CN206200093U - A kind of process units of efficient control continuous casting bleed-out - Google Patents

A kind of process units of efficient control continuous casting bleed-out Download PDF

Info

Publication number
CN206200093U
CN206200093U CN201621247365.5U CN201621247365U CN206200093U CN 206200093 U CN206200093 U CN 206200093U CN 201621247365 U CN201621247365 U CN 201621247365U CN 206200093 U CN206200093 U CN 206200093U
Authority
CN
China
Prior art keywords
induction coil
crystallizer
bleed
river
contact rod
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201621247365.5U
Other languages
Chinese (zh)
Inventor
亢淑梅
陈婷婷
沈明钢
荣子昂
李成威
金辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
University of Science and Technology Liaoning USTL
Original Assignee
University of Science and Technology Liaoning USTL
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by University of Science and Technology Liaoning USTL filed Critical University of Science and Technology Liaoning USTL
Priority to CN201621247365.5U priority Critical patent/CN206200093U/en
Application granted granted Critical
Publication of CN206200093U publication Critical patent/CN206200093U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model is related to a kind of process units of efficient control continuous casting bleed-out, including contact rod, induction coil, the conductive mouth of a river, crystallizer, the conductive mouth of a river is arranged in the middle of crystallizer, the green shell left and right sides below crystallizer is provided with contact rod, induction coil is arranged on crystallizer lower section, and induction coil is arranged on both sides before and after green shell, energization induction coil and energized conductor rod into the magnetic field pointed to inside strand.Advantage is:Equipment is simple, is acted synergistically using the conductive mouth of a river and contact rod, induction coil, makes molten steel under the collective effect of direct current and magnetic field force, reaches the purpose of control bleed-out.According to the size of the breakout prediction temperature difference, the real-time adjust automatically conduction mouth of a river and contact rod, induction coil DC current flow size are quick on the draw, and regulate the speed fast, the features such as green pollution-free, are effectively reduced the incidence of bleed-out, improve slab lumber recovery.

Description

A kind of process units of efficient control continuous casting bleed-out
Technical field
The utility model is related to a kind of process units of efficient control continuous casting bleed-out, and direct current is utilized more particularly, to one kind With the process units that magnetic field force controls continuous casting bleed-out.
Background technology
With continuing to develop for continuous casting technology, high-efficient continuous casting technology has turned into the main direction of studying in continuous casting technology field, And with the raising of casting speed, the risk of bleed-out is consequently increased.Pulling rate change is greatly or pulling rate changes frequent, molten steel matter Amount, submersed nozzle form and Disalignment etc. can influence liquid covering slag to penetrate between green shell and copper plate of crystallizer, cause Green shell is set to be cohered with copper coin.
There is scholar to propose to use convex crystallizer, convex crystallizer is 96 ° in top angle, and it is more steady mutually to pass through face, to changing Kind corner meniscus performance is favourable, and this kind of crystallizer cooling is uniform, can reduce air gap, can prevent bleed-out and face crack.Someone Propose to adjust method reduction casting blank off-square, bleed-out that crystallizer water is stitched according to continuous casting different phase.By the both sides that section is led in branch Special bleed-out guard assembly is installed, the splash face for spilling molten steel, protection lower section fan are reduced by the protective effect of these components Oil pipe, oil grease tube, the water pipe of shape section and both sides etc. be not contaminated, reduces the loss of equipment, improves the processing speed of accident.This A little measures can to a certain extent reduce the generation of bleed-out, but bleed-out is also subject to superheat of liquid steel, carbon content in steel, sulfur content, leaching Enter formula mouth of a river type, misoperation, the influence of the pulling rate change factor such as greatly still has the danger of bleed-out generation, using breakout prediction System can make early warning, therefore the process units that exploitation is combined with steel leakage prediction system to bleed-out, once there is bleed-out Can in time prevent and be very important.
The content of the invention
To overcome the deficiencies in the prior art, the purpose of this utility model to be to provide a kind of production of efficient control continuous casting bleed-out Device, coordinates with forecast system, and continuous casting bleed-out is controlled using direct current and magnetic field force, and equipment is simple, reduces the incidence of bleed-out, Improve slab lumber recovery.
To achieve the above object, the utility model is achieved through the following technical solutions:
A kind of process units of efficient control continuous casting bleed-out, including contact rod, induction coil, the conductive mouth of a river, crystallizer, lead The electric mouth of a river is arranged in the middle of crystallizer, and the green shell left and right sides below crystallizer is provided with contact rod, and induction coil is arranged on crystallization Device lower section, and induction coil is arranged on both sides before and after green shell, energization induction coil and energized conductor rod are into pointing to inside strand Magnetic field.
Described contact rod sidepiece sets hydraulic cylinder, is used to push contact rod to strand.
Described contact rod is set on the same plane with induction coil.
Compared with prior art, the beneficial effects of the utility model are:
Equipment is simple, is acted synergistically using the conductive mouth of a river and contact rod, induction coil, makes molten steel in direct current and magnetic field force Collective effect under, reach control bleed-out purpose.According to the size of the breakout prediction temperature difference, the real-time adjust automatically conduction mouth of a river and Contact rod, induction coil DC current flow size, are quick on the draw, and regulate the speed fast, the features such as green pollution-free, can be effective The incidence of bleed-out is reduced, slab lumber recovery is improved.
Brief description of the drawings
Fig. 1 is structural representation of the present utility model.
Fig. 2 is the A of Fig. 1 to structural representation.
In figure:1- contact rod 2- induction coil 3- molten steel 4- green shells 5- conductions mouth of a river 6- crystallizer 7- strands.
Specific embodiment
The utility model is described in detail with reference to Figure of description, it should be noted that of the present utility model Implementation is not limited to following implementation method.
See Fig. 1, Fig. 2, the efficiently process units of control continuous casting bleed-out, including contact rod 1, induction coil 2, the conductive mouth of a river 5, Crystallizer 6, the conductive mouth of a river 5 is arranged in the middle of crystallizer 6, and green shell 4 (casting blank shell) left and right sides of the lower section of crystallizer 6 is provided with leads Torch 1, induction coil 2 is arranged on the lower section of crystallizer 6, and induction coil 2 is arranged on both sides before and after green shell 4, energization induction coil 2 The magnetic field pointed to inside strand 7 is formed with energized conductor rod 1.
Wherein, the sidepiece of contact rod 1 sets hydraulic cylinder, is used to push contact rod 1 to strand 7.
When using, for the mechanism that sheet billet continuous casting bleed-out occurs, when steel leakage prediction system sends bleed-out early warning signal, root According to alert levels just, control system is passed through 0~50A direct currents to the immersion conduction mouth of a river 5 and contact rod 1, is subject to molten steel 3 The magnetic field force inside molten steel 3 is pointed in direction, so as to control molten steel 3 to flow to, it is to avoid the generation of bleed-out phenomenon.Contact rod 1 and strand 7 Between be passed through pressure 10MPa, flow is 50m3/ h water under high pressures, remove the surface FeO of strand 7, keep contact rod 1 good with strand 7 Good contact.
The inner nozzle of crystallizer 6 sets induction coil 2 using the conductive mouth of a river 5 below crystallizer 6, and logical in induction coil 2 Enter direct current, generation magnetic field intensity is 5~15T D.C. magnetic fields, and the both sides of strand 7 with the sustained height of induction coil 2 are respectively provided with Contact rod 1.When Breakout Prediction System for Continuous Casting sends early warning signal, the size beyond normal temperature value is indicated according to bleed-out, to The mouth of a river and contact rod 1 are passed through 0~50A direct currents, contact rod 1 is contacted with strand 7 while starting hydraulic cylinder, use in the process High-pressure water jet strand 7 surface relative with contact rod 1, so that the oxide layer removal on the surface of strand 7, using magnetic field to powered steel The magnetic field force that liquid 3 is produced, control molten steel 3 is flowed to inside strand 7, it is to avoid the generation of bleed-out phenomenon.
Present apparatus simple structure, it is easy for installation, the incidence of bleed-out is effectively reduced, improve slab lumber recovery.Using leading The electric mouth of a river 5 acts synergistically with contact rod 1, induction coil 2, makes molten steel 3 under the collective effect of direct current and magnetic field force, reaches control The purpose of bleed-out processed, can be according to the size of the bleed-out early warning temperature difference, real-time adjust automatically DC current flow size.The method has anti- Should be sensitive, to regulate the speed fast, low cost, equipment is simple, the features such as green pollution-free, is effectively reduced the generation of bleed-out Rate, improves slab lumber recovery, increases economic efficiency.

Claims (3)

1. a kind of process units of efficient control continuous casting bleed-out, it is characterised in that including contact rod, induction coil, the conductive mouth of a river, Crystallizer, the conductive mouth of a river is arranged in the middle of crystallizer, and the green shell left and right sides below crystallizer is provided with contact rod, and induction coil sets Put below crystallizer, and induction coil is arranged on both sides before and after green shell, energization induction coil and energized conductor rod into sensing Magnetic field inside strand.
2. it is according to claim 1 it is a kind of it is efficient control continuous casting bleed-out process units, it is characterised in that described conduction Rod sidepiece sets hydraulic cylinder, is used to push contact rod to strand.
3. it is according to claim 1 it is a kind of it is efficient control continuous casting bleed-out process units, it is characterised in that described conduction Rod is set on the same plane with induction coil.
CN201621247365.5U 2016-11-18 2016-11-18 A kind of process units of efficient control continuous casting bleed-out Expired - Fee Related CN206200093U (en)