CN206019687U - A kind of molten steel Determining oxygen probe - Google Patents

A kind of molten steel Determining oxygen probe Download PDF

Info

Publication number
CN206019687U
CN206019687U CN201620867326.9U CN201620867326U CN206019687U CN 206019687 U CN206019687 U CN 206019687U CN 201620867326 U CN201620867326 U CN 201620867326U CN 206019687 U CN206019687 U CN 206019687U
Authority
CN
China
Prior art keywords
cylinder
protection cylinder
molten steel
oxygen probe
quartz ampoule
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201620867326.9U
Other languages
Chinese (zh)
Inventor
杨德帆
杨明江
杨德顺
宋道举
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHONGXIANG ZHONGYUAN ELECTRONIC Co Ltd
Original Assignee
ZHONGXIANG ZHONGYUAN ELECTRONIC Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHONGXIANG ZHONGYUAN ELECTRONIC Co Ltd filed Critical ZHONGXIANG ZHONGYUAN ELECTRONIC Co Ltd
Priority to CN201620867326.9U priority Critical patent/CN206019687U/en
Application granted granted Critical
Publication of CN206019687U publication Critical patent/CN206019687U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of molten steel Determining oxygen probe, including:Plastic stent, offers two vertical perforation thereon, is provided with several buckles on its outer peripheral edge, extends upward and form vertical rack in the middle part of which, and the upper end of vertical rack forms fixing hole;The steel outer protection cylinder of lower ending opening, including thin cylinder, thick cylinder and level connection joint portion, the upper end of thin cylinder forms the top cover of taper, and the lower end of thick cylinder forms flange;Lower ending opening and the steel interior protection cylinder being arranged in outer protection cylinder, the upper end of interior protection cylinder form the top cover of taper, and its peripheral edge of bottom extends out to form boss;Several fastening holes are offered on the madial wall of boss, and buckle is fastened in fastening hole correspondingly;Boss is fixed on flange and between level connection joint portion by clamping;U-shaped quartz ampoule, two upper ends wiry are connected through after a pin of U-shaped quartz ampoule in bending part respectively upward, and a footmuff of U-shaped quartz ampoule is located in fixing hole;Overmolded coated sand rod.The molten steel Determining oxygen probe can easily pass through slag.

Description

A kind of molten steel Determining oxygen probe
Technical field
The utility model is related to sensor technical field in smelting industry, and in particular to a kind of molten steel in smelting industry is fixed Oxygen probe.
Background technology
Mainly by oxygen sand head is determined and paper tube is constituted, it is mainly used in the steelmaking process of smelting industry Determining oxygen probe, Measurement liquid steel temperature and oxygen content, belong to the high-tech product for smelting detection technique, the quality technology controlling and process of smelting process are had Important directive function, is requirement of each big steel mill in smelting process, and is expendable consumed product, per stove molten steel all The multiple measurement of this product is had to pass through, the requirement needed for completing to make steel.1.2 meters of long paper pipes on oxygen sand headgear are determined during use, Engagement Special industrial PC apparatus for determination of oxygens are connected to determines oxygen rifle, then the front end for determining oxygen rifle is inserted in paper tube and is mutually inserted with oxygen sand head is determined Connect, by determine oxygen sand head front end insert molten steel in, the data that all processes are measured were rapidly completed in 8 seconds, to molten steel in into Divide and oxygen content, steel quality, the consumption of lumber recovery play conclusive effect.
Due to when inserting in molten steel, needing to pass through as early as possible slag to protect zirconium pipe and thermocouple before measuring, otherwise Due to the obstruction of slag may lead to not to measure or indeterminacy molten steel in oxygen content.It is thus desirable to one kind conveniently passes through slag Molten steel Determining oxygen probe.
Utility model content
For solving the above problems, the utility model provides a kind of molten steel Determining oxygen probe for conveniently passing through slag.
A kind of molten steel Determining oxygen probe that the utility model is provided, including thermocouple and zirconium pipe, thermocouple includes two metal bars And two wires, metal bar is electrically connected to the reference electrode that arrange in zirconium pipe by wire, also includes:
Plastic stent, offers two vertical perforation thereon, is provided with several buckles on the outer peripheral edge of plastic stent, modeling Material mid-stent extends to form a vertical rack upward, and the upper end of vertical rack forms a fixing hole;
The steel outer protection cylinder of lower ending opening, the thick cylinder of thin cylinder, bottom including top and is integrally connected thin cylinder and thick The level connection joint portion of cylinder, the upper end of thin cylinder form the top cover of taper, and the lower end of thick cylinder extends to form flange inwardly;
Lower ending opening and the steel interior protection cylinder being arranged in outer protection cylinder, the upper end of interior protection cylinder form the top of taper Lid, the peripheral edge of bottom of interior protection cylinder extend out to form boss;Several fastening holes, one a pair of buckle is offered on the madial wall of boss It is fastened in fastening hole with answering;Boss is fixed on flange and between level connection joint portion by clamping;
U-shaped quartz ampoule, two upper ends wiry respectively upward through after a pin of U-shaped quartz ampoule U-shaped quartz ampoule folding It is connected in crook, a footmuff of U-shaped quartz ampoule is located in fixing hole;
The coated sand rod being overmolded onto outside thin cylinder lower end, thick cylinder and metal bar lower end.
Preferably, molten steel Determining oxygen probe also includes that the support ring being set in outside interior protection cylinder, the outer rim of support ring are abutted On the inner edge of outer protection cylinder.
Preferably, protrude out outwardly to form a locating ring in interior protection cylinder, the lower end of support ring is connected to locating ring upper surface.
Preferably, molten steel Determining oxygen probe also includes that the end cap being set in outside thin cylinder, end cap are fixed on coated sand rod Upper surface on.
Description of the drawings
Fig. 1 is the structural representation of the molten steel Determining oxygen probe of a preferred embodiment.
Specific embodiment
The technical solution of the utility model is clearly and completely described below in conjunction with accompanying drawing.In the utility model Description in, " " center ", " on ", D score, "left", "right", " vertical ", " level ", " interior ", " outward " it should be noted that term Deng instruction orientation or position relationship be based on orientation shown in the drawings or position relationship, be for only for ease of description this practicality newly Type is described with simplifying, rather than is indicated or implied that the device or element of indication must be with specific orientation, with specific orientation Construction and operation, therefore it is not intended that to restriction of the present utility model.Additionally, term " first ", " second ", " the 3rd " are only used In description purpose, and it is not intended that indicating or hint relative importance.
In description of the present utility model, it should be noted that unless otherwise clearly defined and limited, term " peace Dress ", " being connected ", " connection " should be interpreted broadly, for example, it may be fixedly connected, or be detachably connected, or integratedly Connection;Can be mechanically connected, or electrically connect;Can be joined directly together, it is also possible to be indirectly connected to by intermediary, It can be the connection of two element internals.For the ordinary skill in the art, above-mentioned art can be understood with concrete condition Concrete meaning of the language in the utility model.
Refer to Fig. 1.Fig. 1 shows the molten steel Determining oxygen probe that the utility model is provided, including thermocouple 3 and zirconium pipe (not Illustrate), thermocouple includes two metal bars, 34,35 and two wire 32,33, and metal bar 34 is electrically connected to by wire (not shown) The reference electrode arranged in zirconium pipe, the junction of the metal bar 34,35 is formed visits point.The metal bar 34,35 and wire 32,33 Material difference is had according to different types of thermocouple.Especially, the thermocouple its can be standardized S types thermocouple.
The molten steel Determining oxygen probe of the present embodiment also includes:
Plastic stent 5, offers two vertical perforation (unmarked in figure) thereon, sets on the outer peripheral edge of plastic stent 5 Several buckles 51 are equipped with, are extended in the middle part of plastic stent 5 upward and is formed a vertical rack 52, the upper end of vertical rack 52 forms one admittedly Determine hole (unmarked in figure);
The steel outer protection cylinder 1 of lower ending opening, thick cylinder 11 including the thin cylinder 10, bottom on top and is integrally connected thin cylinder 10 and the level connection joint portion 12 of thick cylinder 11, the upper end of thin cylinder 10 forms the top cover 1A of taper, and the lower end of thick cylinder 11 extends shape inwardly Into flange 13;
Lower ending opening and the steel interior protection cylinder 2 being arranged in outer protection cylinder 1, the upper end of interior protection cylinder 2 form taper Top cover 2A, the peripheral edge of bottom of interior protection cylinder 2 extend out to form boss 21;Several fastening holes are offered on the madial wall of boss 21 22, buckle 51 is fastened in fastening hole 22 correspondingly;Boss 21 is fixed on flange 13 and in level connection joint portion 12 by clamping Between;
U-shaped quartz ampoule 31, the upper end difference of two wires 34,35 is upward through after a pin of U-shaped quartz ampoule 31 in U-shaped stone It is connected in the bending part of English pipe 31, a footmuff of U-shaped quartz ampoule 31 is located in fixing hole;
It is overmolded onto 10 lower end of thin cylinder, thick cylinder 11 and metal bar 34, the coated sand rod 6 outside 35 lower ends.
So, by arranging outer protection cylinder, interior protection cylinder and its upper end being set to taper, slag pair can more be reduced The resistance of molten steel Determining oxygen probe, can not only preferably protect molten steel Determining oxygen probe and can easily pass through slag.Thus, by which The Oxygen Content in Liquid Steel for measuring is more stable and accurate.Additionally by this connected mode between outer protection cylinder and interior protection cylinder, Easily and accurately can be fixed together, can pole facilitate the shaping of coated sand rod on ground.
Preferably, molten steel Determining oxygen probe also includes that the support ring 4 being set in outside interior protection cylinder 2, the outer rim of support ring 4 are supported It is connected on the inner edge of outer protection cylinder 1.As such, it is possible to strengthen the intensity of molten steel Determining oxygen probe head, therefore, it is possible to more easily wear More slag.
It is further preferred that protruding out outwardly to form a locating ring 23 in interior protection cylinder 2, the lower end of support ring 4 is connected to 23 upper surface of locating ring.So, the movement of support ring can be prevented in moulding resin precoated sand rod.
Preferably, molten steel Determining oxygen probe also includes that the end cap 7 being set in outside thin cylinder 10, end cap 7 are fixed on resin coating On the upper surface of sand rod 6.As such, it is possible to prevent the end of the coated sand rod in measurement to be damaged and introduce in molten steel miscellaneous Matter.
In the utility model, other non-detailed portions belong to prior art, therefore will not be described here.
Finally it should be noted that:Various embodiments above is only in order to illustrating the technical solution of the utility model, rather than which is limited System;Although being described in detail to the utility model with reference to foregoing embodiments, one of ordinary skill in the art should Understand:Which still can be modified to the technical scheme described in foregoing embodiments, or to which part or whole Technical characteristic carries out equivalent;And these modifications or replacement, do not make the essence of appropriate technical solution depart from this practicality new The scope of each embodiment technical scheme of type.

Claims (4)

1. a kind of molten steel Determining oxygen probe, including thermocouple and zirconium pipe, the thermocouple includes two metal bars and two wires, the metal Rod is electrically connected to the reference electrode that arrange in the zirconium pipe by wire, it is characterised in that also include:
Plastic stent, offers two vertical perforation thereon, is provided with several buckles on the outer peripheral edge of the plastic stent, the modeling Material mid-stent extends to form a vertical rack upward, and the upper end of the vertical rack forms a fixing hole;
The steel outer protection cylinder of lower ending opening, the thick cylinder of thin cylinder, bottom including top and is integrally connected the thin cylinder and this is thick The level connection joint portion of cylinder, the upper end of the thin cylinder form the top cover of taper, and the lower end of the thick cylinder extends to form flange inwardly;
Lower ending opening and the steel interior protection cylinder being arranged in the outer protection cylinder, the upper end of the interior protection cylinder form the top of taper Lid, the peripheral edge of bottom of the interior protection cylinder extend out to form boss;Several fastening holes are offered on the madial wall of the boss, the buckle It is fastened in the fastening hole correspondingly;The boss is fixed on the flange and between the level connection joint portion by clamping;
U-shaped quartz ampoule, two upper end wiry is respectively upward through after a pin of the U-shaped quartz ampoule in the U-shaped quartz ampoule It is connected in bending part, a footmuff of the U-shaped quartz ampoule is located in the fixing hole;
The coated sand rod being overmolded onto outside the thin cylinder lower end, the thick cylinder and the metal bar lower end.
2. molten steel Determining oxygen probe as claimed in claim 1, it is characterised in that also include be set in outside the interior protection cylinder Pushing out ring, the outer rim of the support ring are connected on the inner edge of the outer protection cylinder.
3. molten steel Determining oxygen probe as claimed in claim 2, it is characterised in that protrude out outwardly to form a positioning in the interior protection cylinder Ring, the lower end of the support ring are connected to the locating ring upper surface.
4. molten steel Determining oxygen probe as claimed in claim 3, it is characterised in that also include the end cap being set in outside the thin cylinder, The end cap is fixed on the upper surface of the coated sand rod.
CN201620867326.9U 2016-08-11 2016-08-11 A kind of molten steel Determining oxygen probe Active CN206019687U (en)