CN205048958U - Kiln is smelted to vanadium nitrogen alloy closed - Google Patents

Kiln is smelted to vanadium nitrogen alloy closed Download PDF

Info

Publication number
CN205048958U
CN205048958U CN201520790855.9U CN201520790855U CN205048958U CN 205048958 U CN205048958 U CN 205048958U CN 201520790855 U CN201520790855 U CN 201520790855U CN 205048958 U CN205048958 U CN 205048958U
Authority
CN
China
Prior art keywords
kiln section
kiln
section
smelting
cooling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201520790855.9U
Other languages
Chinese (zh)
Inventor
陈建中
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhengzhou Songshan Industry Kilns & Furnaces Co Ltd
Original Assignee
Zhengzhou Songshan Industry Kilns & Furnaces Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhengzhou Songshan Industry Kilns & Furnaces Co Ltd filed Critical Zhengzhou Songshan Industry Kilns & Furnaces Co Ltd
Priority to CN201520790855.9U priority Critical patent/CN205048958U/en
Application granted granted Critical
Publication of CN205048958U publication Critical patent/CN205048958U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides a kiln is smelted to vanadium nitrogen alloy closed, by the furnace frame, preheat the kiln section, smelt the kiln section, cooling kiln section, fill thermal -insulation layer, fire -resistant furnace constitute, smelting the kiln section and compriseing two symmetrical's oven and top cap, the top prefabrication of oven has the wall shoulder, and the bottom prefabrication has rather than the vertically bottom plate, the utilization equipment of bending rolls over the wall shoulder for the inclined plane, rolls over the bottom plate to be 90 perpendicular, and the edge portion of two bottom plates is through welding seam welded fastening, like this, only need a welding seam in the manufacture process of smelting kiln section, can realize that overall structure's connection is fixed, it is fixed with the top cap to connect between two wall shoulders, like this, confined smelting kiln section can be constituteed in the connection of two walls shoulder and top cap. Sealing capacity is good, the handling ease, and the process velocity is fast, and the appearance is pleasing to the eye. The both ends that smelt the kiln section respectively through the wallboard with preheat the kiln section and be connected with cooling kiln section and fix, arbitrary part wherein be can conveniently change, kiln is smelted to vanadium nitrogen alloy closed's maintenance and maintenance are favorable to.

Description

VN alloy closed smelts kiln
Technical field
The utility model relates to smelts kiln field, and particularly a kind of VN alloy closed smelts kiln.
Background technology
VN alloy and vanadium nitride.VN alloy is a kind of novel alloy additive, can substitute the production of vanadium iron for micro alloyed steel.Vanadium nitride makes an addition to the comprehensive mechanical performances such as intensity, toughness, ductility and the thermal fatigue resistance that can improve steel in steel, and makes steel have good solderability.Reaching under same intensity, adding vanadium nitride and save vanadium addition 30-40%, and then reduce cost.VN alloy can be used for structural steel, tool steel, pipe line steel, in reinforcing bar and cast iron.VN alloy is applied in Aldecor can carry out effective vanadium, nitrogen microalloying simultaneously, promotes the precipitation of carbon, vanadium, nitrogen compound in steel, more effective performance sedimentation strengthening and Grain refinement.VN alloy is the blank be made up of raw material such as vanadic anhydride, carbon dust, activating agents, and under normal pressure, nitrogen atmosphere protection, under 1500 ~ 1800 DEG C of conditions of high temperature, reaction generates VN alloy.Its key processing equipment is continous way atmosphere push pedal high temperature furnace, adopts the heatings such as Si-Mo rod to obtain thermal source.At present, the key processing equipment producing VN alloy is continous way atmosphere push pedal high temperature furnace, and the body of heater of this kiln adopts Plate Welding; The defect existed and deficiency are: 1. weld seam is too much, and manufacturing cost is higher, and service life is shorter, are not easy to maintenance; 2. airtight difficulty, causes poor thermal insulation property, the wasting of resources.
Utility model content
The purpose of this utility model is to provide a kind of VN alloy closed to smelt kiln, only needs a weld seam, can realize integrally-built being connected and fixed in the manufacture process of smelting kiln section; Top cover is fixedly connected with between two wall shoulders; Like this, the connection of two wall shoulders and top cover, can form closed smelting kiln section.
For achieving the above object, the utility model have employed such technical scheme: described VN alloy closed smelts kiln, is made up of grate, preheating kiln section, smelting kiln section, cooling kiln section, filling heat insulating wall, refractory burner hearth; It is characterized in that: the two ends of smelting kiln section are provided with connection wallboard, wherein one end of preheating kiln section and cooling kiln section is provided with connection wallboard; The two ends of smelting kiln section are connected and fixed respectively by wallboard and preheating kiln section and cooling kiln section; Grate is provided with preheating kiln section and smelting kiln section and cooling kiln section, and wherein, preheating kiln section is connected with grate by end support with cooling kiln section; Smelting kiln section is connected with grate with end plate by crossbeam, and the two ends of crossbeam are welded with end plate; Through refractory burner hearth is provided with in preheating kiln section and smelting kiln section and cooling kiln section; Filling heat insulating wall is provided with between the inwall of refractory burner hearth and preheating kiln section and smelting kiln section and cooling kiln section; Smelting kiln section is made up of two furnace walls be symmetrically welded and top cover, and the top of furnace wall is prefabricated with wall shoulder, and bottom is prefabricated with perpendicular base plate; Being welded and fixed by weld seam along portion of two base plates; Top cover is fixedly connected with between two wall shoulders; The side of one of them furnace wall is provided with heating switch board.
After adopting such structure, smelting kiln section is made up of two furnace walls be symmetrically welded and top cover, and the top of furnace wall is prefabricated with wall shoulder, and bottom is prefabricated with perpendicular base plate; Described prefabricated referring to utilizes bending equipment, is inclined-plane by wall shoulder folding, is the vertical plane of 90 ° by base plate folding, being welded and fixed by weld seam along portion of two base plates; Like this, only need a weld seam in the manufacture process of smelting kiln section, integrally-built being connected and fixed can be realized; Top cover is fixedly connected with between two wall shoulders; Like this, the connection of two wall shoulders and top cover, can form closed smelting kiln section.Its good effect is, airtight performance is good, handling ease, and process velocity is fast, good looking appearance.
In addition, the two ends of smelting kiln section are connected and fixed respectively by wallboard and preheating kiln section and cooling kiln section; Arbitrary parts wherein can be convenient for changing, be conducive to maintenance and maintenance that VN alloy closed smelts kiln, improve service life, saved processing cost.
Accompanying drawing explanation
Fig. 1 is the concrete structure schematic diagram that the utility model VN alloy closed smelts kiln;
Fig. 2 is the enlarged drawing of the broken section of A-A shown in Fig. 1.
Detailed description of the invention
As shown in the figure, described VN alloy closed smelts kiln, is made up of grate 8, preheating kiln section 1, smelting kiln section 6, cooling kiln section 7, filling heat insulating wall 14, refractory burner hearth 12; It is characterized in that: the two ends of smelting kiln section 6 are provided with and connect wallboard 2, and preheating kiln section 1 is provided with wherein one end of cooling kiln section 7 and is connected wallboard 2; The two ends of smelting kiln section 6 are connected and fixed respectively by wallboard 2 and preheating kiln section 1 and cooling kiln section 7;
Grate 8 is provided with preheating kiln section 1 and smelting kiln section 6 and cooling kiln section 7, and wherein, preheating kiln section 1 is connected with grate 8 by end support 9 with cooling kiln section 7; Smelting kiln section 6 is connected with grate 8 with end plate 10 by crossbeam 13, and the two ends of crossbeam 13 are welded with end plate 10;
Through refractory burner hearth 12 is provided with in preheating kiln section 1 and smelting kiln section 6 and cooling kiln section 7; Filling heat insulating wall 14 is provided with between the inwall of refractory burner hearth 12 and preheating kiln section 1 and smelting kiln section 6 and cooling kiln section 7;
Smelting kiln section 6 is made up of two furnace walls be symmetrically welded 5 and top cover 3, and the top of furnace wall 5 is prefabricated with wall shoulder 4, and bottom is prefabricated with perpendicular base plate 15; Being welded and fixed by weld seam 16 along portion of two base plates 15; Top cover 3 is fixedly connected with between two wall shoulders 4; The side of one of them furnace wall 5 is provided with heating switch board 11.

Claims (1)

1. VN alloy closed smelts a kiln, is made up of grate (8), preheating kiln section (1), smelting kiln section (6), cooling kiln section (7), filling heat insulating wall (14), refractory burner hearth (12); It is characterized in that: the two ends of smelting kiln section (6) are provided with and connect wallboard (2), and preheating kiln section (1) is provided with wherein one end of cooling kiln section (7) and is connected wallboard (2); The two ends of smelting kiln section (6) are connected and fixed respectively by wallboard (2) and preheating kiln section (1) and cooling kiln section (7);
Grate (8) is provided with preheating kiln section (1) and smelting kiln section (6) and cooling kiln section (7), wherein, preheating kiln section (1) is connected with grate (8) by end support (9) with cooling kiln section (7); Smelting kiln section (6) is connected with grate (8) with end plate (10) by crossbeam (13), and the two ends of crossbeam (13) are welded with end plate (10);
Through refractory burner hearth (12) is provided with in preheating kiln section (1) and smelting kiln section (6) and cooling kiln section (7); Filling heat insulating wall (14) is provided with between the inwall of refractory burner hearth (12) and preheating kiln section (1) and smelting kiln section (6) and cooling kiln section (7);
Smelting kiln section (6) is made up of two furnace walls be symmetrically welded (5) and top cover (3), and the top of furnace wall (5) is prefabricated with wall shoulder (4), and bottom is prefabricated with perpendicular base plate (15); Being welded and fixed by weld seam (16) along portion of two base plates (15); Top cover (3) is fixedly connected with between two walls shoulder (4); The side of one of them furnace wall (5) is provided with heating switch board (11).
CN201520790855.9U 2015-10-08 2015-10-08 Kiln is smelted to vanadium nitrogen alloy closed Expired - Fee Related CN205048958U (en)