CN206671103U - 一种应力导向氢致开裂试验试样加载的装置 - Google Patents
一种应力导向氢致开裂试验试样加载的装置 Download PDFInfo
- Publication number
- CN206671103U CN206671103U CN201720271236.8U CN201720271236U CN206671103U CN 206671103 U CN206671103 U CN 206671103U CN 201720271236 U CN201720271236 U CN 201720271236U CN 206671103 U CN206671103 U CN 206671103U
- Authority
- CN
- China
- Prior art keywords
- main frame
- camber beam
- component
- test sample
- stress test
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型公开了一种应力导向氢致开裂试验试样加载的装置,包括主框架、M形组件、U形组件、和推力螺杆,所述M形组件为固定弯梁试样中间定距栓的预制件且将一对弯梁试样置于所述主框架的一侧,所述推力螺杆经所述主框架内弯梁试样的对应外侧开孔向内推进或退出所述U形组件,一对弯梁试样两端对称设有加载螺栓且伸出于所述主框架外侧。本实用新型的有益效果是:结构简单,成本低廉,操作容易,使用方便、工作效率高。
Description
技术领域
本实用新型涉及一种试样加载模具,特别涉及一种应力导向氢致开裂试验试样加载的装置。
背景技术
应力导向氢致开裂(SOHIC)是一种硫化物应力腐蚀开裂试验,国际现行的评价湿硫化氢环境下钢板抗应力导向氢致开裂的标准试验。该试验标准规定每组试样由两个外侧带预制裂纹的弯梁、两个圆柱形定距栓、两个螺栓和两个螺母组成。根据标准公式计算需给弯梁加载的挠度数值,装配好的试样是两个弯梁中间夹两个圆柱形定距栓,通过弯梁两端螺栓螺母加载,两定距栓距离为定值且两定距栓中线与两弯梁上预制裂纹重合。以上诸多要求,使得试样装配加载困难,生产效率低。
发明内容
本实用新型所要解决的技术问题是提供一种能够提高工作效率、方便简单、容易使用的专用装配加载模具。
为了解决上述技术问题,本实用新型采用的技术方案是:一种应力导向氢致开裂试验试样加载的装置,包括主框架、M形组件、 U形组件、和推力螺杆,所述M形组件为固定弯梁试样中间定距栓的预制件且将一对弯梁试样置于所述主框架的一侧,所述推力螺杆经所述主框架内弯梁试样的对应外侧开孔向内推进或退出所述U 形组件,一对弯梁试样两端对称设有加载螺栓且伸出于所述主框架外侧。
所述M形组件设有与所述定距栓相适配的栓孔。
所述M形组件上设有定位标记。
所述主框架侧面下方有缓冲应力槽。
本实用新型的有益效果是:结构简单,成本低廉,操作容易,使用方便、工作效率高。
附图说明
图1为本实用新型的一种应力导向氢致开裂试验试样加载的装置结构主视示意图;
图2为本实用新型的一种应力导向氢致开裂试验试样加载的装置结构俯视结构示意图;
图3为本实用新型的一种应力导向氢致开裂试验试样加载的装置结构的M形组件侧视示意图。
图中:
1.弯梁试样 2.U形组件 3.主框架 4.M形组件
5.定距栓 6.推力螺杆 7.加载螺栓
8.缓冲应力槽
具体实施方式
下面结合附图和具体实施方式对本实用新型作进一步详细说明:
如图1、图2所示,一种应力导向氢致开裂试验试样加载的装置包括弯梁试样1、U形组件2、主框架3、M形组件4、定距栓5、推力螺杆6、加载螺栓7。首先,将两个定距栓5放入M形组件4 内。将装配好的M形组件4放在两个弯梁试样1中间,利用M形组件4上的定位线与弯梁1上预制裂纹线进行初步对准定位。其次,用U形组件2两个支点顶住弯梁1,用推力螺杆6顶住U形组件2 另一侧面,微调M形4装配组件与弯梁的相对位置,旋转推力螺杆 6施加预推力。最后,将加载螺栓7放入弯梁试样1两端孔中,用扳手旋紧螺母加载至试验预设强度所对应的挠度。旋松推力螺杆6,抽出M形组件4,即可完成一套加载好的SOHIC试样待试验。
通过手动调节模具主框架3上的推力螺杆6可以满足对不同厚度弯梁试样1装配时施加预推力,两个弯梁试样1间有M形组件4 用于定位定距栓5及定距栓5与弯梁试样1的相对位置,通过U形组件2的两个固定支点及主框架3侧面可以稳固一对弯梁试样1及之间定距栓组件,确保一对弯梁试样1加载过程中整套试样各部分位置稳固,M形组件4上有定位标记,加载模具主框架3固定面拐角处预留有缓冲应力槽8。
弯梁试样1装配加载模具,可以将两个圆柱形定距栓7装入M 形组件4内,该组件主要有两个作用,一是准确定位两圆柱形支点和两个弯梁试样的相对位置;二是固定两个圆柱形支点的距离。将装有定距栓5的M形组件4置于一对弯梁试样1之间,并竖立在模具主框架3上。U形框架2两个支点顶住弯梁试样1侧面,通过主框架3上的螺栓杆6顶住U形框架2另外一侧面。最后微调两一对弯梁试样1与M形组件4的相对位置。旋紧推力螺杆6。最后装配弯梁试样1两端加载螺栓7到试验预设强度所对应的挠度。
Claims (4)
1.一种应力导向氢致开裂试验试样加载的装置,其特征是:包括主框架(3)、M形组件(4)、U形组件(2)、和推力螺杆(6),所述M形组件(4)为固定弯梁试样中间定距栓(5)的预制件且将一对弯梁试样(1)置于所述主框架(3)的一侧,所述推力螺杆(6)经所述主框架(3)内弯梁试样(1)的对应外侧开孔向内推进或退出所述U形组件(2),一对弯梁试样(1)两端对称设有加载螺栓(7)且伸出于所述主框架(3)外侧。
2.根据权利要求1所述的一种应力导向氢致开裂试验试样加载的装置,其特征是:所述M形组件(4)设有与所述定距栓(5)相适配的栓孔。
3.根据权利要求2所述的一种应力导向氢致开裂试验试样加载的装置,其特征是:所述M形组件(4)上设有定位标记。
4.根据权利要求1所述的一种应力导向氢致开裂试验试样加载的装置,其特征是:所述主框架(3)侧面下方有缓冲应力槽(8)。