CN211143584U - Spliced microcrystalline glass plate - Google Patents
Spliced microcrystalline glass plate Download PDFInfo
- Publication number
- CN211143584U CN211143584U CN201921738447.3U CN201921738447U CN211143584U CN 211143584 U CN211143584 U CN 211143584U CN 201921738447 U CN201921738447 U CN 201921738447U CN 211143584 U CN211143584 U CN 211143584U
- Authority
- CN
- China
- Prior art keywords
- recess
- groove
- glass board
- glass
- main part
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a concatenation formula microcrystalline glass board in architectural decoration material technical field aims at solving the technical problem that current concatenation formula microcrystalline glass board is not convenient for change, and this glass board includes the glass board main part and sets up the first recess of glass board main part A side the B side of glass board main part is equipped with the second recess corresponding with first recess, and sliding connection has first magnet piece in the second recess. The utility model discloses be equipped with first recess and second recess respectively on the adjacent limit of two adjacent glass boards to sliding connection has first magnet piece in first recess and second recess, makes two adjacent glass boards connect as an organic wholely in sliding into first recess by the second spout through first magnet piece, and the separation of two adjacent glass boards is made in the second recess by first spout is slided into to the rethread first magnet piece, the quick installation and the change of the glass board of being convenient for.
Description
Technical Field
The utility model relates to a glass board concatenation technical field, concretely relates to concatenation formula micrite glass board.
Background
The microcrystalline glass plate has the advantages of high strength, high hardness, smoothness, flatness, thin thickness and the like. For example, chinese patent publication No. CN207892167U discloses "a spliced microcrystalline glass sheet", which comprises a sheet main body, wherein one side of the sheet is provided with a protruding strip, the other side is provided with a groove, the protruding strip and the groove are matched, and the protruding strip is in a horizontal T shape; the glass-ceramic plate of this kind of structure makes two adjacent glass boards connect as an organic wholely in inserting the recess of adjacent glass board through the strip that will stand out, has effectively solved the protruding not hard up problem of glass board, but in the in-service use process, appear damaged back when certain glass board, when needing to be changed the glass board, because two adjacent glass boards connect as an organic wholely, cause the glass board to change the difficulty, need tear all glass boards open and reinstall, the amount of labour is too big, and efficiency is too low.
Therefore, the market is in urgent need of a splicing type microcrystalline glass plate which is convenient to replace.
SUMMERY OF THE UTILITY MODEL
In view of this, the utility model aims at providing a concatenation formula microcrystalline glass board to solve the technical problem that current concatenation formula microcrystalline glass board is not convenient for change.
The utility model discloses the technical scheme who adopts does:
the utility model provides a splice type micrite glass board, includes the glass board main part and sets up the first recess of glass board main part A side the B side of glass board main part is equipped with the second recess corresponding with first recess, and sliding connection has first magnet piece in the second recess.
Preferably, the length of the first magnet block is greater than the groove depth of the first groove and less than or equal to the groove depth of the second groove.
Preferably, the cross sections of the second groove and the first groove are the same, and the groove depth of the second groove is 1.5-2 times that of the first groove.
Preferably, the a side is not adjacent to the B side.
Preferably, the number of the first grooves and the number of the second grooves are 1-3.
Preferably, the side C of glass board main part is equipped with the third recess, the side D of glass board main part is equipped with and corresponds with the third recess and get the fourth recess, and sliding connection has the second magnet piece in the fourth recess.
Compared with the prior art, the utility model has the advantages that:
1. the utility model discloses be equipped with first recess and second recess respectively on the adjacent limit of two adjacent glass boards to sliding connection has first magnet piece in first recess and second recess, make two adjacent glass boards connect as an organic wholely in sliding into first recess by the second spout through first magnet piece, make two adjacent glass board separation in the rethread first magnet piece slides into the second recess by first spout, the quick installation and the change of the glass board of being convenient for, and the protruding not hard up problem of glass board has been solved.
Drawings
Fig. 1 is one of the schematic structural diagrams of the present invention;
fig. 2 is a second schematic structural diagram of the present invention;
FIG. 3 is a reference diagram of the present invention in use;
the glass plate comprises a glass plate main body 1, a first groove 2, a second groove 3, a first magnet block 4, a third groove 5, a fourth groove 6 and a second magnet block 7.
Detailed Description
The following embodiments are only intended to illustrate the present invention in detail, and do not limit the scope of the present invention in any way. The unit module components, structures, mechanisms, sensors and other devices referred to in the following examples are all conventional and commercially available products unless otherwise specified.
Example (b): as shown in fig. 1, a splicing type microcrystalline glass plate comprises a glass plate main body 1, wherein 1-3 first grooves 2 are arranged on the side a of the glass plate main body 1, second grooves 3 corresponding to the first grooves 2 are arranged on the side B of the glass plate main body 1, first magnet blocks 4 are connected in the second grooves 3 in a sliding mode, the length of each first magnet block 4 is larger than the depth of each first groove 2 and smaller than or equal to the depth of each second groove 3, the cross sections of the second grooves 3 and the cross sections of the first grooves 2 are the same, and the depth of each second groove 3 is 1.5-2 times that of each first groove 2.
In this embodiment, the a side and the B side are not adjacent, for example, the a side is the left side of the glass plate body 1, and the B side is the right side of the glass plate body 2.
In other embodiments, as shown in fig. 2, a third groove 5 is formed on the side C of the glass plate body 1, a fourth groove 6 corresponding to the third groove 5 is formed on the side D of the glass plate body 1, and a second magnet 7 is slidably connected in the fourth groove 6.
The operation and use method of the glass plate is as follows:
as shown in fig. 3, during installation, the first magnet block 4 is completely slid into the second groove 3, and is fixed on the ground or wall in an aligned manner like a common glass plate, and then the first magnet block 4 is slowly slid into the first groove 2 from the second groove 3 by the magnet placed on the glass plate, so that two adjacent glass plates can be connected into a whole.
Finally, the above embodiments are only used for illustrating the technical solutions of the present invention and not for limiting, and other modifications or equivalent replacements made by the technical solutions of the present invention by those of ordinary skill in the art should be covered within the scope of the claims of the present invention as long as they do not depart from the spirit and scope of the technical solutions of the present invention.
Claims (5)
1. The utility model provides a concatenation formula microcrystalline glass board, includes the glass board main part and sets up the first recess of glass board main part A side, its characterized in that: and a second groove corresponding to the first groove is formed in the side B of the glass plate main body, a first magnet block is connected in the second groove in a sliding mode, and the length of the first magnet block is larger than the groove depth of the first groove and smaller than or equal to the groove depth of the second groove.
2. The spliced microcrystalline glass sheet of claim 1, wherein: the cross sections of the second groove and the first groove are the same, and the groove depth of the second groove is 1.5-2 times that of the first groove.
3. The spliced microcrystalline glass sheet of claim 2, wherein: the A side is not adjacent to the B side.
4. The spliced microcrystalline glass sheet of claim 3, wherein: the number of the first grooves and the number of the second grooves are 1-3.
5. The spliced crystallized glass sheet of any one of claims 1 to 4, wherein: the side C of glass board main part is equipped with the third recess, the side D of glass board main part is equipped with and corresponds the fourth recess with the third recess, and sliding connection has the second magnet piece in the fourth recess.