CN208316785U - A kind of gradual change GDM3D glass hand-set lid - Google Patents
A kind of gradual change GDM3D glass hand-set lid Download PDFInfo
- Publication number
- CN208316785U CN208316785U CN201820842056.5U CN201820842056U CN208316785U CN 208316785 U CN208316785 U CN 208316785U CN 201820842056 U CN201820842056 U CN 201820842056U CN 208316785 U CN208316785 U CN 208316785U
- Authority
- CN
- China
- Prior art keywords
- glass
- glass substrate
- gradual change
- fixedly connected
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a kind of gradual change GDM3D glass hand-set lids, including glass substrate, the glass substrate bottom is fixedly connected with adhesive plate, it is opened up at the top of the glass substrate fluted, the bottom portion of groove is fixedly connected with ink layer, gradual change glass is fixedly connected at the top of the ink layer, gradual change glass top surface is flushed with glass substrate top surface, 3D glassy layer is fixedly connected at the top of the glass substrate, the 3D glassy layer top surface is fixedly connected with strengthened glass layer, the strengthened glass layer top surface is fixedly connected with abrasionproof glassy layer, the utility model relates to hand-set lid device arts.Gradual change GDM3D glass hand-set lid device, achieve the purpose that image morphing is shown, show image more stable, and pass through the setting of spacing and glass substrate groove, achieve the purpose that make the more succinct safety of process, fraction defective is reduced, improves work efficiency, increases economic benefit.
Description
Technical field
The utility model relates to hand-set lid device arts, specially a kind of gradual change GDM3D glass phone cover
Plate.
Background technique
Complicated entirely produced and processed of the process of mobile phone 3D glass cover-plate production and processing technology carries out in dust-free workshop entirely, right
Production environment requirement is very high,
Master operation has: whether confirmation customer drawings can produce, and make our factory's drawing and the film, and confirm process.Under
Up to instruction sheet, sample is completely tracked.It by glass sawing sheet, is cleaned up into single groove ultrasonic, returns again to lower process production, will open
Expect that the material to come carries out processing and forming, the consistent shape of drawing provided with client is provided.It will require the product of slot position
It slots, is completed by stablizing accurately permanent remote digital-controlled carving machine.The product that vehicle side is completed carries out edging processing, wants by client
The requirement for reaching appearance and performance is asked, processing grinding wheel bistrique is designed by engineering staff, realizes that straight flange bevel edge is once completed.Mainly will
It needs to punch and begin a theatrical performance the glass product that the general technologies such as rank are not accomplished to be processed, also can replace vehicle side, fluting, bevelling etc.
Technique.After CNC has precisely been carved, also to be cleaned up into single groove ultrasonic, then remove plain grinding.The product that bevelling is completed carries out
The requirement of surface smoothness, and the thickness requirement of glass is controlled, this link is essential, and to select quality good plain grinding is set
It is standby.The product that plain grinding is completed the process carries out intensive treatment after cleaning up, and proposes the surface hardness of glass and shock resistance
Height, to reach customer requirement;It wants plain grinding good before tempering, plain grinding a few minutes is also wanted after tempering, then be cleaned by ultrasonic completely, in ultrasound
In cleaning process, it should be noted that cleaning agent for optical glass is chosen, into plating or silk-screen process;Need the glass lens of tempering
It is needed before tempering there is scuffing, the eyeglass of chipping will be picked out.The white tiles product that plain grinding is completed is subjected to plating or silk-screen
Effect process achievees the effect that eyeglass requirement.By the good eyeglass of silk-screen or plating strip, it is put into ultrasonic wave and cleaning agent cleaning is added
Completely, the effect after cleaning is to be not allow for scratching, watermark, white point, finger-marks, and milling, dust residue above, is being that will not go out
Existing dust-free workshop effect has to handle well.Often the problem is relatively more in this process for many manufacturers, it is also difficult to solve
Certainly, the problem of being often the cleaning agent for optical glass that you use with this reason, good cleaning agent for optical glass scratch, water
Print, white point, finger-marks, milling, choosing cleaning agent is also an a matter of great account.It completes by effect process and reaches client to want
The product asked is cleaned, is examined, is packed, and when packaging is packed with low viscous protective film, and when overlay film cannot have bubble phenomenon.
Utility model content
(1) the technical issues of solving
In view of the deficiencies of the prior art, the utility model provides a kind of gradual change GDM3D glass hand-set lid, solves hand
Cover glass sheet image shows single problem, while it is complicated to solve process, need to repeatedly slot edging the problem of.
(2) technical solution
In order to achieve the above object, the utility model is achieved by the following technical programs: a kind of gradual change GDM3D glass hand
Cover plate, including glass substrate, the glass substrate bottom are fixedly connected with adhesive plate, offer at the top of the glass substrate recessed
Slot, the glass substrate top edge and groove top edge spacing one are set as 4mm, the glass substrate both sides of the edge with it is recessed
Slot both sides of the edge spacing two is set as 1.5mm, and the bottom portion of groove is fixedly connected with ink layer, fixed company at the top of the ink layer
It is connected to gradual change glass, gradual change glass top surface is flushed with glass substrate top surface, fixed at the top of the glass substrate
It is connected with 3D glassy layer, the 3D glassy layer top surface is fixedly connected with strengthened glass layer, table at the top of the strengthened glass layer
Face is fixedly connected with abrasionproof glassy layer.
Preferably, the glass substrate is set as cuboid, and the angle at the top of cuboid with two sides is set as fillet.
Preferably, the adhesive plate top side offers camera hole, opens at the top of the adhesive plate far from camera hole side
Equipped with photographic hole.
Preferably, the camera hole and photographic hole through glass substrate and 3D glassy layer and extend to strengthened glass bottom.
Preferably, the glass substrate bottom margin and bottom portion of groove edge spacing three are set as 2mm.
Preferably, the 3D glassy layer top surface is provided with display panel.
(3) beneficial effect
The utility model provides a kind of gradual change GDM3D glass hand-set lid.Have it is following the utility model has the advantages that
(1), gradual change GDM3D glass hand-set lid is fixedly connected with adhesive plate, glass substrate by glass substrate bottom
Top opens up fluted, and glass substrate top edge and groove top edge spacing one are set as 4mm, glass substrate both sides of the edge
It is set as 1.5mm with groove both sides of the edge spacing two, bottom portion of groove is fixedly connected with ink layer, is fixedly connected at the top of ink layer
Gradual change glass, gradual change glass top surface are flushed with glass substrate top surface, are fixedly connected with 3D glass at the top of glass substrate
Layer, having reached makes handset image display image purpose abundant, while having reached the problem of preventing ink from escaping.
(2), gradual change GDM3D glass hand-set lid is fixedly connected with strengthened glass layer by 3D glassy layer top surface,
The problem of strengthened glass layer top surface is fixedly connected with abrasionproof glassy layer, has reached protection hand-set lid surface, extends hand
The service life of cover plate.
Detailed description of the invention
FIG. 1 is a schematic structural view of the utility model;
Fig. 2 is the structural schematic diagram of the utility model lid surface;
Fig. 3 is the structural schematic diagram of the utility model 3D glassy layer;
Fig. 4 is the structural schematic diagram of the utility model A-A.
In figure: 1 glass substrate, 2 adhesive plates, 3 grooves, 4 spacing one, 5 spacing two, 6 ink layers, 7 gradual change glass, 83D glass
Glass layer, 9 strengthened glass layers, 10 abrasionproof glassy layers, 11 fillets, 12 camera holes, 13 photographic holes, 14 spacing three, 15 display panels.
Specific embodiment
The following will be combined with the drawings in the embodiments of the present invention, carries out the technical scheme in the embodiment of the utility model
Clearly and completely describe, it is clear that the described embodiments are only a part of the embodiments of the utility model, rather than whole
Embodiment.Based on the embodiments of the present invention, those of ordinary skill in the art are without making creative work
Every other embodiment obtained, fall within the protection scope of the utility model.
Fig. 1-4 is please referred to, the utility model provides a kind of technical solution: a kind of gradual change GDM3D glass hand-set lid, including
Glass substrate 1,1 bottom of glass substrate are fixedly connected with adhesive plate 2, fluted 3 are opened up at the top of glass substrate 1, glass substrate 1 pushes up
Portion edge and 3 top edge spacing 1 of groove are set as 4mm, 1 both sides of the edge of glass substrate and 3 both sides of the edge spacing 25 of groove
It is set as 1.5mm, 3 bottom of groove is fixedly connected with ink layer 6, and gradual change glass 7, gradual change glass are fixedly connected at the top of ink layer 6
7 top surface of glass is flushed with 1 top surface of glass substrate, 3D glassy layer 8 is fixedly connected at the top of glass substrate 1, having reached makes
Handset image display image purpose abundant, while having reached the problem of preventing ink from escaping, 8 top surface of 3D glassy layer is fixed
It is connected with strengthened glass layer 9,9 top surface of strengthened glass layer is fixedly connected with abrasionproof glassy layer 10, has reached protection phone cover
The problem of plate surface, extends the service life of hand-set lid.
Glass substrate 1 is set as cuboid, and the angle at the top of cuboid with two sides is set as fillet 11.
2 top side of adhesive plate offers camera hole 12, and 2 top of adhesive plate offers photographic hole far from 12 side of camera hole
13。
Camera hole 12 and photographic hole 13 through glass substrate 1 and 3D glassy layer 8 and extend to 9 bottom of strengthened glass layer.
1 bottom margin of glass substrate and 3 bottom margin spacing 3 14 of groove are set as 2mm.
8 top surface of 3D glassy layer is provided with display panel 15.
In use, ink layer 6 is located at the bottom of the groove 3 inside glass substrate 1, and the top surface of ink layer 6 is fixed
It is connected with gradual change glass 7, has reached the problem of preventing ink from escaping, while having reached the mesh for making image show more vivid
, while passing through the setting of strengthened glass layer 9 and abrasionproof glassy layer 10, achieve the purpose that protect 3D glassy layer, extend simultaneously
The service life of hand-set lid.
It should be noted that, in this document, relational terms such as first and second and the like are used merely to a reality
Body or operation are distinguished with another entity or operation, are deposited without necessarily requiring or implying between these entities or operation
In any actual relationship or order or sequence.Moreover, the terms "include", "comprise" or its any other variant are intended to
Non-exclusive inclusion, so that the process, method, article or equipment including a series of elements is not only wanted including those
Element, but also including other elements that are not explicitly listed, or further include for this process, method, article or equipment
Intrinsic element.In the absence of more restrictions.By sentence " element limited including one ..., it is not excluded that
There is also other identical elements in the process, method, article or apparatus that includes the element ".
While there has been shown and described that the embodiments of the present invention, for the ordinary skill in the art,
It is understood that these embodiments can be carried out with a variety of variations in the case where not departing from the principles of the present invention and spirit, repaired
Change, replacement and variant, the scope of the utility model is defined by the appended claims and the equivalents thereof.
Claims (6)
1. a kind of gradual change GDM3D glass hand-set lid, including glass substrate (1), it is characterised in that: glass substrate (1) bottom
Portion is fixedly connected with adhesive plate (2), is opened up fluted (3) at the top of the glass substrate (1), glass substrate (1) top sides
Edge and groove (3) top edge spacing one (4) are set as 4mm, glass substrate (1) both sides of the edge and groove (3) two sides
Intermarginal to be set as 1.5mm away from two (5), groove (3) bottom is fixedly connected with ink layer (6), solid at the top of the ink layer (6)
Surely it is connected with gradual change glass (7), gradual change glass (7) top surface is flushed with glass substrate (1) top surface, the glass
It is fixedly connected with 3D glassy layer (8) at the top of substrate (1), 3D glassy layer (8) top surface is fixedly connected with strengthened glass layer
(9), strengthened glass layer (9) top surface is fixedly connected with abrasionproof glassy layer (10).
2. a kind of gradual change GDM3D glass hand-set lid according to claim 1, it is characterised in that: the glass substrate (1)
It is set as cuboid, and the angle at the top of cuboid with two sides is set as fillet (11).
3. a kind of gradual change GDM3D glass hand-set lid according to claim 1, it is characterised in that: adhesive plate (2) top
Portion side offers camera hole (12), offers photographic hole (13) far from camera hole (12) side at the top of the adhesive plate (2).
4. a kind of gradual change GDM3D glass hand-set lid according to claim 3, it is characterised in that: the camera hole (12)
Through glass substrate (1) and 3D glassy layer (8) and strengthened glass layer (9) bottom is extended to photographic hole (13).
5. a kind of gradual change GDM3D glass hand-set lid according to claim 1, it is characterised in that: the glass substrate (1)
Bottom margin and groove (3) bottom margin spacing three (14) are set as 2mm.
6. a kind of gradual change GDM3D glass hand-set lid according to claim 1, it is characterised in that: the 3D glassy layer (8)
Top surface is provided with display panel (15).