CN202977948U - Wire harness welding machine - Google Patents

Wire harness welding machine Download PDF

Info

Publication number
CN202977948U
CN202977948U CN 201220716066 CN201220716066U CN202977948U CN 202977948 U CN202977948 U CN 202977948U CN 201220716066 CN201220716066 CN 201220716066 CN 201220716066 U CN201220716066 U CN 201220716066U CN 202977948 U CN202977948 U CN 202977948U
Authority
CN
China
Prior art keywords
welded joint
wire harness
welding
roof
lower welded
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN 201220716066
Other languages
Chinese (zh)
Inventor
谢兴明
郑善发
张建国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Jingsai Technology Holding Co ltd
Original Assignee
TONGLING CITY JINGSAI ELECTRONIC CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGLING CITY JINGSAI ELECTRONIC CO Ltd filed Critical TONGLING CITY JINGSAI ELECTRONIC CO Ltd
Priority to CN 201220716066 priority Critical patent/CN202977948U/en
Application granted granted Critical
Publication of CN202977948U publication Critical patent/CN202977948U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model relates to a wire harness welding machine, which comprises upper and lower welding heads, wherein the upper and lower welding heads are respectively provided with ladder-shaped steps which are matched with each other; upper and lower side walls of the two steps are in surface contact under a mold closing state; the vertical distance between the step of the upper welding head and a bottom wall, and between the step of the lower welding head and a top wall, is no less than the diameter of the end part of a wire harness; when the mold is closed, the steps of the upper and lower welding heads form the top wall and the bottom wall of a welding cavity respectively, and the lower side wall of the step of the upper welding head and the upper side wall of the step of the lower welding head form two side walls of the welding cavity respectively. The wire harness welding machine can be shaped through one-time sintering, enables the welding efficiency to be improved greatly, and can save energy.

Description

The wire harness heat sealing machine
Technical field
The utility model relates to a kind of wire harness heat sealing machine that multiple conducting wires is welded together by sintering.
Background technology
Usually, for the connecting line that forms external connection electrical apparatus than thin wire by many, in order to improve its overcurrent performance, two ends need to be carried out sintering with heat sealing machine and be melted, and make thin wire be fused into integral body, could be with its welding on the input of electrical equipment, output chip.That this heat sealing machine generally arranges in the middle of lower welded joint roof is downward, be used for placing the welding die cavity of wire harness end, and upper and lower welded joint matched moulds and heating are compacted into wire harness and sinter into block spade tip.This heat sealing machine just can be completed by three sintering of needs.Because wire harness end multiple conducting wires is deposited in the welding die cavity, it is more that its top exceeds the welding die cavity, during welding for the first time the part wire can landing to the roof of lower welded joint welding die cavity both sides, form projection in spade tip both sides, need that turnback is turned in the end of welding for the first time in the welding die cavity and carry out welding shaping for the second time, eliminate the both sides bossing, and then it is turned over turnback carry out the sintering typing.
Summary of the invention
The purpose of this utility model is for the deficiencies in the prior art, and a kind of wire harness heat sealing machine is provided, and only needs once sintered can the typing, has advantages of that welding efficient is high.
The utility model is achieved in that and comprises upper and lower welded joint; Be respectively equipped with the stairstepping step that cooperatively interacts on upper and lower welded joint, the width of step equates with spade tip cross-sectional length after fusion molding; The upper side wall of two steps, lower wall are respectively the face contact under the matched moulds state; Vertical range between upper welded joint step and diapire and lower welded joint step and roof is not less than the diameter of wire harness end; When upper and lower welded joint matched moulds, the step of upper and lower welded joint consists of respectively roof and the diapire of welding die cavity, and the upper side wall of the lower wall of upper welded joint step and lower welded joint step consists of respectively two sidewalls of welding die cavity.
During sintering, first the wire harness end is placed on lower welded joint step by the gap between lower welded joint roof and upper welded joint step.During matched moulds, upper welded joint is descending, and upper side wall, the lower wall of two steps contact respectively, the wire harness end total is enclosed in the cavity that two steps and sidewall thereof surround, again to the matched moulds state, when making the wire harness end capacity compression wire can landing to outside, once sintered can the typing.
Preferred version of the utility model is: upper welded joint diapire extends to below the step place or step of lower welded joint; Gap between lower welded joint roof and upper welded joint step is enough to make the wire harness end to be passed through.The lower wall of upper welded joint step and lower welded joint step and upper side wall thereof consist of the welding die cavity, the wire harness end is all inserted in the welding die cavity by the gap between lower welded joint roof and upper welded joint step, the part wire can not occur and be scattered to the step outside of lower welded joint.
The utility model forms dynamic welding die cavity by sidewall of welding die cavity is arranged on upper welded joint.During matched moulds, the wire harness end total is enclosed in the cavity that two steps and sidewall thereof surround, then to the matched moulds state, when making the wire harness pressurized wire can landing to outside, once sintered can the typing makes the welding efficiency width improve, and can conserve energy.
Description of drawings
Fig. 1 is the utility model structural representation;
Fig. 2 is view before the utility model matched moulds;
Fig. 3 is the utility model matched moulds completion status schematic diagram;
Fig. 4 is another example structure schematic diagram of the utility model.
Embodiment
As shown in Figure 1 to Figure 3, upper and lower welded joint 1,2 is fixed on heat sealing machine by installing handle 15,25 respectively.Be respectively equipped with the stairstepping step 13,23 that cooperatively interacts on upper and lower welded joint 1,2, step 13,23 width equate with spade tip 41 cross-sectional length after fusion molding; Two steps 13,23 upper side wall 14,22, and lower wall 12,24 is respectively the face contact under the matched moulds state; Vertical range between upper welded joint step 13 and diapire 14 and lower welded joint step 23 and roof 21 is not less than the diameter of wire harness end 4; When upper and lower welded joint 1,2 matched moulds, upper and lower welded joint 1,2 step 13,23 consist of respectively roof and the diapire of welding die cavity, and the upper side wall 22 of 12 times welded joint steps 2 of lower wall of upper welded joint step 1 consists of respectively two sidewalls of welding die cavity.
Its operation principle as shown in Figure 2 and Figure 3.During sintering, first wire harness end 4 is placed on lower welded joint step 23.During matched moulds, upper welded joint 1 is descending, the upper side wall 14 of two steps, 22 and lower wall 12,24 contact respectively, with wire harness end 4 be completely enclosed within two steps 13,23 and the cavity that surrounds of sidewall 12,22 in, it is position shown in Figure 2, again to the matched moulds state be Fig. 3 position, can once sintered typing.
Fig. 4 is another example structure of the present utility model.Upper welded joint 1 diapire 11 extends to below step 23 places or step of lower welded joint 2, makes the lower wall 12 of welded joint step and lower welded joint step 23 and upper side wall 22 thereof consist of welding die cavitys 5.Gap 3 between lower welded joint roof 21 and upper welded joint step 13 is enough to make the wire harness end to be passed through.The wire harness end is all inserted in welding die cavity 5 by the gap 3 between lower welded joint roof 21 and upper welded joint step 13, the part wire can not occur and be scattered to the step outside of lower welded joint.

Claims (2)

1. the wire harness heat sealing machine, comprise upper and lower welded joint (1,2); It is characterized in that: be respectively equipped with the stairstepping step (13,23) that cooperatively interacts on upper and lower welded joint (1,2), the width of step (13,23) equates with spade tip (41) cross-sectional length after fusion molding; The upper side wall (14,22) of two steps (13,23), lower wall (12,24) are respectively the face contact under the matched moulds state; Vertical range between upper welded joint step (13) and diapire (11) and lower welded joint step (23) and roof (21) is not less than the diameter of wire harness end (4); When upper and lower welded joint (1,2) matched moulds, the step of upper and lower welded joint (13,23) consists of respectively roof and the diapire of welding die cavity, and the upper side wall (22) of the lower wall of upper welded joint step (12) and lower welded joint step consists of respectively two sidewalls of welding die cavity.
2. wire harness heat sealing machine according to claim 1 is characterized in that: the step (23) that upper welded joint diapire (11) extends to lower welded joint is located or the step below; Gap (3) between lower welded joint roof (21) and upper welded joint step (13) is enough to make wire harness end (4) to be passed through.
CN 201220716066 2012-12-21 2012-12-21 Wire harness welding machine Expired - Lifetime CN202977948U (en)