CN207508075U - A kind of stamping die - Google Patents

A kind of stamping die Download PDF

Info

Publication number
CN207508075U
CN207508075U CN201721660732.9U CN201721660732U CN207508075U CN 207508075 U CN207508075 U CN 207508075U CN 201721660732 U CN201721660732 U CN 201721660732U CN 207508075 U CN207508075 U CN 207508075U
Authority
CN
China
Prior art keywords
die
die cavity
mould
cut
location hole
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201721660732.9U
Other languages
Chinese (zh)
Inventor
陈爱仪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Jinlong Run Overflow Hardware Co Ltd
Original Assignee
Shenzhen Jinlong Run Overflow Hardware Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Jinlong Run Overflow Hardware Co Ltd filed Critical Shenzhen Jinlong Run Overflow Hardware Co Ltd
Priority to CN201721660732.9U priority Critical patent/CN207508075U/en
Application granted granted Critical
Publication of CN207508075U publication Critical patent/CN207508075U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of stamping die, including upper mold and with the corresponding lower mould part in upper mold position, upper mold is provided with the punch of evagination, lower mould part includes slightly cutting mould and fine cut lower die into setting up and down successively, it is thick cut mould be provided with matched first die cavity of punch, fine cut lower die is provided with and matched second die cavity of punch, the first die cavity and the connection of the second die cavity, the longitudinal axis center of first die cavity and the second die cavity overlaps, and punch is pressed into the first die cavity and the second die cavity successively.The lower mould part of the stamping die of the utility model includes slightly cutting mould and fine cut lower die into setting up and down successively, and first the longitudinal axis center of die cavity and the second die cavity overlap, it is simple in structure, the thick of part can be completed in a procedure to cut and fine cut, only need one-time positioning, it does not need to reposition after thick cut, so the stamping die presswork rate of the utility model is high, manufacturing procedure is simple, does not allow to be also easy to produce substandard products, production cost is low.

Description

A kind of stamping die
Technical field
The utility model is related to technical field of mold, more particularly to a kind of stamping die.
Background technology
Stamping die is in Cold Press Working, by material(Metal is nonmetallic)It is processed into part(Or semi-finished product)'s A kind of special process equipment.At present, mobile phone Hardware fitting, intelligence dresses accessory (intelligent meter, Mobile phone camera bracket etc.), aluminium closes The outside punching press generally use stamping die of gold and stainless steel metal carries out punching press.To obtain preferable outside punching press effect, lead to Often be divided into and slightly cut stamping die and fine cut stamping die, i.e. workpiece after slightly cutting stamping die and slightly being cut, taking-up partly into Product obtain finished part after carrying out fine cut using fine cut stamping die.
Because the stamping die of the prior art is only slightly cut or the function of fine cut, part will obtain preferable outside punching press effect Thick cut need to be passed through to complete with fine cut twice manufacturing procedure, processing technology program is more, is required for positioning per procedure, and it is fixed to be easy to cause Position is inaccurate, and then generates bad finished product, therefore the stamping die yield rate of the prior art is low, and production cost is high.
Utility model content
The purpose of this utility model is that avoid shortcoming of the prior art and provide it is a kind of it is simple in structure, strike out The stamping die that product rate is high, manufacturing procedure is simple, production cost is low.
A kind of stamping die, including upper mold and with the corresponding lower mould part in upper mold position, the upper mold is provided with The punch of evagination, the lower mould part include successively into it is setting up and down it is thick cut mould and fine cut lower die, it is described thick to cut mould and set Be equipped with matched first die cavity of the punch, the fine cut lower die be provided with matched second die cavity of the punch, First die cavity is connected with second die cavity, and the longitudinal axis center of first die cavity and second die cavity overlaps, described Punch is pressed into first die cavity and second die cavity successively.
Preferably, the punch both sides of above-mentioned upper mold, which are provided with, positions the upper mold and the lower mould part during punching press Guide post, it is described thick to cut mould and be provided with and the matched first positioning hole of the guide post, the fine cut
Lower die is provided with and matched second location hole of the guide post, the first positioning hole and second location hole Connection, the guide post are sequentially inserted into the first positioning hole and second location hole.
Preferably, first die cavity of above-mentioned fine cut lower die and the bore of the second die cavity connectivity part, which are less than, slightly cuts The bore of mould lower end.
Preferably, the top of above-mentioned second die cavity is the cutting portion that inner wall is through state, lower part be inner wall be upper bore it is small, The big horn-like discharge part of lower relative aperture.
Preferably, above-mentioned stamping die be additionally provided with positioning it is described slightly cut mould and the pin of the fine cut lower die, it is described Fine cut lower die be provided with the matched third location hole of the pin, it is described it is thick cut mould and be provided with matched with the pin The 4th location hole, the third location hole connects with the 4th location hole, and the pin is sequentially inserted into the third positioning Hole and the 4th location hole.
Preferably, it is provided with buffer plate at the top of above-mentioned upper mold.
The utility model has the following advantages compared with prior art:The lower mould part packet of the stamping die of the utility model It includes and slightly cuts mould and fine cut lower die into setting up and down successively, slightly cut the first die cavity of mould and the second die cavity of fine cut lower die connects It is logical.During punching press, punch is pressed into first die cavity and second die cavity successively, i.e., embryo material, which disposably first passes through, slightly cuts mould First die cavity slightly cut, carry out fine cut using the second die cavity of fine cut lower die after, the part that is come out from fine cut lower die bottom Finished product.Since the lower mould part of the stamping die of the utility model includes slightly cutting under mould and fine cut into setting up and down successively Mould, and the longitudinal axis center of the first die cavity and the second die cavity overlaps, it is simple in structure, the thick of part can be completed in a procedure and is cut And fine cut, one-time positioning is only needed, does not need to reposition after thick cut, so the stamping die presswork rate of the utility model Height, manufacturing procedure are simple, do not allow to be also easy to produce substandard products, and production cost is low.
Description of the drawings
Using attached drawing, the utility model is described in further detail, but the embodiment in attached drawing is not formed to the utility model Any restrictions.
Fig. 1 is a kind of structure diagram of stamping die of the utility model.
Specific embodiment
The utility model is further described with attached drawing with the following Examples:
A kind of stamping die, as shown in Figure 1, including upper mold 10 and with the corresponding lower mould part 30 in 10 position of upper mold, on Mould 10 is provided with the punch 11 of evagination, and lower mould part 30 is included successively into setting up and down thick
Mould 40 and fine cut lower die 50 are cut, mould 40 is slightly cut and is provided with and 11 matched first die cavity 41 of punch, fine cut Lower die 50 is provided with to be connected with 11 matched second die cavity 51 of punch, the first die cavity 41 with the second die cavity 51, the first die cavity 41 It is overlapped with the longitudinal axis center of the second die cavity 51, punch 11 is pressed into the first die cavity 41 and the second die cavity 51 successively.
The lower mould part 30 of the stamping die of the utility model includes slightly cutting mould 40 and fine cut into setting up and down successively Lower die 50, the first die cavity 41 for slightly cutting mould 40 are connected with the second die cavity 51 of fine cut lower die 50.During punching press, punch 11 is pressed successively Enter the first die cavity 41 and the second die cavity 51, i.e. embryo material disposably first passes through thick the first die cavity 41 for cutting mould 40 and slightly cut, again After the second die cavity 51 by fine cut lower die 50 carries out fine cut, from the finished part of 50 bottom of fine cut lower die out.Due to this reality Included slightly cutting mould 40 and fine cut lower die 50, and first into setting up and down successively with the lower mould part 30 of novel stamping die The longitudinal axis center of 41 and second die cavity 51 of die cavity overlaps, simple in structure, and the thick of part can be completed in a procedure and is cut and smart It cuts, only needs one-time positioning, do not need to reposition after thick cut, so the stamping die presswork rate height of the utility model, Manufacturing procedure is simple, does not allow to be also easy to produce substandard products, and production cost is low.
Preferably, as shown in Figure 1,11 both sides of punch of upper mold 10 position upper mold 10 and lower mould part 30 when being provided with punching press Guide post 20, slightly cut mould 40 be provided with 20 matched first positioning hole 42 of guide post, fine cut lower die 50 is provided with and guide post 20 matched second location holes 52, first positioning hole 42 are connected with the second location hole 52, and guide post 20 is sequentially inserted into the first positioning 42 and second location hole 52 of hole.When the punch 11 of upper mold 10 is pressed into the first die cavity 41 and the second die cavity 51, guide post 20 is inserted successively Enter 42 and second location hole 52 of first positioning hole, positioning is played in guide post 20 and first positioning hole 42, the cooperation of the second location hole 52 The effect of upper mold 10 and lower mould part 30, prevents in punching course, 30 dystopy of upper mold 10 and lower mould part, to ensure stamping die The stability of 30 relative position of upper mold 10 and lower mould part during tool punching press, and then ensure the yield rate of stamping products.
Preferably, as shown in Figure 1, the bore of 51 connectivity part of the first die cavity 41 and the second die cavity of fine cut lower die 50 is less than slightly Cut the bore of 40 lower end of mould.Because fine cut is cut on the basis of thick cut, the first die cavity 41 of fine cut lower die 50 and the second mould The bore of 51 connectivity part of chamber is less than the bore for slightly cutting 40 lower end of mould, i.e., fine cut lower die 50 is in the first die cavity 41 and the second die cavity 51 Protrusion cutting position 53 can be formed on the top of connectivity part, and when embryo material enters fine cut, the rim charge of embryo material can be kept under fine cut after fine cut On the cutting position 53 that mould 50 protrudes, rim charge is not fallen out to the second die cavity 51, therefore is not in get stuck in punching course, is had Fine cut is smoothed out conducive to fine cut lower die 50.
Preferably, as shown in Figure 1, the top of the second die cavity 51 is the cutting portion 54 that inner wall is through state, under
Portion is that inner wall is the horn-like discharge part 55 that upper bore is small, lower relative aperture is big.The cutting portion 54 of through state is to embryo material Carry out fine cut, for that upper bore is small, lower relative aperture is big is horn-like, the inner wall of discharge part 55 has certain oblique for the inner wall of discharge part 55 Spend r so that rim charge and finished part after embryo material fine cut can be discharged smoothly, be not in get stuck.
Preferably, as shown in Figure 1, stamping die be additionally provided with positioning slightly cut mould 40 and the pin 70 of fine cut lower die 50, Fine cut lower die 50 be provided with 70 matched third location hole 56 of pin, slightly cut mould 40 be provided with it is matched with pin 70 4th location hole 46, third location hole 56 are connected with the 4th location hole 46, and pin 70 is sequentially inserted into third location hole 56 and the 4th Location hole 46.Pin 70 is sequentially inserted into 56 and the 4th location hole 46 of third location hole, i.e. pin 70 plays positioning and slightly cuts mould 40 It with the effect of fine cut lower die 50, can prevent in punching course, slightly cut mould 40 and fine cut lower die 50 since the effect of impulse force is produced Raw dystopy.
Preferably, as shown in Figure 1, the top of upper mold 10 is provided with buffer plate 80.Buffer plate 80 is loaded on upper mold 10 Buffering after 10 punching press of upper mold cutting during return, is played the role of in top.
Finally it should be noted that above example is only to illustrate the technical solution of the utility model rather than to this reality With the limitation of novel protected range, although being explained in detail with reference to preferred embodiment to the utility model, this field it is general Lead to it will be appreciated by the skilled person that can be modified or replaced equivalently to the technical solution of the utility model, without departing from this The spirit and scope of utility model technical solution.

Claims (6)

1. a kind of stamping die, which is characterized in that including upper mold and with the corresponding lower mould part in upper mold position, it is described on Mould is provided with the punch of evagination, the lower mould part include successively into it is setting up and down it is thick cut mould and fine cut lower die, it is described thick It cuts mould and is provided with and be provided with and the punch matched with matched first die cavity of the punch, the fine cut lower die Two die cavitys, first die cavity are connected with second die cavity, the longitudinal axis center weight of first die cavity and second die cavity It closes, the punch is pressed into first die cavity and second die cavity successively.
2. a kind of stamping die according to claim 1, it is characterised in that:The punch both sides of the upper mold are provided with Position the guide post of the upper mold and the lower mould part during punching press, the thick mould that cuts is provided with and the guide post matched the A positioning hole, the fine cut lower die are provided with and matched second location hole of the guide post, the first positioning hole and described Second location hole connects, and the guide post is sequentially inserted into the first positioning hole and second location hole.
3. a kind of stamping die according to claim 2, it is characterised in that:First die cavity of the fine cut lower die and The bore of the second die cavity connectivity part is less than the bore for slightly cutting mould lower end.
4. a kind of stamping die according to claim 3, it is characterised in that:It is straight that the top of second die cavity, which is inner wall, The cutting portion of logical shape, lower part are that inner wall is the horn-like discharge part that upper bore is small, lower relative aperture is big.
5. a kind of stamping die according to claim 4, it is characterised in that:The stamping die is additionally provided with described in positioning It is thick to cut mould and the pin of the fine cut lower die, the fine cut lower die be provided with the matched third location hole of the pin, It is described thick to cut mould and be provided with and matched 4th location hole of the pin, the third location hole and the 4th location hole Connection, the pin are sequentially inserted into the third location hole and the 4th location hole.
6. a kind of stamping die according to claim 5, it is characterised in that:Cushion pad is provided at the top of the upper mold Plate.
CN201721660732.9U 2017-12-01 2017-12-01 A kind of stamping die Expired - Fee Related CN207508075U (en)