CN207494342U - Mold - Google Patents
Mold Download PDFInfo
- Publication number
- CN207494342U CN207494342U CN201721289818.5U CN201721289818U CN207494342U CN 207494342 U CN207494342 U CN 207494342U CN 201721289818 U CN201721289818 U CN 201721289818U CN 207494342 U CN207494342 U CN 207494342U
- Authority
- CN
- China
- Prior art keywords
- lower die
- mold
- curvature
- radius
- heating tube
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model provides a kind of mold, includes:Upper die and lower die, the shape of the bottom surface of the upper mold is arc-shaped, the top surface of the lower die and the shape of the bottom surface of the upper mold match, the radius of curvature at the middle part of the bottom surface of the upper mold is more than the radius of curvature positioned at two sides part of the both sides at the middle part, the lower die is provided with several heating tubes, and the heating tube runs through the lower die.Heating tube is increased by the lower die in mold, different radius of curvature is designed in the contact surface of upper die and lower die, so that the mold does not need to be put into heating furnace and can produce the tungsten alloy plate of predetermined arc, the efficiency of processing is substantially increased, and save the cost of processing.
Description
Technical field
The utility model is related to a kind of Stamping Die Technology fields, and in particular to a kind of mold.
Background technology
In modern medical equipment, X-ray equipment is relatively common, such as CT machines, apparats for treating tumor (gamma knife) etc., this
For a little equipment in use, to prevent X-ray from revealing, common stereotype covers the gap of equipment.With being constantly progressive for technology, tungsten
Alloy material radian plate is more used, instead of the stereotype used originally.
At present, the making of tungsten alloy radian plate, typically using machining and the method for electrical discharge machining, both processing
Mode is required for the material for taking monoblock to be processed, and the utilization rate of material is very low, and process will also occupy largely
Process equipment, efficiency is very low, and cost is very high.
Utility model content
The technical problems to be solved in the utility model is the processing in order to overcome the making tungsten alloy radian plate of the prior art
Efficiency is low, it is of high cost the defects of, a kind of mold is provided.
The utility model is to solve above-mentioned technical problem by following technical proposals:
A kind of mold, includes:Upper die and lower die, the shape of the bottom surface of the upper mold be it is arc-shaped, the lower die
The shape of top surface and the bottom surface of the upper mold matches, the radius of curvature at the middle part of the bottom surface of the upper mold be more than be located at it is described in
The radius of curvature of two sides part of the both sides in portion, the lower die are provided with several heating tubes, and the heating tube is through described
Lower die.
Preferably, distance of the heating tube apart from the top surface of the lower die is 20mm-40mm.
Preferably, several described heating tubes are uniformly arranged in the lower die.
Preferably, the quantity of the heating tube is 8-15.
Preferably, the arc length of the middle part and the side part is equal.
Preferably, the radius of curvature at the middle part is 170mm, the radius of curvature of the side part is 148.5mm.
Preferably, the mold further includes hydraulic press, the hydraulic press includes hydraulic stem and base platform, the hydraulic stem
It is moved on the direction close to and far from the base platform, the upper mold is connected to the hydraulic stem, and the lower die is fixed
In the base platform.
The positive effect of the utility model is:Heating tube is increased by the lower die in mold, in upper die and lower die
Contact surface design different radius of curvature so that the mold, which does not need to be put into heating furnace and can produce the tungsten of predetermined arc, to be closed
Golden radian plate, substantially increases the efficiency of processing, and saves the cost of processing.
Description of the drawings
Fig. 1 is the dimensional structure diagram of the mold of the preferred embodiment of the utility model, and wherein tungsten alloy radian plate is put
It is placed in mold.
Fig. 2 is the structure diagram of the upper mold of the preferred embodiment of the utility model.
Reference sign
Upper mold 10
Middle part 11
Side part 12
Heating tube 20
Lower die 30
Hydraulic stem 40
Base platform 50
Tungsten alloy radian plate 60
Specific embodiment
The utility model is further illustrated below by the mode of embodiment, but be not therefore limited in the utility model
Among the embodiment described range.
As shown in Figs. 1-2, mold includes:Upper mold 10 and lower die 30, the shape of the bottom surface of upper mold 10 is arc-shaped, lower die 30
The shape of top surface and the bottom surface of upper mold 10 match, the radius of curvature at the middle part 11 of the bottom surface of upper mold 10, which is more than, is located at middle part 11
The radius of curvature of two sides part 12 of both sides, lower die 30 are provided with several heating tubes 20, and heating tube 20 runs through lower die 30.On
The bottom surface of mould 10 for arc-shaped and lower die 30 top surface shape it is matching be to meet processing tungsten alloy radian plate 60
Needs, the radius of curvature at the middle part 11 of upper mold 10 is identical with the radius of curvature of tungsten alloy radian plate 60 to complete, two
The radius of curvature of side part 12 is slightly less than the radius of curvature at middle part 11.When carrying out punch process to tungsten alloy radian plate 60, due to
Its rigidity is stronger, can generate certain rebound, and the radius of curvature of two sides part 12 is less than the design of the radius of curvature at middle part 11
It can solve the problems, such as that tungsten alloy radian plate 60 is sprung back in processing.Lower die 30 is designed with heating tube 20, and heating tube 20 runs through
Lower die 30 is in order to which lower die 30 is enable to heat tungsten alloy radian plate 60, in existing processing technology, to tungsten alloy arc
The processing temperature of degree plate 60 will reach 800-900 degrees Celsius, and reaching this temperature can only realize in heating furnace, and use the dress
Putting only needs lower die 30 being worked into 300-400 degrees Celsius, then coordinates the design of the radian of middle part 11 and two sides part 12, with regard to energy
It realizes the processing effect that original high temperature can be only achieved, also, can not need to operate in heating furnace using the device, significantly
Processing cost is saved, improves processing efficiency.
Distance of the heating tube 20 apart from the top surface of lower die 30 is 20mm-40mm.Heating tube 20 to lower die 30 top surface away from
From be by experiment repeatedly obtain as a result, keeping with a distance from this on the one hand to make lower die 30 heated rapidly, on the other hand
Avoid the structural stability that lower die 30 is influenced through lower die 30 due to heating tube 20.
Heating tube 20 is uniformly arranged in lower die 30.Also, the quantity of heating tube 20 is 8-15.The quantity of heating tube 20
It is also by obtained by experiment repeatedly, certainly, the quantity of heating tube 20 is more, the speed that lower die 30 heats will be faster, still,
Excessive heating tube 20 can improve the manufacture cost of mold, and the heating speed of the heating tube 20 of this quantity does not interfere with
Normal to use, heating tube 20 is uniformly arranged also for lower die 30 is enable to be evenly heated, the temperature phase of entire lower die 30
Together, so as to obtaining better processing effect.
Middle part 11 is equal with the arc length of side part 12.Also, the radius of curvature at middle part 11 be 170mm, two sides part 12
Radius of curvature be 148.5mm.The arc length of middle part 11 and two sides part 12 is equal and the curvature of middle part 11 and side part 12
The The concrete specification of radius is summarized by repetition test, can preferably solve returning after tungsten alloy radian plate 60 is processed
Bullet problem.
Mold further includes hydraulic press, and a part for hydraulic press is only illustrated in figure.Hydraulic press includes hydraulic stem 40 and pedestal
Platform 50, hydraulic stem 40 move on the direction close to and far from base platform 50, and upper mold 10 is connected to hydraulic stem 40, lower die
30 are fixed on base platform 50.In process, upper mold 10 and lower die 30 will be under the cooperations of hydraulic press to tungsten alloy radian plate
60 are operated, and hydraulic stem 40 connects upper mold 10 and moved, and lower die 30 is fixed on base platform 50.
The utility model is not limited to the above embodiment, no matter making any variation in its shape or structure, all falls within
Within the scope of protection of the utility model.The scope of protection of the utility model is defined by the appended claims, this field
Technical staff under the premise of the principle and essence without departing substantially from the utility model, a variety of changes can be made to these embodiments
More or change, but these change and modification each fall within the scope of protection of the utility model.
Claims (7)
1. a kind of mold, which is characterized in that it includes:Upper die and lower die, the shape of the bottom surface of the upper mold is arc-shaped, institute
The shape for stating the top surface and the bottom surface of the upper mold of lower die matches, and the radius of curvature at the middle part of the bottom surface of the upper mold is more than position
Radius of curvature in two sides part of the both sides at the middle part, the lower die are provided with several heating tubes, the heating tube
Through the lower die.
2. mold as described in claim 1, which is characterized in that distance of the heating tube apart from the top surface of the lower die be
20mm-40mm。
3. mold as described in claim 1, which is characterized in that several described heating tubes are uniformly arranged in the lower die.
4. the mold as described in any one of claim 1-3, which is characterized in that the quantity of the heating tube is 8-15.
5. mold as described in claim 1, which is characterized in that the arc length of the middle part and the side part is equal.
6. mold as described in claim 1, which is characterized in that the radius of curvature at the middle part is 170mm, the side part
Radius of curvature is 148.5mm.
7. mold as described in claim 1, which is characterized in that the mold further includes hydraulic press, and the hydraulic press includes liquid
Compression bar and base platform, the hydraulic stem move on the direction close to and far from the base platform, the upper mold connection
In the hydraulic stem, the lower die is fixed on the base platform.