CN204325523U - A kind of fixture of aluminium alloy anode oxide - Google Patents

A kind of fixture of aluminium alloy anode oxide Download PDF

Info

Publication number
CN204325523U
CN204325523U CN201420825526.9U CN201420825526U CN204325523U CN 204325523 U CN204325523 U CN 204325523U CN 201420825526 U CN201420825526 U CN 201420825526U CN 204325523 U CN204325523 U CN 204325523U
Authority
CN
China
Prior art keywords
cathode bar
oxidation
oxidation cathode
anode rod
bar
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201420825526.9U
Other languages
Chinese (zh)
Inventor
彭丽霞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xian International University
Original Assignee
Xian International University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xian International University filed Critical Xian International University
Priority to CN201420825526.9U priority Critical patent/CN204325523U/en
Application granted granted Critical
Publication of CN204325523U publication Critical patent/CN204325523U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A fixture for aluminium alloy anode oxide, includes the oxidizing anode rod be located on processing parts fixing sleeve; Oxidizing anode rod is connected with one end of insulation wood, and the other end of insulation wood is connected with oxidation cathode bar; The lower end of oxidation cathode bar is through the through hole on processing parts fixing sleeve; Described oxidation cathode bar is hollow aluminum pipe, and hollow aluminum pipe lower end is provided with several holes; The crossbeam be suspended to above oxidation trough by oxidizing anode rod connects positive source; Oxidation cathode bar connects power cathode, makes hollow aluminium bar, and processes some holes at below 1/3rd place; The lower end closed of oxidation cathode bar, the other end plastic hose connects with pneumatic line; Oxidizing anode rod and oxidation cathode bar are fixed by processing parts fixing sleeve; The sleeve type workpiece of processing is inserted below oxidation cathode bar; Have the advantages that structure is simple, cost is low, simple to operate.

Description

A kind of fixture of aluminium alloy anode oxide
Technical field
The utility model belongs to aluminum alloy processing technology field, particularly a kind of fixture of aluminium alloy anode oxide.
Background technology
For the Al alloy parts of tubulose, the mode usually adopting vertical dress to hang in traditional course of processing, is stirred air bottom tank liquor, is distributed the heat produced in workpiece process by the pressurized air bottom oxidation trough.
According to bubble force analysis in the solution, during pressurized air stirred solution, bubble to the process of motion of melt surface, is not vertical uplift from bottom, but curved track rises.This pneumatic line that bottom land is evenly arranged, it is uneven after the pressurized air that passes into arrives liquid level of solution, there is very big-difference in liquid level bubble center position and compressed air outlet position, this species diversity is along with the intensification of solution deep and the change of solution sectional area become greatly and constantly large, and cannot accurately control.In actual parts operating process, after part dress extension pre-process and post-process completes, enter hard oxidation trough, the general stirring state first observing solution according to the size of liquid level bubble of operator, and part is placed in the position selecting stirring good.But due to the unstable of bubble motion, along with the change of time, the bubble area of liquid level also can change, and this just has influence on the cooling-down effect of this position part.
Because tubular member sectional area is too little, the pressurized air of bottom also cannot ensure to pass from part mesopore, simultaneously, part also cannot ensure that in tank liquor 100% is vertical, easily cause the solution temperature in Central of the parts hole too high, film layer dissolves speed is greater than the speed of growth, occurs parts locally dissolution phenomena.
Summary of the invention
In order to overcome above-mentioned the deficiencies in the prior art, the purpose of this utility model is to provide a kind of fixture of aluminium alloy anode oxide, solve the stirring problem of inner bore of part solution, avoid the local superheating of interior hole solution, cause part dissolution phenomena, have the advantages that structure is simple, cost is low, simple to operate.
For achieving the above object, the technical solution adopted in the utility model is: a kind of fixture of aluminium alloy anode oxide, includes the oxidizing anode rod be located on processing parts fixing sleeve; Oxidizing anode rod is connected with one end of insulation wood, and the other end of insulation wood is connected with oxidation cathode bar; The lower end of oxidation cathode bar is through the through hole on processing parts fixing sleeve; Described oxidation cathode bar is hollow aluminum pipe, and hollow aluminum pipe lower end is provided with several holes.
Described oxidation cathode bar lower end closed; Described hole is located at upwards 1/3rd places, hollow aluminum pipe lower end.
The beneficial effects of the utility model are:
Compared with prior art, the utility model, for this type of part, changes the aluminium bar used in oxidising process into hollow aluminum pipe, blocks bottom hollow aluminum pipe, and the position in portion 1/3 evenly gets out aperture on the lower, as auxiliary cathode, also plays the effect compressing stirring pipe of taking offence.Hollow aluminum pipe is connected with power cathode, uses plastic hose to be connected by the pressurized air of itself and production line simultaneously, like this, in hard oxidising process, just solve the stirring problem of inner bore of part solution, avoid the local superheating of interior hole solution, cause part dissolution phenomena.
Accompanying drawing explanation
Fig. 1 is structural representation of the present utility model.
Embodiment
Below in conjunction with accompanying drawing, structural principle of the present utility model and principle of work are described in further detail.
See Fig. 1, a kind of fixture of aluminium alloy anode oxide, includes the oxidizing anode rod 1 be located on processing parts fixing sleeve 4; Oxidizing anode rod 1 is connected with one end of insulation wood 3, and the other end of insulation wood 3 is connected with oxidation cathode bar 2; The lower end of oxidation cathode bar 2 is through the through hole on processing parts fixing sleeve 4; Described oxidation cathode bar 2 is hollow aluminum pipe, and hollow aluminum pipe lower end is provided with several holes.
Described oxidation cathode bar 2 lower end closed; Described hole 5 is located at upwards 1/3rd places, hollow aluminum pipe lower end.
Principle of work of the present utility model is:
During use, oxidizing anode rod 1 to be suspended on the crossbeam above oxidation trough and to connect positive source; Oxidation cathode bar 2 connects power cathode, makes hollow aluminium bar, and processes some holes 5 at below 1/3rd place; The lower end closed of oxidation cathode bar 2, the other end plastic hose connects with pneumatic line; Oxidizing anode rod 1 and oxidation cathode bar 2 are fixed by processing parts fixing sleeve 4; The sleeve type workpiece of processing is inserted below oxidation cathode bar 2, fastening by processing parts fixing sleeve 4.

Claims (2)

1. a fixture for aluminium alloy anode oxide, includes the oxidizing anode rod (1) be located on processing parts fixing sleeve (4); Oxidizing anode rod (1) is connected with one end of insulation wood (3), and the other end of insulation wood (3) is connected with oxidation cathode bar (2); The lower end of oxidation cathode bar (2) is through the through hole on processing parts fixing sleeve (4); Described oxidation cathode bar (2) is hollow aluminum pipe, and hollow aluminum pipe lower end is provided with several holes.
2. the fixture of a kind of aluminium alloy anode oxide according to claim 1, is characterized in that, described oxidation cathode bar (2) lower end closed; Described hole is located at upwards 1/3rd places, hollow aluminum pipe lower end.
CN201420825526.9U 2014-12-22 2014-12-22 A kind of fixture of aluminium alloy anode oxide Expired - Fee Related CN204325523U (en)