CN209812851U - Rubber refining roller - Google Patents
Rubber refining roller Download PDFInfo
- Publication number
- CN209812851U CN209812851U CN201920424095.8U CN201920424095U CN209812851U CN 209812851 U CN209812851 U CN 209812851U CN 201920424095 U CN201920424095 U CN 201920424095U CN 209812851 U CN209812851 U CN 209812851U
- Authority
- CN
- China
- Prior art keywords
- pipe
- cooling
- water
- rotor
- cylindrical part
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a rubber refining roller, which comprises a rotor, wherein the rotor comprises a body with a cylindrical part and a rib spirally arranged on the outer peripheral surface of the cylindrical part, a cooling cavity is formed between the rib and the cylindrical part, a cooling pipe is welded on the inner wall of the rib, and the cooling pipe spirally surrounds along the outer side of the cylindrical part; an inner cavity is arranged in the body, extends along the axial direction of the rotor and is provided with a cavity opening on the end surface of one end of the rotor; the cooling pipe is a half pipe, and a channel for cooling water to flow is formed between the half pipe and the rib; the inner cavity is provided with a water inlet pipe and a water outlet pipe, the water inlet pipe is communicated with a water inlet of the cooling pipe, the water outlet pipe is communicated with a water outlet of the cooling pipe, the outer side of the cavity opening is provided with a double-channel rotary joint, and the water inlet pipe and the water outlet pipe are respectively communicated with a channel. The temperature of bead can be reduced effectively in this application, and produced heat is taken away when will smelt the glue, can suitably improve the speed and the pressure of smelting the roller, improves production efficiency.
Description
Technical Field
The utility model relates to a part of rubber refining equipment, concretely relates to a rubber smelts roller that is used for extruding rubber in the banbury mixer.
Background
In the rubber product production process, need refine the crude rubber, be called and smelt gluey, at the gluey in-process, the heat that refining roller department produced is the most, be difficult to distribute away relatively fast, for distributing away the produced heat of refining in-process, set up the shower in the inner chamber of refining roller, cool off the inner wall of refining roller, take away the heat through the cooling water, but because refining roller is in the rotation, the shower is relatively poor to the cooling effect of the roll body when being in upper portion, cause holistic cooling effect relatively poor, restricted the refining in-process, the rotational speed and the pressure of refining roller, influence the efficiency of smelting gluey.
SUMMERY OF THE UTILITY MODEL
An object of the utility model is to overcome above-mentioned defect, provide a can improve the roller of smelting of cooling effect to improve and smelt gluey efficiency, specific technical scheme is:
a rubber refining roller comprises a rotor, wherein the rotor comprises a body with a cylindrical part and ribs spirally arranged on the outer circumferential surface of the cylindrical part, a cooling cavity is formed between each rib and the cylindrical part, cooling pipes are welded on the inner walls of the ribs and spirally surround along the outer side of the cylindrical part; an inner cavity is arranged in the body, extends along the axial direction of the rotor and is provided with a cavity opening on the end surface of one end of the rotor; the cooling pipe is a half pipe, and a channel for cooling water to flow is formed between the half pipe and the inner wall of the convex rib;
a water inlet pipe and a water outlet pipe are arranged in the inner cavity, a first inlet end and a first outlet end are respectively formed at two ends of the water inlet pipe, and a second inlet end and a second outlet end are respectively formed at two ends of the water outlet pipe; the first outlet end is communicated with a water inlet of the cooling pipe, and the second inlet end is communicated with a water outlet of the cooling pipe; and a rotary joint with two channels is arranged outside the cavity opening, a first inlet end is communicated with one channel of the two channels, and a second outlet end is communicated with the other channel of the two channels. Preferably, the rib is welded to the outer circumferential surface of the cylindrical portion.
In this application, the mode that adopts the independent setting forms the bead at the surface of body, this bead is used for extrudeing the refining to the crude rubber, weld the cooling tube on the inner wall of bead, the cooling tube is half a pipe, be about to the pipeline divide into two halves back along the axis direction, weld two sides of half a pipe on the inner wall of bead, make the flow channel who forms the cooling water between the inner wall of half a pipe and bead, because the cooling water is restricted in a narrow and small cavity, can directly cool off the bead, can take away the produced heat of elastomeric in-process fast, in order to reduce the temperature of bead, because can directly take away the produced heat when extruding the crude rubber fast, can suitably improve the speed and the pressure of refining the roller, in order to improve production efficiency.
Furthermore, in order to facilitate installation and adjustment of connection of the water inlet pipe, the water outlet pipe and the cooling pipe, the first outlet end is communicated with the water inlet of the cooling pipe through the first metal soft joint, and the second inlet end is communicated with the water outlet of the cooling pipe through the second metal soft joint. After the metal soft joint is adopted, the expansion amount of the pipeline caused by expansion with heat and contraction with cold can be buffered, and the connection effectiveness of the water inlet pipe, the water outlet pipe and the cooling pipe is ensured.
Furthermore, in order to conveniently position the water inlet pipe and the water outlet pipe during installation, a supporting piece for fixing the water inlet pipe and the water outlet pipe is arranged in the inner cavity of the body.
Description of the drawings:
fig. 1 is a schematic view of an embodiment of the present invention.
The specific implementation mode is as follows:
referring to fig. 1, a rubber refining roller includes a rotor 10, the rotor 10 including a body 11 having a cylindrical part 111 and ribs 21 spirally disposed on an outer circumferential surface of the cylindrical part 111, a cooling chamber 24 being formed between the ribs 21 and the cylindrical part 111, and a cooling pipe 22 welded to an inner wall of the ribs 24, the cooling pipe 22 spirally surrounding along an outer side of the cylindrical part. In this embodiment, the rib is connected to the outer circumferential surface of the cylindrical portion by welding. The cooling pipe 22 is made of a half pipe, and a passage for cooling water to flow is formed between the half pipe and the inner wall of the rib.
An inner cavity 13 is provided in the body 11, the inner cavity 13 extending in the direction of the axis 100 of the rotor and having a cavity opening 131 formed in an end face of one end of the rotor.
A water inlet pipe 31 and a water outlet pipe 33 are arranged in the inner cavity, a first inlet end 311 and a first outlet end 312 are respectively formed at two ends of the water inlet pipe 31, and the first outlet end 312 is communicated with the water inlet of the cooling pipe 22 through a first metal soft joint 23.
The two ends of the water outlet pipe 33 form a second inlet end 331 and a second outlet end 332 respectively; the second inlet end 331 is connected to the outlet of the cooling pipe through a second metal soft joint 25.
The outlet pipe 33 extends along the axis 100, and the inlet pipe 31 is sleeved in the outlet pipe 33 and extends out of the outlet pipe 33 in the middle of the outlet pipe 33. In order to fix the water inlet pipe and the water outlet pipe, a support member 12 is arranged in an inner cavity 13 of the body, the water outlet pipe penetrates through the support member 12 and is supported on the support member, in the embodiment, the support member is a circular ring and is in clearance fit with the inner circumferential surface of the inner cavity, the installation is convenient, and the support member is welded on the water outlet pipe in a spot welding mode.
A rotary joint 40 is arranged outside the cavity opening, and the rotary joint has two channels, namely a first channel 41 and a second channel 42, wherein the water inlet pipe 31 is communicated with the first channel 41, and the water outlet pipe is communicated with the second channel 42.
Claims (4)
1. A rubber refining roller is characterized by comprising a rotor, wherein the rotor comprises a body with a cylindrical part and ribs spirally arranged on the outer peripheral surface of the cylindrical part, a cooling cavity is formed between each rib and the cylindrical part, cooling pipes are welded on the inner walls of the ribs and spirally surround along the outer side of the cylindrical part; an inner cavity is arranged in the body, extends along the axial direction of the rotor and is provided with a cavity opening on the end surface of one end of the rotor; the cooling pipe is a half pipe, and a channel for cooling water to flow is formed between the half pipe and the inner wall of the convex rib;
a water inlet pipe and a water outlet pipe are arranged in the inner cavity, a first inlet end and a first outlet end are respectively formed at two ends of the water inlet pipe, and a second inlet end and a second outlet end are respectively formed at two ends of the water outlet pipe; the first outlet end is communicated with a water inlet of the cooling pipe, and the second inlet end is communicated with a water outlet of the cooling pipe; and a rotary joint with two channels is arranged outside the cavity opening, a first inlet end is communicated with one channel of the two channels, and a second outlet end is communicated with the other channel of the two channels.
2. The rubber mixing roll of claim 1, wherein the first outlet end is in communication with a water inlet of the cooling pipe via a first metal flexible joint and the second inlet end is in communication with a water outlet of the cooling pipe via a second metal flexible joint.
3. The rubber mixing roll of claim 1, wherein a support member is disposed in the inner cavity of the body for securing the inlet and outlet conduits.
4. The rubber mixing roll according to claim 1, wherein the rib is welded to the outer peripheral surface of the cylindrical portion.