CN212128263U - Annealing softening installation of almag silk - Google Patents
Annealing softening installation of almag silk Download PDFInfo
- Publication number
- CN212128263U CN212128263U CN202020330553.4U CN202020330553U CN212128263U CN 212128263 U CN212128263 U CN 212128263U CN 202020330553 U CN202020330553 U CN 202020330553U CN 212128263 U CN212128263 U CN 212128263U
- Authority
- CN
- China
- Prior art keywords
- fixed
- pivot
- slide
- annealing
- bull stick
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model belongs to the technical field of the almag silk technique and specifically relates to an annealing softening installation of almag silk, the desk comprises a table, the desk bottom is fixed with the support, install the motor on the support, be connected with the pivot on the motor, pivot one end is passed the desk and is upwards extended, pivot and desk contact department are fixed with the connection bearing, the desk top is provided with changes the board, and changes and be connected through coupling mechanism between board bottom and the pivot, it all is provided with the bull stick to change board top both sides, the slide opening has all been seted up to change the board both sides, the bull stick below is fixed with the slide, and the slide slides and sets up in the slide opening. This softening installation is through fixing almag silk on the bull stick, and the motor is restarted, and the motor can drive the pivot and rotate, and the pivot rotates and just can drive the commentaries on classics board through coupling mechanism and rotate, changes the board and rotates just can make the bull stick twine almag silk.
Description
Technical Field
The utility model relates to an almag silk technical field especially relates to an almag silk's annealing softening installation.
Background
The aluminum-magnesium alloy wire is mainly made of aluminum, and a small amount of magnesium or other metal materials are added to enhance the hardness of the aluminum-magnesium alloy wire. The aluminum alloy wire using magnesium as a main additive element is also called as antirust aluminum alloy because of its good corrosion resistance. Because the metal is metal, the heat conducting property and the strength of the metal are particularly outstanding. The aluminum magnesium alloy wire needs to be softened after annealing, but the existing softening is inconvenient to use.
SUMMERY OF THE UTILITY MODEL
The utility model aims at solving the defect of inconvenient use in the prior art and providing an annealing softening device of aluminum magnesium alloy wires.
In order to achieve the above purpose, the utility model adopts the following technical scheme:
the utility model provides an annealing softening installation of almag silk, includes the table, the table bottom is fixed with the support, install the motor on the support, be connected with the pivot on the motor, pivot one end is passed the table and is upwards extended, pivot and table contact department are fixed with the connection bearing, the table top is provided with changes the board, and changes and be connected through coupling mechanism between board bottom and the pivot, it all is provided with the bull stick to change board top both sides, the slide opening has all been seted up to change board both sides, the bull stick below is fixed with the slide, and the slide slides and set up in the slide opening, the slide opening lateral wall is fixed with the slide bar, slide bar one end is passed the slide and is fixed at another lateral wall of slide opening, the cover is equipped with the spring on the slide bar, spring one end is fixed at the slide opening lateral wall, the spring other end is fixed on the.
Preferably, the bottom of the bracket is fixed with a non-slip mat.
Preferably, coupling mechanism includes sleeve pipe and inserted block, the sleeve pipe is fixed in the bottom of changeing the board, the inserted block is fixed in the one end of pivot, and the inserted block inserts and establish in the sleeve pipe, the sideslip hole has all been seted up to sleeve pipe department all around, the inserted block department all is fixed with the limiting plate all around, and the limiting plate inserts and establishes in the sideslip hole.
Preferably, the rotating rod is provided with anti-skid grains.
Preferably, the spring is in a compressed state.
The utility model provides an annealing softening installation of almag silk, beneficial effect lies in: this softening installation is through fixing the almag silk on the bull stick, and the motor is restarted, and the motor can drive the pivot and rotate, and the pivot rotates and just can drive the commentaries on classics board through coupling mechanism and rotate, changes the board and just can make the bull stick twine the almag silk, because the almag silk twines the atress and can be different, just can make the bull stick move that stretches out and draws back through the spring to this can soften the almag silk.
Drawings
Fig. 1 is a schematic structural view of an annealing and softening device for an aluminum-magnesium alloy wire according to the present invention.
Fig. 2 is a schematic top view of the annealing and softening apparatus for aluminum-magnesium alloy wire according to the present invention.
Fig. 3 is a schematic structural view of a connection mechanism of an annealing and softening device for aluminum magnesium alloy wires according to the present invention.
In the figure: the table comprises a table plate 1, a support 2, an anti-skid pad 3, a motor 4, a connecting mechanism 5, a sleeve 51, an insertion block 52, a side sliding hole 53, a limiting plate 54, a rotating shaft 6, a connecting bearing 7, a rotating plate 8, a sliding hole 9, a sliding plate 10, a rotating rod 11, a sliding rod 12 and a spring 13.
Detailed Description
The technical solutions in the embodiments of the present invention will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only some embodiments of the present invention, not all embodiments.
Example 1
Referring to fig. 1-2, an annealing softening installation of almag silk, including table 1, table 1 bottom is fixed with support 2, support 2 bottom is fixed with slipmat 3, install motor 4 on the support 2, be connected with pivot 6 on the motor 4, 6 one end of pivot is passed table 1 and is upwards extended, pivot 6 is fixed with connection bearing 7 with table 1 contact department, table 1 top is provided with commentaries on classics board 8, and be connected through coupling mechanism 5 between 8 bottoms of commentaries on classics board and the pivot 6, through fixing almag silk on bull stick 11, restart motor 4, motor 4 can drive pivot 6 and rotate, pivot 6 rotates and just can drive commentaries on classics board 8 through coupling mechanism 5 and rotate, commentaries on classics board 8 rotates and just can make bull stick 11 twine almag silk.
Commentaries on classics 8 top both sides all are provided with bull stick 11, anti-skidding line has been seted up on the bull stick 11, slide opening 9 has all been seted up to 8 both sides of commentaries on classics board, 11 below of bull stick is fixed with slide 10, and slide 10 slides and sets up in slide opening 9, slide opening 9 lateral wall is fixed with slide bar 12, slide bar 12 one end is passed slide 10 and is fixed at another lateral wall of slide opening 9, the cover is equipped with spring 13 on slide bar 12, spring 13 one end is fixed at slide opening 9 lateral wall, the spring 13 other end is fixed on slide 10, spring 13 is compression state, because the almag silk carries out the winding atress and can be different, just can make bull stick 11 carry out the concertina removal through spring 13, so that can soften almag silk.
Example 2
Referring to fig. 3, as another preferred embodiment of the present invention, the difference from embodiment 1 lies in that the connecting mechanism 5 includes a sleeve 51 and an insert 52, the sleeve 51 is fixed at the bottom of the rotating plate 8, the insert 52 is fixed at one end of the rotating shaft 6, and the insert 52 is inserted into the sleeve 51, the sleeve 51 has all the side sliding holes 53 all around, the insert 52 has all the limiting plates 54 all around, and the limiting plates 54 are inserted into the side sliding holes 53, and the connecting mechanism 5 can connect the rotating shaft 6 and the rotating plate 8.
The above, only be the concrete implementation of the preferred embodiment of the present invention, but the protection scope of the present invention is not limited thereto, and any person skilled in the art is in the technical scope of the present invention, according to the technical solution of the present invention and the utility model, the concept of which is equivalent to replace or change, should be covered within the protection scope of the present invention.
Claims (5)
1. The utility model provides an annealing softening installation of almag silk, includes table (1), its characterized in that, table (1) bottom is fixed with support (2), install motor (4) on support (2), be connected with pivot (6) on motor (4), pivot (6) one end is passed table (1) and upwards extends, pivot (6) and table (1) contact department are fixed with connection bearing (7), table (1) top is provided with commentaries on classics board (8), and is connected through coupling mechanism (5) between commentaries on classics board (8) bottom and the pivot (6), commentaries on classics board (8) top both sides all are provided with bull stick (11), commentaries on classics board (8) both sides have all been seted up slide opening (9), bull stick (11) below is fixed with slide plate (10), and slide plate (10) slide and set up in slide opening (9), slide opening (9) lateral wall is fixed with slide bar (12), slide bar (12) one end is passed slide plate (10) and is fixed at another lateral wall of slide opening (9), the cover is equipped with spring (13) on slide bar (12), spring (13) one end is fixed at slide opening (9) lateral wall, the spring (13) other end is fixed on slide plate (10).
2. An aluminum magnesium alloy wire annealing and softening device according to claim 1, wherein a non-slip mat (3) is fixed to the bottom of the bracket (2).
3. The annealing and softening device of the aluminum-magnesium alloy wire according to claim 1, wherein the connecting mechanism (5) comprises a sleeve (51) and an insert block (52), the sleeve (51) is fixed at the bottom of the rotating plate (8), the insert block (52) is fixed at one end of the rotating shaft (6), the insert block (52) is inserted into the sleeve (51), side sliding holes (53) are formed in the periphery of the sleeve (51), limiting plates (54) are fixed on the periphery of the insert block (52), and the limiting plates (54) are inserted into the side sliding holes (53).
4. The annealing and softening device of aluminum magnesium alloy wires according to claim 1, wherein the rotating rod (11) is provided with anti-slip lines.
5. An apparatus for annealing and softening an aluminum-magnesium alloy wire according to claim 1, wherein the spring (13) is in a compressed state.