CN206264501U - Anti-dazzle frosted film - Google Patents

Anti-dazzle frosted film Download PDF

Info

Publication number
CN206264501U
CN206264501U CN201621338079.XU CN201621338079U CN206264501U CN 206264501 U CN206264501 U CN 206264501U CN 201621338079 U CN201621338079 U CN 201621338079U CN 206264501 U CN206264501 U CN 206264501U
Authority
CN
China
Prior art keywords
layer
silica gel
covered
setting
ultraviolet resistant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201621338079.XU
Other languages
Chinese (zh)
Inventor
陈元平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan East New Material Co Ltd
Original Assignee
Dongguan East New Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan East New Material Co Ltd filed Critical Dongguan East New Material Co Ltd
Priority to CN201621338079.XU priority Critical patent/CN206264501U/en
Application granted granted Critical
Publication of CN206264501U publication Critical patent/CN206264501U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of anti-dazzle frosted film, includes and uses layer, layer of silica gel, release layer, ultraviolet resistant layer, anti-reflection layer, cushion and wearing layer;The layer of silica gel is covered on the bottom surface using layer, and the release layer is fitted in the bottom surface of layer of silica gel, and the ultraviolet resistant layer is covered on the surface using layer, and the anti-reflection layer is covered on the surface of ultraviolet resistant layer.By setting layer of silica gel; so that this product is repeatable and pasting and not staying any vestige; by setting ultraviolet resistant layer; ultraviolet can effectively be prevented; strengthen the colorfulness of display screen; by setting anti-reflection layer, can effectively prevent light from reflecting, so as to avoid dazzle from producing; by setting cushion; part direct collision can be effectively absorbed, display screen is preferably protected, by setting wearing layer; and the surface on wearing layer forms frosting; can be effectively antifouling, and further antireflection, while the abrasion of style of writing can be prevented effectively.

Description

Anti-dazzle frosted film
Technical field
The utility model is related to protection of film art, refers in particular to a kind of anti-dazzle frosted film.
Background technology
With the development of science and technology the use of intelligent terminal is more and more universal.The display screen of usual intelligent terminal Be LCDs or LED display, its have the advantages that it is thin, light, can touch-control sensing, but these display screen not scratch resistances Wipe, while be also easy to be damaged because colliding with or clashing into, so generally paste layer protecting film in display screen surface or increase patch One layer of stiffened film layer, to improve the service life of display.
However, it is all more single currently used for the diaphragm 26S Proteasome Structure and Function on display screen, easily produce dazzle, influence to use The use at family.Therefore, it is necessary to be improved to current display screen protection film.
The content of the invention
In view of this, in view of the existing deficiencies of the prior art, its main purpose is to provide a kind of anti-dazzle to the utility model Frosted film, it can effectively solve the problems, such as that existing display screen protection film 26S Proteasome Structure and Function is single and easily produce dazzle.
To achieve the above object, the utility model is using following technical scheme:
A kind of anti-dazzle frosted film, includes and uses layer, layer of silica gel, release layer, ultraviolet resistant layer, anti-reflection layer, buffering Layer and wearing layer;The layer of silica gel is covered on the bottom surface using layer, and the release layer is fitted in the bottom surface of layer of silica gel, the UV resistance Line layer is covered on the surface using layer, and the anti-reflection layer is covered on the surface of ultraviolet resistant layer, and the cushion is covered in anti- On the table in reflecting layer, the wearing layer is covered on the surface of cushion, and the surface of wearing layer is frosting.
Preferably, the use layer is 90-100 μm.
Preferably, the thickness of the layer of silica gel is 20-25 μm.
Preferably, the release layer is PET materials, and its thickness is 10-15 μm.
Preferably, the thickness of the ultraviolet resistant layer is 30-35 μm.
Preferably, the thickness of the anti-reflection layer is 25-30 μm.
Preferably, the thickness of the cushion is 30-35 μm.
Preferably, the thickness of the wearing layer is 30-35 μm.
The utility model has clear advantage and beneficial effect compared with prior art, specifically, by above-mentioned technology Scheme understands:
By setting layer of silica gel so that this product is repeatable to paste and do not stay any vestige, by setting antiultraviolet Layer, can effectively prevent ultraviolet, strengthen the colorfulness of display screen, by setting anti-reflection layer, can effectively prevent light from reflecting, so that Avoid dazzle from producing, by setting cushion, can effectively absorb part direct collision, preferably protect display screen, by setting Wearing layer, and the surface formation frosting on wearing layer, can be effectively antifouling, and further antireflection, while can effectively prevent The abrasion of style of writing.
More clearly to illustrate architectural feature of the present utility model and effect, come right with specific embodiment below in conjunction with the accompanying drawings The utility model is described in detail.
Brief description of the drawings
Fig. 1 is the sectional view of the preferred embodiment of the utility model.
Accompanying drawing identifier declaration:
10th, layer 20, layer of silica gel is used
30th, release layer 40, ultraviolet resistant layer
50th, anti-reflection layer 60, cushion
70th, wearing layer 71, frosted layer.
Specific embodiment
Refer to shown in Fig. 1, that show the concrete structure of the preferred embodiment of the utility model, include and use layer 10th, layer of silica gel 20, release layer 30, ultraviolet resistant layer 40, anti-reflection layer 50, cushion 60 and wearing layer 70.
This is the PET materials of good toughness using layer 10, is hardly damaged, and the use of the thickness of layer 10 is 90-100 μm.
The layer of silica gel 20 is covered on the bottom surface using layer 10, and the thickness of the layer of silica gel 20 is 20-25 μm, can prevent gas Bubble is formed, and repeatable stickup does not stay any vestige.
The release layer 30 is fitted in the bottom surface of layer of silica gel 20, and the release layer 30 is PET materials, and its thickness is 10-15 μm.
The ultraviolet resistant layer 40 is covered on the surface using layer 10, and the thickness of the ultraviolet resistant layer 40 is 30-35 μm, It is non-reflective without rainbow line, the effect with antiultraviolet and enhancing display screen colorfulness.
The anti-reflection layer 50 is covered on the surface of ultraviolet resistant layer 40, and the thickness of the anti-reflection layer 50 is 25-30 μm, To prevent reflection.
The cushion 60 is covered on the table of anti-reflection layer 50, and the thickness of the cushion 60 is 30-35 μm, can effectively be inhaled Display screen is protected in receiving portions direct collisions.
The wearing layer 70 is covered on the surface of cushion 60, and the surface of wearing layer 70 is frosting 71, described wear-resisting The thickness of layer 70 is 30-35 μm, can effectively prevent the abrasion of style of writing, and with antifouling effect, hardness up to 3H, with wear-resisting effect Really.
During making, first shaping uses layer 10, then, layer of silica gel 20 is formed in the bottom-surface coated silica gel using layer 10, connects , release layer 30 be fitted in the bottom surface of layer of silica gel 20, then, ultraviolet resistant layer 40 is covered on the surface using layer 10, Then, the surface of ultraviolet resistant layer 40 is coated with anti-reflection material and forms anti-reflection layer 50, then, cushion 60 is covered in anti- On the surface in reflecting layer 50, finally, wearing layer 70 is molded on the surface of cushion 60, and surface to wearing layer 70 carries out table Face frosted is processed and forms frosted layer 71.
When using, release layer 30 is torn, then, layer of silica gel 20 is fitted with the surface of display screen.
Design focal point of the present utility model is:By setting layer of silica gel so that this product is repeatable to paste and do not remain in office What vestige, by setting ultraviolet resistant layer, can effectively prevent ultraviolet, strengthen the colorfulness of display screen, by setting antireflection Layer, can effectively prevent light from reflecting, and so as to avoid dazzle from producing, by setting cushion, can effectively absorb part direct collision, more Display screen is protected well, by setting wearing layer, and surface on wearing layer forms frosting, can be effectively antifouling, go forward side by side one Step antireflection, while the abrasion of style of writing can be prevented effectively.
Know-why of the present utility model is described above in association with specific embodiment.These descriptions are intended merely to explain this reality With new principle, and can not by any way be construed to the limitation to the utility model protection domain.Based on explanation herein, Those skilled in the art associates other specific embodiments of the present utility model by would not require any inventive effort, These modes are fallen within protection domain of the present utility model.

Claims (8)

1. a kind of anti-dazzle frosted film, it is characterised in that:Include and use layer, layer of silica gel, release layer, ultraviolet resistant layer, counnter attack Penetrate layer, cushion and wearing layer;The layer of silica gel is covered on the bottom surface using layer, and the release layer is fitted in the bottom of layer of silica gel Face, the ultraviolet resistant layer is covered on the surface using layer, and the anti-reflection layer is covered on the surface of ultraviolet resistant layer, the buffering Layer is covered on the table of anti-reflection layer, and the wearing layer is covered on the surface of cushion, and the surface of wearing layer is frosting.
2. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The use layer is 90-100 μm.
3. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The thickness of the layer of silica gel is 20-25 μm.
4. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The release layer is PET materials, and its thickness is 10-15μm。
5. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The thickness of the ultraviolet resistant layer is 30-35 μm.
6. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The thickness of the anti-reflection layer is 25-30 μm.
7. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The thickness of the cushion is 30-35 μm.
8. anti-dazzle frosted film as claimed in claim 1, it is characterised in that:The thickness of the wearing layer is 30-35 μm.
CN201621338079.XU 2016-12-08 2016-12-08 Anti-dazzle frosted film Expired - Fee Related CN206264501U (en)