CN207990010U - A kind of pre- repaired mouth steel pipe of weld bond - Google Patents

A kind of pre- repaired mouth steel pipe of weld bond Download PDF

Info

Publication number
CN207990010U
CN207990010U CN201721369152.4U CN201721369152U CN207990010U CN 207990010 U CN207990010 U CN 207990010U CN 201721369152 U CN201721369152 U CN 201721369152U CN 207990010 U CN207990010 U CN 207990010U
Authority
CN
China
Prior art keywords
steel pipe
weld bond
short tube
stainless steel
repaired mouth
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201721369152.4U
Other languages
Chinese (zh)
Inventor
韩文礼
李广华
田黎明
郭继银
林竹
杨耀辉
张彦军
魏国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CNPC Research Institute of Engineering Technology
CNPC Engineering Technology Research Institute Co Ltd
Original Assignee
CNPC Engineering Technology Research Institute Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CNPC Engineering Technology Research Institute Co Ltd filed Critical CNPC Engineering Technology Research Institute Co Ltd
Application granted granted Critical
Publication of CN207990010U publication Critical patent/CN207990010U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of pre- repaired mouth steel pipes of weld bond, including:Steel pipe;Stainless steel short tube, is arranged in steel pipe, and the distance of first end to the weld bond end of steel pipe of stainless steel short tube is more than second end to the distance of weld bond end;First overlay cladding, is attached at steel pipe inner wall, is connect with first end;From first end, First terminal point is extended to along the direction far from short tube;Second overlay cladding is attached at the steel pipe inner wall, is connect with the second end;From the second end, the weld bond end is extended to;Wherein, the stainless steel short tube inner surface is smoothly overlapped with first overlay surface;The stainless steel short tube inner surface is smoothly overlapped with second overlay surface.The pre- repaired mouth steel pipe of weld bond provided by the present application is for solving that the high technical problem of internal corrosion prevention joint coating of steel tube task difficulty exists in the prior art, realizing reduces repaired mouth process and difficulty, extend pipeline life cycle, reduces the technique effect of safety and environmental protection risk caused by corrosive pipeline leakage.

Description

A kind of pre- repaired mouth steel pipe of weld bond
Technical field
The utility model is related to pipe technology field more particularly to a kind of pre- repaired mouth steel pipes of weld bond.
Background technology
Steel pipe weld bond is the most weak link of corrosion resistance, in all corrosive pipeline leakage accidents, pipeline weldering Mouth corrosion accounts for 60% or more, is on active service the period to extend pipeline, in internal coat pipeline construction, needs to the progress of pipe welding port inner wall Preservative treatment, this process are known as " pipeline internal joint patch ";
What pipeline internal joint patch was realized generally by repaired mouth robot, it needs first to clear up pipe welding port inner wall Operation, then spraying liquid anticorrosive paint, keeps pipeline internal corrosion layer continuous;Since unsuitable robot enters small bore pipe Inside road, spraying internal joint patch cannot achieve;
For small-bore pipeline, the general method using live coating squeezing and coating carries out internal joint patch operation, due to can not be to small Aperture pipe welding port inner wall carries out prune job, and coating adhesion is insufficient, can not ensure the quality of internal joint patch erosion resistant coating;
That is, the high technical problem of internal corrosion prevention joint coating of steel tube task difficulty exists in the prior art.
Utility model content
The utility model solves anti-corrosion in steel pipe existing in the prior art by providing a kind of pre- repaired mouth steel pipe of weld bond The high technical problem of repaired mouth task difficulty.
In order to solve the above technical problems, the utility model provides following technical solution:
A kind of pre- repaired mouth steel pipe of weld bond, including:
Steel pipe;
Stainless steel short tube is arranged in the steel pipe, and the first end and second end of the stainless steel short tube is respectively positioned on described In steel pipe;Wherein, the distance of the first end to the weld bond end of the steel pipe is more than the second end to the weld bond end Distance;
First overlay cladding is attached at the steel pipe inner wall, is connect with the first end;From the first end, along separate The direction of the short tube extends to First terminal point;
Second overlay cladding is attached at the steel pipe inner wall, is connect with the second end;From the second end, extend to The weld bond end;
Wherein, the stainless steel short tube inner surface is smoothly overlapped with first overlay surface;The stainless steel short tube Inner surface is smoothly overlapped with second overlay surface.
Optionally, the stainless steel short tube and the steel pipe are interference fit.
Optionally, the thickness of first overlay cladding successively decreases along the direction of the first end to the First terminal point.
Optionally, the thickness of second overlay cladding is identical as the thickness of stainless steel short tube.
Optionally, the weld bond end is groove shape.
Optionally, the outer diameter of the stainless steel short tube is bigger 0.05mm~0.08mm than the internal diameter of the steel pipe, to realize It is full of assembly.
Optionally, the welding bead overlapping rate of first overlay cladding is 3mm.
One or more technical solutions provided in the embodiments of the present application have at least the following technical effects or advantages:
1, pre- repaired mouth steel pipe provided by the embodiments of the present application inside sets the first overlay cladding, stainless steel short tube in steel pipe weld bond side With the second overlay cladding, anti-corrosion function can be provided, therefore does not need and carries out interior corrosion-resistanting interpolating port process at butt welding mouth again, reduces repaired mouth work Sequence and difficulty.
2, pre- repaired mouth steel pipe provided by the embodiments of the present application, increases by using stainless steel short tube and steel pipe metallurgical binding The thickness of pipe end improves the mechanical property of pipe end.
3, pre- repaired mouth steel pipe provided by the embodiments of the present application can be prevented using the structure of overlay cladding plus stainless steel short-tube filling Chromium carbide pin hole only is formed in pre- repaired mouth layer surface, prevents caused by pure built-up welding corrosion resistant alloy component diluent due to reduce pre- benefit The corrosion resistance of mouth layer, further increases the corrosion resistance of pipe end, extends pipeline life cycle, reduces corrosive pipeline leakage Caused safety and environmental protection risk.
Description of the drawings
It is required in being described below to embodiment in order to illustrate more clearly of the technical scheme in the embodiment of the utility model Attached drawing to be used is briefly described, it should be apparent that, the accompanying drawings in the following description is only the embodiments of the present invention, For those of ordinary skill in the art, without creative efforts, it can also be obtained according to the attached drawing of offer Obtain other attached drawings.
Fig. 1 is the structure chart of pre- repaired mouth steel pipe in the embodiment of the present application;
Fig. 2 is the machining sketch chart of pre- repaired mouth steel pipe in the embodiment of the present application.
Specific implementation mode
The embodiment of the present application solves and anti-corrosion in steel pipe exists in the prior art by providing a kind of pre- repaired mouth steel pipe of weld bond The high technical problem of repaired mouth task difficulty, realizing reduces repaired mouth process and difficulty, extends pipeline life cycle, reduces pipeline The technique effect of safety and environmental protection risk caused by corrosion leakage.
In order to solve the above technical problems, the general thought that the embodiment of the present application provides technical solution is as follows:
The application provides a kind of pre- repaired mouth steel pipe of weld bond, including:
Steel pipe;
Stainless steel short tube is arranged in the steel pipe, and the first end and second end of the stainless steel short tube is respectively positioned on described In steel pipe;Wherein, the distance of the first end to the weld bond end of the steel pipe is more than the second end to the weld bond end Distance;
First overlay cladding is attached at the steel pipe inner wall, is connect with the first end;From the first end, along separate The direction of the short tube extends to First terminal point;
Second overlay cladding is attached at the steel pipe inner wall, is connect with the second end;From the second end, extend to The weld bond end;
Wherein, the stainless steel short tube inner surface is smoothly overlapped with first overlay surface;The stainless steel short tube Inner surface is smoothly overlapped with second overlay surface.
Pre- repaired mouth steel pipe provided by the embodiments of the present application, in steel pipe weld bond side, inside set the first overlay cladding, stainless steel short tube and Second overlay cladding can provide anti-corrosion function, therefore do not need and carry out interior corrosion-resistanting interpolating port process at butt welding mouth again, reduce repaired mouth process And difficulty.
In order to better understand the above technical scheme, being carried out to above-mentioned technical proposal below in conjunction with specific embodiment It is described in detail, it should be understood that the specific features in the utility model embodiment and embodiment are to the detailed of technical scheme Thin explanation, rather than to the restriction of technical scheme, in the absence of conflict, the embodiment of the present application and embodiment In technical characteristic can be combined with each other.
In the present embodiment, as shown in Figure 1, providing a kind of pre- repaired mouth steel pipe of weld bond, including:
Steel pipe 1;
Stainless steel short tube 2 is arranged in the steel pipe 1, and the first end 201 and second end 202 of the stainless steel short tube 2 are equal In the steel pipe 1;Wherein, the distance of the first end 201 to the weld bond end 101 of the steel pipe 1 is more than described second The distance of end 202 to the weld bond end 101;
First overlay cladding 3, is attached at the steel pipe inner wall, is connect with the first end 201;From the first end 201, First terminal point 301 is extended to along the direction far from the short tube;
Second overlay cladding 4, is attached at the steel pipe inner wall, is connect with the second end 202;From the second end 202, Extend to the weld bond end 101;
Wherein, 2 inner surface of stainless steel short tube is overlapped with 3 smooth surface of the first overlay cladding;The stainless steel is short 2 inner surface of pipe is overlapped with 4 smooth surface of the second overlay cladding.
In the following, the structure that the application provides steel pipe is discussed in detail in conjunction with Fig. 1 and Fig. 2.
In specific implementation process, the steel pipe 1 can be mild steel parent metal steel pipe or medium carbon content steel pipe, herein not It is restricted.
In the embodiment of the present application, in order to ensure the abundant fixation of stainless steel short tube 2 and steel pipe 1, can be arranged it is described not Rust steel short tube 2 is interference fit with the steel pipe 1.
Further, it is possible to the outer diameter that the stainless steel short tube 2 is set it is bigger 0.05mm than the internal diameter of the steel pipe 1~ 0.08mm, to realize elastic conjunction.
In specific implementation process, in order to ensure the filling of stainless steel short tube 2, can first it be machined in 1 pipe end of steel pipe Wall ensures inner wall of the pipe within certain depth dimensions and the margin of tolerance, and ensures that metal sheet is exposed in machined surface cleaning Color;1 pipe end of sensing heating steel pipe again makes its expansion, is processed next, prefabricated stainless steel short tube 2 is packed into pipe end Endoporus in, it is cooling after stainless steel short tube 2 combine closely with steel pipe 1, realize and be interference fitted.
Specifically, in pipe end pre- repaired mouth layer using stainless steel short tube 2 and with 1 metallurgical binding of steel pipe, on the one hand, increase The thickness of pipe end improves the mechanical property of pipe end;On the other hand, 2 coefficient of expansion of stainless steel short tube is more than steel pipe 1, Play the role of to 1 pipe end of steel pipe it is expanding, play control 1 bottlenecking of steel pipe.
In the embodiment of the present application, the first overlay cladding 3 and the second overlay cladding 4 are to assemble 2 post-processing of stainless steel short tube It is formed, stainless steel welding stick specifically may be used, fill silk built-up welding, forms the first overlay cladding 3 and the second built-up welding of stainless steel Layer 4.
Specifically, can be the interface for first going deep into stainless steel short tube and steel pipe inner wall in steel pipe with welding gun, i.e., from first Point 201, steel pipe rotates under numerical control, and simultaneously axial wobble is moved away from displacement, welding bead is taken tungsten needle starting the arc wire feed along 5 built-up welding of first direction Rate 3mm is met, until heap is soldered to design width, i.e. heap is welded to the First terminal point 301;Wherein, the design width is welded by pipeline It connects heat affected area not damaging premised on pipe end inner anticorrosioning coating, Pipeline butt is avoided to connect heat input butt welding mouth inner wall area anti-corrosion The destruction of coating, to realize the continuous of pipeline internal corrosion layer.
Then, from the First terminal point 301, along the second direction 6 close to the weld bond end 101, welding gun is moved away from shifting Position, argon gas electric arc axial wobble fusing overlay cladding (solid solution) again, until 201 position of first end of stainless steel short tube 2, described in formation First overlay cladding 3 continuously moves to second end next, welding gun, which stops axial wobble, is changed to spiral displacement and high current 202, stainless steel is formed with melting stainless steel short tube 2 and is dissolved overlay cladding so that the inner surface of stainless steel short tube 2 and first heap Layer 3 connects transition.
In the embodiment of the present application, the thickness of first overlay cladding 3 is along the first end to the side of the First terminal point To successively decreasing, to realize the smooth excessiveness of stainless steel short tube 2, the first overlay cladding, 1 inner wall of steel pipe, convenient for subsequently to 1 inner wall of steel pipe into Row preservative treatment.
In the embodiment of the present application, the formation process of second overlay cladding 4 can use melting pole gun instead from stainless The second end 202 of steel short tube 2 starts, and built-up welding is up to the weld bond end 101 of steel pipe 1.
After forming the second overlay cladding 4, can by the techniques such as polish, make the thickness of second overlay cladding 4 with it is described The thickness of stainless steel short tube 2 is identical, and then ensures in the stainless steel short tube 2 just face and 4 smooth surface of the second overlay cladding Transition, convenient for the Forming Quality of weld bond in welding and guarantee.
Further, it is possible to which the weld bond end 101 of polishing is groove shape, further it is convenient for the company of steel pipe 1 and other steel pipes It connects.
Specifically, the filled solid dissolving method of built-up welding is used in the application pipe end, on the one hand, prevent in pre- repaired mouth layer surface The corrosion resistance of pre- repaired mouth layer is reduced due to form chromium carbide pin hole, prevent caused by pure built-up welding corrosion resistant alloy component diluent Energy;On the other hand, keep the visual interface of pre- repaired mouth layer and mild steel base material smoothed by the reversed solid solution craft method of positive built-up welding It crosses, ensures the bond quality with inner anticorrosioning coating, can effectively extend pipeline life cycle, caused by reducing corrosive pipeline leakage Safety and environmental protection risk.
Technical solution in above-mentioned the embodiment of the present application, at least has the following technical effect that or advantage:
1, pre- repaired mouth steel pipe provided by the embodiments of the present application inside sets the first overlay cladding, stainless steel short tube in steel pipe weld bond side With the second overlay cladding, anti-corrosion function can be provided, therefore does not need and carries out interior corrosion-resistanting interpolating port process at butt welding mouth again, reduces repaired mouth work Sequence and difficulty.
2, pre- repaired mouth steel pipe provided by the embodiments of the present application, increases by using stainless steel short tube and steel pipe metallurgical binding The thickness of pipe end improves the mechanical property of pipe end.
3, pre- repaired mouth steel pipe provided by the embodiments of the present application can be prevented using the structure of overlay cladding plus stainless steel short-tube filling Chromium carbide pin hole only is formed in pre- repaired mouth layer surface, prevents caused by pure built-up welding corrosion resistant alloy component diluent due to reduce pre- benefit The corrosion resistance of mouth layer, further increases the corrosion resistance of pipe end, extends pipeline life cycle, reduces corrosive pipeline leakage Caused safety and environmental protection risk.
Although the preferred embodiment of the utility model has been described, once a person skilled in the art knows basic Creative concept, then additional changes and modifications may be made to these embodiments.It is wrapped so the following claims are intended to be interpreted as It includes preferred embodiment and falls into all change and modification of the scope of the utility model.
Obviously, those skilled in the art can carry out the utility model various modification and variations without departing from this practicality Novel spirit and scope.If in this way, these modifications and variations of the present invention belong to the utility model claims and Within the scope of its equivalent technologies, then the utility model is also intended to include these modifications and variations.

Claims (8)

1. a kind of pre- repaired mouth steel pipe of weld bond, which is characterized in that including:
Steel pipe;
Stainless steel short tube is arranged in the steel pipe, and the first end and second end of the stainless steel short tube is respectively positioned on the steel pipe It is interior;Wherein, the first end to the weld bond end of the steel pipe distance be more than the second end to the weld bond end away from From;
First overlay cladding is attached at the steel pipe inner wall, is connect with the first end;From the first end, along far from described The direction of short tube extends to First terminal point;
Second overlay cladding is attached at the steel pipe inner wall, is connect with the second end;From the second end, extend to described Weld bond end;
Wherein, the stainless steel short tube inner surface is smoothly overlapped with first overlay surface;Table in the stainless steel short tube Face is smoothly overlapped with second overlay surface.
2. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that the stainless steel short tube and the steel pipe were It is full of cooperation.
3. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that the thickness of first overlay cladding is along described Successively decrease in the direction of one end to the First terminal point.
4. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that the thickness of second overlay cladding with it is described not The thickness of rust steel short tube is identical.
5. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that the weld bond end is groove shape.
6. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that the outer diameter of the stainless steel short tube is than the steel Big 0.05mm~the 0.08mm of internal diameter of pipe, to realize elastic conjunction.
7. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that the welding bead overlapping rate of first overlay cladding is 3mm。
8. the pre- repaired mouth steel pipe of weld bond as described in claim 1, which is characterized in that first overlay cladding and second built-up welding Layer is stainless steel weld overlays.
CN201721369152.4U 2016-11-07 2017-10-23 A kind of pre- repaired mouth steel pipe of weld bond Expired - Fee Related CN207990010U (en)