Utility model content
The purpose of this utility model is to provide a kind of frangible anti-demolition electronic tags, are meeting anti-metal by designing one kind
Under the premise of again with the electronic tag of fragility and tamper, avoid existing electronic tag because it is non-friable and can be by
Original place is pasted go back to once more after complete dismounting, leads to not antitheft problem.
The utility model provides a kind of frangible anti-demolition electronic tags, includes at least: plane materiel, the antenna being sequentially stacked
Layer, foamed cotton layer and ground paper layer;Further include: the first glue-line being located between the plane materiel and the antenna stack is located in institute
The second glue-line between antenna stack and the foamed cotton layer is stated, the third glue being located between the foamed cotton layer and the ground paper layer
Layer.
As an embodiment of the present invention, the frangible anti-demolition electronic tags further include metal film layer and the 4th glue
Layer;The metal film layer is set between the third glue-line and the ground paper layer, and the 4th glue-line is set to the gold
Belong between film layer and the ground paper layer.
As an embodiment of the present invention, the antenna stack includes that radio frequency chip and aluminium sheet etch the signal to be formed and emit
Antenna.
As an embodiment of the present invention, the metal film layer is that aluminium foil, copper foil, nickel film or aluminium copper are thin
Film.
As an embodiment of the present invention, the third glue-line is two-sided sandwich rubber.
As an embodiment of the present invention, the foamed cotton layer is polyethylene foam or ethylene-vinyl acetate c
Object foam.
As an embodiment of the present invention, the plane materiel is polyethylene terephthalate plastics.
As an embodiment of the present invention, the plane materiel is igelite.
As an embodiment of the present invention, the frangible anti-demolition electronic tags edge, which is formed with, to be prevented tearing the edge of a knife.
As an embodiment of the present invention, the thickness of the frangible anti-demolition electronic tags is less than 5mm.
It includes plane materiel, the first glue-line, antenna stack, the second glue-line, foamed cotton layer, third glue that the utility model, which provides a kind of,
Layer, metal film layer, the 4th glue-line and ground paper layer frangible anti-demolition electronic tags, a kind of meeting anti-metal by designing
Under the premise of again with fragility and tamper electronic tag, avoid existing electronic tag because it is non-friable can be complete
The problem that original place can not be antitheft is pasted back after dismounting and again.
Specific embodiment
In order to make the purpose of the utility model, technical solutions and advantages more clearly understood, below in conjunction with attached drawing and implementation
Example, the present invention will be further described in detail.It should be appreciated that specific embodiment described herein is only used to explain
The utility model is not used to limit the utility model.
In the description of the present invention, it should be understood that term " first ", " second " are used for description purposes only, and
It cannot be understood as indicating or implying relative importance or implicitly indicate the quantity of indicated technical characteristic.It defines as a result,
The feature of " first ", " second " can explicitly or implicitly include one or more of the features.
Fig. 1 is the structural schematic diagram of the frangible anti-demolition electronic tags in the utility model embodiment one, can from Fig. 1
Out, the frangible anti-demolition electronic tags in the present embodiment include the plane materiel being sequentially stacked, antenna stack, foamed cotton layer and base stock
Layer;Wherein, it is also folded with the first glue-line between plane materiel and antenna stack, the second glue-line is also folded between antenna stack and foamed cotton layer,
Third glue-line is also folded between foamed cotton layer and ground paper layer.
In the present embodiment, can be made by the third glue-line in frangible anti-demolition electronic tags easy in the utility model
Broken anti-demolition electronic tags are tightly sticked to metal surface, in use, tear ground paper layer, can be by electronics by third glue-line
Label is affixed on article.Specifically, metal has suction-operated, metal pair to electromagnetic signal because radiofrequency signal is electromagnetic signal
Have very big interference effect in radiofrequency signal, by by foamed cotton layer be set to antenna stack and to make between metal article it is frangible
Anti-demolition electronic tags have the characteristics that anti-metal.
Fig. 2 is the structural schematic diagram of the frangible anti-demolition electronic tags in the utility model embodiment two, can from Fig. 2
It arrives, the frangible anti-demolition electronic tags in the present embodiment further include metal film layer and the 4th glue-line, and metal film layer is set to
Between three glue-lines and ground paper layer, the 4th glue-line is also formed between ground paper layer and metal film layer, by the way that metallic film is arranged
Layer, can use the reflectivity of metallic film, radiofrequency signal can be reflected, and avoids metal and penetrates to radio frequency chip reception
The interference of frequency signal.Specifically, in use, tearing ground paper layer, electronic tag can be affixed on by object by the 4th glue-line
On product.
In the present embodiment, foamed cotton layer has the characteristics that frangible, and the foam of use is a kind of to be foamed with plastic pellet
Therefore foamed cotton layer is arranged between the second glue-line and third glue-line in material, so that the foamed cotton layer in frangible anti-demolition electronic tags exists
It can rupture and can not restore in artificial demolishing process, can find that in time electronic tag is moved through by people as a user views it.
As an embodiment of the present invention, the 4th glue-line is hot-fusible pressure-sensitive adhesive.In the present embodiment, due to melt pressure sensitive
Glue be affected by temperature it is larger and to presser sensor, in use slightly firmly can be Nian Jie with adherend, do not need to make
With solvent or other assisted class bonding agents, therefore, antenna stack and plane materiel being glued by hot-fusible pressure-sensitive adhesive in the present embodiment
It is connected together, so that electronic tag is not easy to be torn to pieces in disassembly process.
As an embodiment of the present invention, the first glue-line and the second glue-line all can be hot-fusible pressure-sensitive adhesive, by using
Frangible anti-demolition electronic tags are pasted together by hot-fusible pressure-sensitive adhesive with metal.
As an embodiment of the present invention, antenna stack includes that radio frequency chip and aluminium etch the signal transmitting antenna to be formed.
In the present embodiment, radio frequency chip is for storing data and handle received signal, specifically, radio frequency chip also with
Aluminium etches the signal transmitting antenna to be formed connection, makes aluminium flake can be used as antenna by being patterned etching processing to aluminium flake
Sending and receiving for signal is carried out well.
As an embodiment of the present invention, metal film layer is aluminium foil, copper foil, nickel film, aluminium copper film.At this
In embodiment, metal film layer is aluminium foil, copper foil, nickel film, aluminium copper film, can be used for increasing the read-write of electronic tag
Distance.
As an embodiment of the present invention, third glue-line is two-sided sandwich rubber.Specifically, the two-sided sea in the present embodiment
Continuous glue is using frangible foam as substrate, and on its two sides, coating hot-fusible pressure-sensitive adhesive is made, so that electronic tag is easy in moving process
Stress fragmentation.
As an embodiment of the present invention, foamed cotton layer is polyethylene (polyethylene, PE) foam or ethylene-second
Vinyl acetate copolymer (ethylene-vinyl acetate copolymer, EVA) foam.In the present embodiment, polyethylene
Foam or EVA foam have the advantages that abscess is fine and smooth, environmentally friendly.
As an embodiment of the present invention, plane materiel is polyethylene terephthalate (Polyethylene
Terephthalate, PET) plastics.
As an embodiment of the present invention, plane materiel is polyvinyl chloride (Polyvinyl chloride, PVC) plastics.
As an embodiment of the present invention, frangible anti-demolition electronic tags are formed with by cross cutting to be prevented tearing the edge of a knife.
As an embodiment of the present invention, the thickness of frangible anti-demolition electronic tags is less than 5mm.In the present embodiment, electric
Subtab miniaturization, can by electronic tag into portable device, such as in the Application in Anti-counterfeiting of valuables, by using
The rapid wear tamper of this electronic tag, user can obtain the electronic tag to avoid criminal and be attached to fake and forged quotient again
To achieve the purpose that mix the spurious with the genuine on product.
It includes plane materiel, the first glue-line, antenna stack, the second glue-line, foamed cotton layer, third glue that the utility model, which provides a kind of,
Layer, metal film layer, the 4th glue-line and ground paper layer frangible anti-demolition electronic tags, a kind of meeting anti-metal by designing
Under the premise of again with fragility and tamper electronic tag, avoid existing electronic tag because it is non-friable and can be complete
Original place is pasted go back to once more after whole dismounting, leads to not antitheft problem.
The above is only the preferred embodiment of the utility model only, is not intended to limit the utility model, all at this
Made any modifications, equivalent replacements, and improvements etc., should be included in the utility model within the spirit and principle of utility model