CN205653391U - Improvement structure of double faced adhesive tape - Google Patents

Improvement structure of double faced adhesive tape Download PDF

Info

Publication number
CN205653391U
CN205653391U CN201620442252.4U CN201620442252U CN205653391U CN 205653391 U CN205653391 U CN 205653391U CN 201620442252 U CN201620442252 U CN 201620442252U CN 205653391 U CN205653391 U CN 205653391U
Authority
CN
China
Prior art keywords
layer
protective layer
double faced
adhesive tape
holding sheet
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201620442252.4U
Other languages
Chinese (zh)
Inventor
李志启
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan Dongchen Industrial Co Ltd
Original Assignee
Dongguan Dongchen Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan Dongchen Industrial Co Ltd filed Critical Dongguan Dongchen Industrial Co Ltd
Priority to CN201620442252.4U priority Critical patent/CN205653391U/en
Application granted granted Critical
Publication of CN205653391U publication Critical patent/CN205653391U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses an improvement structure of double faced adhesive tape, including can stretch sticky two -sided bond line, bottom and a protective layer, bottom, bond line, protective layer are followed and are up laminated in proper order down, be provided with the centre gripping layer between bond line and the bottom, the relative centre gripping layer that sets up the looks isostructure between bond line and protective layer, two the symmetry laminating of centre gripping layer is in bond line length direction's one end, it has the hot melt adhesive granule to go back discrete distribution between bond line and the protective layer, set up an intermediate layer in the bond line. The utility model discloses the hot melt adhesive granule is treated and is pasted the object and play the effect of keeping apart the buffering, becomes the thin layer hot melt adhesive counterpointing in advance to soften the hot melt adhesive granule after good, causes object and bond line to paste fixedly according to the exact position, electronic component heat dissipating can be assisted to heat conduction graphite film's intermediate layer, the electromagnetic signal between the electronic component can be kept apart to the intermediate layer that electromagnetic shielding film made.

Description

A kind of structure-improved of double faced adhesive tape
Technical field
This utility model relates to double faced adhesive tape, particularly to the structure-improved of a kind of double faced adhesive tape.
Background technology
Along with the development of science and technology, being required for of a lot of electronic devices and components temporarily or permanently fixedly mounts, and adhesive tape has become as indispensable article in electronics, electrical apparatus industry.Interim the fixing that wherein both may be used for object element by stretching the easy-to-draw double faced adhesive tape of removable viscosity can be used for being permanently fixed of element, and this distinctive character makes easy-to-draw double faced adhesive tape the most extensively apply in industries such as electronics, electrical equipment, glass.
Easy-to-draw double faced adhesive tape has a problem that in use, because the moment adhesive property of easy-to-draw double faced adhesive tape, do not notice that the object displacement being easy for be pasted causes pasting dislocation, the object pasted is difficult to go mobile again, if double faced adhesive tape tearing stickup again can lose viscosity or sticking effect is bad.Also have, easy-to-draw double faced adhesive tape needs specific performance at the installation environment of some special electronic devices and components, as the electronic components such as the electronic components such as battery need auxiliary heat dissipation, circuit substrate need to shield electromagnetic signal, this is required for improving existing easy-to-draw double sided adhesive tape structure.
Utility model content
The purpose of this utility model is the structure-improved overcoming the deficiencies in the prior art to provide a kind of double faced adhesive tape.
For achieving the above object, this utility model adopts the following technical scheme that: the structure-improved of a kind of double faced adhesive tape, and including double-sided adhesive layer, bottom and the protective layer of a stretchable vanishing viscosity, described bottom, adhesive layer, protective layer are fitted the most successively;Being provided with holding sheet between described adhesive layer and bottom, relative arranges mutually isostructural holding sheet between adhesive layer with protective layer, and two described holding sheet symmetries are fitted in one end of adhesive layer length direction;Between described adhesive layer and protective layer, also Discrete Distribution has hot-melt adhesive granules;One interlayer is set in described adhesive layer.
Scheme is expanded on further, and described bottom, protective layer and holding sheet are mould release membrance.
Scheme is expanded on further, and described bottom is Ge Laxin release paper, and described protective layer is PET mould release membrance or PC mould release membrance, and described holding sheet is polyester release film or PET mould release membrance.
Scheme is expanded on further, and the off-type force of described bottom is less than the off-type force of protective layer, and the off-type force of protective layer is less than the off-type force of holding sheet.
Scheme is expanded on further, and described adhesive layer extends wedge angle along its length in the one end away from holding sheet, and the limit of described wedge angle and the length direction of holding sheet are 30 degree of angles.
Scheme, described adhesive layer every 1cm are expanded on further2On be evenly distributed 1-3 hot-melt adhesive granules.
Scheme is expanded on further, and described interlayer is heat-conducting layer, and described heat-conducting layer is conductive graphite thin film.
Scheme is expanded on further, and described interlayer is electro-magnetic screen layer, and described electro-magnetic screen layer is electromagnetic wave shield film.
This utility model has the beneficial effects that: hot-melt adhesive granules is treated substrates and played the effect of isolation buffer, is softened by hot-melt adhesive granules and become thin layer PUR after pre-para-position is good, causes object to paste fixing according to correct position with adhesive layer;The interlayer that conductive graphite thin film is made can dispel the heat with auxiliary electronic element;The interlayer that electromagnetic wave shield film is made can be with the electromagnetic signal between insulating electron element.
Accompanying drawing explanation
Fig. 1 is this utility model structural representation.
Fig. 2 is the top view of a kind of embodiment of this utility model.
Fig. 3 is the use view of a kind of embodiment of this utility model.
Fig. 4 is the top view of this utility model another embodiment.
Fig. 5 is the use view of this utility model another embodiment.
Drawing reference numeral illustrates: 1, protective layer;2, holding sheet;3, adhesive layer;4, interlayer;5, bottom;6, hot-melt adhesive granules;61, thin layer PUR;71, the first plate object;72, first substrate;81, the Second Board object;82, second substrate.
Detailed description of the invention
Introduce detailed description of the invention of the present utility model below in conjunction with the accompanying drawings.
As shown in Figure 1; a kind of structure-improved of double faced adhesive tape; the protective layer 1 that the bottom 5 and PET mould release membrance made including the double-sided adhesive layer 3 of a stretchable vanishing viscosity made with easy-to-draw glue, Ge Laxin release paper is made, bottom 5, adhesive layer 3, protective layer 1 are fitted the most successively;The holding sheet 2 that PET mould release membrance is made it is provided with between adhesive layer 3 and bottom 5; relative arranges mutually isostructural holding sheet 2 between adhesive layer 3 with protective layer 1; two holding sheet 2 symmetries are fitted in one end of adhesive layer 3 length direction; the other end of adhesive layer 3 length direction extends outward the wedge angle of 60 degree, and the limit of wedge angle is 30 degree of angles with the length direction of holding sheet 2;With 1/cm between adhesive layer 3 and protective layer 12Density variance distribution hot-melt adhesive granules 6;Wherein the off-type force of bottom 5 is less than the off-type force of protective layer 1, and the off-type force of protective layer 1 is less than the off-type force of holding sheet 2.A functional interlayer 4 it is provided with in adhesive layer 3.
Embodiment one:
As shown in Figure 2 and Figure 3, the double faced adhesive tape of the present embodiment is ribbon, one end laminating holding sheet 2 of adhesive layer 3 length direction, the other end of adhesive layer 3 length direction extends outward the wedge angle of 60 degree, wedge angle is 30 degree of angles with the length direction with holding sheet 2, the heat-conducting layer that interlayer 4 is made for conductive graphite thin film.
nullWhen the double faced adhesive tape of the present embodiment uses,First tear bottom 5,Adhesive layer 3 is attached on first substrate 72,Tear protective layer 1 again,First plate object 71 touched hot-melt adhesive granules 6 before this,The hot-melt adhesive granules 6 viscosity when not melting is relatively low,First plate object 71 can move adjustment position relative to first substrate 72 and adhesive layer 3,Postpone moving to specific bit,Heat to the first plate object 71 or the first plate object 71 with the joint face of first substrate 72 by slight fever sources such as electric-heating air blowers,Hot-melt adhesive granules 6 is heated to the softening temperature of 60-70 degree,Hot-melt adhesive granules 6 soften become plastic or flow regime after under the self gravitation or external force extruding of the first plate object 71, become thin layer PUR 61,First plate object 71 just can be pasted onto on adhesive layer 3,Complete the bonding fastening of the first plate object 71 and first substrate 72.
Internal heat is derived by the interlayer 4 that the first plate object 71 is made by conductive graphite thin film with first substrate 72, helps the first plate object 71 or first substrate 72 to dispel the heat.When the first plate object 71 needs separately with first substrate 72, after thin layer PUR 61 being heated to plastic or flow regime by electric-heating air blower, adhesive layer 3 is driven to stretch by pullling holding sheet 2, after the adhesive layer 3 of stretcher strain loses viscosity, just can thin layer PUR 61, interlayer 4 and adhesive layer 3 be pulled out easily, the first plate object 71 just can separate with first substrate 72.When adhesive layer 3 is stretched to the position of wedge angle, if adhesive layer 3 uses rectangular shape, last straight flange can be entered to middle concave when by concentrating on middle tensile force, after being easily trapped at the two of straight flange angles during disengaging, and 60 degree of horn structure of the present utility model can deform the surface departing from upper and lower object easily.
Embodiment two:
As shown in Figure 4, Figure 5, the double faced adhesive tape of the present embodiment is rectangle lamellar, one end laminating holding sheet 2 of adhesive layer 3 length direction, the other end of adhesive layer 3 length direction extends outward three connected 60 degree wedge angles, the limit of wedge angle is 30 degree of angles with the length direction of holding sheet 2, the electro-magnetic screen layer that interlayer 4 is made for electromagnetic wave shield film.
nullWhen the double faced adhesive tape of the present embodiment uses,First tear bottom 5,Adhesive layer 3 is attached on second substrate 82,Tear protective layer 1 again,The Second Board object 81 touched hot-melt adhesive granules 6 before this,The hot-melt adhesive granules 6 viscosity when not melting is relatively low,The Second Board object 81 can move adjustment position relative to second substrate 82 and adhesive layer 3,Postpone moving to specific bit,Heated to the joint face of the Second Board object 81 or the Second Board object 81 and second substrate 82 by slight fever sources such as electric-heating air blowers,Hot-melt adhesive granules 6 is heated to the softening temperature of 60-70 degree,After hot-melt adhesive granules 6 softens and becomes plastic or flow regime,Thin layer PUR 61 is become under the self gravitation or external force extruding of the Second Board object 81,The Second Board object 81 just can be pasted onto on adhesive layer 3,Complete the bonding fastening of the Second Board object 81 and second substrate 82.
The interlayer 4 that the electromagnetic signal that second substrate 82 produces is made by electromagnetic wave shield film is isolated without being delivered on the Second Board object 81, and the relative electromagnetic signal in the Second Board object 81 generation is not transferred on second substrate 82.When the Second Board object 81 needs separately with second substrate 82, after thin layer PUR 61 being heated to plastic or flow regime by electric-heating air blower, adhesive layer 3 is driven to stretch by pullling holding sheet 2, after the adhesive layer 3 of stretcher strain loses viscosity, just can easily thin layer PUR 61, interlayer 4 and adhesive layer 3 be pulled out, the Second Board object 81 just can separate with second substrate 82, and 60 degree of horn structure of the present utility model can deform the surface departing from upper and lower object easily, it is to avoid the situation about being trapped in below of corner occurs.
Technical scope of the present utility model is not imposed any restrictions by the above, all according to this utility model technical spirit, any amendment, equivalent variations and the modification being made above embodiment, all still falls within the range of the technical solution of the utility model.

Claims (8)

1. a structure-improved for double faced adhesive tape, including double-sided adhesive layer, bottom and the protective layer of a stretchable vanishing viscosity, described bottom, adhesive layer, protective layer are fitted the most successively;It is characterized in that: be provided with holding sheet between described adhesive layer and bottom, relative arranges mutually isostructural holding sheet between adhesive layer with protective layer, and two described holding sheet symmetries are fitted in one end of adhesive layer length direction;Between described adhesive layer and protective layer, also Discrete Distribution has hot-melt adhesive granules;One interlayer is set in described adhesive layer.
The structure-improved of a kind of double faced adhesive tape the most according to claim 1, it is characterised in that: described bottom, protective layer and holding sheet are mould release membrance.
The structure-improved of a kind of double faced adhesive tape the most according to claim 2, it is characterised in that: described bottom is Ge Laxin release paper, and described protective layer is PET mould release membrance or PC mould release membrance, and described holding sheet is polyester release film or PET mould release membrance.
The structure-improved of a kind of double faced adhesive tape the most according to claim 3, it is characterised in that: the off-type force of described bottom is less than the off-type force of protective layer, and the off-type force of protective layer is less than the off-type force of holding sheet.
The structure-improved of a kind of double faced adhesive tape the most according to claim 1, it is characterised in that: described adhesive layer extends wedge angle along its length in the one end away from holding sheet, and the limit of described wedge angle and the length direction of holding sheet are 30 degree of angles.
The structure-improved of a kind of double faced adhesive tape the most according to claim 1, it is characterised in that: the every 1cm of described adhesive layer2On be evenly distributed 1-3 hot-melt adhesive granules.
The structure-improved of a kind of double faced adhesive tape the most according to claim 1, it is characterised in that: described interlayer is heat-conducting layer, and described heat-conducting layer is conductive graphite thin film.
The structure-improved of a kind of double faced adhesive tape the most according to claim 1, it is characterised in that: described interlayer is electro-magnetic screen layer, and described electro-magnetic screen layer is electromagnetic wave shield film.
CN201620442252.4U 2016-05-16 2016-05-16 Improvement structure of double faced adhesive tape Expired - Fee Related CN205653391U (en)