CN206467974U - A kind of novel negative ion purification air removes aldehyde health care wear-resisting floor wearing floor - Google Patents
A kind of novel negative ion purification air removes aldehyde health care wear-resisting floor wearing floor Download PDFInfo
- Publication number
- CN206467974U CN206467974U CN201621284991.1U CN201621284991U CN206467974U CN 206467974 U CN206467974 U CN 206467974U CN 201621284991 U CN201621284991 U CN 201621284991U CN 206467974 U CN206467974 U CN 206467974U
- Authority
- CN
- China
- Prior art keywords
- floor
- layer
- health care
- purification air
- wear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model is related to a kind of novel negative ion purification air and removes aldehyde health care wear-resisting floor wearing floor, including, floor body, the anion that the floor body includes from top to bottom closely setting successively expedites the emergence of particle coating, wear resistant paint surface layer, high artificial stereo graining flaggy, wooden substrate layer, and balance layer;The lower surface of the floor body is uniformly provided with some interior grooves along the length direction of floor body;Wherein described high artificial stereo graining flaggy includes the upper high artificial stereo graining flaggy, magnetic therapy layer and lower high artificial stereo graining flaggy from top to bottom fitted successively;And two groups of relative side end faces of the floor body are provided with the T-shaped connected structure for grafting.
Description
Technical field
The utility model belongs to construction material, and in particular to a kind of novel negative ion purification air removes aldehyde health care wear-resistingly
Plate.
Background technology
Floor is due to after ground, it is impossible to arbitrarily change, therefore, improves wearability the making for floor on floor
It is extremely important with the life-span.Floor is all that the splicing of one piece of block is used on ground, therefore, stitching portion compared to floor other surface layers more
Easily worn and torn by sole, if not doing breakage-proof design, it is easy to broken in the outer surface of stitching portion with the growth of use time
Damage.
Remove the enhancing that aldehyde is realized as health of people purifies air, people also can floor performance propose it is more rich will
Ask, be no longer single durability, aldehyde and healthcare function are removed with greater need for purification air is met.Anion is otherwise known as, and " air is tieed up
Raw element ", can not only facilitate human body to synthesize and vitamin storage, and the physiological activity of reinforcing and human activin, therefore production
The floor for possessing negative ion releasing function can be in domestic environment, and floor covering layers area is wide, thus can discharge on a large scale bear from
Son, purifies air, strengthens body immunity.
Utility model content
The purpose of this utility model is to provide a kind of novel negative ion purification air and removes aldehyde health care wear-resisting floor wearing floor, to realize tool
There is release anion fine-purification air to remove aldehyde and bound edge breakage-proof, anti abrasive technique effect.
In order to solve the above-mentioned technical problem, the utility model provides a kind of novel negative ion purification air except aldehyde health care is resistance to
Floor is ground, including, floor body, the anion that the floor body includes from top to bottom closely setting successively expedites the emergence of particle painting
Layer, wear resistant paint surface layer, high artificial stereo graining flaggy, wooden substrate layer, and balance layer;The lower surface of the floor body
It is uniformly provided with some interior grooves along the length direction of floor body;Wherein described high artificial stereo graining flaggy includes
Upper high artificial stereo graining flaggy, magnetic therapy layer and the lower high artificial stereo graining flaggy from top to bottom fitted successively;
And two groups of relative side end faces of the floor body are provided with the T-shaped connected structure for grafting;Described T-shaped grafting knot
Structure includes being respectively arranged on the male tenon tongue of the relative two side ends in floor and the female tenon groove with the male tenon tongue form fit;The male tenon
Tongue includes public big tenon shoulder, joint tongue and public small tenon shoulder;The female tenon groove includes female vat shoulder, slotted eyes and female sulculus shoulder;It is described public big
Tenon shoulder top is provided with arc angling with floor body upper surface intersection;Handed over floor body upper surface on female vat shoulder top
Arc angling is provided with boundary.
Further, the upper surface of the wooden substrate layer is provided with the groove that several are in genesis analysis;And the groove
Inside is filled with tourmaline powder.
Further, the balance layer lower surface is additionally provided with bacteria mildew-proof layer;Bacteria mildew-proof layer uses FS bacteria mildew-proofs
Dope layer.
Further, the vertical height of the joint tongue is less than the vertical height of described slotted eyes;And the joint tongue upper surface
Horizontal length be less than described slotted eyes in upper surface horizontal length;The public affairs on one of floor in i.e. adjacent two pieces of floors
The female tenon eye access section of joint tongue and another floorboard forms a gap.
Further, the upper surface of the joint tongue is provided with the card article that section is isosceles triangle;And the slotted eyes is interior
Upper surface is provided with the neck that the section being caught in suitable for described card article is isosceles triangle.
Further, the upper high artificial stereo graining flaggy and lower high artificial stereo graining flaggy include one
Substrate, lays one layer of plastic uptake film on this substrate, and the plastic uptake film surface printing is textured, and the texture is and wood texture one
The stereo wood pattern of the convex-concave structure of cause.
Further, the wear resistant paint surface layer includes transparent priming, the Al set gradually from bottom to up2O3Wear-resistant primer, two layers
UV finish paints and one layer of nano wearproof paint.
Further, the balance layer uses melamine balance paper, and its specification is 120g.
Further, the outer surface of the T-shaped connected structure is coated with wax layer;And said wax layer uses the nanometer emulsified waxes of EM
Layer.
Further, the quantity of the interior groove is 4-6 bars.
The beneficial effects of the utility model are that this novel negative ion purification air removes aldehyde health care wear-resisting floor wearing floor, by setting
Anion expedite the emergence of particle coating, can discharge anion, kill the bacterium that floor body shows, pure and fresh room air strengthens people
The immunity of body.The magnetic field formed by the magnetic therapy layer of setting can influence body current distribution, the motion of charged microparticle, sarolemma system
The permeability of system and the magnetic moment orientation of boiomacromolecule etc., change histiocytic physiology, biochemical process, produce analgesia, disappear
Swollen, the promotion effect such as blood and Lymphatic Circulation, can play good magnetic therapy effect.By on public big the tenon shoulder top and floor
Body upper surface intersection is provided with arc angling;Fallen with floor body upper surface intersection provided with arc on female vat shoulder top
Angle so that two pieces of timber floor stitching portions form the chamfering bound edge of arc, the chamfering of arc improves floor general right angle
Breakage-proof.By the bacteria mildew-proof layer of setting, with antibacterial, mould proof effect, because floor is laid immediately on ground,
Ground easily breed bacteria, therefore bacteria mildew-proof layer is set in the floor end face adjacent with ground under moist weather,
Be conducive to isolating the bacterium of ground surface, prevent invasion and attack of the bacterium to floor body.Further through the T set at the two ends of floor body
Shape connected structure, T shape connected structure buckles are compared with the male tenon and female tenon for being traditionally used for grafting, and contact area is bigger, with reference to tighter
Close, the non-deformability service life for adding floor is long.
Brief description of the drawings
The utility model is further illustrated with reference to the accompanying drawings and examples.
Fig. 1 is the side structure schematic diagram that novel negative ion purification air of the present utility model removes aldehyde health care wear-resisting floor wearing floor;
Fig. 2 is novel negative ion purification air of the present utility model except knot at two pieces of floor splicings of aldehyde health care wear-resisting floor wearing floor
Structure schematic diagram;
Fig. 3 is the cross-sectional view that novel negative ion purification air of the present utility model removes aldehyde health care wear-resisting floor wearing floor.
In figure:Male big tenon shoulder 1, joint tongue 2, male small tenon shoulder 3, female vat shoulder 4, slotted eyes 5, female sulculus shoulder 6, arc angling 7, card
Bar 8, neck 9, interior groove 10, gap 11, anion expedite the emergence of particle coating 12, wear resistant paint surface layer 13, upper high artificial stereo wood grain
Decorative plies 14, magnetic therapy layer 15, lower high artificial stereo graining flaggy 16, wooden substrate layer 17, balance layer 18, bacteria mildew-proof layer
19th, groove 20.
Embodiment
The utility model is described in further detail presently in connection with accompanying drawing.These accompanying drawings are simplified schematic diagram,
Only illustrate basic structure of the present utility model in a schematic way, therefore it only shows the composition relevant with the utility model.
As shown in Figure 1 to Figure 3, a kind of novel negative ion purification air of the present utility model removes aldehyde health care wear-resisting floor wearing floor, bag
Include, floor body, the anion that the floor body includes from top to bottom closely setting successively expedites the emergence of particle coating 12, wear resistant paint
Surface layer 13, high artificial stereo graining flaggy, wooden substrate layer 17, and balance layer 18;The lower surface of the floor body is equal
It is even to be provided with some interior grooves 10 along the length direction of floor body;Wherein described high artificial stereo graining flaggy includes
Upper high artificial stereo graining flaggy 14, magnetic therapy layer 15 and the lower high artificial stereo wood grain decorative sheet from top to bottom fitted successively
Layer 16;And two groups of relative side end faces of the floor body are provided with the T-shaped connected structure for grafting;Described T-shaped
Connected structure includes being respectively arranged on the male tenon tongue 2 of the relative two side ends in floor and the female tenon groove with the form fit of male tenon tongue 2;
The male tenon tongue 2 includes public big tenon shoulder 1, joint tongue 2 and public small tenon shoulder 3;The female tenon groove includes female vat shoulder 4, slotted eyes 5 and mother
Sulculus shoulder 6;The public big top of tenon shoulder 1 is provided with arc angling 7 with floor body upper surface intersection;On female vat shoulder 4
Portion is provided with arc angling 7 with floor body upper surface intersection.
The permanent magnet specifically, the magnetic therapy layer 15 is uniformly arranged, the pole polarity of the permanent magnet is identical, magnetic field intensity phase
Together.The magnetic field of permanent magnet formation can influence body current distribution, the motion of charged microparticle, the permeability of sarolemma system and biology high
Magnetic moment orientation of molecule etc., changes histiocytic physiology, biochemical process, produces analgesia, detumescence, promotes blood and lymph to follow
Ring etc. is acted on, and can play good magnetic therapy effect.
Specifically, the thickness of the wooden substrate layer 17 is 0.85- 1.1cm.Optionally, the wooden substrate layer 17 is using pine
Wood or birch are made, environmental protection.
The upper surface of the wooden substrate layer 17 is provided with the groove 20 that several are in genesis analysis;And in the groove 20
Portion is filled with tourmaline powder.By being filled with tourmaline powder inside the wooden upper surface upper groove 20 of substrate layer 17, with tourmaline powder
It is used as anion occurring source so that wooden substrate layer 17, which can turn into, produces anion source, further enhances of the present utility modelly
The negative ion releasing function of plate.
The lower surface of balance layer 18 is additionally provided with bacteria mildew-proof layer 19;Bacteria mildew-proof layer 19 is applied using FS bacteria mildew-proofs
The bed of material.With antibacterial, mould proof effect, because floor is laid immediately on ground, ground is easily grown under moist weather
Endophytic bacteria, therefore bacteria mildew-proof layer 19 is set in the floor end face adjacent with ground, be conducive to isolating the bacterium of ground surface,
Prevent invasion and attack of the bacterium to floor body.
The vertical height of the joint tongue 2 is less than the vertical height of described slotted eyes 5;And the water of the upper surface of joint tongue 2
Flat length is less than the horizontal length of upper surface in described slotted eyes 5;The male tenon on one of floor in i.e. adjacent two pieces of floors
The female tenon eye access section of tongue 2 and another floorboard forms a gap 11.The gap 11 is conducive to providing space to a certain extent
To buffer wooden substrate layer 17 due to natural expansion and contraction, wooden dipper may occur in use, turn round or the deformation such as split and be existing
As.
The upper surface of the joint tongue 2 is provided with the card article 8 that section is isosceles triangle;And the interior upper end of the slotted eyes 5
Face is provided with the neck 9 that the section being caught in suitable for described card article 8 is isosceles triangle.Improved by the engaging of card article 8 and neck 9
Snap-in force during two pieces of wood board splicings, because with the growth of plank use time, outside the stitching portion of male tenon tongue 2 and female tenon groove
Surface may wear and tear, and cause snap-in force to reduce.
The upper high artificial stereo graining flaggy 14 and lower high artificial stereo graining flaggy 16 include a base
Bottom, and one layer of plastic uptake film is laid on this substrate, the plastic uptake film surface printing is textured, and the texture is and wood texture
The stereo wood pattern of consistent convex-concave structure.Specifically, the substrate is using such as, but not limited to timber or other non-wood plants
Any one in material (such as stalk, grass blade), such as particieboard, glued board, fiberboard.Optionally, the plastic uptake film is adopted
Use PVC plastic uptakes.
The wear resistant paint surface layer 13 includes transparent priming, the Al set gradually from bottom to up2O3Wear-resistant primer, two layers of UV face
Paint and one layer of nano wearproof paint.
The balance layer 18 uses melamine balance paper, and its specification is 120g.Balance layer 18 can be balanced in floor body
Portion's stress, and play a part of preventing moisture, moisture in concrete floor to be corroded into floor body.
The outer surface of the T-shaped connected structure is coated with wax layer;And said wax layer uses the nanometer emulsified wax layers of EM.Using
The nanometer emulsified waxes of EM and common paraffin phase ratio, the fusing point of the nanometer emulsified waxes of EM is up to 58 degree, significantly larger than common paraffin
Fusing point (common melting point of paraffin wax is 30 degree), so if using traditional paraffin, when indoor temperature is higher than 30 degree, paraffin
Layer can be tacky, so as to influence the normal of floor to use, and uses the problem of nanometer emulsified waxes of EM are not in then similar.And EM
Nanometer emulsified wax is nano level emulsifying wax, and the molecular structure of wax is thinner, and the fiber for being easier to go deep into timber than common paraffin is led
Pipe, its time of penetration is short, permeates deeper into thorough, reaches that depth oozes the purpose of wax, rather than rest on the surface layer of plank.
Optionally, the nanometer emulsified waxes of the EM are received using the EM of such as, but not limited to Shanghai Joule Wax Industry Co., Ltd production
Rice emulsifying wax.
The quantity of the interior groove 10 is 4- 6.6 are preferably arranged to, is uniformly equally spaced in the lower end of floor body
Face.
Using it is above-mentioned according to desirable embodiment of the present utility model as enlightenment, pass through above-mentioned description, related work people
Member can carry out various changes and amendments in the range of without departing from this utility model technological thought completely.This reality
The content on specification is not limited to new technical scope, it is necessary to its technology is determined according to right
Property scope.
Claims (10)
1. a kind of novel negative ion purification air removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that including, floor body, describedly
The anion that plate body includes from top to bottom closely setting successively expedites the emergence of particle coating, wear resistant paint surface layer, high artificial stereo wood grain
Decorative plies, wooden substrate layer, and balance layer;The lower surface of the floor body is uniformly provided with some length along floor body
Spend the interior groove in direction;Wherein
The high artificial stereo graining flaggy include from top to bottom fit successively upper high artificial stereo graining flaggy,
Magnetic therapy layer and lower high artificial stereo graining flaggy;And
Two groups of relative side end faces of the floor body are provided with the T-shaped connected structure for grafting;
Described T-shaped connected structure include be respectively arranged on the relative two side ends in floor male tenon tongue and with the male tenon ligulate shape
The female tenon groove matched somebody with somebody;
The male tenon tongue includes public big tenon shoulder, joint tongue and public small tenon shoulder;The female tenon groove includes female vat shoulder, slotted eyes and female sulculus
Shoulder;The public big tenon shoulder top is provided with arc angling with floor body upper surface intersection;Female vat shoulder top and floor
Body upper surface intersection is provided with arc angling.
2. anion fine-purification air according to claim 1 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the wooden base material
The upper surface of layer is provided with the groove that several are in genesis analysis;And
The inside grooves are filled with tourmaline powder.
3. anion fine-purification air according to claim 2 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the balance layer
Lower surface is additionally provided with bacteria mildew-proof layer;Bacteria mildew-proof layer uses FS bacteria mildew-proof dope layers.
4. anion fine-purification air according to claim 3 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the joint tongue
Vertical height is less than the vertical height of described slotted eyes;And
The horizontal length of the joint tongue upper surface is less than the horizontal length of upper surface in described slotted eyes;I.e.
The female tenon groove access section of the male tenon tongue on one of floor and another floorboard forms a gap in adjacent two pieces of floors.
5. anion fine-purification air according to claim 4 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the joint tongue
Upper surface is provided with the card article that section is isosceles triangle;And
The interior upper surface of the slotted eyes is provided with the neck that the section being caught in suitable for described card article is isosceles triangle.
6. anion fine-purification air according to claim 5 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the upper Gao Fang
True stereo wood grain decoration board layer and lower high artificial stereo graining flaggy include a substrate, and one layer of suction is laid on this substrate
Plastic film, the plastic uptake film surface printing is textured, and the texture is the stereo wood pattern of the convex-concave structure consistent with wood texture.
7. anion fine-purification air according to claim 6 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the wear resistant paint
Surface layer includes transparent priming, the Al set gradually from bottom to up2 O3Wear-resistant primer, two layers of UV finish paint and one layer of nano wearproof paint.
8. anion fine-purification air according to claim 7 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the balance layer
Using melamine balance paper, its specification is 120g.
9. anion fine-purification air according to claim 8 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that the T-shaped is inserted
The outer surface of binding structure is coated with wax layer;And
Said wax layer uses the nanometer emulsified wax layers of EM.
10. anion fine-purification air according to claim 9 removes aldehyde health care wear-resisting floor wearing floor, it is characterised in that described interior logical
The quantity of groove is 4-6 bars.