CN203900151U - Surface treatment mould for metal wire rods - Google Patents

Surface treatment mould for metal wire rods Download PDF

Info

Publication number
CN203900151U
CN203900151U CN201420332973.0U CN201420332973U CN203900151U CN 203900151 U CN203900151 U CN 203900151U CN 201420332973 U CN201420332973 U CN 201420332973U CN 203900151 U CN203900151 U CN 203900151U
Authority
CN
China
Prior art keywords
mould
scalping
surface treatment
sleeve
diaphragm capsule
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201420332973.0U
Other languages
Chinese (zh)
Inventor
李阳
田琳
白景年
豆卫涛
赵岐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Western Superconducting Technologies Co Ltd
Original Assignee
Western Superconducting Technologies Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Western Superconducting Technologies Co Ltd filed Critical Western Superconducting Technologies Co Ltd
Priority to CN201420332973.0U priority Critical patent/CN203900151U/en
Application granted granted Critical
Publication of CN203900151U publication Critical patent/CN203900151U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model discloses a surface treatment mould for metal wire rods. The surface treatment mould comprises a mould box, wherein a centering mould and a positioning sleeve are arranged at the two sides of the mould box respectively; the positioning sleeve is provided with a scalping mould; the scalping mould and the centering mould are coaxially arranged; a sleeve is arranged outside the scalping mould; the scalping mould and the sleeve are connected through a scalping mould pressing cover; the sleeve is fixed on a separation plate; the separation plate is fixed in the mould box; a bearing is mounted outside the sleeve; a belt wheel is mounted on an outer ring of the bearing; the belt wheel is connected with scrap pulling rods through a fastening bolt; the mould box is further provided with a water inlet and a water outlet respectively. According to the surface treatment mould for the metal wire rods, the wire rods which are not scalped are accurately centered through the centering mould, scraps generated by scalping can be cut off by the scrap pulling rods, and cooling water is introduced into the mould box through the water inlet to cool the scalping mould, so that the problems that the existing scalping mould cannot be accurately centered, the scrap cutting is not smooth and the cooling performance of the mould is poor are solved, and the machining efficiency and the yield are improved.

Description

A kind of wire wire rod surface treatment mould
Technical field
The utility model belongs to tinsel timber die technical field, is specifically related to a kind of wire wire rod surface treatment mould.
Background technology
Metal wire material surface in the hot procedures such as rolling and drawing can produce one deck oxide skin and some defects, so need to it be repaiied and be removed by process of surface treatment, conventionally by stripping off the skin, it is processed, but larger with the Centreless lathe task difficulty that strips off the skin for small dimension silk material, in industry, conventionally adopt scalping mold to carry out the operation that strips off the skin of a material.Existing scalping mold exists centering to be forbidden, partially take off phenomenon, and chip breaking is not smooth, exists smear metal to pile up, and mold cools down is poor, has a strong impact on the service life of mould and the yield rate of metal wire material.
Utility model content
The purpose of this utility model is to provide a kind of wire wire rod surface treatment mould, has solved that the centering of existing scalping mold is inaccurate, chip breaking is smooth, the poor problem of mold cools down.
The technical scheme that the utility model adopts is: a kind of wire wire rod surface treatment mould, comprise diaphragm capsule, diaphragm capsule both sides are respectively arranged with centering mould and location jacket casing, positioning tube puts and is provided with scalping mold, scalping mold coaxially arranges with centering mould, scalping mold is outside equipped with sleeve, scalping mold is connected by scalping mold gland with sleeve, sleeve is fixed on dividing plate, dividing plate is fixed in diaphragm capsule, sleeve is provided with bearing outward, and belt pulley is installed on bearing outer ring, and belt pulley is connected with group bits bar by fastening bolt; On diaphragm capsule, be also respectively arranged with water inlet and delivery port.
Feature of the present utility model is also,
On centering mould, be fixed with centering mould gland, centering mould gland is connected with diaphragm capsule by fishbolt.
Distance between scalping mold and centering mould is 200-300mm.
Location jacket casing is welded on diaphragm capsule side plate, and location jacket casing is welded with gusset near diaphragm capsule end.
Location jacket casing contacts with scalping mold face.
Scalping mold gland and sleeve are fixed on scalping mold between scalping mold gland and abutment sleeve by threaded engagement.
Between scalping mold gland and scalping mold, be provided with sealing ring.
Belt pulley is also provided with belt pulley backplate outward, and belt pulley backplate is fixed on diaphragm capsule by backplate fastening bolt.
Belt pulley is connected with motor.
On the base of diaphragm capsule, be provided with installing hole.
The beneficial effects of the utility model are: a kind of wire wire rod of the utility model surface treatment mould, by centering mould, bits bar is accurately felt relieved, dialled to the silk material before stripping off the skin cuts off the smear metal producing that strips off the skin, by water inlet, to passing into cooling water in diaphragm capsule, to scalping mold, carry out cooling, solved that the centering of existing scalping mold is inaccurate, chip breaking is smooth, the poor problem of mold cools down, improved working (machining) efficiency and yield rate.
Accompanying drawing explanation
Fig. 1 is the structural representation of the utility model wire wire rod surface treatment mould;
Fig. 2 is the structural representation of the utility model wire wire rod surface treatment mould scalping mold;
Fig. 3 is the top view of the utility model wire wire rod surface treatment mould.
In figure, 1. fishbolt, 2. centering mould gland, 3. centering mould, 4. diaphragm capsule, 5. fastening bolt, 6. group bits bar, 7. bearing, 8. belt pulley, 9. gusset, 10. locate jacket casing, 11. scalping molds, 12. scalping mold glands, 13. sleeves, 14. dividing plates, 15. water inlets, 16. delivery ports, 17. belt pulley backplates, 18. backplate fastening bolts.
The specific embodiment
Below in conjunction with the drawings and specific embodiments, the utility model is elaborated.
A kind of wire wire rod of the utility model surface treatment mould, as shown in Figure 1, comprise diaphragm capsule 4, diaphragm capsule 4 both sides are respectively arranged with centering mould 3 and location jacket casing 10, on centering mould 3, be fixed with centering mould gland 2, centering mould gland 2 is connected with diaphragm capsule 4 by fishbolt 1, jacket casing 10 one end, location are welded on diaphragm capsule 4 side plates, the other end is fixed with scalping mold 11, abutment sleeve 10 is realized face with scalping mold 11 and is contacted, location jacket casing 10 is welded with gusset 9 near diaphragm capsule 4 ends, to meet strength demand, scalping mold 11 is 200-300mm with the centering coaxial setting of mould 3 and spacing, as shown in Figure 2, scalping mold 11 is outside equipped with sleeve 13, scalping mold 11 is connected by scalping mold gland 12 with sleeve 13, threading on scalping mold gland 12 external cylindrical surfaces, sleeve 13 machining internal threads, scalping mold gland 12 and sleeve 13 are fixed on scalping mold 11 between scalping mold gland 12 and abutment sleeve 10 by threaded engagement, between scalping mold gland 12 and scalping mold 11, be also provided with sealing ring, prevent that cooling water from flowing out from gap, sleeve 13 is welded on dividing plate 14, dividing plate 14 is welded in diaphragm capsule 4, on sleeve 13 external cylindrical surfaces, bearing 7 is installed, bearing is provided with belt pulley 8 on 7 outer rings, belt pulley 8 is connected with group bits bar 6 by fastening bolt 5, as shown in Figure 3, the outer belt pulley backplate 17 that is also provided with of belt pulley 8, belt pulley backplate 17 is fixed on diaphragm capsule 4 by backplate fastening bolt 18, belt pulley 8 is also connected with motor, on diaphragm capsule 4, be also respectively arranged with water inlet 15 and delivery port 16, on the base of diaphragm capsule 4, be provided with installing hole.
Silk material needed to carry out online annealing in process before stripping off the skin, and had reduced the difficulty that strips off the skin of silk material, but plasticity increase, the silk material after annealing was free state before entering scalping mold, had greatly increased the risk that a material is taken off partially.In order to guarantee the bark effect of taking off of a material, need to feel relieved to the silk material entering before scalping mold 11, the method that centering adopts is to enter the front first process of scalping mold 11 centering mould 3 at silk material, realizes the good centering of silk material self.Centering mould 3 and scalping mold 11 guarantees concentric, and both guarantee between 200-300mm distance, the too short guiding certralizing ability that do not have of distance, apart from oversize between two moulds a material there is deflection, do not have equally the effect of centering.
The difficult point that silk material strips off the skin is chip breaking voluntarily, leans on external force traction smear metal, in order to avoid at scalping mold 11 cutting edge bulk depositions, cause the interruption that strips off the skin in the process that in the past strips off the skin.Therefore, go out to consider to be worth doing end two groups of bits bars 6 are installed at scalping mold 11, the smear metal producing is dialed at a high speed, the end of group bits bar 6 is processed into pointed, in chip surface, forms cut, is convenient to easy chip breaking in dialling bits bar 6 placement process.Dial bits bar 6 for two and be connected in belt pulley 8 sides by fastening bolt 5, follow belt pulley rotation.The installing hole of dialling bits bar 6 is processed into the radial position that strip hole is convenient to dial according to the difference adjustment of silk material diameter bits bar.
Scalping mold 11 can produce a large amount of heat in silk material strips off the skin process, if cooling not in time can cause cutting edge passivation, has a strong impact on the service life of scalping mold 11, must carry out cooling to scalping mold 11 for this reason.By water inlet 15, in diaphragm capsule 4, pass into cooling water, it is full of around scalping mold 11 and location jacket casing 10, water inlet 15 and delivery port 16 guarantee that cooling water temperature meets the cooling needs of scalping mold 11.
During use, need to carry out surface-treated wire wire rod first feels relieved by centering mould 3, enter in diaphragm capsule 4, then enter the processing that strips off the skin in scalping mold 11, dial bits bar 6 with belt pulley 8 rotations, the smear metal that is deposited in scalping mold 11 and goes out bits end is interrupted, by water inlet 15, in diaphragm capsule 4, pass into cooling water, make scalping mold 11 and location jacket casing 10 be full of cooling water around, scalping mold 11 is cooled, the wire rod after stripping off the skin passes diaphragm capsule 4 through location jacket casing 10.
A kind of wire wire rod of the utility model surface treatment mould, overcome that the phenomenon that partially strips off the skin that wire wire rod strips off the skin in the past, chip breaking are smooth, the poor shortcoming of mold cools down, realize the good centering that silk thread material strips off the skin, stablized chip breaking, fully cooling, improved working (machining) efficiency and yield rate.

Claims (10)

1. a wire wire rod surface treatment mould, it is characterized in that, comprise diaphragm capsule (4), described diaphragm capsule (4) both sides are respectively arranged with centering mould (3) and location jacket casing (10), on described location jacket casing (10), be provided with scalping mold (11), described scalping mold (11) coaxially arranges with described centering mould (3), described scalping mold (11) is outside equipped with sleeve (13), described scalping mold (11) is connected by scalping mold gland (12) with described sleeve (13), described sleeve (13) is fixed on dividing plate (14), described dividing plate (14) is fixed in diaphragm capsule (4), the outer bearing (7) that is provided with of described sleeve (13), described bearing (7) is provided with belt pulley (8) on outer ring, described belt pulley (8) is connected with group bits bar (6) by fastening bolt (5), on described diaphragm capsule (4), be also respectively arranged with water inlet (15) and delivery port (16).
2. a kind of wire wire rod surface treatment mould as claimed in claim 1, it is characterized in that, on described centering mould (3), be fixed with centering mould gland (2), described centering mould gland (2) is connected with described diaphragm capsule (4) by fishbolt (1).
3. a kind of wire wire rod surface treatment mould as claimed in claim 1 or 2, is characterized in that, the distance between described scalping mold (11) and described centering mould (3) is 200-300mm.
4. a kind of wire wire rod surface treatment mould as claimed in claim 1, it is characterized in that, described location jacket casing (10) is welded on described diaphragm capsule (4) side plate, and described location jacket casing (10) is welded with gusset (9) near described diaphragm capsule (4) end.
5. a kind of wire wire rod surface treatment mould as claimed in claim 1, is characterized in that, described location jacket casing (10) contacts with described scalping mold (11) face.
6. a kind of wire wire rod surface treatment mould as claimed in claim 1, it is characterized in that, described scalping mold gland (12) and described sleeve (13) are fixed on scalping mold (11) between scalping mold gland (12) and abutment sleeve (10) by threaded engagement.
7. a kind of wire wire rod surface treatment mould as described in claim 1 or 6, is characterized in that, between described scalping mold gland (12) and described scalping mold (11), is provided with sealing ring.
8. a kind of wire wire rod surface treatment mould as claimed in claim 1, it is characterized in that, described belt pulley (8) is outer is also provided with belt pulley backplate (17), and described belt pulley backplate (17) is fixed on described diaphragm capsule (4) by backplate fastening bolt (18).
9. a kind of wire wire rod surface treatment mould as described in claim 1 or 8, is characterized in that, described belt pulley (8) is connected with motor.
10. a kind of wire wire rod surface treatment mould as claimed in claim 1, is characterized in that, on the base of described diaphragm capsule (4), is provided with installing hole.
CN201420332973.0U 2014-06-20 2014-06-20 Surface treatment mould for metal wire rods Expired - Lifetime CN203900151U (en)