CN203712035U - Laser soldering tin device for soldering mobile phone camera - Google Patents
Laser soldering tin device for soldering mobile phone camera Download PDFInfo
- Publication number
- CN203712035U CN203712035U CN201420028557.1U CN201420028557U CN203712035U CN 203712035 U CN203712035 U CN 203712035U CN 201420028557 U CN201420028557 U CN 201420028557U CN 203712035 U CN203712035 U CN 203712035U
- Authority
- CN
- China
- Prior art keywords
- laser
- mobile phone
- tin
- phone camera
- soldering
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model provides a laser soldering tin device for soldering a mobile phone camera. The laser soldering tin device comprises a laser generator, a beam expander, a diaphragm, a laser galvanometer, an F-Theta field lens and a pulse-width modulation (PWM) modulating circuit, wherein the beam expander is arranged at an output end of the laser generator, the diaphragm is disposed at an output end of the beam expander, the laser galvanometer is mounted at an output end of the diaphragm, the F-Theta field lens is installed at an output end of the laser galvanometer, the PWM modulating circuit is connected with the laser generator, and the F-Theta field lens rightly faces a processing platform. The laser soldering tin device for soldering the mobile phone camera is low in costs and capable of effectively preventing tin paste from splashing during tin soldering.
Description
Technical field
The utility model relates to laser weld field, relates in particular to a kind of for welding mobile phone camera laser tin-soldering device and method.
Background technology
Reserved position, place that at present mobile phone camera need to weld is very little, and the little gap scolding tin to only reserved 0.59mm is even less, for camera scolding tin, from manual scolding tin, develops into laser scolding tin now.
Due to the demand of production capacity, laser scolding tin has become a kind of trend, and laser scolding tin also exists several defects when raising the efficiency; as tin cream splashes; non-welding portion burn, can solve problems although painting protection liquid adds cleaning, and this increases production process and production cost.
Utility model content
The purpose of this utility model is to overcome the defect of prior art, provide a kind of cost low, can effectively prevent scolding tin time tin cream splash for welding mobile phone camera laser tin-soldering device.
The utility model is achieved in that a kind of for welding the laser tin-soldering device of mobile phone camera, comprise laser generator, be arranged on described laser generator output beam expanding lens, be arranged on described beam expanding lens output diaphragm, be arranged on described diaphragm output laser galvanometer, be arranged on the F-Theta field lens of described laser galvanometer output and the PWM(pulse width modulation being connected with described laser generator, PWM:Pulse Width Modulation) modulation circuit, described F-Theta field lens is right against processing platform.
Further, described processing platform is in positive out of focus position.
Further, described laser generator is 532nm laser instrument.
Further, described beam expanding lens is 5 power beam expansion lens, and the described aperture of the diaphragm is 2mm, and described F-Theta field lens focal length is 254mm.
It is a kind of for welding the laser tin-soldering device of mobile phone camera that the utility model provides, by laser generator emission pulse laser process beam expanding lens, diaphragm, laser galvanometer and F-Theta field lens arrive processing platform and carry out scolding tin, the time of a scolding tin is divided into a plurality of time periods that connect successively, by described PWM modulation circuit, adjust the dutycycle of described laser pulse, laser pulse dutycycle in each time period remains unchanged, the dutycycle of the laser pulse that different time sections is corresponding increases gradually, thereby simulate a discrete scolding tin curve from low temperature to high temperature, the temperature for the treatment of solder(ing) paste is increased gradually, in the situation that guarantee mean power and the constant peak power that reduces laser of frequency of laser, thereby also reduced the power density at processing place laser facula, effectively prevented because temperature excursion causes tin cream to splash the problem with the scald of non-weld.
Accompanying drawing explanation
In order to be illustrated more clearly in the utility model embodiment or technical scheme of the prior art, to the accompanying drawing of required use in embodiment or description of the Prior Art be briefly described below, apparently, accompanying drawing in the following describes is only embodiment more of the present utility model, for those of ordinary skills, do not paying under the prerequisite of creative work, can also obtain according to these accompanying drawings other accompanying drawing.
Fig. 1 for the utility model embodiment provide a kind of for welding the structural representation of the laser tin-soldering device of mobile phone camera.
The specific embodiment
Below in conjunction with the accompanying drawing in the utility model embodiment, the technical scheme in the utility model embodiment is clearly and completely described, obviously, described embodiment is only the utility model part embodiment, rather than whole embodiment.Embodiment based in the utility model, those of ordinary skills are not making the every other embodiment obtaining under creative work prerequisite, all belong to the scope of the utility model protection.
As Fig. 1, it is a kind of for welding the laser tin-soldering device of mobile phone camera that the utility model embodiment provides, comprise laser generator 1, be arranged on the beam expanding lens 2 of described laser generator 1 output, be arranged on the diaphragm 3 of described beam expanding lens 2 outputs, be arranged on the laser galvanometer 4 of described diaphragm 3 outputs, be arranged on the F-Theta field lens 5 of described laser galvanometer 4 outputs and the PWM modulation circuit being connected with described laser generator 1, described F-Theta field lens 5 is right against processing platform 6, in preferred embodiment of the present utility model, described laser generator 1 is 532nm end pumping coupling fiber solid state laser, the pulse width of Output of laser is nanosecond, it is a kind of for welding the laser tin-soldering device of mobile phone camera that the utility model provides, by laser generator 1 emission pulse laser, through beam expanding lens 2, diaphragm 3, laser galvanometer 4 and F-Theta field lens 5, arrive processing platform 6 and carry out scolding tin, laser scolding tin device structure of the present utility model is simple, and cost is low.
A kind of for welding the embodiment of the laser tin-soldering device of mobile phone camera at the utility model, described processing platform 6 is in positive out of focus position, can be by adjusting the distance between whole laser tin-soldering device and processing platform 6, adjust the distance between F-Theta field lens 5 and processing platform 6, the top of the focus that makes laser in processing platform 6, it is positive out of focus, adopt positive out of focus, make laser spot outside soldered tin cream, the laser power density at soldered like this tin cream place is also relatively little, the phenomenon of having avoided tin cream variations in temperature acutely to splash.
Further, described beam expanding lens 2 is 5 power beam expansion lens 2, and described diaphragm 3 apertures are 2mm left and right, and described F-Theta field lens 5 focal lengths are 254mm.
It is a kind of for welding the method for the laser tin-soldering device welding mobile phone camera of mobile phone camera that embodiment of the present utility model provides, and comprising:
Step 1, mobile described laser tin-soldering device to described F-Theta field lens 5 are right against processing platform 6, and a plurality of mobile phone cameras to be welded are housed on described processing platform 6;
Step 2, described laser generator 1 emission pulse laser, described laser passes through described beam expanding lens 2 successively, diaphragm 3, laser galvanometer 4 and F-Theta field lens 5 are got on the mobile phone camera to be welded on processing platform 6, carry out scolding tin, welded a mobile phone camera, by laser galvanometer 4, adjust the position of laser, laser is moved to next mobile phone camera place, carry out scolding tin next time, the time of a scolding tin is generally 350ms, described PWM modulation circuit is adjusted the dutycycle of described laser pulse, one time scolding tin process was comprised of a plurality of time periods that connect successively, the dutycycle of the described laser pulse described in each in time period remains unchanged, in described a plurality of time period, the dutycycle of corresponding described laser pulse increased gradually from first time period to last time period.
A kind of method of using above-mentioned laser tin-soldering device welding mobile phone camera that the utility model embodiment provides, the time of a scolding tin is divided into a plurality of time periods that connect successively, by described PWM modulation circuit, adjust the dutycycle of described laser pulse, laser pulse dutycycle in each time period remains unchanged, the dutycycle of the laser pulse that different time sections is corresponding increases gradually, the pulse width that is laser pulse corresponding to different time sections increases gradually, thereby simulate a discrete scolding tin curve from low temperature to high temperature, the temperature for the treatment of solder(ing) paste is increased gradually, in the situation that guarantee mean power and the constant peak power that reduces laser of frequency of laser, thereby also reduced the power density at processing place laser facula, effectively prevented because temperature excursion causes tin cream to splash the problem with the scald of non-weld.
In the embodiment of a kind of method of using above-mentioned laser tin-soldering device welding mobile phone camera of the utility model, after described step 1, adjust spot size to treat solder(ing) paste sizableness, adjust redirect speed and make whole scolding tin effect stability, simultaneously when described laser generator 1 emission pulse laser, suppress first pulse, prevent that laser from getting to suddenly on tin cream, make tin cream temperature excursion and splash.
Further, the time span of last time period in described a plurality of time periods is maximum, and the time span of last time period is all larger than other any one time spans, and after guaranteeing that like this tin cream temperature is gone up, concentrated energy carries out scolding tin.
In the preferred embodiment of a kind of method of using laser tin-soldering device welding mobile phone camera of the utility model, a scolding tin time can be divided into three time periods, be respectively very first time section, the second time period and the 3rd time period, described very first time section accounts for 15%~25% of the scolding tin time, described the second time period accounts for 15%~25% of the scolding tin time, described the 3rd time period accounts for 55%~65% of the scolding tin time, further, described very first time section accounts for 20% of the scolding tin time, the second time period accounted for 20% of the scolding tin time, described the 3rd time period accounts for 60% of the scolding tin time.
In other embodiment of the present utility model, also a scolding tin time can be divided into four time periods, five time periods etc., shared time scale of each time period is also identical with above-mentioned situation not to the utmost, specifically depending on mobile phone camera quality requirement to be welded and different product.
The foregoing is only preferred embodiment of the present utility model; not in order to limit the utility model; all within spirit of the present utility model and principle, any modification of doing, be equal to replacement, improvement etc., within all should being included in protection domain of the present utility model.
Claims (4)
1. one kind for welding the laser tin-soldering device of mobile phone camera, it is characterized in that, comprise laser generator, be arranged on described laser generator output beam expanding lens, be arranged on described beam expanding lens output diaphragm, be arranged on described diaphragm output laser galvanometer, be arranged on the F-Theta field lens of described laser galvanometer output and the PWM modulation circuit being connected with described laser generator, described F-Theta field lens is right against processing platform.
2. as claimed in claim 1 for welding the laser tin-soldering device of mobile phone camera, it is characterized in that: described processing platform is in positive out of focus position.
3. as claimed in claim 1 for welding the laser tin-soldering device of mobile phone camera, it is characterized in that: described laser generator is 532nm laser instrument.
4. as claimed in claim 1 for welding the laser tin-soldering device of mobile phone camera, it is characterized in that: described beam expanding lens is 5 power beam expansion lens, the described aperture of the diaphragm is 2mm, described F-Theta field lens focal length is 254mm.