CN205520942U - Metal base ceramic coating metallographic specimen experimental apparatus - Google Patents
Metal base ceramic coating metallographic specimen experimental apparatus Download PDFInfo
- Publication number
- CN205520942U CN205520942U CN201620360332.5U CN201620360332U CN205520942U CN 205520942 U CN205520942 U CN 205520942U CN 201620360332 U CN201620360332 U CN 201620360332U CN 205520942 U CN205520942 U CN 205520942U
- Authority
- CN
- China
- Prior art keywords
- metallographic specimen
- pressing plate
- ceramic coating
- coating metallographic
- metal matrix
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a metal base ceramic coating metallographic specimen experimental apparatus has solved current experiment frock and has made ceramic coating peel off, harm easily, and the problem of accuracy is tested in the influence. It includes metal base ceramic coating metallographic specimen, first clamp plate and second clamp plate, first clamp plate and second clamp plate press respectively in the upper surface and the lower surface of metal base ceramic coating metallographic specimen, first clamp plate and second clamp plate measure -alike and all be greater than the size of metal base ceramic coating metallographic specimen, first clamp plate and second clamp plate pass through bolted connection, compress tightly metal base ceramic coating metallographic specimen. The utility model discloses a metal base ceramic coating metallographic specimen experimental apparatus through the cooperation of metal base ceramic coating metallographic specimen, first clamp plate and second clamp plate etc. Can conveniently clip metal base ceramic coating metallographic specimen and as a whole experiment, prevent peeling off, haring of ceramic coating, influence experiment effect.
Description
Technical field
This utility model relates to a kind of metallographic specimen frock, particularly relates to a kind of metal matrix ceramic composite coating metallographic specimen experimental provision.
Background technology
Traditional metallographic specimen preparation method includes: first, carries out sample corase grind on grinder;Secondly, carry out sample fine grinding with a series of varigrained sand paper, fine grinding can on sample grinding machine automatic grinding, it is possible to carry out underhand polish;Again, buffing machine carries out sample polishing;Finally, sample corrosion.For metal matrix ceramic composite coating metallographic specimen, there are the following problems: first, owing to ceramic coating has characteristic hard, crisp, is acted on by grinding force in preparation process, it is easy to occurs to peel off or peel off with metallic matrix, affects coating structure;Second, polishing agent is easily accessible in the crackle formed because of ceramic coating and Metal Substrate stripping, causes experiment effect inaccurate.
Utility model content
The purpose of this utility model is: provide a kind of metal matrix ceramic composite coating metallographic specimen experimental provision preventing ceramic coating from peeling off, damaging.
This utility model is achieved through the following technical solutions: metal matrix ceramic composite coating metallographic specimen experimental provision, including metal matrix ceramic composite coating metallographic specimen, the first pressing plate and the second pressing plate, the first described pressing plate and the second pressing plate are pressed on the upper and lower surface of metal matrix ceramic composite coating metallographic specimen respectively;The first described pressing plate and the second pressing plate equivalently-sized and be all higher than the size of metal matrix ceramic composite coating metallographic specimen;The first described pressing plate and the second pressing plate are bolted, and compress metal matrix ceramic composite coating metallographic specimen.
For preventing from weighing wounded ceramic coating, the first described pressing plate is provided with polypropylene elastic rubber layer near one side and second pressing plate of metal matrix ceramic composite coating metallographic specimen near the one side of metal matrix ceramic composite coating metallographic specimen.
For increasing friction force, prevent metal matrix ceramic composite coating metallographic specimen from sliding, a coarse designs of described polypropylene elastic rubber layer contacting metal base ceramic coating metallographic specimen.
For convenience of clamping, the first described pressing plate and the second pressing plate are provided with the latch closure of convenient clamping.
This utility model compared with prior art, has the following advantages and beneficial effect:
(1) metal matrix ceramic composite coating metallographic specimen experimental provision of the present utility model, cooperation by metal matrix ceramic composite coating metallographic specimen, the first pressing plate and the second pressing plate etc., metal matrix ceramic composite coating metallographic specimen can be clamped easily test as an entirety, prevent the peeling of ceramic coating, damage, affect experiment effect.
(2) polypropylene elastic rubber layer is set, can further prevent the damage of ceramic coating, polypropylene elastic rubber layer coarse designs from the slip of metal matrix ceramic composite coating metallographic specimen with increasing friction force, can be prevented, improve the accuracy of experiment.
(3) latch closure is set, can easily whole metal matrix ceramic composite coating metallographic specimen experimental provision be clamped.
Accompanying drawing explanation
Fig. 1 is a kind of structural representation of metal matrix ceramic composite coating metallographic specimen experimental provision of the present utility model;
In figure, 1 first pressing plate, 2 second pressing plates, 3 bolts, 4 polypropylene elastic rubber layers, 5 metal matrix ceramic composite coating metallographic specimens, 6 latch closures.
Detailed description of the invention
Below in conjunction with embodiment, this utility model is described in further detail, but embodiment of the present utility model is not limited to this.
Embodiment 1:
As shown in Figure 1, metal matrix ceramic composite coating metallographic specimen experimental provision of the present utility model, including metal matrix ceramic composite coating metallographic specimen the 5, first pressing plate 1 and the second pressing plate 2, the first described pressing plate 1 and the second pressing plate 2 are pressed on the upper and lower surface of metal matrix ceramic composite coating metallographic specimen 5 respectively;The first described pressing plate 1 and the second pressing plate 2 equivalently-sized and be all higher than the size of metal matrix ceramic composite coating metallographic specimen 5;The first described pressing plate 1 and the second pressing plate 2 are connected by bolt 3, compress metal matrix ceramic composite coating metallographic specimen 5.Metal matrix ceramic composite coating metallographic specimen experimental provision of the present utility model, cooperation by metal matrix ceramic composite coating metallographic specimen the 5, first pressing plate 1 and the second pressing plate 2 etc., metal matrix ceramic composite coating metallographic specimen 5 can be clamped easily test as an entirety, prevent the peeling of ceramic coating, damage, affect experiment effect.During use, metal matrix ceramic composite coating metallographic specimen 5 is positioned between the first pressing plate 1 and the second pressing plate 2, and screwed by bolt 3, then by whole metal matrix ceramic composite coating metallographic specimen experimental provision, together as experimental subject, prevent the peeling of ceramic coating, damage, impact experiment accuracy.
Embodiment 2:
As preferably, the first described pressing plate 1 is provided with polypropylene elastic rubber layer 4 near one side and second pressing plate 2 of metal matrix ceramic composite coating metallographic specimen 5 near the one side of metal matrix ceramic composite coating metallographic specimen 5, can further prevent the damage of ceramic coating.
Embodiment 3:
As preferably, a coarse designs of described polypropylene elastic rubber layer 4 contacting metal base ceramic coating metallographic specimen 5, it is therefore prevented that the slip of metal matrix ceramic composite coating metallographic specimen, improve the accuracy of experiment.
Embodiment 4:
As preferably, the first described pressing plate 1 and the second pressing plate 2 are provided with the latch closure 6 of convenient clamping, can be clamped easily by hook-like assembly unit, improve conventional efficient.
It should be noted that experiment mentioned in this article is primarily referred to as wear-resisting experiment, resistance to oxidation experiment and microscope observation experiment etc., and the participation of first grip block the 1, second blessing plate and bolt 3 is not had influential experiment.
The foregoing is only preferred embodiment of the present utility model, not in order to limit this utility model, all any amendment, equivalent and improvement etc. made within spirit of the present utility model and principle, within should be included in protection domain of the present utility model.
Claims (4)
1. metal matrix ceramic composite coating metallographic specimen experimental provision, it is characterized in that: include that metal matrix ceramic composite coating metallographic specimen (5), the first pressing plate (1) and the second pressing plate (2), described the first pressing plate (1) and the second pressing plate (2) are pressed on the upper and lower surface of metal matrix ceramic composite coating metallographic specimen (5) respectively;Described the first pressing plate (1) and the second pressing plate (2) equivalently-sized and be all higher than the size of metal matrix ceramic composite coating metallographic specimen (5);Described the first pressing plate (1) and the second pressing plate (2) are connected by bolt (3), compress metal matrix ceramic composite coating metallographic specimen (5).
Metal matrix ceramic composite coating metallographic specimen experimental provision the most according to claim 1, it is characterised in that: described the first pressing plate (1) is provided with polypropylene elastic rubber layer (4) near one side and second pressing plate (2) of metal matrix ceramic composite coating metallographic specimen (5) near the one side of metal matrix ceramic composite coating metallographic specimen (5).
Metal matrix ceramic composite coating metallographic specimen experimental provision the most according to claim 2, it is characterised in that: a coarse designs of described polypropylene elastic rubber layer (4) contacting metal base ceramic coating metallographic specimen (5).
4. according to the metal matrix ceramic composite coating metallographic specimen experimental provision described in claim 1,2 or 3, it is characterised in that: it is provided with the latch closure (6) of convenient clamping on described the first pressing plate (1) and the second pressing plate (2).