CN206011577U - The process units of annex is directly molded on fiberboard - Google Patents
The process units of annex is directly molded on fiberboard Download PDFInfo
- Publication number
- CN206011577U CN206011577U CN201620904224.XU CN201620904224U CN206011577U CN 206011577 U CN206011577 U CN 206011577U CN 201620904224 U CN201620904224 U CN 201620904224U CN 206011577 U CN206011577 U CN 206011577U
- Authority
- CN
- China
- Prior art keywords
- annex
- injection
- fiberboard
- die cavity
- molded
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model is related to a kind of process units of directly injection annex on fiberboard, it is characterised in that:Include that fiber panel moulding apparatus and injection machine, the fiber panel moulding apparatus include the first upper and lower mould successively, to realize hot-forming fiberboard, in the first upper and lower die body, be drilled with logical oil circuit, use for mould heating;The injection machine includes that the plastic-blasting pipe being molded with the injection bed die of annex die cavity, top board and toward in injection annex die cavity, the top board are pressed on fibreboard surface, and the plastic-blasting pipe is stretched into by perforation and is molded in annex die cavity;Or be directly molded in die cavity from bed die side, i.e., injection molding nozzle and die cavity are in the same side.Technique effect of the present utility model:1st, injection annex can achieve without glue bonding, it is to avoid the risk caused by VOC detections;2nd, product structure and production technology is simplified, production cost is reduced;3rd, reinforcement can be molded at the position of natural fiber plate strength weak by Shooting Technique, increases product strength.
Description
Technical field
The utility model is related to a kind of process units of directly injection annex on fiberboard.
Background technology
At present in automotive trim, the most of or inside gadget using plastic injection technological forming correlation.But with light
Quantify, under the motor trend with energy-saving and emission-reduction, to be increasingly widely used in using the inside gadget of natural fiber material
In automotive field.But due to natural fiber be made of by hot-forming technique, relative to traditional plastics interior trim, naturally fine
Dimension directly can not onboard be molded the structures such as the buckle for auxiliary installation.Mode general at present is after natural fiber hot pressing
Again on the surface by the mode adhered plastics part such as PUR, to realize corresponding effect structure.By way of glue bonding
Production cost and production process can be increased, the complexity for becoming product structure, while may examine to the VOC of automobile using glue bonding
Survey and cause certain risk.
Content of the invention
The purpose of this utility model is the process units for providing directly injection annex on a kind of fiberboard, on the fiberboard
Directly the process units of injection annex is conducive to simple production process and simplifies product structure, can be completely without any glue just
Can be with molding bonded.
The process units of annex is directly molded on the utility model fiberboard, it is characterised in that:Include successively fiberboard into
Type machine and injection machine, the fiber panel moulding apparatus include the first upper and lower mould, to realize hot-forming fiberboard, on described first,
Logical oil circuit is drilled with lower mold body, is used for mould heating;The injection machine include with injection annex die cavity bed die,
Top board and the plastic-blasting pipe toward injection in injection annex die cavity, the top board are pressed on fibreboard surface, the plastic-blasting pipe
Stretched in injection annex die cavity by perforation;Or be directly molded in die cavity from bed die side, i.e., injection molding nozzle and die cavity are same
Side.
Further, drilling machine or punching apparatus are provided between above-mentioned fiber panel moulding apparatus and injection machine.
Further, on the first of above-mentioned fiber panel moulding apparatus, mould is provided with lower contact pin, wears fiberboard and formed under
Perforation.
Further, above-mentioned punch position is located on the position of injection annex.
Further, above-mentioned perforation is located at opposite injection for the big nose end of shoulder hole or bellmouth, shoulder hole or bellmouth
On the one side of annex.
Technique effect of the present utility model:
1st, the utility model device can achieve injection annex without glue bonding, it is to avoid the risk caused by VOC detections;
2nd, product structure and production technology is simplified, production cost is reduced;
3rd, reinforcement can be molded at the position of natural fiber plate strength weak by the utility model device, increases product strong
Degree.
Description of the drawings
Fig. 1 is the organigram of the directly process units of injection annex on fiberboard;
Fig. 2 is the organigram of the process units another kind embodiment of directly injection annex on fiberboard;
Fig. 3 is the principle schematic of the utility model fiber panel moulding apparatus;
Fig. 4 is the principle schematic of the utility model injection;
Fig. 5 is a kind of organigram of embodiment of boring a hole;
Fig. 6 is the organigram of another kind of embodiment of perforation.
Specific embodiment
The production technology of annex is directly molded on the utility model fiberboard, and fiberboard is first hot-forming on mould to be become
Product, then drills on the fiberboard of shaping, and the one side that the fiberboard of shaping intends being molded annex is placed on injection then
In die cavity, be molded toward in injection die cavities by drilling, that is, complete annex 8 is molded on fiberboard.
Hot-forming in order to be conducive to, above-mentioned fiberboard is by mestha, jute or wood-fibred etc. sponge and PP
Material is mixed.
For improve production efficiency, it is directly entered in injection die cavities after above-mentioned fiberboard is hot-forming and is molded.Using
This mode is in the case where production line is allowed, it is not necessary to is detained or moves fiberboard, and can save follow-up injection needs to preheat
The step of fiberboard.
If cannot realize being directly entered injection step, then the hot-forming fiberboard for having cooled down needs first to preheat 6-10
Enter back in injection die cavities after minute and be molded, preheating temperature is 70 ~ 120 degree, it is advantageously ensured that noting after injection after first preheating
It is more firm that modeling annex is connected with fiberboard.
In order that connection is firm, above-mentioned bore position is located on the position of injection annex, and above-mentioned drilling is shoulder hole or cone
The big nose end of shape hole, shoulder hole or bellmouth is located on the one side of injection annex opposite to each other, using setting for shoulder hole or bellmouth
Meter so that having in shoulder hole or bellmouth so that injection annex with
The bonding strength of fiberboard is significantly improved, and bonding strength improves more than 3 times, the diameter control of above-mentioned drilling or perforation 0.6 ~
The end diameter of 1.5mm, a diameter of shoulder hole or bellmouth.The taper of bellmouth is 100 degree.
Further, in injection, the pressure being pressed against in injection die cavities is applied with fiberboard, the pressure is conjunction
Molding pressure, more than tens of tonnes of pressure, to avoid flash.
Further, in injection, the injection rate of plastic material is 0.6 kilogram per second.
The above-mentioned material for being molded can be the thermoplastics such as PP, PA, ABS, PC, and add in above material
Plus the composite of glass fibre or other thermoplastics.
Above-mentioned finished product can be used for door-plate inside gadget etc..
Drilling can adopt drilling machine or perforating press.
The process units of annex is directly molded on the utility model fiberboard, includes fiber panel moulding apparatus 1 and injection successively
Machine 2, can be provided with continuous conveyer belt 3, or move half by artificial mode between the fiber panel moulding apparatus and injection machine
Finished product, the fiber panel moulding apparatus include the first upper and lower mould 101,102, to realize hot-forming fiberboard, on described first,
Logical oil circuit is drilled with lower mold body 101,102, is used for mould heating, a diameter of 20 ~ 30mm of oil circuit, to ensure mould
The recycle oil of interior storage is enough, it is to avoid during production, mold temperature is unstable;The injection machine 2 is included with injection
The bed die 201 of annex die cavity, top board 202 and the plastic-blasting pipe 203 toward injection in injection annex die cavity, the top board 202 are pressed
Put on 7 surface of fiberboard, the plastic-blasting pipe 203 is stretched in injection annex die cavity by perforation 4.Or directly from bed die 201
Side is molded in die cavity, i.e., injection molding nozzle and die cavity are in the same side.
Further, drilling machine 5 is provided between above-mentioned fiber panel moulding apparatus and injection machine;Or in the fiber sheet metal forming
On the first of machine, mould is provided with lower contact pin 6, wears fiberboard and form perforation 4 under.Using being directly provided with mould on first
Lower contact pin 6, lower 6 lower end of contact pin are in pointed shape, so as to hot pressing perforation shaping perforation 4 while hot-forming fiberboard, subtract
The step of having lacked other drilling, save time and cost.
Technique effect of the present utility model:
1st, the utility model device can achieve injection annex without glue bonding, it is to avoid the risk caused by VOC detections;
2nd, product structure and production technology is simplified, production cost is reduced;
3rd, reinforcement can be molded at the position of natural fiber plate strength weak by the utility model device, increases product strong
Degree.
The foregoing is only preferred embodiment of the present utility model, all become according to the utility model claim is accomplished
Change and modification should all belong to covering scope of the present utility model.
Claims (5)
1. the process units of annex is directly molded on a kind of fiberboard, it is characterised in that:Include fiber panel moulding apparatus and note successively
Molding machine, the fiber panel moulding apparatus include the first upper and lower mould, to realize hot-forming fiberboard, in the first upper and lower die body
Logical oil circuit is drilled with, is used for mould heating;The injection machine include with the injection bed die of annex die cavity, top board and
The plastic-blasting pipe of injection toward in injection annex die cavity, the top board are pressed on fibreboard surface, and the plastic-blasting pipe is by perforation
Stretch in injection annex die cavity;Or be directly molded in die cavity from bed die side, i.e., injection molding nozzle and die cavity are in the same side.
2. the process units of annex is directly molded on fiberboard according to claim 1, it is characterised in that:The fiberboard into
Drilling machine or punching apparatus are provided between type machine and injection machine.
3. the process units of annex is directly molded on fiberboard according to claim 1, it is characterised in that:The fiberboard into
On the first of type machine, mould is provided with lower contact pin, wears fiberboard and form perforation under.
4. the process units of annex is directly molded on fiberboard according to claim 1, it is characterised in that:The punch position
It is located on the position of injection annex.
5. the process units of annex is directly molded on fiberboard according to claim 1, it is characterised in that:The perforation is rank
The big nose end of terraced hole or bellmouth, shoulder hole or bellmouth is located on the one side of injection annex opposite to each other.