CN212749300U - Weather-resistant reflective film - Google Patents
Weather-resistant reflective film Download PDFInfo
- Publication number
- CN212749300U CN212749300U CN202021165934.8U CN202021165934U CN212749300U CN 212749300 U CN212749300 U CN 212749300U CN 202021165934 U CN202021165934 U CN 202021165934U CN 212749300 U CN212749300 U CN 212749300U
- Authority
- CN
- China
- Prior art keywords
- layer
- corrosion
- viscose
- coating
- resistant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a weatherability reflection of light film, including main part, finishing oil coating, small glass bead layer, focus layer, reflection stratum, corrosion resistant layer, viscose inoxidizing coating and tear line, the top of main part is equipped with finishing oil coating, be equipped with in the main part the tear line, the main part from top to bottom does respectively small glass bead layer, focus layer, reflection stratum, corrosion resistant layer, viscose layer and the viscose inoxidizing coating. The utility model discloses in, the design has the tear line convenience under the condition of outdoor or not carrying sharp ware, uses the reflector film disconnection, and the design has corrosion-resistant layer to improve the corrosion resisting property of reflector film, increase of service life, and the oil varnish coating improves the weatherability of reflector film simultaneously, and the design has the ability that the focusing layer improves the reflector film and collects light, is equipped with triangular prism in the reflector layer, reflects light through triangular prism and improves light reflection efficiency.
Description
Technical Field
The utility model relates to a reflective membrane technical field particularly, relates to a weatherability reflection of light film.
Background
With the continuous expansion of the volume of the domestic market, the continuous perfection and maturity of the domestic enterprises on the product manufacturing technology, the advantages of domestic inherent human resources and the like on the cost, the difference between the local brand and the foreign manufacturers on the product quality is continuously reduced, the substitution phenomenon of 'homogeneous low price' is realized in partial fields, and the domestic reflective film production enterprises come in spring.
Most of reflective films in the current market only pay attention to the reflection efficiency, but the quality of the reflective films is not paid attention to, so that the problems of short service life and weather resistance of the reflective films are caused, and meanwhile, the reflective films are not integrally connected and cannot be disconnected from the reflective films without scissors, so that the reflective films are inconvenient to use.
An effective solution to the problems in the related art has not been proposed yet.
SUMMERY OF THE UTILITY MODEL
An object of the utility model is to provide a weatherability reflection of light film to solve the problem that proposes in the above-mentioned background art.
In order to achieve the above object, the utility model provides a following technical scheme: the utility model provides a weatherability reflection of light film, includes main part, overprint varnish coating, small glass bead layer, focuses layer, reflecting layer, corrosion resistant layer, viscose inoxidizing coating and tear line, the top of main part is equipped with overprint varnish coating, be equipped with in the main part the tear line, the main part from top to bottom is respectively small glass bead layer, focuses layer, reflecting layer, corrosion resistant layer, viscose layer and the viscose inoxidizing coating.
Furthermore, the varnish coating is positioned at the top end of the main body, the varnish coating is coated on the surface of the main body, and the varnish coating is fixedly connected with the main body.
Further, the tearing line penetrates through the main body and is in a dotted line shape.
Furthermore, the small glass bead layer is located on the top end of the main body, glass beads are arranged inside the small glass bead layer, and the glass beads are uniformly distributed inside the small glass bead layer.
Further, focus the layer with the reflection stratum reflects light jointly, focus the layer and be located the bottom on small glass pearl layer, the bottom on focus the layer is equipped with the reflection stratum, the reflection stratum is inside to be equipped with a plurality of triangular prism, triangular prism with the bottom fixed connection on reflection stratum.
Further, the corrosion-resistant layer is located at the bottom end of the reflecting layer, and the corrosion-resistant layer is fixedly connected with the reflecting layer.
Furthermore, the adhesive layer is located at the bottom end of the corrosion-resistant layer, the adhesive protective layer is arranged at the bottom end of the adhesive layer, the adhesive layer is fixedly connected with the corrosion-resistant layer, and the adhesive layer is bonded with the adhesive protective layer.
Compared with the prior art, the utility model discloses following beneficial effect has:
1. the utility model discloses in, the design has the tear line to make things convenient for under the outdoor or the condition that does not carry sharp ware, uses the reflective membrane disconnection.
2. The utility model discloses in, the design has corrosion resistant layer to improve the corrosion resisting property of reflective membrane, increase of service life, and the oil coating that coats with light improves the weatherability of reflective membrane simultaneously.
3. The utility model discloses in, the design has the focusing layer to improve the ability that the reflective membrane collected light, is equipped with triangular prism in the reflection stratum, reflects light through triangular prism and improves light reflection efficiency.
Drawings
In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required to be used in the embodiments will be briefly described below, and it is obvious that the drawings in the following description are only some embodiments of the present invention, and for those skilled in the art, other drawings can be obtained according to these drawings without creative efforts.
Fig. 1 is a schematic structural diagram of an entire embodiment of the present invention;
fig. 2 is a top view of an embodiment according to the invention as a whole;
fig. 3 is a cross-sectional view of an entirety of an embodiment according to the invention.
Reference numerals:
1. a main body; 2. a overprint varnish coating; 3. a layer of tiny glass beads; 4. a focusing layer; 5. a reflective layer; 6. a corrosion-resistant layer; 7. an adhesive layer; 8. gluing a protective layer; 9. glass beads; 10. a triangular prism; 11. and (6) tearing the line.
Detailed Description
The technical solution in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, rather than all embodiments, and all other embodiments obtained by a person of ordinary skill in the art without creative work belong to the protection scope of the present invention based on the embodiments of the present invention.
In the description of the present invention, it should be noted that the terms "top", "bottom", "one side", "the other side", "front", "back", "middle part", "inside", "top", "bottom", etc. indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, which is only for the convenience of description and simplification of the description, but does not indicate or imply that the device or element referred to must have a specific orientation, be constructed in a specific orientation, and be operated, and thus, should not be construed as limiting the present invention; the terms "first," "second," and "third" are used for descriptive purposes only and are not to be construed as indicating or implying relative importance; furthermore, unless expressly stated or limited otherwise, the terms "mounted," "connected," and "connected" are to be construed broadly, as they may be fixedly connected, detachably connected, or integrally connected, for example; can be mechanically or electrically connected; they may be connected directly or indirectly through intervening media, or they may be interconnected between two elements. The specific meaning of the above terms in the present invention can be understood in specific cases to those skilled in the art.
Please refer to fig. 1-3, according to the embodiment of the present invention, a weather-resistant reflective film comprises a main body 1, a finishing oil coating 2, a small glass bead layer 3, a focusing layer 4, a reflecting layer 5, an anti-corrosion layer 6, an adhesive layer 7, an adhesive protective layer 8 and a tear line 11, wherein the top end of the main body 1 is provided with the finishing oil coating 2, the main body 1 is provided with the tear line 11, and the main body 1 is the small glass bead layer 3, the focusing layer 4, the reflecting layer 5, the anti-corrosion layer 6, the adhesive layer 7 and the adhesive protective layer 8 from top to bottom.
The oil coating 2 is located at the top end of the main body 1, the oil coating 2 is coated on the surface of the main body 1, and the oil coating 2 is fixedly connected with the main body 1.
Wherein, the tearing line 11 penetrates through the main body 1, and the tearing line 11 is in a dotted line shape.
The small glass bead layer 3 is located at the top end of the main body 1, the glass beads 9 are arranged inside the small glass bead layer 3, and the glass beads 9 are uniformly distributed inside the small glass bead layer 3.
Wherein, focus layer 4 with reflection stratum 5 reflects light jointly, focus layer 4 is located the bottom on little glass pearl layer 3, the bottom on focus layer 4 is equipped with reflection stratum 5, reflection stratum 5 is inside to be equipped with a plurality of triangular prism 10, triangular prism 10 with reflection stratum 5's bottom fixed connection.
Wherein the corrosion-resistant layer 6 is positioned at the bottom end of the reflecting layer 5, and the corrosion-resistant layer 6 is fixedly connected with the reflecting layer 5.
Wherein, the viscose layer 7 is located the bottom of corrosion-resistant layer 6, the bottom of viscose layer 7 is equipped with viscose inoxidizing coating 8, viscose layer 7 with corrosion-resistant layer 6 fixed connection, viscose layer 7 with viscose inoxidizing coating 8 bonds.
Principle of operation
When specifically using, tear the reflective membrane that the area is fit for through tear line 11, tear viscose inoxidizing coating 8 afterwards, paste the reflective membrane at assigned position through viscose layer 7, wherein overprint varnish coating 2 is used for improving the weatherability of reflective membrane, the while has pleasing to the eye effect, small glass bead layer 3, focusing layer 4 and 5 component light reflection system jointly of reflection stratum, gather the reflection to the light that shines on the reflective membrane, corrosion-resistant layer 6 increases the corrosion resisting property of reflective membrane, the life of extension reflective membrane.
In addition, the design has tear line 11 to make things convenient for under the outdoor or the circumstances that does not carry sharp weapon, uses the reflective membrane disconnection, and the design has corrosion-resistant layer 6 to improve the corrosion resisting property of reflective membrane, increase of service life, and the design has focusing layer 4 to improve the ability that the reflective membrane collected light, is equipped with triangular prism 10 in the reflection stratum 5, carries out the reflection of light through triangular prism 10 and improves light reflection efficiency.
Finally, it should be noted that: although the present invention has been described in detail with reference to the foregoing embodiments, it will be apparent to those skilled in the art that modifications may be made to the embodiments described in the foregoing embodiments, or equivalents may be substituted for elements thereof. Any modification, equivalent replacement, or improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims (7)
1. The utility model provides a weatherability reflection of light film, its characterized in that includes main part (1), finishing oil coating (2), small glass bead layer (3), focus layer (4), reflection stratum (5), corrosion resistant layer (6), viscose layer (7), viscose inoxidizing coating (8) and tear line (11), the top of main part (1) is equipped with finishing oil coating (2), be equipped with on main part (1) tear line (11), main part (1) from top to bottom do respectively small glass bead layer (3), focus layer (4), reflection stratum (5), corrosion resistant layer (6), viscose layer (7) and viscose inoxidizing coating (8).
2. The weather-resistant reflective film according to claim 1, wherein the overprint varnish coating (2) is disposed on the top of the main body (1), the overprint varnish coating (2) is coated on the surface of the main body (1), and the overprint varnish coating (2) is fixedly connected to the main body (1).
3. The weatherable reflective film according to claim 1, wherein said tear line (11) penetrates said body (1), said tear line (11) having a dotted line shape.
4. The weather-resistant reflective film according to claim 1, wherein the micro glass bead layer (3) is located at the top end of the main body (1), the micro glass bead layer (3) is internally provided with glass beads (9), and the glass beads (9) are uniformly distributed inside the micro glass bead layer (3).
5. The weather-resistant reflective film according to claim 1, wherein the focusing layer (4) and the reflective layer (5) reflect light together, the focusing layer (4) is located at the bottom end of the micro glass bead layer (3), the reflective layer (5) is located at the bottom end of the focusing layer (4), a plurality of triangular prisms (10) are arranged inside the reflective layer (5), and the triangular prisms (10) are fixedly connected with the bottom end of the reflective layer (5).
6. The weatherable reflective film according to claim 1, wherein said corrosion resistant layer (6) is located at the bottom end of said reflective layer (5), said corrosion resistant layer (6) is fixedly connected to said reflective layer (5).
7. The weather-resistant reflective film according to claim 1, wherein the adhesive layer (7) is located at the bottom end of the corrosion-resistant layer (6), the adhesive protective layer (8) is disposed at the bottom end of the adhesive layer (7), the adhesive layer (7) is fixedly connected with the corrosion-resistant layer (6), and the adhesive layer (7) is bonded with the adhesive protective layer (8).