CN209441051U - Quick-drying papery printing film - Google Patents

Quick-drying papery printing film Download PDF

Info

Publication number
CN209441051U
CN209441051U CN201821601688.9U CN201821601688U CN209441051U CN 209441051 U CN209441051 U CN 209441051U CN 201821601688 U CN201821601688 U CN 201821601688U CN 209441051 U CN209441051 U CN 209441051U
Authority
CN
China
Prior art keywords
layer
basal
basal layer
close
ink
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201821601688.9U
Other languages
Chinese (zh)
Inventor
刘维春
李华
张卫方
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU XINGTONG BIOTECHNOLOGY GROUP Co Ltd
Original Assignee
JIANGSU XINGTONG BIOTECHNOLOGY GROUP Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU XINGTONG BIOTECHNOLOGY GROUP Co Ltd filed Critical JIANGSU XINGTONG BIOTECHNOLOGY GROUP Co Ltd
Priority to CN201821601688.9U priority Critical patent/CN209441051U/en
Application granted granted Critical
Publication of CN209441051U publication Critical patent/CN209441051U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides a kind of quick-drying papery printing film, is related to printing film field.The quick-drying papery printing film; including basal layer; the two sides up and down of the basal layer include removing glue-line, ink-absorbed coated layer, water absorption layer, non-drying glue layer and protective layer; the two sides up and down of the basal layer with removing glue-line close to a side bonds of basal layer, the side of the removing glue-line far from basal layer and ink-absorbed coated layer close to a side bonds of basal layer.The quick-drying papery printing film, moisture absorption in ink is come out, make not containing moisture into the ink of ink-absorbed coated layer, and then makes the ink quick-drying into ink-absorbed coated layer, less operating personnel's waiting time, the current papery printing film of effective solution, by ink print on film after, more moisture is contained in ink, makes the film curing ink of printing can not Quick-air-drying, the ink marks printed on film is caused to be easy to be caused ink marks fuzzy by external influence.

Description

Quick-drying papery printing film
Technical field
The utility model relates to printing film technical field, specially a kind of quick-drying papery printing film.
Background technique
Current papery printing film, by ink print on film after, in ink contain more moisture, make printing Film curing ink can not Quick-air-drying, cause the ink marks printed on film to be easy to be caused ink marks fuzzy by external influence, and And air-dry time is longer, and the print time is caused to increase, and reduces printing effect.
Utility model content
The purpose of the utility model is to provide a kind of structurally reasonable and novel, the papery printing films with quick-drying function.
Technical solution
In order to achieve the above object, the utility model is achieved by the following technical programs: a kind of quick-drying papery printing glue Piece, including basal layer, the two sides up and down of the basal layer include removing glue-line, ink-absorbed coated layer, water absorption layer, non-drying glue layer and guarantor Sheath, the two sides up and down of the basal layer are with removing glue-line close to a side bonds of basal layer, and the removing glue-line is far from base A side bonds of the side and ink-absorbed coated layer of plinth layer close to basal layer, side and water absorption layer of the ink-absorbed coated layer far from basal layer Close to a side bonds of basal layer, side and non-drying glue layer of the water absorption layer far from basal layer are viscous close to the side of basal layer It connects, the side bonds of side of the non-drying glue layer far from basal layer and protective layer close to basal layer.
The water absorption layer includes silicon dioxide layer, alumina layer, polyacrylamide amine layer and polymethylacrylic acid hydrogen layer, described Silicon dioxide layer is close to the side bonds of side and ink-absorbed coated layer far from basal layer of basal layer, and the silicon dioxide layer is far from base A side bonds of the side and alumina layer of plinth layer close to basal layer, side and polypropylene of the alumina layer far from basal layer A side bonds of the amide layer close to basal layer, side of the polyacrylamide amine layer far from basal layer and polymethylacrylic acid hydrogen layer Close to a side bonds of basal layer, side and non-drying glue layer of the polymethylacrylic acid hydrogen layer far from basal layer are close to basal layer A side bonds.
The protective layer includes antistatic backing, waterproof layer, damp-proof layer and wearing layer, and the antistatic backing is close to basal layer The side bonds of side and non-drying glue layer far from basal layer, side and waterproof layer of the antistatic backing far from basal layer are close to base One side bonds of plinth layer, side of the waterproof layer far from basal layer and damp-proof layer close to basal layer a side bonds, it is described anti- The side bonds of side of the damp layer far from basal layer and wearing layer close to basal layer.
Further, the basal layer be pure wood pulp paper substrate, and basal layer with a thickness of 20 microns or 25 Micron.
Further, the inside of the basal layer includes enhancement layer, and the surface of the enhancement layer and the inner wall of basal layer are viscous It connecing, the enhancement layer includes high-intensitive layer and talcum bisque, and the bottom of the high intensity layer is Nian Jie with the inner wall bottom of basal layer, The top of the high intensity layer is Nian Jie with the bottom of talcum bisque, viscous at the top of the top of the talcum bisque and the inner wall of basal layer It connects.
Further, the high-intensitive layer is any one in carbon fiber layer and polyimide layer.
Further, the thickness of the silicon dioxide layer, alumina layer, polyacrylamide amine layer and polymethylacrylic acid hydrogen layer Than for 1:1:1:1.
Further, side of the wearing layer far from basal layer includes extinction layer, and the wearing layer is far from basal layer Close to a side bonds of basal layer, the extinction layer is nano oxidized silicon coating for side and extinction layer.
1, the quick-drying papery printing film, by be arranged water absorption layer, water absorption layer respectively by silicon dioxide layer, alumina layer, Polyacrylamide amine layer and polymethylacrylic acid hydrogen layer are constituted, in silicon dioxide layer, alumina layer, polyacrylamide amine layer and poly- methyl Under the mating reaction of acrylic acid hydrogen layer, the moisture absorption in ink is come out, makes not containing water into the ink of ink-absorbed coated layer Point, and then make the ink quick-drying into ink-absorbed coated layer, less operating personnel's waiting time, the current papery of effective solution is beaten Print film, by ink print on film after, in ink contain more moisture, make printing film curing ink can not quick wind It is dry, cause the ink marks printed on film to be easy it is fuzzy to be caused ink marks, and air-dry time is longer, causes by external influence Print time increases, and reduces printing effect.
2, the quick-drying papery printing film is made by setting removing glue-line convenient for separating basal layer and ink-absorbed coated layer Basal layer is used multiple times, moreover, making film face have antistatic, waterproof, moisture-proof and wear-resisting function by setting protective layer Can, so that the normal service life of the film is improved, meanwhile, by the way that enhancement layer is arranged, there is basal layer high-intensitive and flexible Property, effectively raise the normal service life of basal layer.
Detailed description of the invention
FIG. 1 is a schematic structural view of the utility model;
Fig. 2 is the structural schematic diagram of the utility model water absorption layer;
Fig. 3 is the structural schematic diagram of the utility model protective layer;
Fig. 4 is the structural schematic diagram of the utility model basal layer.
Wherein, 1 basal layer, 2 removing glue-lines, 3 ink-absorbed coated layers, 4 water absorption layers, 41 silicon dioxide layers, 42 alumina layers, 43 are gathered Acrilamide layer, 44 polymethylacrylic acid hydrogen layers, 5 non-drying glue layers, 6 protective layers, 61 antistatic backings, 62 waterproof layers, 63 damp-proof layers, 64 wearing layers, 7 enhancement layers, 71 high-intensitive layers, 72 talcum bisques, 8 extinction layers.
Specific embodiment
As shown in Figs 1-4, the utility model embodiment provides a kind of quick-drying papery printing film, including basal layer 1, basis Layer 1 is pure wood pulp paper substrate, and basal layer 1 with a thickness of 20 microns or 25 microns, the inside of basal layer 1 includes increasing Strong layer 7, the surface of enhancement layer 7 is Nian Jie with the inner wall of basal layer 1, and enhancement layer 7 includes high-intensitive layer 71 and talcum bisque 72, high-strength The bottom for spending layer 71 is Nian Jie with the inner wall bottom of basal layer 1, and high-intensitive layer 71 is any in carbon fiber layer and polyimide layer One kind makes the intensity with higher of basal layer 1, effectively enhances the normal use of basal layer 1 by the way that high-intensitive layer 71 is arranged The top in service life, high-intensitive layer 71 is Nian Jie with the bottom of talcum bisque 72, the top of talcum bisque 72 and the inner wall top of basal layer 1 Portion's bonding makes the flexibility with higher of basal layer 1, is convenient for operating personnel that basal layer 1 is curved by the way that talcum bisque 72 is arranged Song, the two sides up and down of basal layer 1 include removing glue-line 2, ink-absorbed coated layer 3, water absorption layer 4, non-drying glue layer 5 and protective layer 6, basis The two sides up and down of layer 1 with removing glue-line 2 close to a side bonds of basal layer 1, remove side of the glue-line 2 far from basal layer 1 with Ink-absorbed coated layer 3 removes glue-line 2 by setting, convenient for separating basal layer 1 with ink-absorbed coated layer 3 close to a side bonds of basal layer 1 It opens, is used multiple times basal layer 1, side of the ink-absorbed coated layer 3 far from basal layer 1 and water absorption layer 4 are viscous close to the side of basal layer 1 It connects, side of the water absorption layer 4 far from basal layer 1 and non-drying glue layer 5 are close to a side bonds of basal layer 1, and non-drying glue layer 5 is far from basis The side of layer 1 is with protective layer 6 close to a side bonds of basal layer 1.
Water absorption layer 4 includes silicon dioxide layer 41, alumina layer 42, polyacrylamide amine layer 43 and polymethylacrylic acid hydrogen layer 44, side and ink-absorbed coated layer 3 side bonds far from basal layer 1 of the silicon dioxide layer 41 close to basal layer 1, silicon dioxide layer 41 Far from basal layer 1 side and alumina layer 42 close to basal layer 1 a side bonds, alumina layer 42 far from basal layer 1 one Side is with polyacrylamide amine layer 43 close to a side bonds of basal layer 1, side of the polyacrylamide amine layer 43 far from basal layer 1 and poly- first Base acrylic acid hydrogen layer 44 close to basal layer 1 a side bonds, side of the polymethylacrylic acid hydrogen layer 44 far from basal layer 1 with do not do A side bonds of the glue-line 5 close to basal layer 1, silicon dioxide layer 41, alumina layer 42, polyacrylamide amine layer 43 and polymethyl The thickness ratio of sour hydrogen layer 44 is 1:1:1:1, and by the way that water absorption layer 4 is arranged, water absorption layer 4 is respectively by silicon dioxide layer 41, alumina layer 42, polyacrylamide amine layer 43 and polymethylacrylic acid hydrogen layer 44 are constituted, in silicon dioxide layer 41, alumina layer 42, polyacrylamide Under the mating reaction of amine layer 43 and polymethylacrylic acid hydrogen layer 44, the moisture absorption in ink is come out, makes to enter ink-absorbed coated layer 3 Ink in do not contain moisture, and then make the ink quick-drying into ink-absorbed coated layer 3, less operating personnel's waiting time.
Protective layer 6 includes antistatic backing 61, waterproof layer 62, damp-proof layer 63 and wearing layer 64, and antistatic backing 61 is close to basis The side of layer 1 and a side bonds of the non-drying glue layer 5 far from basal layer 1, antistatic backing 61 are polyvinyl chloride layer, and antistatic backing 61 is remote Close to a side bonds of basal layer 1, waterproof layer 62 is that tetrafluoroethene layer waterproof layer 62 is remote for side and waterproof layer 62 from basal layer 1 Side and a side bonds of the damp-proof layer 63 close to basal layer 1 from basal layer 1,63 melamine layer of damp-proof layer, damp-proof layer 63 are remote Close to a side bonds of basal layer 1, wearing layer 64 is synthetic resin layer, passes through setting for side and wearing layer 64 from basal layer 1 Protective layer 6 makes film face have antistatic, waterproof, moisture-proof and wear-resisting functions, to improve the normal use longevity of the film Life, side of the wearing layer 64 far from basal layer 1 includes extinction layer 8, and side of the wearing layer 64 far from basal layer 1 is leaned on extinction layer 8 One side bonds of nearly basal layer 1, extinction layer 8 are nano oxidized silicon coating, by the way that extinction layer 8 is arranged, reduce daylight to film It influences, effective solution daylight for a long time, leads to the problem that ink marks is fuzzy on film to film.

Claims (6)

1. a kind of quick-drying papery printing film, including basal layer (1), the two sides up and down of the basal layer (1) include removing glue Layer (2), ink-absorbed coated layer (3), water absorption layer (4), non-drying glue layer (5) and protective layer (6), it is characterised in that: the basal layer (1) Upper and lower two sides are with removing glue-line (2) close to a side bonds of basal layer (1), and removing glue-line (2) is far from basal layer (1) Side and ink-absorbed coated layer (3) close to basal layer (1) a side bonds, side of the ink-absorbed coated layer (3) far from basal layer (1) with A side bonds of the water absorption layer (4) close to basal layer (1), side and non-drying glue layer of the water absorption layer (4) far from basal layer (1) (5) close to a side bonds of basal layer (1), side and protective layer (6) of the non-drying glue layer (5) far from basal layer (1) are close One side bonds of basal layer (1);
The water absorption layer (4) includes silicon dioxide layer (41), alumina layer (42), polyacrylamide amine layer (43) and polymethyl Sour hydrogen layer (44), the silicon dioxide layer (41) is close to the side of basal layer (1) and ink-absorbed coated layer (3) far from basal layer (1) One side bonds, the one of side and alumina layer (42) close basal layer (1) of the silicon dioxide layer (41) far from basal layer (1) Side bonds, the one of side and polyacrylamide amine layer (43) close basal layer (1) of the alumina layer (42) far from basal layer (1) Side bonds, side and polymethylacrylic acid hydrogen layer (44) of the polyacrylamide amine layer (43) far from basal layer (1) are close to basis One side bonds of layer (1), side and non-drying glue layer (5) of the polymethylacrylic acid hydrogen layer (44) far from basal layer (1) are close One side bonds of basal layer (1);
The protective layer (6) includes antistatic backing (61), waterproof layer (62), damp-proof layer (63) and wearing layer (64), it is described prevent it is quiet Side and non-drying glue layer (5) side bonds far from basal layer (1) of the electric layer (61) close to basal layer (1), the antistatic backing (61) side bonds of the side far from basal layer (1) and waterproof layer (62) close basal layer (1), the waterproof layer (62) are separate The side and damp-proof layer (63) of basal layer (1) are close to a side bonds of basal layer (1), and the damp-proof layer (63) is far from basal layer (1) side bonds of the side and wearing layer (64) close to basal layer (1).
2. quick-drying papery printing film according to claim 1, it is characterised in that: the basal layer (1) is pure wood pulp paper Matter substrate, and basal layer (1) with a thickness of 20 microns or 25 microns.
3. quick-drying papery printing film according to claim 1, it is characterised in that: the inside of the basal layer (1) includes The surface of enhancement layer (7), the enhancement layer (7) is Nian Jie with the inner wall of basal layer (1), and the enhancement layer (7) includes high-intensitive layer (71) and talcum bisque (72), the bottom of the high intensity layer (71) is Nian Jie with the inner wall bottom of basal layer (1), the high intensity The top of layer (71) is Nian Jie with the bottom of talcum bisque (72), the top of the talcum bisque (72) and the inner wall of basal layer (1) Top bonding.
4. quick-drying papery printing film according to claim 3, it is characterised in that: the high intensity layer (71) is carbon fiber Layer and any one in polyimide layer.
5. quick-drying papery printing film according to claim 1, it is characterised in that: the silicon dioxide layer (41), oxidation The thickness ratio of aluminium layer (42), polyacrylamide amine layer (43) and polymethylacrylic acid hydrogen layer (44) is 1:1:1:1.
6. quick-drying papery printing film according to claim 1, it is characterised in that: the wearing layer (64) is far from basal layer (1) side includes extinction layer (8), and side and extinction layer (8) of the wearing layer (64) far from basal layer (1) are close to basal layer (1) a side bonds, the extinction layer (8) are nano oxidized silicon coating.
CN201821601688.9U 2018-09-29 2018-09-29 Quick-drying papery printing film Active CN209441051U (en)