CN203049053U - 30ka液态阴极金属钙电解槽 - Google Patents

30ka液态阴极金属钙电解槽 Download PDF

Info

Publication number
CN203049053U
CN203049053U CN 201320012881 CN201320012881U CN203049053U CN 203049053 U CN203049053 U CN 203049053U CN 201320012881 CN201320012881 CN 201320012881 CN 201320012881 U CN201320012881 U CN 201320012881U CN 203049053 U CN203049053 U CN 203049053U
Authority
CN
China
Prior art keywords
bar group
copper bar
anode
groove
metal trough
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn - After Issue
Application number
CN 201320012881
Other languages
English (en)
Inventor
李景春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HANZHONG ZINC INDUSTRY SPECIALTY MATERIALS Co Ltd
Original Assignee
HANZHONG ZINC INDUSTRY SPECIALTY MATERIALS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HANZHONG ZINC INDUSTRY SPECIALTY MATERIALS Co Ltd filed Critical HANZHONG ZINC INDUSTRY SPECIALTY MATERIALS Co Ltd
Priority to CN 201320012881 priority Critical patent/CN203049053U/zh
Application granted granted Critical
Publication of CN203049053U publication Critical patent/CN203049053U/zh
Anticipated expiration legal-status Critical
Withdrawn - After Issue legal-status Critical Current

Abstract

一种能够生产高纯金属钙的30KA液态阴极金属钙电解槽。由铁槽外周设有保温绝缘层,保温绝缘层外周设有槽外壳,槽外壳外底下设有槽瓷瓶,铁槽右下角向下伸出杆下头上连接阴极铜排组,阴极铜排组下设有铜排组瓷瓶;铁槽内下部是熔融态铜钙合金,熔融态铜钙合金上面是熔融态电解质,熔融态电解质内上部设有石墨阳极,石墨阳极后面的铁槽、保温绝缘层、槽外壳上设有形状、大小相应的氯气出口,石墨阳极上头上连接阳极铜排组,阳极铜排组下面设有铜排组瓷瓶,石墨阳极上方设有阳极升降机,铁槽内左部设有出料抽管,铁槽左部上端上设有出渣口盖,铁槽右部上端上设有进料口盖构成。它用于生产高纯金属钙。

Description

30KA液态阴极金属钙电解槽
技术领域
本实用新型涉及一种电解装置,尤其是30KA液态阴极金属钙电解槽。
背景技术
目前,公知的热还原法生产金属钙,纯度低。达不到某些企业在生产某些高技术产品,对金属钙纯度高的要求。
发明内容
为了克服现有技术热还原法生产的金属钙纯度低的不足,本实用新型提供一种30KA液态阴极金属钙电解槽,能够生产高纯金属钙,满足某些企业在生产某些高技术产品中,对金属钙纯度高的要求。
本实用新型解决其技术问题所采用的新技术方案是:30KA液态阴极金属钙电解槽。由铁槽外周设有保温绝缘层,保温绝缘层外周设有槽外壳,槽外壳外底下设有槽瓷瓶,铁槽右下角向下伸出杆下头上连接阴极铜排组,阴极铜排组下设有铜排组瓷瓶;铁槽内下部是熔融态铜钙合金,熔融态铜钙合金上面是熔融态电解质,熔融态电解质上部设有石墨阳极,石墨阳极后面的铁槽、保温绝缘层、槽外壳上设有形状、大小相应的氯气出口,石墨阳极上头上连接阳极铜排组,阳极铜排组下面设有铜排组瓷瓶,石墨阳极上方设有阳极升降机,铁槽内左部设有出料抽管,铁槽左部上端上设有出渣口盖,铁槽右部上端上设有进料口盖构成。
本实用新型的有益效果是,设计合理、结构紧凑,生产高纯金属钙。一是填补国内空白,满足国内市场迫切需求,二是出口,增强高纯金属钙在国际市场的竞争力。
附图说明:
图1是本实用新型剖面构造示意图。
图中:1、阳极铜排组  2、阳极升降机  3、石墨阳极4、出渣口盖  5、出料抽管  6、氯气出口  7、进料口盖8、熔融态电解质  9、熔融态铜钙合金  10、铁槽11、保温绝缘层  12、槽外壳  13、槽瓷瓶  14、阴极铜排组  15、铜排组瓷瓶
具体实施方式
下面结合附图和实施例对本实用新型作进一步说明。
在图1中:30KA液态阴极金属钙电解槽。由铁槽10外周设有保温绝缘层11,保温绝缘层11外周设有槽外壳12,槽外壳12外底下设有槽瓷瓶13,铁槽10右下角向下伸出杆下头上连接阴极铜排组14,阴极铜排组14下面设有铜排组瓷瓶15;铁槽10内下部是熔融态铜钙合金9,熔融态铜钙合金9上面是熔融态电解质8,熔融态电解质8内上部设有石墨阳极3,石墨阳极3后面的铁槽10、保温绝缘层11、槽外壳12上设有形状、大小相应的氯气出口6,石墨阳极3上头上连接阳极铜排组1,阳极铜排组1下面设有铜排组瓷瓶15,石墨阳极3上方设有阳极升降机2,铁槽10内左部设有出料抽管5,铁槽10左部上端上设有出渣口盖4,铁槽10右部上端上设有进料口盖7构成。

Claims (1)

1.一种30KA液态阴极金属钙电解槽,其特征在于:它包括:由铁槽(10)外周设有保温绝缘层(11),保温绝缘层(11)外周设有槽外壳(12),槽外壳(12)外底下设有槽瓷瓶(13),铁槽(10)右下角向下伸出杆下头上连接阴极铜排组(14),阴极铜排组(14)下面设有铜排组瓷瓶(15);铁槽(10)内下部是熔融态铜钙合金(9),熔融态铜钙合金(9)上面是熔融态电解质(8),熔融态电解质(8)内上部设有石墨阳极(3),石墨阳极(3)后面的铁槽(10)、保温绝缘层(11)、槽外壳(12)上设有形状、大小相应的氯气出口(6),石墨阳极(3)上头上连接阳极铜排组(1),阳极铜排组(1)下面设有铜排组瓷瓶(15),石墨阳极(3)上方设有阳极升降机(2),铁槽(10)内左部设有出料抽管(5),铁槽(10)左部上端上设有出渣口盖(4),铁槽(10)右部上端上设有进料口盖(7)构成。
CN 201320012881 2013-01-05 2013-01-05 30ka液态阴极金属钙电解槽 Withdrawn - After Issue CN203049053U (zh)