CN210837914U - Bridge-spanning welding structure for battery inner pole and auxiliary jig thereof - Google Patents

Bridge-spanning welding structure for battery inner pole and auxiliary jig thereof Download PDF

Info

Publication number
CN210837914U
CN210837914U CN201922247329.9U CN201922247329U CN210837914U CN 210837914 U CN210837914 U CN 210837914U CN 201922247329 U CN201922247329 U CN 201922247329U CN 210837914 U CN210837914 U CN 210837914U
Authority
CN
China
Prior art keywords
inner pole
welding
die
pole
gap
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201922247329.9U
Other languages
Chinese (zh)
Inventor
孟祥辉
王玉
潘生泉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hebei Allgrand Power Source Co ltd
Original Assignee
Hebei Allgrand Power Source Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hebei Allgrand Power Source Co ltd filed Critical Hebei Allgrand Power Source Co ltd
Priority to CN201922247329.9U priority Critical patent/CN210837914U/en
Application granted granted Critical
Publication of CN210837914U publication Critical patent/CN210837914U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a bridge-crossing welding structure of battery inner pole and an auxiliary tool thereof, wherein the top of the inner pole is provided with a groove, a secondary step is arranged below the groove, when two ladder inner poles are butted, an inner pole whole body is formed when the two ladder inner poles are combined, through the above structure arrangement, a solder storage tank with a T-shaped structure can be formed between the two ladder inner poles, and then a purpose-made welding clamp is matched, the welding clamp is provided with an inner pole support die, through the opening and closing of the inner pole support die, the support between the bottom surface of the secondary step and a middle partition plate can be effectively realized through a bottom die, when welding is carried out, a gap is arranged between the outer diameter of the inner pole and the inner wall of a counter bore, a gap is also arranged between the two inner poles through the bottom die support, the two gaps exist simultaneously, so that the flame of a, the welding effect is optimal.

Description

Bridge-spanning welding structure for battery inner pole and auxiliary jig thereof
Technical Field
The utility model belongs to the technical field of battery assembly, especially, relate to a bridge welded structure is striden to utmost point post in battery and supplementary tool thereof.
Background
In recent years, with the rapid development of new energy technology, the application field of lead-acid storage batteries is continuously expanded, the demand is greatly increased, and the demand of batteries of various specifications such as electric vehicles, UPS standby power supplies, GFM series and the like is continuously increased. The bridge-spanning structure between the cell clusters inside the battery plays an important role in current transmission and battery life. The bridge welding is striden except that piercing wall welds at present, and interior utmost point post crosses the bridge and welds the structure and have a great deal of problem, and its main manifestation is: the welding contact area is small, the conventional bridge-spanning welding depth is about 4-5mm, the contact area is small, the resistance of a welding part is large, the welding part becomes a bottleneck point of current conduction, local high temperature and fusing phenomena are easily generated, the battery is scrapped, and even the 3C discharge requirement cannot be met; aiming at the defects in the prior art, in order to meet the 3C discharge requirement, the welding area is usually increased by increasing the diameter of an inner pole, increasing the size of a bridge clamp and other measures in the industry at present, so that the 3C discharge requirement is met, but the defect of local high temperature phenomenon caused by the fact that the welding area is smaller than the area of the pole cannot be fundamentally solved all the time by the improvement mode, so that the technical change has hidden quality danger, the cost input is further increased by about 30%, and waste is caused.
Disclosure of Invention
In view of the above shortcoming of prior art, the utility model aims to provide a bridge welded structure is striden to utmost point post in battery and supplementary tool thereof increases the depth of welding through striding bridge welding supplementary tool and adopting the welding method that corresponds, increases the area of contact of welding department, and the heat that the balanced current switched on the production promotes battery life-span.
The utility model provides a technical scheme that its technical problem adopted is:
a bridge-spanning welding structure of battery inner pole columns and an auxiliary jig thereof are disclosed, wherein each busbar is provided with a step-shaped inner pole column, the top of each step-shaped inner pole column is provided with a groove, a secondary step is arranged below the groove, when the two step-shaped inner pole columns are butted and combined with each other, an inner pole column whole body is formed, a gap width A is formed in each inner pole column, and the gap width A is 7-10 mm; the distance between the bottom surface of the secondary step and the inner partition plate is B, and the distance B is 3-5 mm;
a gap C is formed between the whole inner pole and the side face of the partition plate in the shell, and the gap C is 1.5-2 mm and is used for filling sealant;
the welding tongs are matched with the stepped internal pole for use, an internal pole supporting die in an openable design is arranged at the end part of the welding tongs, the internal pole supporting die consists of two supporting die bodies, the two parts are respectively welded on the jaws of the welding tongs, and the welding tongs can be closed through the action of the jaws; the inner pole support die is characterized in that half counter bores are arranged inside the inner pole support die, each half counter bore is provided with a bottom through hole, the bottom through holes are divided into two parts by a bottom die, the bottom through holes are used for enabling the inner poles to vertically penetrate through, and the bottom die is used for supporting the secondary step bottom surface to the middle partition plate; the bottom of the counter bore is provided with a blocking edge for blocking the solder above from infiltrating downwards.
And after the inner pole penetrates through the counter bore, a welding gap is formed between the outer diameter of the inner pole and the inner wall of the counter bore.
The welding tongs comprise three parts, including a tong handle in a hinged design, wherein a tong opening at the front end of the tong handle is provided with an arc-shaped block, the arc-shaped block is used for connecting the inner pole support die and the tong opening into a whole, and the angle D of the tong handle after being combined with the inner pole support die is 120-145.
The inner pole support die is made of high-temperature-resistant metal.
The utility model discloses following beneficial effect has: through the design, the utility model is provided with a groove at the top of the inner pole, a secondary step is arranged below the groove, when the two stepped internal poles are butted and then combined, an internal pole whole body is formed, and through the structure arrangement, a solder storage tank with a T-shaped structure can be formed between the two, and the structure is arranged and matched with a special welding clamp, an inner pole support die is arranged on the welding clamp, the bottom die can be effectively used for realizing the support from the bottom surface of the secondary step to the middle partition plate through the opening and closing of the inner pole support die, when welding, a gap is formed between the outer diameter of the inner pole and the inner wall of the counter bore, a gap is also formed between the two inner poles through bottom die support, and welding gun flame can enter the inner part due to the two gaps, so that the inner and outer welding temperatures are uniform, and the welding effect is optimal.
Through the design of the scheme, in the improved bridge-crossing welding structure of the inner polar columns of the battery cluster, the inherent characteristics of the traditional oblique welding structure are overcome, and through the matching of the structure and instruments, the two parts of inner polar columns are integrated in a mold cavity to achieve a complete fusion state and ensure the requirement of a required fusion surface; moreover, because of the design of the size of the mould, a sealant gap is reserved among the inner pole, the inner partition plate and the sealing groove of the shell, so that the sealing is firm and the air leakage is prevented.
Drawings
The present invention will be further explained with reference to the drawings and examples.
Fig. 1 is a schematic perspective view of the present invention;
fig. 2 is a schematic top view of the solution of the present invention;
fig. 3 is a schematic view of the fit structure of the inner pole and the inner pole support mold according to the present invention;
FIG. 4 is a schematic view of a three-dimensional structure of a welding tongs according to the present invention;
FIG. 5 is a schematic view of the structure of the inner pole column combined with the sealing groove of the housing according to the present invention;
FIG. 6 is a schematic view of the overall bonding angle of the welding tongs;
in the figure, 1, a battery case, 2, a cluster, 3, a bus bar, 4, an inner pole, 5, welding tongs, 6, a tongs handle, 7, an arc block, 8, an inner pole supporting die, 81, a supporting die body, 82, a counter bore, 83, a bottom die, 84, a blocking edge, 85, a bottom through hole, 9, an inner partition plate, 10, a welding gap, 11, a groove, 12, a secondary step, 13, a middle welding gap, 14 and a shell sealing groove.
Detailed Description
The invention will be further described by means of embodiments,
the utility model provides a bridge welded structure is striden to utmost point post in battery and supplementary tool thereof, as shown in fig. 1 and fig. 2, battery case 1 is inside to be provided with the multiunit cluster, and the top of every cluster 2 is provided with a busbar 3, as shown in the figure, all is provided with an utmost point post 4 on every busbar 3, and what this scheme provided is exactly about the welding of utmost point post in.
Before improvement, the inner pole structure is welded, two gaps which are larger than or equal to 2mm appear at the bottom of the inner pole 4, so that the upper surface fusion and root pseudo-welding phenomena are formed (the larger the reserved quantity is, the larger the pseudo-welding depth is). The internal defects are not easy to find, and the welding quality is seriously influenced. The main reasons for this are: when the flame just contacts the top surface of the inner pole 4, the surface lead layer instantly melts, levels and fills the gap of the mold, because the deep layer of the lead piece and the temperature of the mold are lower (the temperature of the mold is always less than or equal to 100 degrees), the filled part of lead liquid is cooled when meeting the cold, and is layered with the workpieces on two sides, and the upper part of the lead piece is gradually and completely melted and combined with the workpieces on two sides along with the lengthening of the welding time. The main reason is that the top and the bottom of the inner pole column are heated differently and the heating temperature is different.
The improvement technology of the scheme is as follows:
the top of the step-shaped inner pole 4 is provided with a groove 11, a secondary step 12 is arranged below the groove 11, when the two inner poles 4 are butted and combined with each other, a cylindrical inner pole is formed, a gap width A is formed in the inner part of the inner pole 4, the gap width A is 7-10 mm, and the optimal gap width is 9 mm; the distance between the bottom surface of the secondary step and the inner baffle 9 is B, the distance B is 3-5mm, and the best distance is 4 mm.
Further, as shown in fig. 5, a gap C is formed between the whole inner pole 4 and the side surface of the partition plate 9 in the housing, wherein the gap C is a gap of 1.5-2 mm, and the gap C is used for filling sealant and is optimally 2 mm.
The improvement of utmost point post structure in realizing above technique, the following improvement that is the supplementary tool of welding:
the welding tongs 5 is matched with the stepped inner pole 4 for use, the end part of the welding tongs 5 is provided with an inner pole supporting die 8 which can be opened and closed, the inner pole supporting die is made of high-temperature-resistant metal materials, the inner pole supporting die 8 consists of two supporting die bodies 81, the two parts are respectively welded on jaws of the welding tongs 5, and the welding tongs can be closed through the action of the tongs handle 6; the inner pole support die 8 is internally provided with half counter bores 82, each half counter bore 82 is provided with a bottom through hole 85, a bottom die 83 divides the bottom through hole 85 into two parts, the bottom through hole 85 is used for enabling the inner pole to vertically penetrate through, the bottom die 83 is used for supporting the secondary step bottom surface and the middle partition plate, the bottom of the counter bore 82 is provided with a blocking edge 84, the blocking edge 84 is used for blocking the upper solder from penetrating downwards, a welding gap 10 is formed in the area above the blocking edge during welding, and a solder molten pool is formed through the welding gap 10;
in order to be more convenient for an operator to use, the welding tongs 5 comprises three parts, including a tong handle 6 in a hinged design, wherein a tong opening at the front end of the tong handle 6 is provided with an arc-shaped block 7, the arc-shaped block 7 is used for connecting the inner pole support die 8 and the tong opening into a whole, as shown in fig. 6, the angle formed by combining the tong handle 6 and the inner pole support die 8 is 120-145, 135 is the best, and the structure arrangement is more convenient for the operator to carry out handheld operation.
When the utility model is in operation, the butt joint part of the inner pole adopts step transition, and the secondary step 12 is respectively made at the position 4mm away from the bottom of the middle clapboard, namely the position with the size B, and the butt joint width A is increased to 9 mm; before welding, the inner pole is clamped and fixed by the welding clamp 5, a T-shaped solder storage tank is formed between the two, the welding tongs 5 is provided with an inner pole support die 8, and through the opening and closing of the inner pole support die 8, the bottom die 83 can be effectively supported from the bottom surface of the secondary step to the middle partition plate, when in welding, a gap is arranged between the outer diameter of the inner pole and the inner wall of the counter bore 82, a middle welding gap 13 is also arranged between the two inner poles supported by the bottom die 83, the two gaps exist simultaneously, the flame of a welding gun can enter the inner part, the inner and outer welding temperatures are uniform, the flame can completely extend into a 9mm space, the lead material at the bottom can be fused instantly, then continuously pouring the lead around the flame into the middle molten pool along with the melting of the lead around the flame, and continuously filling the lead to form a cylindrical melting point with the depth of more than or equal to 7mm to fill the solder storage tank with the T-shaped structure. The utility model discloses the technique has overcome traditional welding root and has melted impervious pseudo-welding phenomenon. Different flame sizes can be adjusted according to different requirements, welding of different depths is achieved, and different welding areas are achieved.
Through the design of the scheme, in the improved bridge-crossing welding structure of the inner polar columns of the battery cluster, the inherent characteristics of the traditional oblique welding structure are overcome, and through the matching of the structure and instruments, the two parts of inner polar columns are integrated in a mold cavity to achieve a complete fusion state and ensure the requirement of a required fusion surface; moreover, due to the design of the size of the mold, a sealant gap is reserved between the inner pole, the inner partition plate and the casing sealing groove 14, so that the sealing is firm, and the air leakage is prevented.

Claims (2)

1. The utility model provides a bridge welded structure is striden to utmost point post in battery and supplementary tool thereof, its all is provided with the interior utmost point post of a echelonment on every busbar, its characterized in that: the top of the stepped inner pole is provided with a groove, a secondary step is arranged below the groove, the two stepped inner poles are butted and then combined to form an inner pole whole, a gap width A is formed in the inner pole, and the gap width A is 7-10 mm; the distance between the bottom surface of the secondary step and the inner partition plate is B, and the distance B is 3-5 mm;
a gap C is formed between the whole inner pole and the side face of the partition plate in the shell, and the gap C is 1.5-2 mm and is used for filling sealant;
the welding tongs are matched with the stepped internal pole for use, an internal pole supporting die in an openable design is arranged at the end part of the welding tongs, the internal pole supporting die consists of two supporting die bodies, the two parts are respectively welded on the jaws of the welding tongs, and the welding tongs can be closed through the action of the jaws; the inner pole support die is characterized in that half counter bores are arranged inside the inner pole support die, each half counter bore is provided with a bottom through hole, the bottom through holes are divided into two parts by a bottom die, the bottom through holes are used for enabling the inner poles to vertically penetrate through, and the bottom die is used for supporting the secondary step bottom surface to the middle partition plate; a blocking edge is arranged at the bottom of the counter bore to block the solder above from infiltrating downwards;
and after the inner pole penetrates through the counter bore, a welding gap is formed between the outer diameter of the inner pole and the inner wall of the counter bore.
2. The battery inner pole bridging welding structure and the auxiliary jig thereof according to claim 1, wherein: the welding tongs comprise three parts, including a tong handle in a hinged design, wherein a tong opening at the front end of the tong handle is provided with an arc-shaped block, the arc-shaped block is used for connecting the inner pole support die and the tong opening into a whole, and the angle D of the tong handle after being combined with the inner pole support die is 120-145.
CN201922247329.9U 2019-12-06 2019-12-06 Bridge-spanning welding structure for battery inner pole and auxiliary jig thereof Active CN210837914U (en)