CN204657242U - A kind ofly prevent the mould structure turning over bits - Google Patents
A kind ofly prevent the mould structure turning over bits Download PDFInfo
- Publication number
- CN204657242U CN204657242U CN201520351299.5U CN201520351299U CN204657242U CN 204657242 U CN204657242 U CN 204657242U CN 201520351299 U CN201520351299 U CN 201520351299U CN 204657242 U CN204657242 U CN 204657242U
- Authority
- CN
- China
- Prior art keywords
- convex tendon
- stripper plate
- chute
- matrix cavity
- drift
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a kind of mould structure preventing from turning over bits, comprise die, stripper plate is provided with above die, strip matrix cavity is provided with in die, stripper plate is provided with the strip stripper plate hole corresponding with matrix cavity, the punching pin that cross section is strip is coated with in matrix cavity and stripper plate hole, matrix cavity length direction two side is respectively equipped with the scrap guide chute of two through matrix cavity, vertical convex tendon is provided with between two scrap guide chutes, scrap guide chute groove depth and vertical fin height sum are less than product size tolerance, two side, stripper plate hole length direction is respectively equipped with the chute of stepping down in two through stripper plate holes, step down between chute for two and be provided with convex tendon, chute groove depth of stepping down and fin height sum are less than product size tolerance, punching pin drift two side is respectively equipped with and chute and drift convex tendon corresponding to convex tendon and the drift groove of stepping down, the height of drift convex tendon and the degree of depth sum of drift groove are less than product size tolerance.
Description
[technical field]
The utility model relates to a kind of process equipment, is more particularly a kind of mould.
[background technology]
Be continuous winding during the stamping-out products such as the lead frame of electronic product, exfoliation is waste material.Substantially be all simple shape for outer pin, be all oval viewed from front or kidney-shaped, bits are turned in scrap inclination very easily occurred alongst in die, cause die plug to consider to be worth doing.
[utility model content]
The utility model object overcomes the deficiencies in the prior art, provides one to meet product qualified, and scrap can be made again to produce salient point and the mould structure that prevent from turn over bits of groove along the parallel downslide of matrix cavity.
The utility model is achieved through the following technical solutions:
A kind ofly prevent the mould structure turning over bits, comprise die 1, stripper plate 2 is provided with above described die 1, strip matrix cavity 101 is provided with in described die 1, described stripper plate 2 is provided with the strip stripper plate hole 201 corresponding with described matrix cavity 101, the punching pin 3 that cross section is strip is coated with in described matrix cavity 101 and described stripper plate hole 201, described matrix cavity 101 length direction two side is respectively equipped with the scrap guide chute 111 of two through described matrix cavity 101, vertical convex tendon 112 is provided with between scrap guide chute 111 described in two, described scrap guide chute 111 groove depth and described vertical convex tendon 112 height sum are less than product size tolerance, described length direction two side, stripper plate hole 201 is respectively equipped with the chute 211 of stepping down in two through described stripper plate holes 201, stepping down between chute 211 described in two is provided with convex tendon 212, described chute 211 groove depth and the described convex tendon 212 height sum of stepping down is less than product size tolerance, described punching pin 3 drift two side is respectively equipped with and described chute 211 and drift convex tendon 311 corresponding to convex tendon 212 and the drift groove 312 of stepping down, the height of described drift convex tendon 311 and the degree of depth sum of described drift groove 312 are less than product size tolerance.
Prevent the mould structure turning over bits as above, it is characterized in that: described scrap guide chute 111 groove depth and described vertical convex tendon 112 height sum are less than 0.029mm.
Prevent the mould structure turning over bits as above, it is characterized in that: described scrap guide chute 111 groove depth and described vertical convex tendon 112 height sum are 0.011mm.
Prevent strip scrap from turning over the mould structure of bits as above, it is characterized in that: described scrap guide chute 111 and described vertical convex tendon 112 cross section are circular arc.
Compared with prior art, the utility model has the following advantages:
The utility model arranges groove and convex tendon within the scope of product tolerance in matrix cavity and stripper plate hole, product can be met qualified, scrap can be made again to produce salient point with groove along the parallel downslide of matrix cavity, limit scrap to overturn in concave die cavity, play the effect of balance card bits, scrap can not overturn, and parallel through concave die cavity, avoids turning over bits and causes matrix cavity to block.
[accompanying drawing explanation]
Fig. 1 is the utility model structural representation;
Fig. 2 is the utility model die schematic top plan view;
Fig. 3 is the utility model A portion enlarged drawing;
Fig. 4 is the utility model drift schematic diagram;
Fig. 5 is the utility model stripper plate schematic top plan view;
Fig. 6 is the utility model B portion enlarged drawing;
Fig. 7 is the utility model scrap schematic diagram;
Fig. 8 is that the utility model produces product drawing scrap figure.
[detailed description of the invention]
A kind ofly prevent the mould structure turning over bits, comprise die 1, stripper plate 2 is provided with above described die 1, strip matrix cavity 101 is provided with in described die 1, described stripper plate 2 is provided with the strip stripper plate hole 201 corresponding with described matrix cavity 101, the punching pin 3 that cross section is strip is coated with in described matrix cavity 101 and described stripper plate hole 201, described matrix cavity 101 length direction two side is respectively equipped with the scrap guide chute 111 of two through described matrix cavity 101, vertical convex tendon 112 is provided with between scrap guide chute 111 described in two, described scrap guide chute 111 groove depth and described vertical convex tendon 112 height sum are less than product size tolerance, described length direction two side, stripper plate hole 201 is respectively equipped with the chute 211 of stepping down in two through described stripper plate holes 201, stepping down between chute 211 described in two is provided with convex tendon 212, described chute 211 groove depth and the described convex tendon 212 height sum of stepping down is less than product size tolerance, described punching pin 3 drift two side is respectively equipped with and described chute 211 and drift convex tendon 311 corresponding to convex tendon 212 and the drift groove 312 of stepping down, the height of described drift convex tendon 311 and the degree of depth sum of described drift groove 312 are less than product size tolerance.Within the scope of product tolerance, groove and convex tendon are set in matrix cavity and stripper plate hole, product can be met qualified, scrap can be made again to produce salient point with groove along the parallel downslide of matrix cavity, limit scrap to overturn in concave die cavity, play the effect of balance card bits, scrap can not overturn, and parallel through concave die cavity, avoids turning over bits and causes matrix cavity to block.
Described scrap guide chute 111 groove depth and described vertical convex tendon 112 height sum are less than 0.029mm.
Described scrap guide chute 111 groove depth and described vertical convex tendon 112 height sum are preferably 0.011mm.
Described scrap guide chute 111 and described vertical convex tendon 112 cross section are circular arc.
Be provided with die mold insert 110 in described die 1, described matrix cavity 101 is arranged in described die mold insert 110, and described die mold insert 110 is made up of two piecemeal mold inserts of point middle face symmetry with described matrix cavity 101 width.Sectional type insert structure is convenient to processing.
The utility model principle: mould of the present utility model is applicable to the product that tolerance is ± more than 0.03mm, during product stamping-out, form convex tendon and groove in the length direction both sides of product, balance scrap, can meet product qualified, scrap can be made again to produce salient point with groove along the parallel downslide of matrix cavity, limit scrap to overturn in concave die cavity, play the effect of balance card bits, scrap can not overturn, parallel through concave die cavity, avoid turning over bits and cause matrix cavity to block.
Claims (5)
1. one kind prevents the mould structure turning over bits, comprise die (1), described die (1) top is provided with stripper plate (2), strip matrix cavity (101) is provided with in described die (1), described stripper plate (2) is provided with the strip stripper plate hole (201) corresponding with described matrix cavity (101), the punching pin (3) that cross section is strip is coated with in described matrix cavity (101) and described stripper plate hole (201), it is characterized in that: the scrap guide chute (111) described matrix cavity (101) length direction two side being respectively equipped with two through described matrix cavity (101), vertical convex tendon (112) is provided with between scrap guide chute (111) described in two, described scrap guide chute (111) groove depth and described vertical convex tendon (112) height sum are less than product size tolerance, described stripper plate hole (201) length direction two side is respectively equipped with the chute of stepping down (211) in two through described stripper plate holes (201), convex tendon (212) is provided with between chute of stepping down (211) described in two, described chute of stepping down (211) groove depth and described convex tendon (212) height sum are less than product size tolerance, described punching pin (3) drift two side is respectively equipped with the drift convex tendon (311) corresponding with described chute of stepping down (211) and convex tendon (212) and drift groove (312), the height of described drift convex tendon (311) and the degree of depth sum of described drift groove (312) are less than product size tolerance.
2. according to claim 1ly prevent the mould structure turning over bits, it is characterized in that: described scrap guide chute (111) groove depth and described vertical convex tendon (112) height sum are less than 0.029mm.
3. according to claim 2ly prevent the mould structure turning over bits, it is characterized in that: described scrap guide chute (111) groove depth and described vertical convex tendon (112) height sum are 0.011mm.
4. according to claim 3ly prevent the mould structure turning over bits, it is characterized in that: described scrap guide chute (111) and described vertical convex tendon (112) cross section are circular arc.
5. according to claim 1ly prevent the mould structure turning over bits, it is characterized in that: in described die (1), be provided with die mold insert (110), described matrix cavity (101) is arranged in described die mold insert (110), and described die mold insert (110) is made up of two piecemeal mold inserts of point middle face symmetry with described matrix cavity (101) width.