CN209349658U - A kind of welding machine jig promoting dry reed tube yield - Google Patents
A kind of welding machine jig promoting dry reed tube yield Download PDFInfo
- Publication number
- CN209349658U CN209349658U CN201821941235.0U CN201821941235U CN209349658U CN 209349658 U CN209349658 U CN 209349658U CN 201821941235 U CN201821941235 U CN 201821941235U CN 209349658 U CN209349658 U CN 209349658U
- Authority
- CN
- China
- Prior art keywords
- reed tube
- dry reed
- sliding block
- pcb board
- bottom plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a kind of welding machine jigs for promoting dry reed tube yield, including a bottom plate, bottom plate is equipped with one for placing the article putting groove of pcb board, bottom plate upper surface is equipped with a sliding block, sliding block is slidably connected with bottom plate upper surface, and sliding block lateral wall is equipped with a positioning mechanism that can be positioned to the dry reed tube being placed on pcb board;The mode that traditional worker is fixed to dry reed tube by hand is changed to that dry reed tube is fixed on the positioning by a fixed device that ensure that dry reed tube is soldered on pcb board be the accuracy of position, it prevents dry reed tube to occur dry reed tube welding in the welding process to be uneven, the phenomenon of front and back skew, to reduce the probability that rupture occurs during installation in dry reed tube, dress does not occur into phenomenon, yield when dry reed tube detection is improved.
Description
Technical field
The utility model relates to dry reed tube welding technology fields more particularly to a kind of welding machine for promoting dry reed tube yield to control
Tool.
Background technique
In traditional mode of production manufacturing process, this that dry reed tube is welded on pcb board will appear dry Huang often in the process
Pipe welds to be uneven or dry reed tube welds to obtain front and back skew, breaks during installation so as to cause dry reed tube
Split, dress not into the phenomenon that, thereby reduce the yield of product;And the positioning people in tradition between dry reed tube and pcb board are
It is by going fixation manually, people also need to weld dry reed tube and pcb board surface by welding set while fixed
It connects, therefore traditional welding process is inconvenient for operation.
Utility model content
Technical problem to be solved by the utility model is to provide a kind of structure is simple, positioning dry reed tube effect is good, positioning
It is not susceptible to the welding machine jig of dry reed tube displacement afterwards.
The technical scheme in the invention for solving the above technical problem are as follows: it is a kind of promoted dry reed tube yield welding machine control
Tool, including a bottom plate, bottom plate are equipped with one for placing the article putting groove of pcb board, and bottom plate upper surface is equipped with a sliding block, sliding block and bottom
Plate upper surface is slidably connected, and sliding block lateral wall is equipped with a positioning mechanism that can be positioned to the dry reed tube being placed on pcb board.
After using the above structure, the utility model has the advantage that with existing structure comparison
Traditional worker is fixed the side of dry reed tube by a kind of welding machine jig of promotion dry reed tube yield of the utility model by hand
Formula is changed to that dry reed tube is fixed on the positioning by a fixed device that ensure that dry reed tube is soldered on pcb board be the essence of position
True property, it is therefore prevented that dry reed tube occurs dry reed tube welding in the welding process and is uneven, the phenomenon of front and back skew, to reduce
The probability that rupture occurs during installation in dry reed tube, dress does not occur into phenomenon improves yield when dry reed tube detection;
The process of traditional dry reed tube welding are as follows: dry reed tube is placed on one end face of pcb board by operator by hand, is being passed through
One electric welding welding with one end face of pcb board by dry reed tube both ends, this operating process is all by operator due to whole process
Dry reed tube is still placed on the position on pcb board by the process gone to have been manually done, therefore either welded, and requires operator certainly
Oneself goes to assess, so the evaluation process will appear mistake often, leading to dry reed tube is certain mistake occur on being soldered to pcb board
Difference so that dry reed tube loses precision in welding, and then is easy to cause dry reed tube to occur rupturing during installation or fill not
The phenomenon that entering;
And the specifically used process of the welding machine jig of dry reed tube yield is promoted in the technical program are as follows: be placed in pcb board
In article putting groove on bottom plate, then dry reed tube is placed in pcb board upper surface close to sliding block one end, the cunning being slidably disposed in sliding slot
Block, sliding block can be slid laterally on the sliding rail in sliding slot, until the limiting groove of sliding block lower end surface slides to above dry reed tube
When, the inner sidewall of limiting groove can fit with dry reed tube lateral wall, and then complete limiting groove to the positioning limit of dry reed tube
Process;After the completion of limiting groove is to dry reed tube positioning, user need to only be welded by electric welding between dry reed tube and pcb board
It connects;
Entire welding process is in addition to last welding process is to need manpower is dynamic to go to handle in the technical program, others behaviour
Make the fixable positioning mechanism of process to go to complete to position, to improve the accuracy of product space, it is therefore prevented that dry reed tube exists
The not accurate phenomenon of appearance position on pcb board, the welding process in the technical program only need operator by electric welding by dry Huang
Pipe both ends are welded with pcb board, if therefore it is that will not lose dry Huang that the welding process, which carries out welding when dry reed tube is positioned,
Welding precision between pipe and pcb board.
As a kind of preferred: positioning mechanism includes being set to sliding block lateral wall first protrusion on one end face of article putting groove, the
One raised lower end surface is equipped with can be to the limiting groove that dry reed tube is positioned;The fit structure of first protrusion and limiting groove is most
Lower bound degree reduces the locating effect that ensure that positioning mechanism to dry reed tube while the jig cost of manufacture, when sliding block slide into it is dry
When above yellow pipe, the first raised lower end surface retention bead can slip over dry reed tube lateral wall and to dry reed tube carry out the adjustment of position with
Positioning, so that being all located at the same position when dry reed tube being soldered on pcb board every time.
As a kind of preferred: bottom plate upper surface is equipped with a sliding slot, and the sliding rail slided for sliding block is equipped in sliding slot, sliding
Rail upper surface is equipped with the block that an anti-limited slip block skids off sliding rail;The cooperation slide construction of sliding block and sliding rail facilitates sliding block in sliding slot
It is inside slid laterally, improves comfort level of user when using the sliding block, the person of being convenient to use is with sliding block to dry Huang
Pipe is positioned, it is therefore prevented that dry reed tube big positional shift occurs when positioning on pcb board, improves dry reed tube and is soldered to PCB
Precision when on plate.
As a kind of preferred: upper end of slide block face, which is additionally provided with, can be adjusted sliding block height and consolidate to what sliding block was positioned
Determine mechanism;For sliding block after carrying out position to dry reed tube and fixing, positioning can be fixed to sliding block by fixed mechanism in user, prevent
Only dry reed tube is because of the phenomenon that sliding out existing displacement of sliding block, sliding block dry reed tube is carried out position it is fixed after to sliding block into
Row positioning can effectively improve the precision of dry reed tube in the welding process.
As a kind of preferred: fixed mechanism is a screw thread tightened-up structure, and screw thread tightened-up structure includes two and is set on sliding block
After first through hole on end face is also threaded with screw in first through hole, and screw lower end may pass through first through hole lower end surface
It is in clamping connection with the bottom surface of sliding slot;The snap-fit of screw and first through hole ensure that sliding block is sliding into suitable position
When, effectively sliding block can be fixed on the positioning, and when sliding block slides into dry reed tube top suitable position, which is needed
It carries out depending on dry reed tube length from main modulation, user is by the screw in rotation first through hole, by screw into first through hole
Rotational slide is carried out, is badly in need of rotary screw after screw passes through first through hole lower end, screw can be slided to sliding slot bottom surface direction, directly
When offseting to screw lower end and sliding slot bottom surface, the frictional force between screw and sliding slot bottom surface will make sliding block can not be on the slide rail
It is slided, process is in clamping connection to sliding block to complete screw.
As it is a kind of preferably: article putting groove inner sidewall is additionally provided with one convenient for users to will weld the pcb board after dry reed tube from setting
The first groove taken out in object slot;The finger of the design person of being convenient to use of first groove will weld dry reed tube by the first groove
Pcb board afterwards takes out out of article putting groove, after pcb board is placed with plant slot, the upper end of the lower end surface of pcb board and the first groove
There are there are cavitys between the upper surface of the lower end surface and the first groove of certain difference in height and pcb board between face, work as user
The pcb board after dry reed tube will be welded by needing when taking out out of article putting groove, only need to by finger close to the bottom surface of the first groove to pcb board
Direction sliding can be taken out pcb board by the cavity between pcb board and the first groove out of article putting groove.
Detailed description of the invention
Fig. 1 is a kind of structural schematic diagram for the welding machine jig for promoting dry reed tube yield of the utility model.
Fig. 2 be the utility model it is a kind of promoted dry reed tube yield welding machine jig in first protrusion and dry reed tube lateral wall it
Between structural schematic diagram.
In figure, 1, bottom plate, 2, pcb board, 3, dry reed tube, 4, positioning mechanism, 5, fixed mechanism, 101, article putting groove, 102, cunning
Block, 103, sliding slot, 104, sliding rail, 105, block, the 106, first groove, the 401, first protrusion, 402, limiting groove, 501, first
Through-hole, 502, screw.
Specific embodiment
It explains with reference to the accompanying drawing to a kind of specific embodiment of the utility model.
Embodiment 1: referring to fig. 2, pcb board is placed in the article putting groove on bottom plate, then dry reed tube is placed in by applicant
Pcb board upper surface is close to sliding block one end, the sliding block being slidably disposed in sliding slot, and sliding block can carry out laterally sliding on the sliding rail in sliding slot
It is dynamic, until the inner sidewall of limiting groove can be with dry reed tube lateral wall when the limiting groove of sliding block lower end surface is slided to above dry reed tube
It fits, and then completes limiting groove to the positioning limit process of dry reed tube;After the completion of limiting groove is to dry reed tube positioning, make
User need to only be welded by electric welding between dry reed tube and pcb board.
Referring to Fig. 1, the technical scheme in the invention for solving the above technical problem are as follows: a kind of to promote dry reed tube yield
Welding machine jig, including a bottom plate 1, bottom plate 1 are equipped with one for placing the article putting groove 101 of pcb board 2, and 1 upper surface of bottom plate is equipped with one
Sliding block 102, sliding block 102 are slidably connected with 1 upper surface of bottom plate, and 102 lateral wall of sliding block is equipped with one can be to being placed on pcb board 2
The positioning mechanism 4 that dry reed tube 3 is positioned.
After using the above structure, the utility model has the advantage that with existing structure comparison
Traditional worker is fixed the side of dry reed tube by a kind of welding machine jig of promotion dry reed tube yield of the utility model by hand
Formula is changed to that dry reed tube is fixed on the positioning by a fixed device that ensure that dry reed tube is soldered on pcb board be the essence of position
True property, it is therefore prevented that dry reed tube occurs dry reed tube welding in the welding process and is uneven, the phenomenon of front and back skew, to reduce
The probability that rupture occurs during installation in dry reed tube, dress does not occur into phenomenon improves yield when dry reed tube detection;
The process of traditional dry reed tube welding are as follows: dry reed tube is placed on one end face of pcb board by operator by hand, is being passed through
One electric welding welding with one end face of pcb board by dry reed tube both ends, this operating process is all by operator due to whole process
Dry reed tube is still placed on the position on pcb board by the process gone to have been manually done, therefore either welded, and requires operator certainly
Oneself goes to assess, so the evaluation process will appear mistake often, leading to dry reed tube is certain mistake occur on being soldered to pcb board
Difference so that dry reed tube loses precision in welding, and then is easy to cause dry reed tube to occur rupturing during installation or fill not
The phenomenon that entering;
And the specifically used process of the welding machine jig of dry reed tube yield is promoted in the technical program are as follows: be placed in pcb board
In article putting groove on bottom plate, then dry reed tube is placed in pcb board upper surface close to sliding block one end, the cunning being slidably disposed in sliding slot
Block, sliding block can be slid laterally on the sliding rail in sliding slot, until the limiting groove of sliding block lower end surface slides to above dry reed tube
When, the inner sidewall of limiting groove can fit with dry reed tube lateral wall, and then complete limiting groove to the positioning limit of dry reed tube
Process;After the completion of limiting groove is to dry reed tube positioning, user need to only be welded by electric welding between dry reed tube and pcb board
It connects;
Entire welding process is in addition to last welding process is to need manpower is dynamic to go to handle in the technical program, others behaviour
Make the fixable positioning mechanism of process to go to complete to position, to improve the accuracy of product space, it is therefore prevented that dry reed tube exists
The not accurate phenomenon of appearance position on pcb board, the welding process in the technical program only need operator by electric welding by dry Huang
Pipe both ends are welded with pcb board, if therefore it is that will not lose dry Huang that the welding process, which carries out welding when dry reed tube is positioned,
Welding precision between pipe and pcb board.
As a kind of preferred: positioning mechanism 4 includes being set to 102 lateral wall of sliding block first on 101 1 end face of article putting groove
Protrusion 401, the first raised 401 lower end surfaces are equipped with can be to the limiting groove 402 that dry reed tube 3 is positioned;First protrusion and limit
The positioning that the fit structure of groove ensure that positioning mechanism to dry reed tube while bottom line reduces the jig cost of manufacture
Effect, when sliding block slides into above dry reed tube, the first raised lower end surface retention bead can slip over dry reed tube lateral wall and to dry
Yellow pipe carries out the adjustment and positioning of position, so that being all located at the same position when dry reed tube being soldered on pcb board every time.
As a kind of preferred: 1 upper surface of bottom plate is equipped with a sliding slot 103, is equipped in sliding slot 103 and is slided for sliding block 102
Dynamic sliding rail 104,104 upper surface of sliding rail are equipped with the block 105 that an anti-limited slip block 102 skids off sliding rail 104;Sliding block and sliding rail are matched
Conjunction slide construction facilitates sliding block and is slid laterally in sliding slot, improves comfort level of user when using the sliding block,
The person of being convenient to use positions dry reed tube with a sliding block, it is therefore prevented that dry reed tube big position occurs when positioning on pcb board
Offset, improves precision when dry reed tube is soldered on pcb board.
As it is a kind of preferably: 102 upper surface of sliding block be additionally provided with 102 height of sliding block can be adjusted and to sliding block 102 into
The fixed mechanism 5 of row positioning;After carrying out position to dry reed tube and fixing, user can carry out sliding block by fixed mechanism sliding block
Stationary positioned prevents dry reed tube because of the phenomenon that sliding out existing displacement of sliding block, in sliding block solid to dry reed tube progress position
Carrying out positioning to sliding block after fixed can effectively improve the precision of dry reed tube in the welding process.
As a kind of preferred: fixed mechanism 5 is a screw thread tightened-up structure, and fixed mechanism 5 includes two and is set on sliding block 102
First through hole 501 on end face is also threaded with screw 502 in first through hole 501, and 502 lower end of screw may pass through first
It is in clamping connection behind 501 lower end surface of through-hole with the bottom surface of sliding slot 103;The snap-fit of screw and first through hole ensure that sliding block
When sliding into suitable position, effectively sliding block can be fixed on the positioning, and when sliding block slides into suitable position above dry reed tube
When setting, which, which needs to regard dry reed tube length, is carried out from main modulation, and user, will by the screw in rotation first through hole
Screw carries out rotational slide into first through hole, is badly in need of rotary screw after screw passes through first through hole lower end, screw can be to cunning
Groove bottom direction sliding, until the frictional force between screw and sliding slot bottom surface will make when screw lower end and sliding slot bottom surface offset
Obtaining sliding block can not be slided on the slide rail, be in clamping connection process to sliding block to complete screw.
As a kind of preferred: 101 inner sidewall of article putting groove is additionally provided with one convenient for users to that will weld the pcb board 2 after dry reed tube 3
The first groove 106 taken out out of article putting groove 101;The finger of the design person of being convenient to use of first groove will by the first groove
Pcb board after welding dry reed tube takes out out of article putting groove, after pcb board is placed with plant slot, the lower end surface of pcb board and first
There are there is sky between the upper surface of the lower end surface and the first groove of certain difference in height and pcb board between the upper surface of groove
Chamber only need to be by finger close to the first groove when user needs to take out the pcb board after welding dry reed tube out of article putting groove
Bottom surface can be taken out pcb board by the cavity between pcb board and the first groove to the sliding of pcb board direction out of article putting groove.
Claims (6)
1. a kind of welding machine jig for promoting dry reed tube yield, including a bottom plate (1), it is characterised in that: the bottom plate (1) is equipped with
One for placing the article putting groove (101) of pcb board (2), and bottom plate (1) upper surface is equipped with a sliding block (102), the sliding block
(102) it is slidably connected with bottom plate (1) upper surface, sliding block (102) lateral wall is equipped with one can be to being placed on pcb board (2)
The positioning mechanism (4) that dry reed tube (3) is positioned.
2. a kind of welding machine jig for promoting dry reed tube yield according to claim 1, it is characterised in that: the positioning mechanism
It (4) include being set to sliding block (102) lateral wall first raised (401) on (101) one end face of article putting groove, first protrusion
(401) lower end surface be equipped with can be to the limiting groove (402) that dry reed tube (3) are positioned.
3. a kind of welding machine jig for promoting dry reed tube yield according to claim 1, it is characterised in that: the bottom plate (1)
Upper surface is equipped with a sliding slot (103), and the sliding rail (104) slided for sliding block (102), institute are equipped in the sliding slot (103)
State the block (105) that sliding rail (104) upper surface skids off sliding rail (104) equipped with an anti-limited slip block (102).
4. a kind of welding machine jig for promoting dry reed tube yield according to claim 1: sliding block (102) upper surface is also set
There is the fixed mechanism (5) that can be highly adjusted to sliding block (102) and be positioned to sliding block (102).
5. a kind of welding machine jig for promoting dry reed tube yield according to claim 4: the fixed mechanism (5) is a screw thread
Tightened-up structure, the first through hole (501) that the fixed mechanism (5) is set on sliding block (102) upper surface including two, described first
It is also threaded with screw (502) in through-hole (501), and the screw (502) lower end may pass through first through hole (501) lower end surface
The bottom surface with sliding slot (103) is in clamping connection afterwards.
6. a kind of welding machine jig for promoting dry reed tube yield according to claim 1: article putting groove (101) inner sidewall is also
The first groove of the taking-up out of article putting groove (101) of the pcb board (2) after dry reed tube (3) will be welded equipped with one
(106)。