CN208359032U - A kind of ceramic powders molding machine mold - Google Patents

A kind of ceramic powders molding machine mold Download PDF

Info

Publication number
CN208359032U
CN208359032U CN201821043972.9U CN201821043972U CN208359032U CN 208359032 U CN208359032 U CN 208359032U CN 201821043972 U CN201821043972 U CN 201821043972U CN 208359032 U CN208359032 U CN 208359032U
Authority
CN
China
Prior art keywords
mold
plate
bottom plate
die
die bottom
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201821043972.9U
Other languages
Chinese (zh)
Inventor
陆剑
曹学刚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Taicang Zhuo Zhi Electronic Equipment Co Ltd
Original Assignee
Taicang Zhuo Zhi Electronic Equipment Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Taicang Zhuo Zhi Electronic Equipment Co Ltd filed Critical Taicang Zhuo Zhi Electronic Equipment Co Ltd
Priority to CN201821043972.9U priority Critical patent/CN208359032U/en
Application granted granted Critical
Publication of CN208359032U publication Critical patent/CN208359032U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of ceramic powders molding machine molds, including die bottom plate, the front of die bottom plate is provided with heating rod, one end of heating rod is provided with electric power connection line, die bottom plate is internally provided with cooling duct, mold mouth and Die and mould plate are respectively arranged at the top of die bottom plate, fixed screw is respectively arranged at the top of Die and mould plate, fixed column and mold slots, one end of fixed screw is provided with nut, die bottom plate is connected with top mold plate by fixed screw, the side of top mold plate is respectively arranged with outlet pipe and filler pipe, feeder is provided at the top of top mold plate, one end of feeder is provided with feed opening, the bottom of top mold plate is respectively arranged with fixed screw mouth and mold inner panel, the outer surface of mold inner panel is provided with fixing port, therefore this kind of die apparatus utilizes its powerful mold mouth, fixed column and heating rod Realize the purpose for preventing from misplacing and improving mold shaping speed.

Description

A kind of ceramic powders molding machine mold
Technical field
The utility model relates to die apparatus technical field, specially a kind of ceramic powders molding machine mold.
Background technique
Mold, in industrial production to be molded, be blow molded, squeeze out, die casting or the methods of forging and forming, smelting, punching press obtain The various moulds and tool of required product, in brief, mold are the tools for making formed article, and this tool is by various Part is constituted, and different molds is made of different parts, it is mainly realized by the change of physical state of the formed material The processing of article shape.
But existing ceramic powders molding machine mold, when making ceramics, internal ceramics at the time of molding some can produce Raw dislocation, leads to the die deformation to form out, and when making forming ceramic, also need to add mold by other equipment Heat allows internal ceramics to form, so that ceramic mold molding is slow.
So how to design a kind of ceramic powders molding machine mold, becoming us will currently be solved the problems, such as.
Utility model content
The purpose of this utility model is to provide a kind of ceramic powders molding machine molds, have at the time of molding to solve ceramics Can lead to the problem of dislocation a bit and ceramic mold form it is slow.
To achieve the above object, the utility model provides the following technical solutions: a kind of ceramic powders molding machine mold, packet Die bottom plate is included, the front of the die bottom plate is provided with heating rod, and one end of the heating rod is provided with electric power connection line, institute The cooling duct that is internally provided with of die bottom plate is stated, mold mouth and Die and mould plate are respectively arranged at the top of the die bottom plate, it is described Fixed screw, fixed column and mold slots are respectively arranged at the top of Die and mould plate, one end of the fixed screw is provided with nut, institute It states die bottom plate and top mold plate is connected with by fixed screw, the side of the top mold plate is respectively arranged with outlet pipe and Jia Shui It manages, is provided with feeder at the top of the top mold plate, one end of the feeder is provided with feed opening, the top mold plate Bottom is respectively arranged with fixed screw mouth and mold inner panel, and the outer surface of the mold inner panel is provided with fixing port.
Further, the feeder is stood vertically at the top of top mold plate, and the feeder is located at top mold plate Center position, while the feeder is through top with top mold plate.
Further, the outer diameter of the fixed column and the internal diameter of fixing port match, and the fixed column and fixing port are living Dynamic connection.
Further, the die bottom plate is process by alloy material, and the smooth outer surface of the die bottom plate, together Shi Suoshu die bottom plate is flexibly connected by fixed screw with top mold plate.
Further, there are four the fixed screw settings, and the length scale of four fixed screws is consistent, simultaneously The fixed screw is closely welded with die bottom plate.
Further, the top mold plate includes in the mold of the feeder and top mold plate bottom at the top of top mold plate Plate, and the mold inner panel is fixedly connected with top mold plate.
Compared with prior art, the utility model has the beneficial effects that this kind of ceramic powders molding machine mold, existing On the basis of device is improved and is promoted, be provided with mold mouth and fixed column, make ceramics when, in top mold plate Mold inner panel is directed at mold mouth, then fixing port alignment and fixation column, then top mold plate is pressed down, mold inner panel and mold The inner wall of mouth will fit closely together, since the inner wall of mold inner panel and mold mouth connects together, make mold top Plate will not driven mold inner panel cannot slide left and right, then made by fixed screw and fixed screw mouth by the extruding of nut Mold inner panel and Die and mould plate fitting together and being fixed tightly, to make top mold plate and die bottom plate that mistake will not occur Position, the mold so to form out would not deform, and be provided with heating rod, when making ceramics, ceramic powders from adding Material mouth is poured into mold, and ceramic powders will be packed together in a model, mold is forming according to internal mold slots When, the electric power connection line on heating rod is connected with power supply line, heating rod, which will give off heat, to be come, and the heat of sending will be transmitted to In top mold plate and die bottom plate, then carrying out heating to ceramic powders comes out ceramic powders firing model, and due to heating The temperature of stick is will to stop heating up after reaching certain temperature, makes the equalized temperature of top mold plate and die bottom plate, makes ceramic powder The last uniform hot briquetting of energy, to accelerate molding speed.
Detailed description of the invention
Fig. 1 is the overall structure diagram of the utility model ceramic powders molding machine mold;
Fig. 2 is the partial structural diagram of the die bottom plate of the utility model ceramic powders molding machine mold;
Fig. 3 is the partial structural diagram of the top mold plate of the utility model ceramic powders molding machine mold;
Fig. 4 is the cross-sectional view of the cooling duct of the utility model ceramic powders molding machine mold.
In figure: 1, fixed screw, 2, nut, 3, feed opening, 4, feeder, 5, top mold plate, 6, outlet pipe, 7, Jia Shui Pipe, 8, die bottom plate, 801, cooling duct, 9, heating rod, 10, electric power connection line, 11, mold mouth, 12, Die and mould plate, 13, fixation Column, 14, mold slots, 15, fixing port, 16, fixed screw mouth, 17, mold inner panel.
The model of heating rod in the utility model embodiment are as follows: BST0001.
Specific embodiment
It is in the description of the present invention, it should be noted that term " center ", "upper", "lower", "left", "right", " perpendicular Directly ", the orientation or positional relationship of the instructions such as "horizontal", "inner", "outside" is to be based on the orientation or positional relationship shown in the drawings, and is only For ease of description the utility model and simplify description, rather than the device or element of indication or suggestion meaning must have it is specific Orientation, be constructed and operated in a specific orientation, therefore should not be understood as limiting the present invention.In addition, term " the One ", " second ", " third " are used for descriptive purposes only and cannot be understood as indicating or suggesting relative importance.
In the description of the present invention, it should be noted that unless otherwise clearly defined and limited, term " is pacified Dress ", " connected ", " connection " shall be understood in a broad sense, for example, it may be being fixedly connected, may be a detachable connection, or integrally Connection;It can be mechanical connection, be also possible to be electrically connected;Can be directly connected, can also indirectly connected through an intermediary, It can be the connection inside two elements.For the ordinary skill in the art, above-mentioned art can be understood with concrete condition The concrete meaning of language in the present invention.
The following will be combined with the drawings in the embodiments of the present invention, carries out the technical scheme in the embodiment of the utility model Clearly and completely describe, it is clear that the described embodiments are only a part of the embodiments of the utility model, rather than whole Embodiment, based on the embodiments of the present invention, those of ordinary skill in the art are without making creative work Every other embodiment obtained, fall within the protection scope of the utility model.
Fig. 1-4 is please referred to, the utility model provides a kind of ceramic powders molding machine mold, including fixed screw 1, nut 2, feed opening 3, feeder 4, top mold plate 5, outlet pipe 6, filler pipe 7, die bottom plate 8, cooling duct 801, heating rod 9, power supply Connecting line 10, mold mouth 11, Die and mould plate 12, fixed column 13, mold slots 14, fixing port 15, fixed screw mouth 16 and mold inner panel 17, die bottom plate 8 is process by alloy material, and the smooth outer surface of die bottom plate 8, while die bottom plate 8 passes through fixation Screw 1 is flexibly connected with top mold plate 5, and the die bottom plate 8 being process by alloy material is more sturdy and durable, die bottom plate 8 Front be provided with heating rod 9, one end of heating rod 9 is provided with electric power connection line 10, and die bottom plate 8 is internally provided with cooling Road 801, the top of die bottom plate 8 are respectively arranged with mold mouth 11 and Die and mould plate 12, and the top of Die and mould plate 12 is respectively arranged with solid Determine screw 1, fixed column 13 and mold slots 14, the internal diameter of the outer diameter and fixing port 15 of fixed column 13 matches, and fixed column 13 with Fixing port 15 is flexibly connected, and fixed column 13 can make mold misplace by being inserted into fixing port 15, and the one of fixed screw 1 End is provided with nut 2, and there are four the settings of fixed screw 1, and the length scale of four fixed screws 1 is consistent, while fixed screw 1 closely welds with die bottom plate 8, and fixed screw 1 can make fixing mould bottom plate 8 for fixing mould bottom plate 8 and top mold plate 5 With snugly even closer of top mold plate 5, die bottom plate 8 is connected with top mold plate 5 by fixed screw 1, and top mold plate 5 is wrapped Include the mold inner panel 17 of 5 bottom of feeder 4 and top mold plate at 5 top of top mold plate, and mold inner panel 17 and top mold plate 5 are fixedly connected, and mold inner panel 17 is for making model use, and mold inner panel 17 is in the mold mouth 11 for being socketed in die bottom plate 8 When, top mold plate 5 can be prevented mobile, the side of top mold plate 5 is respectively arranged with outlet pipe 6 and filler pipe 7, top mold plate 5 Top be provided with feeder 4, feeder 4 is stood vertically at the top of top mold plate 5, and feeder 4 is located at top mold plate 5 Center position, while feeder 4, through the top with top mold plate 5, feeder 4 makes ceramic powders for pouring into ceramic powders Preferably enter in mold, one end of feeder 4 is provided with feed opening 3, and the bottom of top mold plate 5 is respectively arranged with fixed spiral shell Silk mouth 16 and mold inner panel 17, the outer surface of mold inner panel 17 are provided with fixing port 15.
Embodiment one:
Referring to Fig.1-4, firstly, whether each component capabilities of staff's check device are problematic, if finding some what After energy is of poor, it should be repaired or replaced, after each component of device to be checked is normal, device be installed, mold in time Mold inner panel 17 on top plate 5 is directed at mold mouth 11, then 15 alignment and fixation column 13 of fixing port, then down top mold plate 5 The inner wall of pressing, mold inner panel 17 and mold mouth 11 will fit closely together, due to mold inner panel 17 and mold mouth 11 Inner wall connects together, prevent top mold plate 5 will not driven mold inner panel 17 from sliding left and right, then by fixed screw 1 and fixed screw mouth 16 by the extruding of nut 2, make the fitting together and fixing tightly of mold inner panel 17 and Die and mould plate 12 Extremely, ceramic powders are poured into mold from feed opening 3, ceramic powders will be packed together according to internal mold slots 14 In a model, the electric power connection line 10 on heating rod 9 then is connected with power supply line, heating rod 9, which will give off heat, to be come, and is issued Heat will be transmitted in top mold plate 5 and die bottom plate 8, then to ceramic powders carry out heating make ceramic powders be burnt into mould Type comes out, and since the temperature of heating rod 9 is will to stop heating up after reaching certain temperature, makes top mold plate 5 and die bottom plate 8 Equalized temperature, enable the uniform hot briquetting of ceramic powders, after molding out of filler pipe 7 be added water mold is cooled down, Top mold plate 5 and die bottom plate 8 are separately taken out model after cooling, work finishes.
Embodiment two:
Referring to Fig.1-4, firstly, whether each component capabilities of staff's check device are problematic, if finding some what After energy is of poor, it should be repaired or replaced, after each component of device to be checked is normal, device be installed, mold in time Mold inner panel 17 on top plate 5 is directed at mold mouth 11, then 15 alignment and fixation column 13 of fixing port, then down top mold plate 5 The inner wall of pressing, mold inner panel 17 and mold mouth 11 will fit closely together, due to mold inner panel 17 and mold mouth 11 Inner wall connects together, prevent top mold plate 5 will not driven mold inner panel 17 from sliding left and right, then by fixed screw 1 and fixed screw mouth 16 by the extruding of nut 2, make the fitting together and fixing tightly of mold inner panel 17 and Die and mould plate 12 Extremely, ceramic powders are poured into mold from feed opening 3, ceramic powders will be packed together according to internal mold slots 14 In a model, the electric power connection line 10 on heating rod 9 then is connected with power supply line, heating rod 9, which will give off heat, to be come, and is issued Heat will be transmitted in top mold plate 5 and die bottom plate 8, then to ceramic powders carry out heating make ceramic powders be burnt into mould Type comes out, and since the temperature of heating rod 9 is will to stop heating up after reaching certain temperature, makes top mold plate 5 and die bottom plate 8 Equalized temperature, equalized temperature rear mold top plate 5 and die bottom plate 8 it is whole all can heating, so that ceramic powders is uniformly heated Water is added out of filler pipe 7 and cools down to mold, top mold plate 5 and die bottom plate 8 are separately taken after cooling for molding after molding Model out, work finish.
While there has been shown and described that the embodiments of the present invention, for the ordinary skill in the art, It is understood that these embodiments can be carried out with a variety of variations in the case where not departing from the principles of the present invention and spirit, repaired Change, replacement and variant, the scope of the utility model is defined by the appended claims and the equivalents thereof.

Claims (6)

1. a kind of ceramic powders molding machine mold, it is characterised in that: including die bottom plate (8), be installed on the die bottom plate (8) one end of positive heating rod (9), the heating rod (9) is provided with electric power connection line (10), the die bottom plate (8) Be internally provided with cooling duct (801), be respectively arranged with mold mouth (11) and Die and mould plate at the top of the die bottom plate (8) (12), fixed column (13) and mold slots (14), die bottom plate (8) connection are respectively arranged at the top of the Die and mould plate (12) Have top mold plate (5), the side of the top mold plate (5) is respectively arranged with outlet pipe (6) and filler pipe (7), the mold top It is provided at the top of plate (5) feeder (4), one end of the feeder (4) is provided with feed opening (3), the top mold plate (5) Bottom be respectively arranged with fixed screw mouth (16) and mold inner panel (17), the outer surface of the mold inner panel (17) is provided with solid Determine mouth (15).
2. a kind of ceramic powders molding machine mold according to claim 1, it is characterised in that: the feeder (4) is hung down It is directly erected at the tops of top mold plate (5), and the feeder (4) is located at the center position of top mold plate (5), while described added Glassware (4) is through the top with top mold plate (5).
3. a kind of ceramic powders molding machine mold according to claim 2, it is characterised in that: the fixed column (13) Outer diameter and the internal diameter of fixing port (15) match, and the fixed column (13) is flexibly connected with fixing port (15).
4. a kind of ceramic powders molding machine mold according to claim 3, it is characterised in that: the die bottom plate (8) It is process by alloy material, and the smooth outer surface of the die bottom plate (8), while the die bottom plate (8) passes through fixation Screw (1) is flexibly connected with top mold plate (5).
5. a kind of ceramic powders molding machine mold according to claim 4, it is characterised in that: the Die and mould plate (12) Top is provided with fixed screw (1), and one end of the fixed screw (1) is provided with nut (2), fixed screw (1) setting There are four, and the length scale of four fixed screws (1) is consistent, while the fixed screw (1) and die bottom plate (8) are tight Close welding.
6. a kind of ceramic powders molding machine mold according to claim 5, it is characterised in that: the top mold plate (5) Mold inner panel (17) including feeder (4) and top mold plate (5) bottom at the top of top mold plate (5), and in the mold Plate (17) is fixedly connected with top mold plate (5).
CN201821043972.9U 2018-06-29 2018-06-29 A kind of ceramic powders molding machine mold Expired - Fee Related CN208359032U (en)