CN203380467U - 一种破锡刀轮 - Google Patents
一种破锡刀轮 Download PDFInfo
- Publication number
- CN203380467U CN203380467U CN201320318384.2U CN201320318384U CN203380467U CN 203380467 U CN203380467 U CN 203380467U CN 201320318384 U CN201320318384 U CN 201320318384U CN 203380467 U CN203380467 U CN 203380467U
- Authority
- CN
- China
- Prior art keywords
- blade
- tin
- described blade
- knife edge
- edge
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型提供了一种破锡刀轮,所述破锡刀轮包括刀片和可将所述刀片夹紧的夹轮,所述夹轮为两片,所述刀片边缘具有锯齿状刀锋,所述夹轮直径小于所述刀片直径,所述夹轮与所述刀片的直径差小于焊锡丝的直径,所述刀锋对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮的边缘抵住所述焊锡丝。依借上述技术方案,本实用新型所采用的夹轮夹紧所述刀片只露出所述刀片的刀锋,充分利用夹轮的厚度保证了所述刀片的刚性,不但不会发生折弯也不易发生扭曲变形,工作过程中,所述刀锋对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮的边缘抵住所述焊锡丝,防止所述刀锋刺入焊锡丝的深度超标从而使破锡孔连接,避免堵塞送锡通道。
Description
技术领域
本实用新型属于焊接设备领域,尤其涉及用于焊接的锡丝破锡装置。
背景技术
现有技术,在SMT焊接过程中需要对焊锡丝进行破锡,以保证焊锡丝内部高温阻焊剂的压力释放,通常情况下,破锡刀轮采用整体刀片进行破锡,对刀片的刚性要求极高,通常使用日本进口特种钢材制作此类刀片,成本非常高,而且此类刀片虽然刚性满足了,但在长期使用过程中,还是容易发生扭曲,导致刀片在焊锡丝上开孔无法形成直线,如果将刀片的厚度加大后,虽然满足刚性要求,但材料成本,还有加工成本仍然还是加大了,而且加工出来的刀片刀锋超宽会刺破焊锡丝,从而影响锡丝的卷送能力,很容易造成卷送过程中堵死送锡通道。
实用新型内容
本实用新型的目的在于提供一种破锡刀轮,旨在解决现有技术中刀片刚性不足的问题。
本实用新型是这样实现的,一种破锡刀轮,所述破锡刀轮包括刀片和可将所述刀片夹紧的夹轮,所述夹轮为两片,所述刀片边缘具有锯齿状刀锋,所述夹轮直径小于所述刀片直径,所述夹轮与所述刀片的直径差小于焊锡丝的直径,所述刀锋对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮的边缘抵住所述焊锡丝。
优选地,所述夹轮直径小于所述刀片直径,所述夹轮与所述刀片的直径差 小于焊锡丝的直径。
优选地,所述刀片的刀锋呈等腰三角形位于所述刀片的边缘。
优选地,所述刀片的刀锋呈直角三角形位于所述刀片的边缘,所述直角三角形的一条边的延长线垂直交汇所述刀片的圆心,所述直角三角形最小锐角向外形成所述刀锋尖锐部。
优选地,所述刀片的刀锋截面呈由单边斜面所形成的尖锐状。
优选地,所述刀片的刀锋截面呈由双边斜面所形成的尖锐状等腰三角形。
依借上述技术方案,本实用新型所采用的夹轮夹紧所述刀片只露出所述刀片的刀锋,充分利用夹轮的厚度保证了所述刀片的刚性,不但不会发生折弯也不易发生扭曲变形,工作过程中,所述刀锋对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮的边缘抵住所述焊锡丝,防止所述刀锋刺入焊锡丝的深度超标从而使破锡孔连接,避免堵塞送锡通道。
附图说明
图1是本实用新型提供的破锡刀轮立体示意图;
图2是本实用新型提供的刀片立体示意图;
图3是本实用新型实施例提供的一种刀片示意图;
图4是本实用新型实施例提供的一种刀片示意图;
图5是本实用新型实施例提供的一种刀片示意图;
图6是本实用新型实施例提供的一种刀片示意图;
具体实施方式
为了使本实用新型的目的、技术方案及优点更加清楚明白,以下结合附图及实施例,对本实用新型进行进一步详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本实用新型,并不用于限定本实用新型。
参照图1和图2所示,本实施例提供一种破锡刀轮,所述破锡刀轮包括刀 片10和可将所述刀片10夹紧的夹轮20,所述夹轮20为两片,所述刀片10边缘具有锯齿状刀锋11,所述夹轮20直径小于所述刀片10直径,所述夹轮20与所述刀片10的直径差小于焊锡丝的直径。依借上述技术方案,本实用新型所采用的夹轮20夹紧所述刀片10只露出所述刀片10的刀锋11,充分利用夹轮20的厚度保证了所述刀片10的刚性,不但不会发生折弯也不易发生扭曲变形,工作过程中,所述刀锋11对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮20的边缘抵住所述焊锡丝,防止所述刀锋11刺入焊锡丝的深度超标从而使破锡孔连接,避免堵塞送锡通道。
参照图3所示,本实施例可选用下述刀片,所述刀片10的刀锋11呈等腰三角形位于所述刀片10的边缘。
参照图4所示,本实施例可选用下述刀片,所述刀片10的刀锋11呈直角三角形位于所述刀片10的边缘,所述直角三角形的一条边的延长线垂直交汇所述刀片10的圆心,所述直角三角形最小锐角向外形成所述刀锋11尖锐部。
参照图5所示,本实施例可选用下述刀片,所述刀片10的刀锋11截面呈由单边斜面所形成的尖锐状。
参照图6所示,本实施例可选用下述刀片,所述刀片10的刀锋11截面呈由双边斜面所形成的尖锐状等腰三角形。
以上所述仅为本实用新型的较佳实施例而已,并不用以限制本实用新型,凡在本实用新型的精神和原则之内所作的任何修改、等同替换和改进等,均应包含在本实用新型的保护范围之内。
Claims (5)
1.一种破锡刀轮,其特征在于,所述破锡刀轮包括刀片和可将所述刀片夹紧的夹轮,所述夹轮为两片,所述刀片边缘具有锯齿状刀锋,所述夹轮直径小于所述刀片直径,所述夹轮与所述刀片的直径差小于焊锡丝的直径,所述刀锋对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮的边缘抵住所述焊锡丝。
2.如权利要求1所述的破锡刀轮,其特征在于,所述刀片的刀锋呈等腰三角形位于所述刀片的边缘。
3.如权利要求1所述的破锡刀轮,其特征在于,所述刀片的刀锋呈直角三角形位于所述刀片的边缘,所述直角三角形的一条边的延长线垂直交汇所述刀片的圆心,所述直角三角形最小锐角向外形成所述刀锋尖锐部。
4.如权利要求1所述的破锡刀轮,其特征在于,所述刀片的刀锋截面呈由单边斜面所形成的尖锐状。
5.如权利要求1所述的破锡刀轮,其特征在于,所述刀片的刀锋截面呈由双边斜面所形成的尖锐状等腰三角形。