CN206047073U - An a kind of tank ladle - Google Patents
An a kind of tank ladle Download PDFInfo
- Publication number
- CN206047073U CN206047073U CN201621081333.2U CN201621081333U CN206047073U CN 206047073 U CN206047073 U CN 206047073U CN 201621081333 U CN201621081333 U CN 201621081333U CN 206047073 U CN206047073 U CN 206047073U
- Authority
- CN
- China
- Prior art keywords
- slag line
- bag mouth
- course
- inclusion
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a kind of metallurgical technology field, specifically a kind of tank ladle, including inclusion, bag mouth and the slag line in inclusion, the slag line protrusion is arranged on the middle part of inclusion, the upper end of slag line is extended to below bag mouth, connect course between the slag line and bag mouth, the course includes outer layer and internal layer, the outer layer is flat course, the internal layer is laid on end layer, as a result of above-mentioned technical proposal, a kind of tank ladle described in the utility model is by improving the masonry construction of slag line and Bao Zui junctions, not only avoid the generation that shim oozes ferrum accident, and also reduce the cost of refractory material, the most important production for being to ensure a tank ladle safety and stability.
Description
Technical field
This utility model is related to metallurgical technology field, specifically a kind of tank ladle.
Background technology
The Molten Iron Transportation of big-and-middle-sized steel plant, generally using the organization of production of blast furnace → torpedo tank car → ladle → converter
Pattern.Although this kind of pattern has many advantages, such as mobility is good, hot metal temperature drop is little, while having molten iron pretreatment, adjustment
The function such as molten iron temperature and composition and buffering, but, the high benefit pursued with modern metallurgical technology, the target phase of low energy consumption
Than still there is certain gap.It is mainly manifested in, Molten Iron Transportation link is more, production efficiency is relatively low, high energy consumption, three de- effects are poor, one
The aspect such as the investment of secondary property is big, operating cost is higher.In order to overcome the problems referred to above, it is many that some iron and steel corporations employ ladle
Function micronizing technology, i.e., one bag is on earth.One wraps on earth, i.e., using a kind of access for possessing molten iron, transport, buffer reservoir, ferrum
Water pretreatment, converter iron making and hot-metal insulating etc. are multi-functional to contain ferrum container-ladle, and blast furnace molten iron out is being passed through
After necessary technological process is processed, to be changed without the production organization mode of the ladle, directly be blended in converter and smelt, the metallurgy flows
Technical process be referred to as " one bag on earth " Molten Iron Transportation technology, referred to as " a tank system ".
Although a tank Technology has advantage, but many negative effects are brought to refractory material.With torpedo
Tank refractory material is compared, and a tank ladle refractory material is more easily damaged, and the life-span is relatively low.Ladle carries out desulfurization typically using spray
Blow desulphurization and KR stirring desulphurizations, sweetening process can introduce large quantities of lime, fluorite, granule magnesium powder etc., and especially slag line position is corroded
Seriously.Meanwhile, the when of falling molten iron bag mouth similarly bear and wash away erosion from molten iron and slag, as a tank ladle is used
Life-time dilatation, with colding and heat succeed each other repeatedly, bag mouth is using castable and the slag line Al of its seam crossing2O3- SiC-C brick heat is swollen
The difference of swollen coefficient, causes seam crossing transverse joint increasing, seam crossing stress concentration, accelerates the damage of operational layer brick and bag mouth material
Ruin, cause to stitch increasing slag iron constantly penetrating in transverse joint, cause large area shim between slag line working lining and permanent layer, give
The safe operation of ladle brings great hidden danger, once there is the accident of leakage ferrum, consequence will be hardly imaginable.At the same time,
In order to avoid there are the problems referred to above, the general renovation method for changing bag mouth for adopting carries out light maintenance, although so reducing Lou ferrum thing
Therefore probability of happening, but can so improve the holistic cost of ladle, it is often more important that with the increase of light maintenance number of times, lead
Cause ladle to cold and heat succeed each other repeatedly, affect the service life of material.
Utility model content
In order to make up, the above is not enough, and this utility model provides the high tank ferrum of a kind of long service life, safety coefficient
Water bag, to solve the problems, such as in above-mentioned background technology.
The technical solution of the utility model is:
An a kind of tank ladle, including inclusion, bag mouth and the slag line in inclusion, the slag line protrusion are arranged on bag
The middle part of body, the upper end of slag line are extended to below bag mouth, connect course between the slag line and bag mouth, and the course includes outer layer
And internal layer, the outer layer is flat course, and the internal layer is laid on end layer.
Used as preferred technical scheme, the upper end of the course is connected to bag mouth and inclusion junction, the connection of course lower end
In the upper end of slag line.
Used as preferred technical scheme, the course is connected with inclusion from the upper end of the slag line positioned at middle part towards both sides bag mouth
Meet place to extend.
As preferred technical scheme, upper end of the internal layer upper end higher than outer layer.
Used as preferred technical scheme, laid on end seam and the flat puzzle joint of outer layer of the internal layer are crisscross arranged.
As a result of above-mentioned technical proposal, a kind of tank ladle described in the utility model by improve slag line with
The masonry construction of Bao Zui junctions, not only avoid the generation that shim oozes ferrum accident, and also reduce the cost of refractory material,
The most important production for being to ensure a tank ladle safety and stability.
Description of the drawings
In order to be illustrated more clearly that this utility model embodiment or technical scheme of the prior art, below will be to embodiment
Or accompanying drawing to be used is briefly described needed for description of the prior art, it should be apparent that, drawings in the following description are only
It is some embodiments of the present utility model, for those of ordinary skill in the art, before creative labor is not paid
Put, can be with according to these other accompanying drawings of accompanying drawings acquisition.
Fig. 1 is the structural representation of this utility model embodiment;
Fig. 2 is the structure enlarged diagram of part A in Fig. 1;
Fig. 3 is the structural representation of this utility model bag mouth point;
Fig. 4 is the structural representation that this utility model outer layer is laid bricks;
Fig. 5 is the structural representation that this utility model internal layer is laid bricks
Specific embodiment
Embodiment one:As shown in figure 1, a kind of tank ladle described in the utility model, including inclusion 1,2 and of bag mouth
Slag line 3 in inclusion 1, the bag mouth 2 are arranged on the upper end of inclusion 1, and the bag mouth 2 protrudes from 1 outer wall of inclusion and by upper
Bottom diameter is held gradually to increase, the protrusion of the slag line 3 is arranged on the middle part of inclusion 1, the slag line 3 is arranged on inside inclusion 1,
And slag line is fitted on the inwall of inclusion 1, the upper end of slag line 3 is extended to below bag mouth 2, is connected between the slag line 3 and bag mouth 2
Course, the course are the adding layers being connected between slag line 3 and bag mouth 2, and the course structure includes inside and outside two-layer, respectively
Outer layer 4 and internal layer 5, the outer layer 4 are located at the inner side of internal layer 5, and the outer layer 4 fit together with internal layer 5, outer layer 4 and internal layer 5
3 upper end of slag line is extended in, the medial wall of the outer layer 4 is concordant with the inwall of 3 upper end of slag line, and the outer layer 4 is by laying bricks
One layer of flat block working lining is built, the internal layer 5 is to build one layer of laid on end working lining by laying bricks by laying bricks or stones, described to build outer layer 4 and internal layer 5 by laying bricks or stones
Lay bricks and be trapezoidal brick, after the laying bricks of the outer layer 4 and internal layer 5 is built by laying bricks or stones, parcel is smeared by chamotte and is laid bricks, formed fire resisting and apply
Layer.
The upper end of the course is connected to bag mouth 2 and 1 junction of inclusion, and course lower end is connected to the upper end of slag line 3, described
Course is extended with 1 junction of inclusion from the upper end of the slag line 3 positioned at middle part towards both sides bags mouth 2, make course be interspersed in bag mouth 2 with
Between slag line 3, solid layer is formed, the steadiness of course is improved.
Upper end of 5 upper end of the internal layer higher than outer layer 4, the upper end of the outer layer 4 are connected to 2 lower end of bag mouth, internal layer 5 it is upper
The lower end of bag mouth 2 is inserted at end, and the internal layer 5 increases course tight with what bag mouth 2 was connected together with 4 secured fit of outer layer
Soundness.
The laid on end seam of the internal layer 5 is crisscross arranged with the flat puzzle joint of outer layer 4, is reinforced by chamotte filling, increase in course seam
Plus the firmness of integrated connection, it is to avoid produce phenomenon of rupture.
The inner side laminating bag mouth bed of material 6 of the bag mouth 2, is reinforced by dowel 7 between 2 inwall of bag mouth and the bag mouth bed of material 6,
7 one end of the dowel is fixedly attached on bag mouth 2, in 7 other end of the dowel insertion bag mouth bed of material 6, the bag mouth bed of material 6 and Bao Zui
2 upper end welding pressing plate, increases the firmness that the bag mouth bed of material 6 is connected with bag mouth 2.
Ultimate principle of the present utility model, principal character and advantage of the present utility model has been shown and described above.One's own profession
The technical staff of industry it should be appreciated that this utility model is not restricted to the described embodiments, described in above-described embodiment and description
Simply illustrate principle of the present utility model, on the premise of without departing from this utility model spirit and scope, this utility model is also
Various changes and modifications are had, these changes and improvements are both fallen within the range of claimed this utility model.This utility model
Claimed scope is by appending claims and its equivalent thereof.
Claims (5)
1. a kind of tank ladle, including inclusion (1), bag mouth (2) and the slag line (3) being located in inclusion (1), the slag line are convex
Go out to be arranged on the middle part of inclusion (1), the upper end of slag line (3) is extended to below bag mouth (2), it is characterised in that:The slag line (3) with
Connect course between bag mouth (2), the course includes outer layer (4) and internal layer (5), the outer layer (4) is flat course, the internal layer
(5) it is laid on end layer.
2. a kind of tank ladle as claimed in claim 1, it is characterised in that:The upper end of the course is connected to bag mouth
(2) with inclusion (1) junction, course lower end is connected to the upper end of slag line (3).
3. a kind of tank ladle as claimed in claim 1, it is characterised in that:The course is from the slag line positioned at middle part
(3) upper end is extended towards both sides Bao Zui (2) with inclusion (1) junction.
4. the one tank ladle of one kind as described in claim 1 or 3, it is characterised in that:Internal layer (5) upper end is higher than outer layer
(4) upper end.
5. a kind of tank ladle as claimed in claim 4, it is characterised in that:The laid on end seam of the internal layer (5) and outer layer
(4) flat puzzle joint is crisscross arranged.