CN208843939U - A kind of annealing kiln peep hole - Google Patents

A kind of annealing kiln peep hole Download PDF

Info

Publication number
CN208843939U
CN208843939U CN201821527353.7U CN201821527353U CN208843939U CN 208843939 U CN208843939 U CN 208843939U CN 201821527353 U CN201821527353 U CN 201821527353U CN 208843939 U CN208843939 U CN 208843939U
Authority
CN
China
Prior art keywords
peep hole
hole
annealing kiln
kiln
rectangular section
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201821527353.7U
Other languages
Chinese (zh)
Inventor
邢建
刘锐
程明
易星
李晓
王小博
杨阳
刘愿
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China Triumph International Engineering Co Ltd
Original Assignee
China Triumph International Engineering Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China Triumph International Engineering Co Ltd filed Critical China Triumph International Engineering Co Ltd
Priority to CN201821527353.7U priority Critical patent/CN208843939U/en
Application granted granted Critical
Publication of CN208843939U publication Critical patent/CN208843939U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model belongs to a kind of annealing kiln peep hole in glass annealing process field.Technical solution are as follows: on its side wall that annealing kiln kiln body is arranged in, peep hole surrounding hole wall includes rectangular section and on the inside of the rectangular section, the oared segrne pii that connect with rectangular section.The utility model improves the structure of annealing kiln peep hole, optimizes the observation vision on annealing kiln side wall.

Description

A kind of annealing kiln peep hole
Technical field
The utility model belongs to the observation pore structure on glass annealing process field more particularly to a kind of annealing kiln.
Background technique
Annealing kiln is to the equipment of glass " annealing " on glass production line, it makes the advancing glass tape come out from molten tin bath From 600 DEG C it is controlled be cooled to 70 DEG C, while eliminating or reducing the residual stress of glass, inside of glass plate structure is made to tend to be equal It is even, make it have good mechanical performance.Peep hole on annealing kiln is for the ease of each position situation in observation kiln, including kiln Interior glass, roller, internal air hose, electric heater etc., arrange one on the two sides side wall of the every section kiln body of annealing kiln.? Usual peep hole design structure rectangular hole style in production, under the premise of observation hole site determines, vertical direction is seen It examines visual angle and is generally 0~37 °, horizontal direction observation visual angle is generally 0~58 °, the observing effect in the two angulars field of view Unsatisfactory, viewing blind zone and dead angle are very big.Such as by the observation of kiln body side not it is observed that this side glass edge, will see It must be observed to this side glass edge situation by kiln body other side peep hole;It is seen again because each peep hole horizontal view angle is limited It is smaller to examine range, to see glass any position, it is necessary to which in kiln body to open peep hole, reality is three meters of long kilns of every section more A peep hole is respectively opened in body two sides, and it is overstocked unfavorable to insulation of furnace wall to observe pore size distribution, and appearance is also unsightly.
Utility model content
The purpose of this utility model is by providing a kind of annealing kiln peep hole for improving observation pore structure, optimization annealing Observation vision on kiln side wall.
The basic technical scheme of the utility model are as follows: the side wall of annealing kiln kiln body is arranged in a kind of annealing kiln peep hole On, peep hole surrounding hole wall includes rectangular section and on the inside of the rectangular section, the oared segrne pii that connect with rectangular section.
Based on above-mentioned technical characteristic, oared segrne pii and the angle in face where the hole wall of rectangular section phase the same side are 30 °.
Based on above-mentioned technical characteristic, rectangular section accounts for the 2/3 of the observation hole depth.
Based on above-mentioned basic technical scheme, the hole wall of peep hole is folding shape steel plate, rolls over shape steel plate by plain plate and flanged plate Composition, the flanged plate turn down form horn mouth outward.
Based on above-mentioned technical characteristic: the angle in face is 30 ° where flanged plate and plain plate phase the same side hole wall.
Based on above-mentioned technical characteristic: flanged plate turns down at the 2/3 of observation hole depth, and plain plate accounts for observation hole depth 2/3.The purpose being arranged so is to guarantee side wall heat-preservation cotton thickness.Side wall is made of outside plate, inside steel plate, heat-preservation cotton It is filled between inside and outside steel plate, mainly plays function of heat insulation.
The hole wall of peep hole surrounding in the prior art is changed to folding face by plane by the utility model, horizontal wall surface end to Outer folding edge, peep hole style are changed to flared hole by original rectangular opening, i.e., close to kiln body inside wall consent surrounding seben in side Shape is horn-like.Visual angle effect of optimization is unobvious if the fold angle of flanging section is too small, if the fold angle of flanging section is too It is big then visual angle further expansion can be hindered by turning down crest line.So for the annealing kiln generally used currently on the market, flanging section to Outer 30 ° of fold is the selection of optimization, and the vertical direction observation visual angle to before improving can be improved in vertical direction observation visual angle since then About 1.5 times;About 1.3 times of the horizontal direction observation visual angle to before improving can be improved in horizontal direction observation visual angle;Visual angle is aobvious It writes and expands.
After observation visual angle increases, the range that can be seen by a peep hole is wider, can monitor situation in kiln on a large scale. When occurring to anneal abnormal, for example fried plate problem occurs, when tracking lookup glass rupture source by peep hole, does not have to open all Peep hole can easily see the position of glass rupture, and then quick positioning question by opening several wide angle viewing holes Region.And the edge situation of observer place side glass can not only be seen by wide angle viewing hole, it is deposited before eliminating Vision dead zone, moreover it is possible to observe air hose and electric heater situation inside upper edge that can't see in the past upwards.
Detailed description of the invention
Fig. 1 is the structural profile illustration of annealing kiln peep hole in the utility model embodiment.
Fig. 2 is the signal of rectangular viewing aperture horizontal view angle in the prior art.
Fig. 3 is tubaeform peep hole horizontal view angle schematic diagram in the utility model embodiment.
Fig. 4 is rectangular viewing aperture vertical angle of view schematic diagram in the prior art.
Fig. 5 is tubaeform peep hole vertical angle of view schematic diagram in the utility model embodiment.
Fig. 6 is the visual range variation schematic diagram for observing the vertical angle of view that pore structure improves front and back.
Figure label signal are as follows:
1 plain plate
2 flanged plates
3 annealing kilns
4 air hoses
5 glass
A angle
A ' rectangular viewing aperture horizontal view angle
A is tubaeform peep hole horizontal view angle
B ' rectangular viewing aperture vertical angle of view
B is tubaeform peep hole vertical angle of view
L observes hole depth
Specific embodiment
Specific embodiment of the present utility model is described in further detail with reference to the accompanying drawing.These embodiments are only For illustrating the utility model, and it is not limitation of the utility model.
In the description of the present invention, it should be noted that term " center ", " longitudinal direction ", " transverse direction ", "upper", "lower", The orientation or positional relationship of the instructions such as "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom" "inner", "outside" is It is based on the orientation or positional relationship shown in the drawings, is merely for convenience of describing the present invention and simplifying the description, rather than indicate Or imply that signified device or element must have a particular orientation, be constructed and operated in a specific orientation, therefore cannot understand For limitations of the present invention.In addition, term " first ", " second " are used for description purposes only, and should not be understood as instruction or Imply relative importance.
Fig. 1 is the structural profile illustration of annealing kiln peep hole in the utility model embodiment.Peep hole includes rectangular section With the oared segrne pii for being located on the inside of rectangular section, being connect with rectangular section.In the present embodiment, folding that the hole wall of peep hole is arranged by surrounding Shape steel plate is formed, and folding shape steel plate is made of plain plate 1 and flanged plate 2, and fold forms horn mouth, horn mouth pair to flanged plate 2 outward The inside of kiln body.As a kind of optimization, the included angle A in flanged plate 2 and face where 1 phase the same side hole wall of plain plate can be 30 °.Make For another kind optimization, as shown in Figure 1, setting observation hole depth as L, flanged plate turns down at the 2/3 of observation hole depth L, plain plate Account for the 2/3 of the observation hole depth.
Fig. 2 is the schematic diagram of rectangular viewing aperture horizontal view angle a ' in the prior art;Fig. 3 is loudspeaker in the utility model embodiment The schematic diagram of shape peep hole horizontal view angle a.It is compared by Fig. 2 and Fig. 3, it is of same size in the depth and horizontal segment of peep hole In the case of, tubaeform peep hole horizontal view angle a is obviously bigger than rectangular viewing aperture horizontal view angle a '.
Fig. 4 is the schematic diagram of rectangular viewing aperture vertical angle of view b ' in the prior art;Fig. 5 is loudspeaker in the utility model embodiment Shape peep hole vertical angle of view b schematic diagram.It is compared by Fig. 4 and Fig. 5, in the identical feelings of depth and vertical section height of peep hole Under condition, tubaeform peep hole vertical angle of view b is obviously bigger than rectangular viewing aperture vertical angle of view b '.
Fig. 6 is the visual range variation for observing the vertical angle of view that pore structure improves front and back.The left side is rectangular viewing aperture in Fig. 6 Vertical angle of view b ' sees that the right is that tubaeform peep hole is vertical not entirely positioned at the glass 5 of the air hose 4 of 3 internal upper part of annealing kiln and lower part Visual angle b can see the air hose 4 on full top and the glass 5 of lower part.Dash area shown in Fig. 6 is vision dead zone, rectangular viewing aperture After being optimized for tubaeform peep hole, the horizontal viewable and plumb visible range of the tubaeform peep hole after optimization can be expanded. Scene feedback, this corrective measure substantially improve observing effect, improve emergency operation convenience and working efficiency.
The above is only the preferred embodiment of the utility model, it is noted that for the common skill of the art For art personnel, without deviating from the technical principle of the utility model, several improvement and replacement can also be made, these change It also should be regarded as the protection scope of the utility model into replacement.

Claims (6)

1. a kind of annealing kiln peep hole, is arranged on the side wall of annealing kiln kiln body, it is characterised in that: peep hole surrounding hole Wall includes rectangular section and on the inside of the rectangular section, the oared segrne pii that connect with rectangular section.
2. a kind of annealing kiln peep hole according to claim 1, it is characterised in that: the oared segrne pii and the rectangular section The angle in face is 30 ° where the hole wall of phase the same side.
3. a kind of annealing kiln peep hole according to claim 1 or 2, it is characterised in that: the rectangular section accounts for the observation The 2/3 of hole depth.
4. a kind of annealing kiln peep hole according to claim 1, it is characterised in that: the hole wall of the peep hole is folding shape steel Plate, the folding shape steel plate are made of plain plate (1) and flanged plate (2), and fold forms horn mouth to the flanged plate (2) outward.
5. a kind of annealing kiln peep hole according to claim 4, it is characterised in that: the flanged plate (2) and the flat steel The angle in face is 30 ° where the hole wall of plate (1) phase the same side.
6. a kind of annealing kiln peep hole according to claim 4 or 5, it is characterised in that: the plain plate (1) accounts for the sight Examine the 2/3 of hole depth.
CN201821527353.7U 2018-09-18 2018-09-18 A kind of annealing kiln peep hole Active CN208843939U (en)