CN208750287U - A kind of anti-oxidation hot water pipe of resistance to compression - Google Patents

A kind of anti-oxidation hot water pipe of resistance to compression Download PDF

Info

Publication number
CN208750287U
CN208750287U CN201821435174.0U CN201821435174U CN208750287U CN 208750287 U CN208750287 U CN 208750287U CN 201821435174 U CN201821435174 U CN 201821435174U CN 208750287 U CN208750287 U CN 208750287U
Authority
CN
China
Prior art keywords
layer
reinforcing rib
resistance
compression
oxidation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201821435174.0U
Other languages
Chinese (zh)
Inventor
高翔
徐斌
钱荣芳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Jilong Jing Shui Technology Co Ltd
Original Assignee
Suzhou Jilong Jing Shui Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Jilong Jing Shui Technology Co Ltd filed Critical Suzhou Jilong Jing Shui Technology Co Ltd
Priority to CN201821435174.0U priority Critical patent/CN208750287U/en
Application granted granted Critical
Publication of CN208750287U publication Critical patent/CN208750287U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of anti-oxidation hot water pipes of resistance to compression of water pipe technology field, including flowing water layer, the flowing water layer outer wall is enclosed with buffer layer, the buffer layer is uniformly equipped with reinforcing rib one close to flowing water layer one end, the buffer layer inner cavity is uniformly equipped with the reinforcing rib two to match with reinforcing rib one far from flowing water layer side, rubber pad is mounted between reinforcing rib one and reinforcing rib two described in two adjacent groups, the buffer layer outer wall is enclosed with anti oxidation layer, the insulating layer outer wall is enclosed with resistance to compression layer, resistance to compression layer inner cavity is uniformly equipped with fixed link, reinforcing rib two is by impact close to reinforcing rib one, reinforcing rib two is bonded with reinforcing rib with rubber pad, rubber pad carries out snubber to impact, iron foil protective layer and plastic protective sleeve improve pipe outer wall hardness, fixed link is stablized inside support water pipe, the utility model structure is simple , anti-oxidant, the temperature remains within the normal range, and compressive property is good, is not easy because of foreign impacts and corrosion cracking.

Description

A kind of anti-oxidation hot water pipe of resistance to compression
Technical field
The utility model relates to water pipe technology field, specially a kind of anti-oxidation hot water pipe of resistance to compression.
Background technique
Water pipe is the pipeline that a kind of present family commonly conveys hot and cold water, and present water pipe compressive property is poor, and can not It is under pressure and buffers to the external world, be easy to be pressed down when by ambient pressure, and inoxidizability is not strong, be easy to cause inside Corrosion causes water tube life-span to decline.
Summary of the invention
The purpose of this utility model is to provide a kind of anti-oxidation hot water pipes of resistance to compression, to solve to mention in above-mentioned background technique Out the problem of.
To achieve the above object, the utility model provides the following technical solutions: including flowing water layer, the flowing water layer outer wall packet It is wrapped with buffer layer, close flowing water layer one end is uniformly equipped with reinforcing rib one in the buffer layer inner cavity, and the buffer layer inner cavity is remote The reinforcing rib two to match with reinforcing rib one, reinforcing rib one and reinforcing rib described in two adjacent groups are uniformly installed from flowing water layer side Rubber pad is mounted between two, the buffer layer outer wall is enclosed with anti oxidation layer, and the anti oxidation layer outer wall is enclosed with heat preservation Layer, the insulating layer outer wall are enclosed with resistance to compression layer, and resistance to compression layer inner cavity is uniformly equipped with fixed link, the resistance to compression layer outer wall packet It is wrapped with iron foil protective layer, the iron foil protective layer is connected to plastic protective sleeve by glue connection.
Preferably, the anti oxidation layer includes anti-oxidant set, and the anti-oxidant set inner cavity is installed close to one end of buffer layer There is natural resin layer, the natural resin layer is equipped with drier layer far from buffer layer one end, and the drier layer is far from natural One end of resin layer is equipped with rust resisting pigment layer.
Preferably, rock wool layer is installed in the insulating layer inner cavity, rock wool layer is equipped with poly- ammonia far from anti oxidation layer one end Ester froth bed, polyurethane foam are equipped with expanded pearlite layer far from asbestos layer one end.
Preferably, waterproof layer is installed, and waterproof layer is expanded graphite layer between the anti oxidation layer and insulating layer.
Preferably, the fixed link is reinforcement rod, and reinforcing mat is filled in the gap between fixed link and resistance to compression layer.
Preferably, the plastic protective sleeve outer wall is coated with corrosion-resistant coating, and corrosion-resistant coating is aqueous metallic paint.
Compared with prior art, the utility model has the beneficial effects that being equipped with anti oxidation layer, antioxygen in the water pipe inner cavity To change and is oxidized corrosion inside the anti-antipriming pipe of layer, insulating layer prevents temperature is too low from water pipe being caused to become fragile, so that it is broken water pipe, by When to foreign impacts, reinforcing rib two is by impacting close to reinforcing rib one, and reinforcing rib two is bonded with reinforcing rib with rubber pad, rubber pad Snubber is carried out to impact, iron foil protective layer and plastic protective sleeve improve pipe outer wall hardness, and fixed link stablizes support water pipe Inside, the utility model structure is simple, anti-oxidant, and the temperature remains within the normal range, and compressive property is good, is not easy because of foreign impacts and corrosion cracking.
Detailed description of the invention
FIG. 1 is a schematic structural view of the utility model;
Fig. 2 is the utility model anti oxidation layer structural schematic diagram.
In figure: 1 flowing water layer, 2 reinforcing ribs one, 3 rubber pads, 4 reinforcing ribs two, 5 anti oxidation layers, 51 anti-oxidant sets, 52 are naturally Resin layer, 53 drier layers, 54 rust resisting pigment layers, 6 insulating layers, 7 resistance to compression layers, 8 fixed links, 9 iron foil protective layers, the protection of 10 plastics Set, 11 buffer layers.
Specific embodiment
The following will be combined with the drawings in the embodiments of the present invention, carries out the technical scheme in the embodiment of the utility model Clearly and completely describe, it is clear that the described embodiments are only a part of the embodiments of the utility model, rather than whole Embodiment.Based on the embodiments of the present invention, those of ordinary skill in the art are without making creative work Every other embodiment obtained, fall within the protection scope of the utility model.
The utility model provides a kind of technical solution referring to FIG. 1-2: a kind of anti-oxidation hot water pipe of resistance to compression, including stream Water layer 1,1 outer wall of flowing water layer are enclosed with buffer layer 11, and buffer layer 11 is uniformly equipped with reinforcing rib 1 close to 1 one end of flowing water layer, delay It rushes 11 inner cavity of layer and the reinforcing rib 24 to match with reinforcing rib 1 is uniformly installed far from 1 side of flowing water layer, two adjacent groups are reinforced Rubber pad 3 is mounted between muscle 1 and reinforcing rib 24,11 outer wall of buffer layer is enclosed with anti oxidation layer 5,5 outer wall of anti oxidation layer It is enclosed with insulating layer 6,6 outer wall of insulating layer is enclosed with resistance to compression layer 7, and 7 inner cavity of resistance to compression layer is uniformly equipped with fixed link 8, outside resistance to compression layer 7 Wall is enclosed with iron foil protective layer 9, and iron foil protective layer 9 is connected to plastic protective sleeve 10 by glue connection.
Wherein, anti oxidation layer 5 includes anti-oxidant set 51, and anti-oxidant 51 inner cavity of set is equipped with day close to one end of buffer layer 11 Right resin layer 52, natural resin layer 52 are equipped with drier layer 53 far from 11 one end of buffer layer, and drier layer 53 is far from natural tree One end of rouge layer 52 is equipped with rust resisting pigment layer 54, natural resin layer 52, drier layer 53 and the anti-antipriming pipe of antirusting paint layer 54 Inside, which is oxidized corrosion, causes the service life to shorten;
Rock wool layer is installed in 6 inner cavity of insulating layer, rock wool layer is equipped with polyurethane foam far from 5 one end of anti oxidation layer, Polyurethane foam is equipped with expanded pearlite layer far from asbestos layer one end, and insulating layer 6 prevents ambient temperature is lower from water pipe being caused to become Obtaining fragile easy cracking causes water pipe to damage;
Waterproof layer is installed, and waterproof layer is expanded graphite layer between anti oxidation layer 5 and insulating layer 6, expanded graphite layer is inhaled Water expansion prevents water flowing, water leakage in anti-antipriming pipe;
Fixed link 8 is reinforcement rod, and reinforcing mat is filled in the gap between fixed link 8 and resistance to compression layer 7, reinforcing mat and solid Fixed pole 8 cooperates, and enhances the surface hardness of water pipe and absorbs impact ability, and anti-antipriming pipe, which is pressurized, to crack;
10 outer wall of plastic protective sleeve is coated with corrosion-resistant coating, and corrosion-resistant coating is aqueous metallic paint, and aqueous metallic paint prevents Water tube surfaces are corroded, and water tube life-span is caused to reduce.
Working principle: when water pipe is by foreign impacts, iron foil protective layer 9 and the raising pipe outer wall of plastic protective sleeve 10 are hard Degree, fixed link 8 are stablized inside support water pipe, and reinforcing rib 24 is by impact close to reinforcing rib 1, reinforcing rib 24 and reinforcing rib 1 It is bonded with rubber pad 3,3 pairs of impacts of rubber pad carry out snubber, are oxidized corrosion inside the anti-antipriming pipe of anti oxidation layer 5, keep the temperature Layer 6 prevents temperature is too low from water pipe being caused to become fragile, to be broken.
While there has been shown and described that the embodiments of the present invention, for the ordinary skill in the art, It is understood that these embodiments can be carried out with a variety of variations in the case where not departing from the principles of the present invention and spirit, repaired Change, replacement and variant, the scope of the utility model is defined by the appended claims and the equivalents thereof.

Claims (6)

1. a kind of anti-oxidation hot water pipe of resistance to compression, including flowing water layer (1), it is characterised in that: flowing water layer (1) outer wall is enclosed with Buffer layer (11) is uniformly equipped with reinforcing rib one (2) close to flowing water layer (1) one end in buffer layer (11) inner cavity, described slow It rushes layer (11) inner cavity and the reinforcing rib two (4) to match with reinforcing rib one (2) is uniformly installed far from flowing water layer (1) side, it is adjacent It is mounted between reinforcing rib one (2) and reinforcing rib two (4) described in two groups rubber pad (3), buffer layer (11) the outer wall package Have anti oxidation layer (5), anti oxidation layer (5) outer wall is enclosed with insulating layer (6), and insulating layer (6) outer wall is enclosed with resistance to compression Layer (7), resistance to compression layer (7) inner cavity are uniformly equipped with fixed link (8), and resistance to compression layer (7) outer wall is enclosed with iron foil protective layer (9), the iron foil protective layer (9) is connected to plastic protective sleeve (10) by glue connection.
2. the anti-oxidation hot water pipe of a kind of resistance to compression according to claim 1, it is characterised in that: anti oxidation layer (5) packet It including anti-oxidant set (51), anti-oxidant set (51) inner cavity is equipped with natural resin layer (52) close to one end of buffer layer (11), The natural resin layer (52) is equipped with drier layer (53) far from buffer layer (11) one end, and the drier layer (53) is far from day One end of right resin layer (52) is equipped with rust resisting pigment layer (54).
3. the anti-oxidation hot water pipe of a kind of resistance to compression according to claim 1, it is characterised in that: insulating layer (6) inner cavity In rock wool layer is installed, rock wool layer is equipped with polyurethane foam far from anti oxidation layer (5) one end, and polyurethane foam is far from stone Cotton layer one end is equipped with expanded pearlite layer.
4. the anti-oxidation hot water pipe of a kind of resistance to compression according to claim 1, it is characterised in that: the anti oxidation layer (5) with Waterproof layer is installed, and waterproof layer is expanded graphite layer between insulating layer (6).
5. the anti-oxidation hot water pipe of a kind of resistance to compression according to claim 1, it is characterised in that: the fixed link (8) is steel Muscle bar, and reinforcing mat is filled in the gap between fixed link (8) and resistance to compression layer (7).
6. the anti-oxidation hot water pipe of a kind of resistance to compression according to claim 1, it is characterised in that: the plastic protective sleeve (10) Outer wall is coated with corrosion-resistant coating, and corrosion-resistant coating is aqueous metallic paint.
CN201821435174.0U 2018-09-04 2018-09-04 A kind of anti-oxidation hot water pipe of resistance to compression Expired - Fee Related CN208750287U (en)