CN205291750U - Leather with illusion coating - Google Patents

Leather with illusion coating Download PDF

Info

Publication number
CN205291750U
CN205291750U CN201521120173.3U CN201521120173U CN205291750U CN 205291750 U CN205291750 U CN 205291750U CN 201521120173 U CN201521120173 U CN 201521120173U CN 205291750 U CN205291750 U CN 205291750U
Authority
CN
China
Prior art keywords
illusion
leather
thickness
coating
surface resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201521120173.3U
Other languages
Chinese (zh)
Inventor
黄玉真
黄国有
谢煌
杨海景
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGZHOU JINGDIAN POLYMER MATERIALS PRODUCT CO Ltd
Original Assignee
GUANGZHOU JINGDIAN POLYMER MATERIALS PRODUCT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGZHOU JINGDIAN POLYMER MATERIALS PRODUCT CO Ltd filed Critical GUANGZHOU JINGDIAN POLYMER MATERIALS PRODUCT CO Ltd
Priority to CN201521120173.3U priority Critical patent/CN205291750U/en
Application granted granted Critical
Publication of CN205291750U publication Critical patent/CN205291750U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a leather with illusion coating, including the leather, be equipped with waterborne mirror surface resin layer, composite bed and illusion lacquer layer from the inside to surface in proper order on the leather, wherein, the thickness of waterborne mirror surface resin layer is 50~60 mu m, and the thickness on illusion lacquer layer is 30~40 mu m. Owing to adopted the utility model discloses a thickness of waterborne mirror surface resin, consequently, the coating under the effect of tension and contractile force on the leather is difficult to appear the crackle, and the pliability is good in addition, and mirror effect is good. Owing to adopt the utility model discloses an illusion lacquer thickness when shaping illusion lacquer layer, has sufficient time response, makes the reaction of illusion lacquer even, consequently, outward appearance effectual, the pliability might as well simultaneously.

Description

A kind of leather with dreamlike coating
Technical field
This utility model relates to leather.
Background technology
Leather is through the obtained not perishable animal skins of degeneration of depilation and the physics such as tanning, chemical process. In use, in order to allow leather have the features such as attractive in appearance, corrosion resistance, it is necessary at leather trypsin method paint film. Traditional paint film on leather is formed by Vacuum Deposition, so, it is easy to cause environmental pollution. It addition, the leather used requires certain pliability, but at present, when, after varnish formation, its flexibility is bad, and easily cracks.
Summary of the invention
In order to allow leather have pliability, and being not easy to produce crack, appearance looks elegant, this utility model provides a kind of leather with dreamlike coating.
For reaching above-mentioned purpose, a kind of leather with dreamlike coating, including leather, leather is sequentially provided with aqueous minute surface resin bed, composite bed and illusion enamelled coating from the inside to surface, wherein, the thickness of aqueous minute surface resin bed is 50 ~ 60 ��m, and hardness is shore 60-70, and the thickness of illusion enamelled coating is 30 ~ 40 ��m.
Further, the thickness of aqueous minute surface resin bed is 55 ��m, and the thickness of illusion enamelled coating is 35 ��m.
The beneficial effects of the utility model are: owing to have employed the thickness of aqueous minute surface resin of the present utility model, therefore, under the effect of tension force and contractility, the coating on leather is not easy crackle occur, and pliability is good, and mirror effect is good. Owing to adopting illusion paint thickness of the present utility model, when molding illusion enamelled coating, there is time enough react, make the reaction of illusion paint uniform, therefore, outward appearance effective, pliability simultaneously.
Accompanying drawing explanation
Fig. 1 is structural representation of the present utility model.
Detailed description of the invention
Below in conjunction with the drawings and specific embodiments, this utility model is further elaborated.
As shown in Figure 1, the leather with dreamlike coating includes leather 1, a surface of leather 1 is sequentially provided with aqueous minute surface resin bed 2, composite bed 3 and illusion enamelled coating 4 from the inside to surface, wherein, the thickness of aqueous minute surface resin bed is 50 ~ 60 ��m, preferably 55 ��m, the thickness of illusion enamelled coating is 30 ~ 40 ��m, it is preferable that 25 ��m.Described composite bed 3 is diffuseed to form by molecule by illusion enamelled coating 4 and aqueous minute surface resin bed 2, and so, illusion layer 4 is high with the bonding strength of aqueous minute surface resin bed 2, it is not easy to the phenomenon peeled off occur.
In this utility model, when molding illusion enamelled coating, can there is chemical reaction in illusion paint, in chemical reaction process, illusion enamelled coating can produce tension force and contractility, if the thickness of aqueous minute surface resin bed is too thin, aqueous minute surface resin bed is easily by drawing crack, therefore, whole coating has crackle, affect quality and the outward appearance of coating, and if the thickness of aqueous minute surface resin bed is too thin, its mirror effect is bad. For leather, need certain pliability, if pliability is poor, the comfort level then used is poor, if the thickness of aqueous minute surface resin bed is too thick, cost is high on the one hand, and the pliability of leather is poor on the other hand, therefore, this utility model adopts the aqueous minute surface resin of 50 ~ 60 �� m thick.
Illusion paint in illusion enamelled coating is contained within monomer, if the thickness of illusion enamelled coating is too thin, reacts uneven, and the effect of outward appearance is bad, if the thickness of illusion enamelled coating is too thick, poor in flexibility, cost is high, therefore, adopts the dreamlike thickness of paint layer of 30 ~ 40 ��m.
Leather environmental pollution of the present utility model is little, environmental protection. Owing to adopting aqueous minute surface resin bed, the surface of this layer has the effect of minute surface, and therefore, the appearance after illusion enamelled coating molding is good.

Claims (2)

1.A kind of leather with dreamlike coating, including leather, it is characterised in that: on leather, it is sequentially provided with aqueous minute surface resin bed, composite bed and illusion enamelled coating from the inside to surface, wherein, the thickness of aqueous minute surface resin bed is 50 ~ 60 ��m, and the thickness of illusion enamelled coating is 30 ~ 40 ��m.
2.The leather with dreamlike coating according to claim 1, it is characterised in that: the thickness of aqueous minute surface resin bed is 55 ��m, and the thickness of illusion enamelled coating is 35 ��m.
CN201521120173.3U 2015-12-30 2015-12-30 Leather with illusion coating Active CN205291750U (en)