CN203772672U - Device for measuring content of asphalt in emulsified asphalt - Google Patents

Device for measuring content of asphalt in emulsified asphalt Download PDF

Info

Publication number
CN203772672U
CN203772672U CN201420083788.2U CN201420083788U CN203772672U CN 203772672 U CN203772672 U CN 203772672U CN 201420083788 U CN201420083788 U CN 201420083788U CN 203772672 U CN203772672 U CN 203772672U
Authority
CN
China
Prior art keywords
asphalt
emulsified asphalt
emulsified
microwave heating
content
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201420083788.2U
Other languages
Chinese (zh)
Inventor
弓锐
弥海晨
徐鹏
郭彦强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xian Highway Research Institute
Original Assignee
Xian Highway Research Institute
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xian Highway Research Institute filed Critical Xian Highway Research Institute
Priority to CN201420083788.2U priority Critical patent/CN203772672U/en
Application granted granted Critical
Publication of CN203772672U publication Critical patent/CN203772672U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model relates to a device for measuring the content of asphalt in emulsified asphalt. The device comprises a sample pipe for containing the asphalt to be emulsified, a microwave heating pipe for heating the emulsified asphalt in the sample pipe, a weighing device for measuring the mass of the asphalt to be emulsified, a temperature sensor arranged in the microwave heating pipe, and a display for displaying a detection value obtained by the temperature sensor and a weighing value obtained by the weighing device, wherein the microwave heating device is arranged on the weighing device; the sample pipe is arranged in the microwave heating pipe. The device disclosed by the utility model is simple in structure, high in practicability and low in environment pollution, and can realize quick detection on the content of the asphalt in the emulsified asphalt.

Description

The measurement mechanism of emulsified asphalt Asphalt Content
Technical field
The present invention relates to the detection of emulsified asphalt medium pitch effective content, can carry out the detection of common emulsified asphalt, modified emulsifying asphalt Asphalt Content.
Background technology
Emulsified asphalt is as the cold construction material of one, along with its ripe production technology, and the pavement performance of high-quality, simple construction technology, more and more receives professional quarters' concern.Emulsified asphalt is mainly made up of water, emulsifying agent, additive and pitch, and the content of its performance and pitch is closely related.Therefore the effective content of, guaranteeing pitch is the key that ensures emulsified asphalt quality.
At present, the equipment of emulsified asphalt is produced in batch production, general per hourly reaches several tons even tens tons, and therefore, per minute is produced with regard to the emulsified asphalt that has up to a hundred kilograms, is difficult to accurately control the content of emulsified asphalt only according to the adjustment of equipment itself.How can determine fast the content of emulsified asphalt, guarantee the quality of production of emulsified asphalt, most important.
Emulsified Bitumen at Abroad detects, production technology, and the U.S. goes on along in the prostatitis in the world, and the emulsified asphalt residue test method of ASTM has been subjected to accreditation widely in the world, is mainly divided into evaporation method and the way of distillation.
The emulsified asphalt residue test evaporation method of ASTM mainly contains ASTM D6934, ASTMD7404 and ASTMD7497.ASTM D6934 gets about 50g emulsified asphalt sample in container, and moisture is removed in the baking oven evaporation being placed under limiting temperature, or puts into baking oven after heating evaporation again.The method needs respectively 3h and 1h, and experimental period is longer, for produced on-site, within 3 hours, has had tens tons of productions out; ASTM D7404 measures emulsified asphalt residue with moisture analyser, and can obtain at short notice experimental result, and automaticity is high, but cost of equipment is higher, is difficult to popularize.ASTM D7497 adopts low-temperature evaporation technology, and the lower time of low temperature exceedes 1 day, cannot be used for produced on-site.
Domestic existing method for normalizing is on the test method basis of ASTM, determines with reference to Japanese specification, and detection time is longer, is not suitable with the needs of plant produced.
Comprehensive analyze domestic and international present Research, in batch production production testing, require the relatively accurate in a short period of time content that detects emulsified asphalt, and equipment, technique are simple, are easy to promote.Therefore, we have designed emulsified asphalt effective content rapid measurement device, can measure fast pitch effective content, for production, the processing high efficient and reliable of emulsified asphalt, provide technical support.
Summary of the invention
For defect or the deficiency of prior art, the purpose of this utility model is to provide a kind of rapid measurement device of emulsified asphalt Asphalt Content.With solve existing emulsified asphalt effective content efficiency when factory and the site survey not high, need to carry more weighing, heating, mixing plant, the shortcoming such as measuring result error is larger.
The measurement mechanism of the emulsified asphalt Asphalt Content that for this reason, the utility model provides comprises:
Sample hose: for holding emulsified asphalt to be measured;
Microwave heating pipe: heat for the emulsified asphalt to sample hose;
Meausring apparatus: for the quality of emulsified asphalt to be measured;
Temperature sensor: be placed in microwave heating pipe;
Display: for the weighing value of detected value and the meausring apparatus of displays temperature sensor;
Described microwave heating pipe is placed on described meausring apparatus, and described sample hose is placed in described microwave heating pipe.
Preferably, described display is installed on described meausring apparatus.
Further, the measurement mechanism of described emulsified asphalt Asphalt Content also comprises top cover, and this top cover is placed on microwave heating pipe, runs off for the heat that limits heating process, offers steam hole on this top cover simultaneously.
Preferably, described sample hose is of a size of: diameter 30mm, high 100mm.
Compared with prior art, the utility model has the advantage of:
(1) master trip instrument is connected with Weighing system, is then connected with control system, makes the globality of this measurement mechanism better.
(2) pick-up unit is small and exquisite, by a large amount of evidences, the sample quality of code requirement is reduced to 10g, and measured bitumen content result degree of accuracy is high, measurement required time is short.
(3) microwave refers to the electromagnetic wave of frequency at 300MHz~300GMz.Under the effect of microwave electromagnetic field, the polar molecule in dielectric material transfers to and follows the friendship table of microwave electromagnetic field and oriented from original thermal motion state, and microwave energy is converted into the heat in medium, makes material temperature be rendered as the rising in macroscopic view.Microwave heating is current state-of-the-art asphalt pavement material heating means; have that speed is fast, homogeneous heating, thermograde is little, heat loss is few; the flames of anger, without the advantage such as weak seam and weak junction, repairing quality be high and pollution-free; meet that national energy-saving reduces discharging, the requirement of environmental protection, can meet that HIGHWAY MAINTENANCE enters fast, sharp work, the need of work withdrawn fast.Measurement mechanism of the present utility model adopts microwave heating, and environment-friendly high-efficiency is less to the harm of environment.
To sum up, apparatus structure of the present utility model is simple, practical, little to environmental hazard, can realize the fast detecting to emulsified asphalt Asphalt Content.
Brief description of the drawings
Below in conjunction with accompanying drawing and embodiment, the utility model is further explained to explanation.
Fig. 1 is structural representation of the present utility model, and the dimensional units in figure is: mm.
Embodiment
Meausring apparatus of the present utility model is the conventional meausring apparatus of electronic scale or laboratory.
Below provide specific embodiment of the utility model, it should be noted that the utility model is not limited to following specific embodiment, all equivalents of doing on present techniques scheme basis all fall into protection domain of the present utility model.
Embodiment 1:
With reference to figure 1, this measurement mechanism comprises master trip instrument and control system, and described master trip instrument comprises microwave heating pipe 2, sample hose 1, top cover 5, meausring apparatus 3 and display 4.Wherein: sample hose 1 is placed in microwave heating pipe 2, microwave heating pipe 2 is placed on meausring apparatus 3, and top cover 5 is located at microwave heating pipe 2 tops, and meausring apparatus 3 becomes one with display, so that the electrical connection of device.
Specific operation process is as follows:
(1) sample bucket cylinder is cleaned up and dried, put into after microwave heating groove, the above part quality of zero clearing on Weighing system.
(2) sample cylinder is taken out again, add after uniform emulsified asphalt sample 10g ± 1g, again put in microwave heating groove, recording quality display screen quality m 1, accurately to 0.1g.
(3) adopt microwave heating, keep heating-up temperature at 160 DEG C, finish recording quality display screen quality m to quality during without significant change 2, accurately to 0.1g.
(4) the evaporation residue content of emulsified asphalt sample calculates by formula (1), retains 2 significant digits.
p b = m 1 m 2 × 100 % - - - ( 1 )
In formula: p b---the bitumen content in emulsified asphalt, %;
M 1---quality before sample heating, g
M 2---quality after sample heating, g
In the time determining this test unit specimen in use quality, measuring respectively sample quality is 50g, 40g, 30g, 10g and 5g, and records the needed time, by relative error value and required time, and the final sample quality of determining use 10g.
Different quality test findings at table 1160 DEG C
To common several emulsified asphalts and modified emulsifying asphalt, according to method for normalizing and this device, detect respectively bitumen content respectively, the results are shown in Table 2.
Measured value and error testing result after the dissimilar emulsified asphalt operating specification of table 2 method and this device
Can draw by above two groups of test findings, use this new device to measure bitumen content, simple and efficient, measuring error is very little, is far superior to the measured value of code requirement method.Because it is convenient for carrying, easy to operate, high-level efficiency, energy-saving and environmental protection, pollution-free, recommend extensively to promote.

Claims (4)

1. a measurement mechanism for emulsified asphalt Asphalt Content, is characterized in that, comprising:
Sample hose: for holding emulsified asphalt to be measured;
Microwave heating pipe: heat for the emulsified asphalt to sample hose;
Meausring apparatus: for weighing the quality of emulsified asphalt to be measured;
Temperature sensor: be placed in microwave heating pipe;
Display: for the weighing value of detected value and the meausring apparatus of displays temperature sensor;
Described microwave heating pipe is placed on described meausring apparatus, and described sample hose is placed in described microwave heating pipe.
2. the measurement mechanism of emulsified asphalt Asphalt Content as claimed in claim 1, is characterized in that, described display is installed on described meausring apparatus.
3. the measurement mechanism of emulsified asphalt Asphalt Content as claimed in claim 1, it is characterized in that, the measurement mechanism of described emulsified asphalt Asphalt Content also comprises top cover, this top cover is placed on microwave heating pipe, run off for the heat that limits heating process, on this top cover, offer steam hole simultaneously.
4. the measurement mechanism of emulsified asphalt Asphalt Content as claimed in claim 1, is characterized in that, described sample hose is of a size of: diameter 30mm, high 100mm.
CN201420083788.2U 2014-02-26 2014-02-26 Device for measuring content of asphalt in emulsified asphalt Expired - Fee Related CN203772672U (en)