CN205120547U - Attenuate seals glues resistant HF testing arrangement - Google Patents

Attenuate seals glues resistant HF testing arrangement Download PDF

Info

Publication number
CN205120547U
CN205120547U CN201520901592.4U CN201520901592U CN205120547U CN 205120547 U CN205120547 U CN 205120547U CN 201520901592 U CN201520901592 U CN 201520901592U CN 205120547 U CN205120547 U CN 205120547U
Authority
CN
China
Prior art keywords
glass plate
glass board
glass
mark line
resistance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201520901592.4U
Other languages
Chinese (zh)
Inventor
于爱霞
马圆
关启源
黄仁杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Hui Li Electron Material Co Ltd
Original Assignee
Guangzhou Hui Li Electron Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Hui Li Electron Material Co Ltd filed Critical Guangzhou Hui Li Electron Material Co Ltd
Priority to CN201520901592.4U priority Critical patent/CN205120547U/en
Application granted granted Critical
Publication of CN205120547U publication Critical patent/CN205120547U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses an attenuate seals glues resistant HF testing arrangement. Attenuate seals glues resistant HF testing arrangement includes glass board, oil mark line and fixed part. The glass board includes a glass board and the 2nd glass board, a glass board with the 2nd glass packs and puts, and a glass board with the 2nd glass packs postpone, the marginal parallel and level of a glass board in the edge of the 2nd glass board, oil mark line has a plurality ofly, and distributes the 2nd glass board orientation one side of a glass board, and it has to divide equally cloth around the 2nd glass board oil mark line, it is good that fixed part is used for in the fixed superpose temporarily of glueing in -process a glass board reaches the 2nd glass board. The attenuate seals to glue and is used for sealing two glass. The utility model discloses an attenuate seals glues resistant HF testing arrangement, simple manufacture, convenient operation.

Description

The thinning sealing proving installation of resistance to HF
Technical field
The utility model relates to detection field, particularly relates to a kind of thinning sealing proving installation of resistance to HF.
Background technology
Electronic product development rapidly, lighteningly becomes trend instantly, carries out thinning not only can effectively minimizing and takes up room, glass can also be made to have certain flexibility to touch-control glass.Thinning sealing can prevent acid-base solution from entering in liquid crystal cell from edge, destroys sealed plastic box, enters Cell inside, affect properties of product, essential in the production run of touch-control glass, and demand is good at day by day.Producer generally adopts special detecting instrument to detect the inside glass structure after thinning, to have judged whether that acid & alkali liquid enters, operates comparatively numerous and diverse and equipment cost is high.Especially for the manufacturer of thinning sealing, be difficult to meet this operation.
Utility model content
Based on this, be necessary the thinning sealing proving installation of resistance to HF providing a kind of equipment simple, easy to operate.
A kind of thinning sealing proving installation of resistance to HF, comprises
Glass plate, described glass plate comprises the first glass plate and the second glass plate, described first glass plate and described second glass plate stacked, and described first glass plate and described second glass plate stacked after, the edge of described first glass plate flushes in the edge of described second glass plate;
Oiliness mark line, described oiliness mark line has multiple, and is distributed in the side of described second glass plate towards described first glass plate, and the surrounding of described second glass plate is distributed with described oiliness mark line;
Fixed part, described fixed part is used in Process of Applying Glue, fix stacked good described first glass plate and described second glass plate.
Wherein in an embodiment, the length of described oiliness mark line is 3-10mm, and described oiliness mark line is extended to the inside of described second glass plate by the edge of described second glass plate.
Wherein in an embodiment, described oiliness mark line is perpendicular to the side of described second glass plate accordingly.
Wherein in an embodiment, described fixed part is adhesion adhesive tape.
The thinning sealing proving installation of resistance to HF that the utility model relates to; can by the resistance to HF performance test using it to carry out thinning sealing; whether evaluate thinning sealing simply and easily can effectively stop HF to enter the inside of glass plate, thus the inner structure of cover glass plate.The thinning sealing proving installation of resistance to HF that the utility model relates to, simple to operate and without the need to professional equipment.
Accompanying drawing explanation
Fig. 1 is the thinning sealing of the utility model one embodiment proving installation of resistance to HF schematic diagram.
Description of reference numerals
100, the first glass plate; 200, the second glass plate; 300, oiliness mark line.
Embodiment
Present embodiments provide a kind of thinning sealing proving installation of resistance to HF.
Shown in Figure 1, a kind of thinning sealing proving installation of resistance to HF, comprises glass plate, oiliness mark line 300 and fixed part.
Glass plate comprises the first glass plate 100 and the second glass plate 200.First glass plate 100 and the second glass plate 200 stacked, and described first glass plate 100 stacked with described second glass plate 200 after, the edge of concordant described second glass plate 200 in edge of described first glass plate 100.In the present embodiment, the first glass plate 100 and the second glass plate 200 consistent size, the edge of described first glass plate 100 flushes in the edge of described second glass plate 200.
In the present embodiment, the first glass plate 100 and the second glass plate 200 all can be arranged to rectangle, and first glass plate 100 and the second glass plate 200 equidimension.
Described oiliness mark line 300 has multiple, and is distributed in the side of described second glass plate 200 towards described first glass plate 100.The length of described oiliness mark line 300 is 3-10mm.Described oiliness mark line 300 is extended to the inside of described second glass plate 200 by the edge of described second glass plate 200.Described oiliness mark line 300 is perpendicular to the side of described second glass plate 200 accordingly, and oiliness mark line 300 is also covered with the surrounding of described second glass plate 200.
Described fixed part is used for temporary fixing stacked good described first glass plate 100 and described second glass plate 200 in Process of Applying Glue.Described fixed part is adhesion adhesive tape, or other setting tools.Temporaryly in Process of Applying Glue fix two sheet glass, avoid glass slides not align, and releasing after applying glue completes.
The thinning sealing proving installation of resistance to HF that the utility model relates to; can by the resistance to HF test using it to carry out glass thinning sealing; evaluate simply and easily as whether glass thinning sealing can effectively stop HF to enter the inside of two glass plates, thus the inner structure of cover glass plate.The thinning sealing proving installation of resistance to HF that the utility model relates to, simple to operate and without the need to professional equipment.
In the thinning sealing proving installation of resistance to HF that the utility model relates to, oiliness mark line 300 can be drawn short-term with the edge of black permanent pen first glass plate 100 and mark, and needs picture to boundary, 3-10mm.
First glass plate 100 is stacked on the second glass plate 200, and oiliness mark line 300 is towards inner, two glass sheets are vertically stacked together, fix in advance with adhesion adhesive tape, remove again after applying glue.
Be coated with thinning sealing two glass plate surroundings, ensure the gap that glue infiltrates two sheet glass between 2-3mm deeply and solidify, general employing is coated with in addition while solidify after being coated with and being cured again, until four limit completion of cures, also can first be painted with two opposite side, solidification, then be coated with two remaining opposite side, solidification, ensure that glue depth of penetration meets customer requirement, for ease of observing, can just glue furnishing be coloured.
The thinning sealing proving installation of resistance to HF using the utility model to relate to carries out resistance to HF test, if the oiliness mark line 300 steeped between rear first glass plate 100 of acid and the second glass plate 200 is still clear unchanged, the then acid resistance OK of thinning sealing, as the oiliness mark line 300 between the first glass plate 100 and the second glass plate 200 fogs, then represent the inside that acid solution has entered into the second glass plate 200, the acid resistance NG of thinning sealing.
The thinning sealing proving installation of resistance to HF using the utility model to relate to carry out the test experiments of resistance to HF
Citing 1
Can the resistance to HF test of colourless thinning sealing UV3-J1 (T) of the solution of resistance to 15%HF more than 2h
Use material: sailing boat board 7101 microslide ten (elongate in shape), black permanent pen one, adhesion adhesive tape (adhesive tape) volume.
Step:
1. ten microslides are divided into 5 groups, often group is selected a slice to carry out mark as the second glass plate 200 and is formed oiliness mark line 300, and another sheet is as the first glass plate 100;
2, by overlapping for two the microslide alignment often organized, oiliness mark line 300 inwards, is erect and is placed;
2. fixed by each group of microslide adhesion adhesive tape, the upper side of two microslides is without adhesive tape;
3. the upper side applying glue of pair two microslides, treats that glue depth of penetration reaches 2-3mm, UV completion of cure;
4. two microslides are inverted, to former downside (existing upper side) applying glue of two microslides, treat that depth of penetration reaches 2-3mm, UV completion of cure;
5. remove adhesion adhesive tape, respectively by left and right side applying glue completion of cure, ensure that glue depth of penetration is 2-3mm;
6. two microslides having executed glue are put into the HF solution of 35 DEG C 15%, take out after 2h;
7. whether observe institute makes marks clear unchanged.
This glass thinning sealing inner marker after bubble HF process is still clear unchanged, the resistance to HF OK of glass thinning sealing.
Citing 2
Can not the resistance to HF test of colourless UV glue of the solution of resistance to 15%HF more than 2h
Use material: sailing boat board 7101 microslide ten (elongate in shape), black permanent pen one, adhesion adhesive tape (adhesive tape) volume.
Step:
1. ten microslides are divided into 5 groups, often group is selected a slice to carry out mark as the second glass plate 200 and is formed oiliness mark line 300, and another sheet is as the first glass plate 100;
2, by overlapping for two the microslide alignment often organized, oiliness mark line 300 inwards, is erect and is placed;
2. fixed by each group of microslide adhesion adhesive tape, the upper side of two microslides is without adhesive tape;
3. the upper side applying glue of pair two microslides, treats that glue depth of penetration reaches 2-3mm, UV completion of cure;
4. two microslides are inverted, to former downside (existing upper side) applying glue of two microslides, treat that depth of penetration reaches 2-3mm, UV completion of cure;
5. remove adhesion adhesive tape, respectively by left and right side applying glue completion of cure, ensure that glue depth of penetration is 2-3mm;
6. two microslides having executed glue are put into the HF solution of 35 DEG C 15%, take out after 2h;
7. whether observe institute makes marks clear unchanged.
Glass inner marker after bubble HF process of this UV glue process fogs, and local is corroded, the resistance to HF NG of UV glue.
The above embodiment only have expressed several embodiment of the present utility model, and it describes comparatively concrete and detailed, but therefore can not be interpreted as the restriction to the utility model the scope of the claims.It should be pointed out that for the person of ordinary skill of the art, without departing from the concept of the premise utility, can also make some distortion and improvement, these all belong to protection domain of the present utility model.Therefore, the protection domain of the utility model patent should be as the criterion with claims.

Claims (4)

1. the thinning sealing proving installation of resistance to HF, is characterized in that, comprise
Glass plate, described glass plate comprises the first glass plate and the second glass plate, described first glass plate and described second glass plate stacked, and described first glass plate and described second glass plate stacked after, the edge of described first glass plate flushes in the edge of described second glass plate;
Oiliness mark line, described oiliness mark line has multiple, and is distributed in the side of described second glass plate towards described first glass plate, and the surrounding of described second glass plate is distributed with described oiliness mark line;
Fixed part, described fixed part is used in Process of Applying Glue, fix stacked good described first glass plate and described second glass plate.
2. the thinning sealing proving installation of resistance to HF according to claim 1, is characterized in that, the length of described oiliness mark line is 3-10mm, and described oiliness mark line is extended to the inside of described second glass plate by the edge of described second glass plate.
3. the thinning sealing proving installation of resistance to HF according to claim 2, is characterized in that, described oiliness mark line is perpendicular to the side of described second glass plate accordingly.
4. the thinning sealing proving installation of resistance to HF according to Claims 2 or 3, is characterized in that, described fixed part is adhesion adhesive tape.
CN201520901592.4U 2015-11-12 2015-11-12 Attenuate seals glues resistant HF testing arrangement Expired - Fee Related CN205120547U (en)