CN214056726U - Easily-oxidized and easily-cut USB aluminum plate - Google Patents
Easily-oxidized and easily-cut USB aluminum plate Download PDFInfo
- Publication number
- CN214056726U CN214056726U CN202023036796.6U CN202023036796U CN214056726U CN 214056726 U CN214056726 U CN 214056726U CN 202023036796 U CN202023036796 U CN 202023036796U CN 214056726 U CN214056726 U CN 214056726U
- Authority
- CN
- China
- Prior art keywords
- plate
- aluminum plate
- positive
- cut
- usb
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses an easy-oxidation easy-cutting USB aluminum plate, which comprises four positive plates, wherein cutting grooves are arranged between two positive plates, an organic layer is fixedly connected to the lower surface of each positive plate, the cutting grooves are arranged on the surface of one part of the aluminum plate in the process of manufacturing the aluminum plate by arranging the cutting grooves, the other part of the aluminum plate is not added, a large-scale aluminum plate is still produced, a worker can select the needed aluminum plate more as required, the part of the aluminum plate provided with the cutting grooves is relatively thin for the aluminum plate as a whole, the aluminum plate is convenient to cut, the efficiency of cutting the aluminum plate is effectively improved, the aluminum plate is placed in a place with better light by arranging metal oxide and oxidation films, the positive plate and the negative plate are arranged on the upper surface of the aluminum plate, the positive plate can promote hole injection, the negative plate can promote electron injection, and simultaneously, the metal oxide is arranged in the connecting plate, and the connecting plate is wrapped by an oxidation film, so that the oxidation efficiency of the aluminum plate is promoted.
Description
Technical Field
The utility model relates to a USB aluminum plate oxidation technology field specifically is an easy oxidation easily cuts USB aluminum plate.
Background
The aluminum plate is a rectangular plate rolled and processed by an aluminum ingot, and is divided into a pure aluminum plate, an alloy aluminum plate, a thin aluminum plate, a medium-thickness aluminum plate, a patterned aluminum plate, oxidation, which means a chemical reaction of oxygen element and other substance elements in a narrow sense, and is also an important chemical unit process. Oxidation in the broad sense refers to the process of losing electrons (an increase in oxidation number) of a substance. The existing easy-to-oxidize aluminum plate has the following problems:
firstly, the existing easy-to-oxidize aluminum plate is troublesome to cut and wastes time and labor in the process of separating a large aluminum plate;
in addition, the existing easy-to-oxidize aluminum plate needs to be placed in an environment special for oxidation when the aluminum plate is oxidized, and the aluminum plate needs a large amount of money and time.
SUMMERY OF THE UTILITY MODEL
An object of the utility model is to provide an easy oxidation easily cuts USB aluminum plate to solve the problem that proposes in the above-mentioned background art.
In order to achieve the above object, the utility model provides a following technical scheme:
the utility model provides an easy oxidation easy-to-cut USB aluminum plate, includes the positive plate, the positive plate is provided with four, is provided with between two positive plates and cuts cut groove, fixed surface has the organic layer under the positive plate, fixed surface has the negative plate under the organic layer, fixed surface is connected with the connecting plate under the negative plate, the connecting plate.
As a further aspect of the present invention: and an oxidation film is arranged on the lower surface of the connecting plate.
As a further aspect of the present invention: the lower surface of the connecting plate is fixedly connected with a base plate.
As a further aspect of the present invention: and metal oxide is arranged inside the connecting plate.
As a further aspect of the present invention: holes are formed in the two sides of the positive plate and the two sides of the negative plate.
As a further aspect of the present invention: holes are arranged on two sides of the organic layer.
Compared with the prior art, the beneficial effects of the utility model are that:
1. by arranging the cutting grooves, in the process of manufacturing the aluminum plate, the cutting grooves are formed in one part of the surface of the aluminum plate, and the other part of the surface of the aluminum plate is not added, so that the large aluminum plate is still produced, a worker can select the needed aluminum plate according to more requirements, and the part of the aluminum plate, which is provided with the cutting grooves, is relatively thin for the whole aluminum plate, so that the aluminum plate is convenient to cut, and the efficiency of cutting the aluminum plate is effectively improved;
2. through setting up metal oxide and oxide film, place aluminum plate in the better place of light, through set up positive plate and negative plate at aluminum plate upper surface, the positive plate can promote the hole injection, and the negative plate can promote the electron injection, simultaneously through setting up metal oxide in the connecting plate is inside to use oxide film to live the connecting plate parcel, promoted aluminum plate oxidation's efficiency.
Drawings
FIG. 1 is a schematic structural diagram of an easily oxidized and cut USB aluminum plate;
FIG. 2 is a schematic structural diagram of an easily oxidized and cut USB aluminum plate;
FIG. 3 is a schematic structural diagram of a connecting plate in an easily-oxidized and easily-cut USB aluminum plate.
In the figure: 1. a positive plate; 2. a negative plate; 3. an organic layer; 4. oxidizing the thin film; 5. a metal oxide; 6. a hole; 7. a connecting plate; 8. a substrate; 9. and cutting the groove.
Detailed Description
The technical solutions in the embodiments of the present invention will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments in the present invention, all other embodiments obtained by a person skilled in the art without creative work belong to the protection scope of the present invention.
Referring to fig. 1 to 3, in an embodiment of the present invention, an easily-oxidized and easily-cut USB aluminum plate includes a positive plate 1, and is characterized in that: the four positive plates 1 are arranged, the cutting grooves 9 are arranged between the two positive plates 1, the organic layers 3 are fixedly connected to the lower surfaces of the positive plates 1, the negative plates 2 are fixedly connected to the lower surfaces of the organic layers 3, the connecting plates 7 are fixedly connected to the lower surfaces of the negative plates 2, the cutting grooves 9 are arranged on one part of the surface of the aluminum plate in the process of manufacturing the aluminum plate by arranging the cutting grooves 9, the other part of the aluminum plate is not added, a large aluminum plate is still produced, a worker can select the needed aluminum plate as required, the part of the aluminum plate, which is provided with the cutting grooves 9, is relatively thin for the whole aluminum plate, the cutting is convenient, the efficiency of cutting the aluminum plate is effectively improved, the aluminum plate is placed in a place with better light by arranging the metal oxide 5 and the oxide film 4, and the positive plates 1 and the negative plates 2 are arranged on the upper surface of the aluminum plate, so that the positive plates 1 can promote the injection of cavities, and the negative plate 2 can promote electron injection, and meanwhile, the efficiency of aluminum plate oxidation is promoted by arranging the metal oxide 5 in the connecting plate 7 and wrapping the connecting plate 7 by using the oxidation film 4.
Preferably, the lower surface of the connection plate 7 is provided with an oxide film 4.
Preferably, a base plate 8 is fixedly connected to the lower surface of the connecting plate 7.
Preferably, the connection plate 7 is internally provided with a metal oxide 5.
Preferably, holes 6 are formed on both sides of the positive plate 1 and the negative plate 2.
Preferably, the organic layer 3 is provided with holes 6 on both sides.
The utility model discloses a theory of operation is:
during the use, at the in-process of making aluminum plate, set up cutting groove 9 on some aluminum plate surface, any interpolation is not done to another part, still produce large-scale aluminum plate, the staff can have more the demand and select the aluminum plate of needs, the part that sets up cutting groove 9 in the aluminum plate is relatively thin to aluminum plate is whole, the cutting of being convenient for, effectively improve cutting aluminum plate's efficiency, place aluminum plate in the better place of light, through set up positive plate 1 and negative plate 2 on aluminum plate upper surface, positive plate 1 can promote the hole injection, and negative plate 2 can promote the electron injection, simultaneously through setting up metal oxide 5 in connecting plate 7 inside, and use oxide film 4 to live 7 wraps up of connecting plate, the efficiency of aluminum plate oxidation has been promoted.
Although the present invention has been described in detail with reference to the foregoing embodiments, it will be apparent to those skilled in the art that modifications may be made to the embodiments or portions thereof without departing from the spirit and scope of the invention.
Claims (6)
1. The utility model provides an easy oxidation easy-to-cut USB aluminum plate, includes positive plate (1), its characterized in that: the positive plate (1) is provided with four, is provided with between two positive plates (1) and cuts cut groove (9), fixed surface is connected with organic layer (3) under positive plate (1), fixed surface is connected with negative plate (2) under organic layer (3), fixed surface is connected with connecting plate (7) under negative plate (2), connecting plate (7).
2. An easily oxidized and cut-off USB aluminum plate according to claim 1, wherein: and an oxidation film (4) is arranged on the lower surface of the connecting plate (7).
3. An easily oxidized and cut-off USB aluminum plate according to claim 1, wherein: and a base plate (8) is fixedly connected to the lower surface of the connecting plate (7).
4. An easily oxidized and cut-off USB aluminum plate according to claim 1, wherein: and a metal oxide (5) is arranged in the connecting plate (7).
5. An easily oxidized and cut-off USB aluminum plate according to claim 1, wherein: holes (6) are formed in the two sides of the positive plate (1) and the negative plate (2).
6. An easily oxidized and cut-off USB aluminum plate according to claim 1, wherein: holes (6) are arranged on two sides of the organic layer (3).