very troublesome and dangerous, thereby has reduced the practicality of smelting the crucible.
SUMMERY OF THE UTILITY MODEL
Technical problem to be solved
The utility model provides a crucible is smelted to interalloy with cooling function to the not enough of prior art, has solved the problem that proposes in the above-mentioned background art.
(II) technical scheme
In order to achieve the above purpose, the utility model discloses a following technical scheme realizes: an intermediate alloy smelting crucible with a cooling function comprises a crucible body, wherein the top of the crucible body is movably connected with a crucible cover, the crucible cover is provided with a through hole groove, the crucible cover is provided with a rotating rod, the left side of the rotating rod is fixedly connected with a first bevel gear, the inner wall of the crucible cover is rotatably connected with a gear, the central position of the gear is fixedly connected with a second bevel gear, the first bevel gear is meshed with the second bevel gear, the inner wall of the crucible cover is slidably connected with a rack plate, the left side of the rack plate is fixedly connected with a sealing plate, the inner wall of the crucible cover is fixedly connected with a first fixing plate, the top of the first fixing plate is fixedly connected with a first spring, the top of the first spring is fixedly connected with a second fixing plate, the top of the second fixing plate is fixedly connected with a limiting block, and the bottom of the second fixing plate is fixedly connected with a fixing rod, the bottom of the fixed rod is hinged to one end of the connecting rod, and the other end of the connecting rod is hinged to the control rod.
Preferably, the fixing rod passes through the first fixing plate, and the fixing rod is slidably connected with the first fixing plate.
Preferably, the crucible cover is passed through to the dwang, the dwang is connected with the crucible cover rotation.
Preferably, a third fixing plate is fixedly connected to the inner wall of the crucible cover, a second spring is fixedly connected to the left side of the third fixing plate, the left side of the second spring is fixedly connected to the sealing plate, and the top of the sealing plate is slidably connected to the inner wall of the crucible cover.
Preferably, the inner wall of the crucible cover is fixedly connected with a fixed block
Preferably, the right side fixedly connected with bearing of dwang, the bearing is passed to the control lever, control lever and bearing swing joint.
(III) advantageous effects
The utility model provides a crucible is smelted to intermediate alloy with cooling function. The method has the following beneficial effects:
(1) this crucible is smelted to intermediate alloy with cooling function, the through-hole groove has been seted up on the crucible lid, can drive the rack plate through rotating the dwang and remove, the effect that removes at the rack plate drives the closing plate downwards and removes, it can be more convenient to add the solder flux through the through-hole groove, need not open the crucible lid, the crucible is smelted to intermediate alloy with cooling function at present has been solved, when increasing solder flux and reactant inside the crucible, need open whole crucible lid, make this operation very troublesome and dangerous problem.
(2) This intermediate alloy with cooling function smelts crucible is provided with the second spring on the closing plate for remove spacing to the closing plate, can open the through-hole groove automatically, make the operation more convenient, improved this intermediate alloy with cooling function smelts crucible's practicality.
Drawings
FIG. 1 is a schematic structural view of the integrated device of the present invention;
FIG. 2 is a schematic view of the structure of the through hole groove of the present invention;
fig. 3 is an enlarged schematic view of part a of the present invention.
In the figure: 1 crucible body, 2 crucible covers, 3 through-hole grooves, 4 dwang, 5 first bevel gear, 6 second bevel gear, 7 gears, 8 rack plates, 9 sealing plates, 10 first fixed plates, 11 first springs, 12 second fixed plates, 13 limiting blocks, 14 second springs, 15 fixed rods, 16 connecting rods, 17 control rods, 18 bearings, 19 fixed blocks, 20 third fixed plates, 21 bottom sealing plates.
Detailed Description
The technical solutions in the embodiments of the present invention will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments in the present invention, all other embodiments obtained by a person skilled in the art without creative work belong to the protection scope of the present invention.
Referring to fig. 1-3, the present invention provides a technical solution: an intermediate alloy smelting crucible with a cooling function comprises a crucible body 1, wherein the top of the crucible body 1 is movably connected with a crucible cover 2, the crucible cover 2 is provided with a through hole groove 3, the crucible cover 2 is provided with a rotating rod 4, the left side of the rotating rod 4 is fixedly connected with a first bevel gear 5, the inner wall of the crucible cover 2 is rotatably connected with a gear 7, the central position of the gear 7 is fixedly connected with a second bevel gear 6, the first bevel gear 5 is meshed with the second bevel gear 6, the inner wall of the crucible cover 2 is slidably connected with a rack plate 8, the left side of the rack plate 8 is fixedly connected with a sealing plate 9, the inner wall of the crucible cover 2 is fixedly connected with a first fixing plate 10, the top of the first fixing plate 10 is fixedly connected with a first spring 11, the top of the first spring 11 is fixedly connected with a second fixing plate 12, the top of the second fixing plate 12 is fixedly connected with a limiting block 13, and the bottom of the second fixing plate 12 is fixedly connected with a fixing rod 15, the bottom of the fixed rod 15 is hinged with one end of the connecting rod 16, the other end of the connecting rod 16 is hinged with the control rod 17, the fixed rod 15 passes through the first fixed plate 10, the fixed rod 15 is connected with the first fixed plate 10 in a sliding manner, the rotating rod 4 passes through the crucible cover 2, the rotating rod 4 is connected with the crucible cover 2 in a rotating manner, the inner wall of the crucible cover 2 is fixedly connected with the third fixed plate 20, the left side of the third fixed plate 20 is fixedly connected with the second spring 14, the left side of the second spring 14 is fixedly connected with the sealing plate 9, the top of the sealing plate 9 is connected with the inner wall of the crucible cover 2 in a sliding manner, the inner wall of the crucible cover 2 is fixedly connected with the fixed block 19, the right side of the rotating rod 4 is fixedly connected with the bearing 18, the control rod 17 passes through the bearing 18, the control rod 17 is movably connected with the bearing, when the interior of the crucible body 1 needs to be cooled, the bottom sealing plate 21 can be opened to accelerate the cooling of the interior of the crucible body 1, the intermediate alloy melting crucible with the cooling function is provided with the second spring 14 on the sealing plate 9, so that the limit of the sealing plate 9 is relieved, the through hole groove 3 can be automatically opened, the operation is more convenient, the practicability of the intermediate alloy melting crucible with the cooling function is improved, the through hole groove is formed in the crucible cover 2, the rack plate 8 can be driven to move by rotating the rotating rod 4, the sealing plate 9 is driven to move downwards under the action of the movement of the rack plate 8, the convenience is improved by adding a welding flux through the through hole groove 3, the crucible cover 2 does not need to be opened, and the problem of the existing intermediate alloy melting crucible with the cooling function is solved, when adding flux and a reactant to the inside of the crucible, it is necessary to open the entire crucible cover 2, making this operation very troublesome and dangerous.
When the crucible cover is in operation (or in use), when a welding flux needs to be added into the crucible body 1 when the crucible body 1 is in operation, the control rod 17 can be pushed to the left side, the control rod 17 moves to the left side and drives the connecting rod 16 to move to the left side, the connecting rod 16 moves to the left side and drives the fixed rod 15 to move downwards, the fixed rod 15 moves downwards and drives the second fixed plate 12 to move downwards, the fixed plate 12 moves downwards and drives the limiting block 13 to move downwards, the limiting block 13 cannot limit the gear 7 by moving downwards, the sealing plate 9 moves to the right side under the action of the second spring 14, the through hole groove 3 on the crucible cover 2 is opened by moving the sealing plate 9 to the right side, the welding flux is added into the crucible body 1 by the through hole groove 3, then the rotating rod 4 is rotated, the rotating rod 4 drives the first bevel gear 5 to rotate, the first bevel gear 5 drives the second bevel gear 6 to rotate, second bevel gear 6 rotates and drives gear 7 and rotate, it moves to the left side to drive rack plate 8 through gear 7 rotation, rack plate 8 moves to the left side and drives closing plate 9 and move to the left side, it makes closing plate 9 seal through closing plate 9 moves to the left side makes through-hole groove 3, when closing plate 9 moved the position of fixed block 19, loosen control lever 17, second fixed plate 12 upwards moves under the effect of first spring 11, second fixed plate 12 upwards moves and drives stopper 13 rebound, make stopper 13 carry on spacingly to gear 7.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.
Claims (6)
1. The utility model provides an intermediate alloy melting crucible with cooling function, includes crucible body (1), its characterized in that: the crucible cover is characterized in that the crucible cover (2) is movably connected to the top of the crucible body (1), a through hole groove (3) is formed in the crucible cover (2), a rotating rod (4) is arranged on the crucible cover (2), a first bevel gear (5) is fixedly connected to the left side of the rotating rod (4), a gear (7) is rotatably connected to the inner wall of the crucible cover (2), a second bevel gear (6) is fixedly connected to the central position of the gear (7), the first bevel gear (5) is meshed with the second bevel gear (6), a rack plate (8) is slidably connected to the inner wall of the crucible cover (2), a sealing plate (9) is fixedly connected to the left side of the rack plate (8), a first fixing plate (10) is fixedly connected to the inner wall of the crucible cover (2), and a first spring (11) is fixedly connected to the top of the first fixing plate (10), the top fixedly connected with second fixed plate (12) of first spring (11), the top fixedly connected with stopper (13) of second fixed plate (12), the bottom fixedly connected with dead lever (15) of second fixed plate (12), the bottom of dead lever (15) is articulated with the one end of connecting rod (16), the other end and the control lever (17) of connecting rod (16) are articulated.
2. The master alloy melting crucible with the cooling function as set forth in claim 1, wherein: the fixing rod (15) penetrates through the first fixing plate (10), and the fixing rod (15) is connected with the first fixing plate (10) in a sliding mode.
3. The master alloy melting crucible with the cooling function as set forth in claim 1, wherein: the crucible cover (2) is passed in dwang (4), dwang (4) and crucible cover (2) rotate to be connected.
4. The master alloy melting crucible with the cooling function as set forth in claim 1, wherein: fixedly connected with third fixed plate (20) on the inner wall of crucible cover (2), the left side fixedly connected with second spring (14) of third fixed plate (20), the left side and closing plate (9) fixed connection of second spring (14), the top and the inner wall sliding connection of crucible cover (2) of closing plate (9).
5. The master alloy melting crucible with the cooling function as set forth in claim 1, wherein: the inner wall of the crucible cover (2) is fixedly connected with a fixing block (19).
6. The master alloy melting crucible with the cooling function as set forth in claim 1, wherein: the right side fixedly connected with bearing (18) of dwang (4), bearing (18) are passed in control lever (17), control lever (17) and bearing (18) swing joint.