CN208141696U - 2.5D cover board and electronic display - Google Patents

2.5D cover board and electronic display Download PDF

Info

Publication number
CN208141696U
CN208141696U CN201820240804.2U CN201820240804U CN208141696U CN 208141696 U CN208141696 U CN 208141696U CN 201820240804 U CN201820240804 U CN 201820240804U CN 208141696 U CN208141696 U CN 208141696U
Authority
CN
China
Prior art keywords
hardened layer
angle
cover board
flat part
ontology
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201820240804.2U
Other languages
Chinese (zh)
Inventor
兰颖脱
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Junda Optoelectronic Technology Co ltd
Original Assignee
SHENZHEN JUNDA OPTOELECTRONICS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENZHEN JUNDA OPTOELECTRONICS CO Ltd filed Critical SHENZHEN JUNDA OPTOELECTRONICS CO Ltd
Priority to CN201820240804.2U priority Critical patent/CN208141696U/en
Application granted granted Critical
Publication of CN208141696U publication Critical patent/CN208141696U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides 2.5D cover board and electronic display, and 2.5D cover board includes acrylic ontology, and acrylic ontology includes flat part, the first angle 2.5D, the first hardened layer and the second hardened layer, and the outer rim of flat part is connected on the inside of the first angle 2.5D;First hardened layer is set to the upper surface of flat part 11, and hardened layer all standing flat part;Second hardened layer is set to the upper surface of the first hardened layer, and the edge of the second hardened layer extends outwardly and covers the first angle 2.5D;The outside of second hardened layer is equipped with the 2nd angle 2.5D;2.5D cover board provided by the utility model and electronic display enhance the hardness on flat part surface by the first hardened layer;By the design of the second hardened layer, coordinate the first 2.5D angular position more with surface, eliminates break bar print, increase water droplet angle, simultaneously, moreover it is possible to marginal position again stiffened, lid surface be prevented to be scraped off.

Description

2.5D cover board and electronic display
Technical field
The utility model belongs to electronic product Screen Technology field, is to be related to a kind of 2.5D cover board and electricity more specifically Sub- display screen.
Background technique
With the development of technology and the improvement of people ' s living standards, more and more people begin to use mobile phone or intelligence wearing Equipment, and people are higher and higher to the performance requirement of equipment.
Its toughness of acrylic material is high, and plasticity is strong, and transmitance is high, is commonly called as organic glass, but its surface hardness is low, general low In 4B, directly application when its surface easily scratch, meanwhile, in process, the angle 2.5D is generally by beating for 2.5D cover board It grinds to realize its radian, after the polishing of 2.5D cover board, the roughness of 2.5D cambered surface position is high, there is guide wheel print, and appearance is poor, and should Hardness at position is low.
Summary of the invention
The purpose of this utility model is to provide a kind of 2.5D cover board and electronic displays, to solve to exist in the prior art 2.5D cambered surface position at hardness it is lower, rough technical problem.
To achieve the above object, the technical solution adopted in the utility model is:A kind of 2.5D cover board, including acrylic are provided Ontology, the acrylic ontology include flat part, the first angle 2.5D, the first hardened layer and the second hardened layer, the first 2.5D The outer rim of the flat part is connected on the inside of angle;First hardened layer is set to the upper surface of the flat part, and described hard Change flat part described in layer all standing;Second hardened layer is set to the upper surface of first hardened layer, and second hardening The edge of layer extends outwardly and covers the first angle 2.5D;The outside of second hardened layer is equipped with the 2nd angle 2.5D.
Further, the aligned inside of the outer rim of first hardened layer and the first angle 2.5D.
Further, the 2nd angle 2.5D covers the outside at the first angle 2.5D and first hardened layer.
Further, the outer rim at the 2nd angle 2.5D is concordant with the outer rim at the first angle 2.5D.
Further, first hardened layer with a thickness of 3-5um, second hardened layer with a thickness of 3-10um.
Further, a dyne value for the first hardening layer surface is greater than 36 dynes, and the second hardening layer surface reaches Because being worth less than 30 dynes.
Further, the hardness of first hardened layer is greater than 1H, and the hardness of second hardened layer is greater than 4H.
Further, the acrylic ontology is PMMA ontology or PC ontology.
Electronic display, including display screen main body are connected with 2.5D cover board above-mentioned in the display screen main body.
The beneficial effect of 2.5D cover board provided by the utility model and electronic display is:Compared with prior art, originally The 2.5D cover board and electronic display that utility model provides, enhance the hardness on flat part surface by the first hardened layer;Pass through The design of second hardened layer coordinates the first 2.5D angular position more with surface, eliminates break bar print, increases water droplet angle, meanwhile, also Lid surface can be prevented to be scraped off marginal position again stiffened.
Detailed description of the invention
It, below will be to embodiment or the prior art in order to illustrate more clearly of the technical scheme in the embodiment of the utility model Attached drawing needed in description is briefly described, it should be apparent that, the accompanying drawings in the following description is only that this is practical new Some embodiments of type for those of ordinary skill in the art without any creative labor, can be with It obtains other drawings based on these drawings.
Fig. 1 is the structural schematic diagram of 2.5D cover board provided by the embodiment of the utility model;
Wherein, each appended drawing reference in figure:
1- acrylic ontology;11- flat part;The first angle 2.5D 12-;The first hardened layer of 2-;The second hardened layer of 3-;31- Two angles 2.5D.
Specific embodiment
In order to which technical problem to be solved in the utility model, technical solution and beneficial effect is more clearly understood, with Lower combination accompanying drawings and embodiments, the present invention will be further described in detail.It should be appreciated that specific reality described herein It applies example to be only used to explain the utility model, is not used to limit the utility model.
It should be noted that it can be directly another when element is referred to as " being fixed on " or " being set to " another element On one element or indirectly on another element.When an element is known as " being connected to " another element, it can To be directly to another element or be indirectly connected on another element.
Referring to Fig. 1, existing be illustrated 2.5D cover board provided by the utility model.A kind of 2.5D cover board is provided, including Acrylic ontology 1, acrylic ontology 1 include flat part 11 and the first angle 2.5D 12, and the inside at the first angle 2.5D 12 is connected to flat The outer rim in plate portion 11 further includes the first hardened layer 2 and the second hardened layer 3, and the first hardened layer 2 is set to the upper surface of flat part 11, And hardened layer all standing flat part 11;Second hardened layer 3 is set to the upper surface of the first hardened layer 2, and the edge of the second hardened layer 3 Extend outwardly and covers the first angle 2.5D 12;The outside of second hardened layer 3 is equipped with the 2nd angle 2.5D 31.
Compared with prior art, 2.5D cover board provided by the utility model include acrylic ontology 1, the first angle 2.5D 12, First hardened layer 2 and the second hardened layer 3 enhance the hardness on 11 surface of flat part by the first hardened layer 2;Pass through the second hardening The design of layer 3, makes more to coordinate at 12 position of the first angle 2.5D with surface, eliminates break bar print, increases water droplet angle, simultaneously, moreover it is possible to right Marginal position stiffened again, prevents lid surface to be scraped off.
Further, referring to Fig. 1, the aligned inside of the outer rim of the first hardened layer 2 and the first angle 2.5D 12;Make cover board table The hardness in face is reinforced, and prevents from being scratched.
Further, referring to Fig. 1, the outside at the 2nd angle 2.5D 31 covering the first angle 2.5D 12 and the first hardened layer 2;Make It is connected rounder and more smooth with surface at 12 position of the angle 2.5D, increases water droplet angle, has more aesthetic feeling, while can also play and prevent finger line Effect.
Further, referring to Fig. 1, the outer rim at the 2nd angle 2.5D 31 is concordant with the outer rim at the first angle 2.5D 12.It hardens At first angle 2.5D, 12 position, the break bar print at 12 position of the first angle 2.5D is eliminated, finger line can be prevented.
Further, the first hardened layer 2 with a thickness of 3-5um, the second hardened layer 3 with a thickness of 3-10um;First hardening The thickness of layer 2 can guarantee service performance between 3-5um;If thickness is excessive, the first hardened layer 2 is made to be piled up in the of both sides At one angle 2.5D, 12 position, and thickness is excessive, can not achieve uniform coating, wastes raw material;If too thin, hardness number is inadequate, no It can effectively prevent from scratching;The design of the thickness of second hardened layer 3 also has effect so.
Further, dyne value on 2 surface of the first hardened layer is greater than 36 dynes, and dyne value on 3 surface of the second hardened layer is small In 30 dynes;Dyne value on 2 surface of the first hardened layer is greater than 36 dynes, during coating, is easy the first hardened layer 2 attached In the upper of cover board;Dyne value on 3 surface of the second hardened layer less than 30 dynes, can make the second hardened layer 3 it is firm be attached to the On one hardened layer 2, prevents the first hardened layer 2 from falling off, guarantee the persistence used.
Further, the hardness of the first hardened layer 2 is greater than 1H, and the hardness of the second hardened layer 3 is greater than 4H;First hardened layer 2 Hardness be greater than 1H, the hardness of lid surface can be enhanced;In addition, the hardness of the second hardened layer 3 is greater than 4H, lid can be further strengthened The hardness of plate surface, simultaneously, moreover it is possible to enhance the hardness at 12 position of the first angle 2.5D of cover board, it is hard for the cover board after stiffened Du Genggao, wearability are more preferable, moreover it is possible to play the role of preventing finger line.
Further, the first hardened layer 2 is coated on the upper surface of flat part 11;By way of coating, by the first hardening Layer 2 is coated on the upper surface of flat part 11, easy to operate and practical.
Further, the second hardened layer 3 prints on the upper surface and the first angle 2.5D of the first hardened layer 2 by 3D printer 12 upper surface.Since the edge at the first angle 2.5D 12 is exposed outside, by 3D printer at the first exposed angle 2.5D 12 One layer of second hardened layer 3 is printed at position, eliminates break bar print, increases the hardness number at this, and the mode printed can make first The angle 2.5D forms good globoidal structure at 12 position, and external form is more preferable.
Further, acrylic ontology 1 is PMMA ontology or PC ontology;PMMA and PC is transparent material, and is had good Good chemical stability.
Electronic display, including display screen main body are connected with 2.5D cover board above-mentioned in display screen main body;Comprising aforementioned The electronic display of 2.5D cover board, wearability, plasticity are good, and smooth in appearance is mellow and full, can anti-finger line, and it is cheap.
The above is only the preferred embodiment of the utility model only, is not intended to limit the utility model, all at this Made any modifications, equivalent replacements, and improvements etc., should be included in the utility model within the spirit and principle of utility model Protection scope within.

Claims (9)

1.2.5D cover board, including acrylic ontology, the acrylic ontology include flat part and the first angle 2.5D, and described first The outer rim of the flat part is connected on the inside of the angle 2.5D, it is characterised in that:It further include the first hardened layer and the second hardened layer, institute State the upper surface that the first hardened layer is set to the flat part, and flat part described in the hardened layer all standing;Second hardening Layer is set to the upper surface of first hardened layer, and the edge of second hardened layer extends outwardly and covers the first 2.5D The outside at angle, second hardened layer is equipped with the 2nd angle 2.5D.
2. 2.5D cover board as described in claim 1, it is characterised in that:The outer rim of first hardened layer and the first 2.5D The aligned inside at angle.
3. 2.5D cover board as claimed in claim 2, it is characterised in that:2nd angle 2.5D cover the first angle 2.5D and The outside of first hardened layer.
4. 2.5D cover board as claimed in claim 3, it is characterised in that:The outer rim at the 2nd angle 2.5D and the first 2.5D The outer rim at angle is concordant.
5. 2.5D cover board as claimed in claim 4, it is characterised in that:First hardened layer with a thickness of 3-5um, described Two hardened layers with a thickness of 3-10um.
6. 2.5D cover board as claimed in claim 5, it is characterised in that:Dyne value of the first hardening layer surface is greater than 36 and reaches Cause, dyne value of the second hardening layer surface is less than 30 dynes.
7. 2.5D cover board as claimed in claim 6, it is characterised in that:The hardness of first hardened layer is greater than 1H, and described the The hardness of two hardened layers is greater than 4H.
8. the 2.5D cover board as described in claim 1-7 any one, it is characterised in that:The acrylic ontology is PMMA ontology Or PC ontology.
9. electronic display, including display screen main body, it is characterised in that:The display screen main body is equipped with such as claim 1-8 2.5D cover board described in any one.
CN201820240804.2U 2018-02-09 2018-02-09 2.5D cover board and electronic display Active CN208141696U (en)