CN204744464U - Glass -ceramic artificial tooth - Google Patents
Glass -ceramic artificial tooth Download PDFInfo
- Publication number
- CN204744464U CN204744464U CN201520285883.5U CN201520285883U CN204744464U CN 204744464 U CN204744464 U CN 204744464U CN 201520285883 U CN201520285883 U CN 201520285883U CN 204744464 U CN204744464 U CN 204744464U
- Authority
- CN
- China
- Prior art keywords
- glass
- artificial tooth
- enamel coating
- dyeing
- glaze layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model provides a glass -ceramic artificial tooth, including the cutting fashioned glass -ceramic base member, the glass -ceramic matrix surface includes first surface and second surface, be the first surface with the part of gum contact, and the part that does not contact with the gum is the second surface, second surface sinter molding in proper order has dyeing enamel coating and glaze layer. Above -mentioned glass -ceramic artificial tooth and since as the base member of main part for the fashioned glass -ceramic base member of cutting, the wholeness is good, intensity is high, can reduce stress, the result of use is stable, and when using glass -ceramic artificial tooth, be main atress with the first surface of gum contact and concentrate the department, the event will dye the enamel coating sintering in not with the second surface of gum contact, reduced the atress of dyeing enamel coating, reduced the probability of the enamel coating emergence crazing that dyes promptly to the probability that collapses the porcelain has been reduced.
Description
Technical field
This utility model relates to recovery technique of oral cavity field, particularly relates to a kind of glass ceramics artificial tooth.
Background technology
Along with the development of technology and living standard improve day by day, people more and more focus on oral health.Compared to Metal-porcelain artificial tooth, full porcelain artificial tooth artificial tooth meets popular to comfortable and beautiful pursuit.Full porcelain artificial tooth artificial tooth has following advantages: the first, good biocompatibility, because not metal-containing layer, so little to gingival irritation; The second, density and intensity higher, daily requirement of chewing can be met; 3rd, do not affect by ray, because be preced with without in metal, so when doing CT, X-ray, have no significant effect; 4th, good to the permeability of light, close to dermal tooth.But meanwhile, there is the problem that easy porcelain collapses in full porcelain artificial tooth.
Utility model content
Based on this, be necessary to there is for full porcelain artificial tooth the problem that easy porcelain collapses, a kind of glass ceramics artificial tooth is provided.
A kind of glass ceramics artificial tooth, comprise the glass-ceramic substrate of cutting forming, described glass-ceramic substrate surface comprises first surface and second surface, the part contacted with gingiva is first surface, the part do not contacted with gingiva is second surface, and described second surface successively sinter molding has dyeing enamel coating and glaze layer.
Wherein in an embodiment, the apparent height of described first surface is no more than 1/3 of described glass-ceramic substrate apparent height.
Wherein in an embodiment, described dyeing porcelain thickness is 0.2 ~ 0.3mm.
Wherein in an embodiment, described glaze layer comprises the first glaze layer first glaze layer and the second glaze layer.
Wherein in an embodiment, described second glaze layer is carved with developmental groove.
Above-mentioned glass ceramics artificial tooth, owing to being the glass-ceramic substrate of cutting forming as the matrix of main body, good integrity, intensity is high, can reduce stress, and result of use is stablized.And in manufacturing process, enamel coating needs cooling after Overheating Treatment, because the heat conductivity of porcelain is poor, when dyeing enamel coating cooling meat, the larger temperature difference can be there is between glass-ceramic substrate surface and the dyeing enamel coating being attached to glass-ceramic substrate surface outer surface, glass-ceramic substrate surface can limit the contraction of dyeing enamel coating, causes in dyeing enamel coating and produces tensile stress; If dyeing enamel coating is coated on glass-ceramic substrate surface completely, and the thickness of dyeing enamel coating remains unchanged, such meeting is because the apparent height of dyeing enamel coating is excessive, thus the enamel coating that causes dyeing holds tensile stress that can't stand generation and fine fisssure occurs, and life-time service collapses porcelain unavoidably.And when using glass ceramics artificial tooth, the first surface contacted with gingiva is main stressed concentrated place, therefore dyeing enamel coating is sintered in the second surface do not contacted with gingiva, reduces the stressed of dyeing enamel coating, namely reduce the probability of dyeing enamel coating generation fine fisssure, thus reduce the probability collapsing porcelain.
Accompanying drawing explanation
Fig. 1 is the structural representation of glass ceramics artificial tooth.
Detailed description of the invention
Below in conjunction with drawings and Examples, this utility model is described further.
As shown in Figure 1, a kind of glass ceramics artificial tooth 100, comprises enamel coating 110.Described enamel coating 110 outwards comprises glass-ceramic substrate 112 and dyeing enamel coating 114 successively.The surface of described glass-ceramic substrate 112 comprises first surface 1122 and second surface 1124, the part contacted with gingiva 200 is first surface 1122, the part do not contacted with gingiva 200 is second surface 1124, and described dyeing enamel coating 114 is sintered in described second surface 1124.The surperficial sinter molding of described dyeing enamel coating 114 has glaze layer 120.
Above-mentioned glass ceramics artificial tooth 100, owing to being the glass-ceramic substrate of cutting forming as the matrix of main body, good integrity, intensity is high, can reduce stress, and result of use is stablized.And in manufacturing process, enamel coating 110 needs cooling after Overheating Treatment, because the heat conductivity of porcelain is poor, when dyeing enamel coating 114 cooling meat, the larger temperature difference can be there is between glass-ceramic substrate 112 and the dyeing enamel coating 114 being attached to glass-ceramic substrate 112 outer surface, glass-ceramic substrate 112 can limit the contraction of dyeing enamel coating 114, causes in dyeing enamel coating 114 and produces tensile stress; If dyeing enamel coating 114 is coated on glass-ceramic substrate 112 surface completely, and the thickness of dyeing enamel coating 114 remains unchanged, such meeting is because the surface area of dyeing enamel coating 114 is excessive, thus the enamel coating 114 that causes dyeing holds tensile stress that can't stand generation and fine fisssure occurs, and life-time service collapses porcelain unavoidably.And when using glass ceramics artificial tooth 100, the first surface 1122 contacted with gingiva 200 is main stressed concentrated place, therefore dyeing enamel coating 114 is sintered in the second surface 1124 do not contacted with gingiva, decrease the stressed of dyeing enamel coating 114, thus reduce the probability that fine fisssure occurs dyeing enamel coating 114, namely reduce the probability collapsing porcelain.
Wherein in an embodiment, the apparent height of described first surface 1122 is no more than 1/3 of described glass-ceramic substrate 112 apparent height.If described first surface 1122 is long, then described glass ceramics artificial tooth 100 can be caused to embed gingiva 200 excessively dark, when laboratory rodent chow, wear and tear too much to gingiva 200, cause the diseases such as gingivitis, cause human body uncomfortable; If described first surface 1122 is too short, then can cause the surface exposure of glass-ceramic substrate 114 outside gingiva 200, cause whole glass ceramics artificial tooth 100 insecure, have and easily cause glass ceramics artificial tooth 100 to loosen the risk causing coming off.So, the height of first surface 1122 is set to less than 1/3 of the apparent height accounting for described glass-ceramic substrate 114, for comparatively reasonably arranging.
Wherein in an embodiment, described dyeing porcelain thickness is 0.2 ~ 0.3mm.The effect of described dyeing enamel coating 114 mainly makes described glass ceramics artificial tooth 100 closer to the tooth of human body itself, makes glass ceramics artificial tooth 100 intensity larger, longer service life simultaneously.And enamel coating 110 blocked up easily causing cracks, therefore it is comparatively reasonable that the thickness of dyeing enamel coating 114 is arranged on 0.2 ~ 0.3mm.
Wherein in an embodiment, described glaze layer 120 comprises the first glaze layer first glaze layer and the second glaze layer.When making first at unsintered dyeing enamel coating 114 external coating first glaze layer, and together sinter with dyeing enamel coating 114, sinter the second glaze layer at the first glaze layer external coating again, glaze layer 120 like this can as required evenly be reasonably distributed in enamel coating 110 surface, surface quality and result of use good.
Wherein in an embodiment, described glaze layer 120 is carved with developmental groove.In a specific embodiment, developmental groove is engraved on the second glaze layer.The acting as of described developmental groove increases bites power broken when chewing, and chews more abundant.So collapse for reduction porcelain, be not necessary.
The above embodiment only have expressed several embodiment of the present utility model, and it describes comparatively concrete and detailed, but therefore can not be interpreted as the restriction to this utility model the scope of the claims.It should be pointed out that for the person of ordinary skill of the art, without departing from the concept of the premise utility, can also make some distortion and improvement, these all belong to protection domain of the present utility model.Therefore, the protection domain of this utility model patent should be as the criterion with claims.
Claims (5)
1. a glass ceramics artificial tooth, it is characterized in that, comprise the glass-ceramic substrate of cutting forming, described glass-ceramic substrate surface comprises first surface and second surface, the part contacted with gingiva is first surface, the part do not contacted with gingiva is second surface, and described second surface successively sinter molding has dyeing enamel coating and glaze layer.
2. glass ceramics artificial tooth according to claim 1, is characterized in that, the apparent height of described first surface is no more than 1/3 of described glass-ceramic substrate apparent height.
3. glass ceramics artificial tooth according to claim 1, is characterized in that, described dyeing porcelain thickness is 0.2 ~ 0.3mm.
4. glass ceramics artificial tooth according to claim 1, is characterized in that, described glaze layer comprises the first glaze layer first glaze layer and the second glaze layer.
5. glass ceramics artificial tooth according to claim 4, is characterized in that, described second glaze layer is carved with developmental groove.