CN208011085U - A kind of high-performance PPR pipe part - Google Patents

A kind of high-performance PPR pipe part Download PDF

Info

Publication number
CN208011085U
CN208011085U CN201820218999.0U CN201820218999U CN208011085U CN 208011085 U CN208011085 U CN 208011085U CN 201820218999 U CN201820218999 U CN 201820218999U CN 208011085 U CN208011085 U CN 208011085U
Authority
CN
China
Prior art keywords
wall embeded
embeded
performance
gap
ppr
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201820218999.0U
Other languages
Chinese (zh)
Inventor
刘韶云
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Pulima Trading Co Ltd
Original Assignee
Guangzhou Pulima Trading Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Pulima Trading Co Ltd filed Critical Guangzhou Pulima Trading Co Ltd
Priority to CN201820218999.0U priority Critical patent/CN208011085U/en
Application granted granted Critical
Publication of CN208011085U publication Critical patent/CN208011085U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model is related to a kind of high-performance PPR pipe parts, its metal insert connector is used to have the inside wall embeded being integrally connected and outside wall embeded with one end of pipe main body injection molding connection, there is filling gap between inside wall embeded and outside wall embeded, fill the injected plastics material for being filled with pipe main body in gap;When heated, the material thermal expansion coefficients that pipe main body is filled in filling gap are bigger than metal, cause to fill the plastic material expansion jam-packed medial and lateral wall embeded in gap, contact is even closer, and sealing performance is more preferable;When being cooled, the further reduced inner diameter of meeting after the plastic material in gap is shunk is filled in plastic conduit contraction, to the lateral wall of wall embeded on the inside of its madial wall meeting banding, plastic material and connection of the metal material on this face are also even closer, and leak resistance can also be promoted;Therefore the technical solution of the utility model, hot and cold water is general, can effectively prevent the seepy question after the longterm expansion contraction of pipe fitting PPR plastics, is a kind of high performance PPR pipe part.

Description

A kind of high-performance PPR pipe part
Technical field
The utility model belongs to PPR pipe manufacturing technology field, more specifically, being related to a kind of PPR pipe part.
Background technology
PPR pipe part is the tubing of the first birth and Germany in 90 years 20th century, is the third generation PA tube after PPH, PPB Material, PPR pipe part superior performance, which is developed so far, is widely used to civil buildings and industrial discharge drainage facility field;
Existing PPR pipe part, has in quite a few product, is all made of the nipple that copper insert 2 is used as pipe fitting, such as A kind of existing PPR pipe part shown in FIG. 1, when production, are placed on copper insert 2 on the mold of injection molding machine, then with main pipe body 1 Injection molding, copper insert 2 are connected in the pipe of PPR;Due to the thermal expansion coefficients of metal and PPR plastic materials and the diminution that is cooled Coefficient differs greatly;PPR plastics thermal expansion deformations are more than metal material thermal expansion deformation when heated;So that this kind of product with During the use of hot water pipeline, be located inside metalwork expansion it is small, be located at outside plastic material expansion it is big, repeatedly by After hot, multiple cold cycling, copper insert 2 is easy and 1 component of main pipe body, obscission occurs, thereby reduces the anti-of pipe fitting The performance of leakage, is also easy to produce leakage accident.
Utility model content
In order to overcome the shortcomings of the prior art, the utility model to provide a kind of high-performance PPR pipe part, hot and cold water is logical With, can effectively prevent pipe fitting PPR plastics longterm expansion shrink after seepy question.
Technical solution adopted by the utility model to solve its technical problems is:
A kind of high-performance PPR pipe part, including main pipe body, connect with main pipe body injection molding positioned at main pipe body end Metal insert connector;One end that the metal insert connector is used to connect with main pipe body has the inside being integrally connected Wall embeded and outside wall embeded have the filling for being injection molding material filling after injection molding between inside wall embeded and outside wall embeded Gap;The inside wall embeded is used to be connected to the inside of pipe main body after injection molding, and the outside wall embeded is used for through injection molding The outside of pipe main body is connected to after processing.
A kind of high-performance PPR pipe part in above-mentioned technical proposal, metal insert connector, which is used to be molded with pipe main body, to be connected The one end connect has the inside wall embeded being integrally connected and outside wall embeded, has filling gap between inside wall embeded and outside wall embeded, The injected plastics material that pipe main body is filled in gap is filled, in the actual use process, when being heated, pipe main body is filled in The material thermal expansion coefficients filled in gap are bigger than metal, cause the plastic material expansion jam-packed medial and lateral filled in gap embedding Wall, contact is even closer, and sealing performance is more preferable;When being cooled, plastic conduit is shunk, and fills meeting after the plastic material in gap is shunk Further reduced inner diameter, to the lateral wall of wall embeded on the inside of its madial wall meeting banding, plastic material is with metal material at this Connection on face is also even closer, and leak resistance can also be promoted;The technical solution of the utility model in summary, hot and cold water are logical With, can effectively prevent pipe fitting PPR plastics longterm expansion shrink after seepy question, be a kind of high performance PPR pipe part.
The axial length of the outside wall embeded is longer than the axial length of inside wall embeded.Keep connection more firm.
The lower end of the medial surface of the outside wall embeded is equipped with lug boss.Keep connection more firm.
The boss is under the lower face of inside wall embeded.The filling that material in gap is filled when injection molding is not interfered, If being arranged in filling gap, the intensity of injection-moulded plastic in filling gap is easily reduced.
On the inside wall embeded and/or outside wall embeded also uneven distribution have it is several for being injection molding material after injection molding Expect the through hole of filling.Keep connection more firm.
The utility model has the beneficial effects that:A kind of high-performance PPR pipe part of the utility model, metal insert connector For to there is the inside wall embeded being integrally connected and outside wall embeded, inside wall embeded and outside wall embeded with one end of pipe main body injection molding connection Between there is filling gap, the injected plastics material of pipe main body is filled in filling gap, it is in the actual use process, heated When, the material thermal expansion coefficients that pipe main body is filled in filling gap are bigger than metal, cause to fill the plastics material in gap Material expansion jam-packed medial and lateral wall embeded, contact is even closer, and sealing performance is more preferable;When being cooled, plastic conduit is shunk, and fills gap The further reduced inner diameter of meeting after interior plastic material is shunk, to the lateral wall of wall embeded on the inside of its madial wall meeting banding, plastics Material and connection of the metal material on this face are also even closer, and leak resistance can also be promoted;The utility model in summary Technical solution, hot and cold water is general, can effectively prevent pipe fitting PPR plastics longterm expansion shrink after seepy question, be a kind of High performance PPR pipe part.
Description of the drawings
The utility model is further illustrated with reference to the accompanying drawings and examples.
Fig. 1 is a kind of structural schematic diagram of existing PPR pipe part described in background technology;
Fig. 2 is a kind of structural schematic diagram of high-performance PPR pipe part described in the utility model.
Specific implementation mode
The utility model is described in further detail presently in connection with attached drawing.These attached drawings are simplified schematic diagram, Only illustrate the basic structure of the utility model in a schematic way, therefore it only shows composition related with the utility model.
A kind of high-performance PPR pipe part as shown in Figure 2, including main pipe body 1, be located at 1 end of main pipe body and pipe fitting master The metal insert connector 2 of 1 injection molding of body connection;One end that the metal insert connector 2 is used to connect with main pipe body 1 With the inside wall embeded 21 and outside wall embeded 22 being integrally connected, have for through injection molding between inside wall embeded 21 and outside wall embeded 22 The filling gap 23 of material filling is injection molding after processing;The inside wall embeded 21 after injection molding for being connected to pipe main body 1 inside, the outside wall embeded 22 are used to be connected to the outside of pipe main body 1 after injection molding.
A kind of high-performance PPR pipe part in above-mentioned technical proposal, metal insert connector 2 are used for and 1 note of pipe main body One end of modeling connection has the inside wall embeded 21 being integrally connected and outside wall embeded 22, has between inside wall embeded 21 and outside wall embeded 22 There is filling gap 23, the injected plastics material of pipe main body 1 is filled in filling gap 23, in the actual use process, when being heated, The material thermal expansion coefficients that pipe main body 1 is filled in filling gap 23 are bigger than metal, cause to fill the plastics in gap 23 Material expand jam-packed medial and lateral wall embeded 21,22, contact is even closer, and sealing performance is more preferable;When being cooled, plastic conduit is shunk, and is filled out The further reduced inner diameter of meeting after the plastic material in gap 23 is shunk is filled, so that its madial wall meeting banding inside wall embeded 21 is outer Side wall, plastic material and connection of the metal material on this face are also even closer, and leak resistance can also be promoted;In summary originally The technical solution of utility model, hot and cold water is general, can effectively prevent the leak after the longterm expansion contraction of pipe fitting PPR plastics and asks Topic, is a kind of high performance PPR pipe part.
In the present embodiment, the axial length of the outside wall embeded 22 is longer than the axial length of inside wall embeded 21.Make connection more Add firm.
In the present embodiment, the lower end of the medial surface of the outside wall embeded 22 is equipped with lug boss 25.Keep connection more firm.
In the present embodiment, the lug boss 25 is located under the lower face of inside wall embeded 21.When not interfering injection molding between filling The filling of material in gap 23 easily reduces the intensity of injection-moulded plastic in filling gap 23 if being arranged in filling gap 23.
In the present embodiment, on the inside wall embeded 21 also uneven distribution have it is several for being injection molding material after injection molding Expect the through hole 24 of filling.Keep connection more firm;
In other embodiments, setting through hole 24 or inside wall embeded 21 and outer be can also be on the wall embeded 22 of outside Through hole 24. is set simultaneously on side wall embeded 22
The utility model has the beneficial effects that:A kind of high-performance PPR pipe part of the utility model, metal insert connector For to there is the inside wall embeded being integrally connected and outside wall embeded, inside wall embeded and outside wall embeded with one end of pipe main body injection molding connection Between there is filling gap, the injected plastics material of pipe main body is filled in filling gap, it is in the actual use process, heated When, the material thermal expansion coefficients that pipe main body is filled in filling gap are bigger than metal, cause to fill the plastics material in gap Material expansion jam-packed medial and lateral wall embeded, contact is even closer, and sealing performance is more preferable;When being cooled, plastic conduit is shunk, and fills gap The further reduced inner diameter of meeting after interior plastic material is shunk, to the lateral wall of wall embeded on the inside of its madial wall meeting banding, plastics Material and connection of the metal material on this face are also even closer, and leak resistance can also be promoted;The utility model in summary Technical solution, hot and cold water is general, can effectively prevent pipe fitting PPR plastics longterm expansion shrink after seepy question, be a kind of High performance PPR pipe part.
It is enlightenment, through the above description, related work people with the above-mentioned desirable embodiment according to the utility model Member can carry out various changes and amendments in the range of without departing from this item utility model technological thought completely.This item is real It is not limited to the contents of the specification with novel technical scope, it is necessary to which its technology is determined according to right Property range.

Claims (5)

1. a kind of high-performance PPR pipe part, including main pipe body, it is connect with main pipe body injection molding positioned at main pipe body end Metal insert connector;It is characterized in that:One end that the metal insert connector is used to connect with main pipe body has one Connected inside wall embeded and outside wall embeded has between inside wall embeded and outside wall embeded for being injection molding material after injection molding The filling gap of filling;The inside wall embeded is used to be connected to the inside of pipe main body, the outside wall embeded after injection molding Outside for being connected to pipe main body after injection molding.
2. high-performance PPR pipe part according to claim 1, it is characterised in that:The axial length of the outside wall embeded is longer than The axial length of inside wall embeded.
3. high-performance PPR pipe part according to claim 2, it is characterised in that:The lower end of the medial surface of the outside wall embeded Equipped with lug boss.
4. high-performance PPR pipe part according to claim 3, it is characterised in that:The boss is under the wall embeded of inside Under end face.
5. according to claim 1-4 any one of them high-performance PPR pipe parts, it is characterised in that:The inside wall embeded and/or outer Also uneven distribution has several through holes for being injection molding material filling after injection molding on the wall embeded of side.
CN201820218999.0U 2018-02-08 2018-02-08 A kind of high-performance PPR pipe part Expired - Fee Related CN208011085U (en)