CN207423725U - 一种检测铅膏视密度钢杯装置 - Google Patents
一种检测铅膏视密度钢杯装置 Download PDFInfo
- Publication number
- CN207423725U CN207423725U CN201721247330.6U CN201721247330U CN207423725U CN 207423725 U CN207423725 U CN 207423725U CN 201721247330 U CN201721247330 U CN 201721247330U CN 207423725 U CN207423725 U CN 207423725U
- Authority
- CN
- China
- Prior art keywords
- steel bowl
- cylindrical
- flat
- hemispherical
- apparent density
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型的目的是提供一种检测铅膏视密度钢杯装置。该钢杯腔体底部为半球形。该钢杯外部结构为:上部为圆柱形、下部为平底圆锥型;下部平底圆锥型的平底半径小于上部圆柱形的圆柱半径。进一步,该钢杯腔体上部为圆柱、下部为半球形。进一步,该钢杯腔体为半球形。本实用新型的有益效果是:腔体底部为半球形,这样的结构对比圆柱形腔体结构在敦实铅膏时容易挤出腔体及铅膏中的气体、更达到更好的检测效果。外面结构的上部为圆柱形、下部为平底圆锥型,锥型平底有利于减少钢杯重量。
Description
技术领域
本实用新型涉及铅酸蓄电池生产领域,具体涉及一种检测铅膏视密度钢杯装置。
背景技术
铅膏是极板活性物质的母体,在铅酸蓄电池中为电化学反应提供和储存所需的物质。铅膏视密度是指铅粉分散在硫酸和水的液体中自然堆积后其总重量与总体积之比。铅膏的视密度影响极板活性物质的孔隙率、从而影响铅酸蓄电池的容量和使用寿命。
铅膏视密度的测量方法:取适量的铅膏装入固定容积的钢杯里、使用设备敦实铅膏、使钢杯内无缝隙和气泡、重复进行直到铅膏充满钢杯、用直刀沿着杯口上刮去多余的铅膏、并将钢杯外部擦拭干净、称重、计算出铅膏视密度。目前所使用检测铅膏视密度钢杯装置为圆柱形、底面为平面、装入铅膏敦实时、气泡不容易挤出、影响检测结果。
发明内容
本实用新型的目的是提供一种更准确的检测铅膏视密度钢杯装置。
本实用新型的目的是以下述方式实现的:一种检测铅膏视密度钢杯装置,该钢杯腔体底部为半球形。该钢杯外部结构为:上部为圆柱形、下部为平底圆锥型;下部平底圆锥型的平底半径小于上部圆柱形的圆柱半径。
进一步,该钢杯腔体上部为圆柱、下部为半球形。
进一步,该钢杯腔体为半球形。
本实用新型的有益效果是:腔体底部为半球形,这样的结构对比圆柱形腔体结构在敦实铅膏时容易挤出腔体及铅膏中的气体、更达到更好的检测效果。外面结构的上部为圆柱形、下部为平底圆锥型,锥型平底有利于减少钢杯重量。
附图说明
图1是本实用新型剖视图,其中1为半球形腔体、2为圆柱形、3为平底圆锥形、4为平底
具体实施方式
如图1所示,一种检测铅膏视密度钢杯装置,该钢杯腔体1为半球形腔体,该钢杯腔体1也可以为上面圆柱形、下面半球形。
该钢杯外部结构为:上部为圆柱形2、下部为平底圆锥形3;平底4半径小于上部圆柱形2的半径。
具体实施时,钢杯里面加满铅膏、敦实,再倒铅膏到钢杯里面直到加满、敦实;如此循环3到4次。用直刀沿着杯口上刮去多余的铅膏、并将钢杯外部擦拭干净、称重、计算出铅膏视密度。
Claims (3)
1.一种检测铅膏视密度钢杯装置,其特征在于:钢杯腔体底部为半球形,所述钢杯外面结构的上部为圆柱形、下部为平底圆锥型;所述下部平底圆锥型的平底半径小于上部圆柱形的圆柱半径。
2.根据权利要求1所述一种检测铅膏视密度钢杯装置,其特征在于:所述钢杯腔体上部为圆柱、下部为半球形。
3.根据权利要求1所述一种检测铅膏视密度钢杯装置,其特征在于:所述钢杯腔体为半球形。